CN107414217A - A kind of welded type lengthens screw tap and its processing method - Google Patents

A kind of welded type lengthens screw tap and its processing method Download PDF

Info

Publication number
CN107414217A
CN107414217A CN201710702453.2A CN201710702453A CN107414217A CN 107414217 A CN107414217 A CN 107414217A CN 201710702453 A CN201710702453 A CN 201710702453A CN 107414217 A CN107414217 A CN 107414217A
Authority
CN
China
Prior art keywords
screw tap
main body
extension bar
welded type
tap main
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710702453.2A
Other languages
Chinese (zh)
Inventor
孙盛丽
李蕊秀
崔会彬
董靖涵
李辉
赵祎昕
刘剑
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Harbin Turbine Co Ltd
Original Assignee
Harbin Turbine Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Harbin Turbine Co Ltd filed Critical Harbin Turbine Co Ltd
Priority to CN201710702453.2A priority Critical patent/CN107414217A/en
Publication of CN107414217A publication Critical patent/CN107414217A/en
Pending legal-status Critical Current

Abstract

A kind of welded type lengthens screw tap and its processing method, and it is related to a kind of screw tap and its processing method, and in particular to a kind of welded type lengthens screw tap and its processing method.When the present invention is in order to solve existing process scheme processing final blage locking screw holes, the problem of screw tap service life is short, screw crudy difference.The present invention includes screw tap main body and extension bar, and the rear end of screw tap main body and the front end of extension bar connect.The invention belongs to field of machining.

Description

A kind of welded type lengthens screw tap and its processing method
Technical field
The present invention relates to a kind of screw tap and its processing method, and in particular to a kind of welded type lengthens screw tap and its processing side Method, belong to field of machining.
Background technology
After turbine blade is assembled to rotor blade root groove, final blage is locked using plug screw, and the screwed hole half is in rotor Upper half is not only cut discontinuously on blade during tapping, and rotor is two kinds of different materials from blade, and cutting ability is not Together, there is great requirement to screw tap, the screw tap original attacks pattern with for overall high speed steel material screw tap, two, and cutter life is short, In order to improve the machining status, it have developed welded type and lengthen screw tap and its processing method.
The content of the invention
When the present invention processes final blage locking screw holes to solve existing process scheme, screw tap service life is short, screw processing Ropy problem, and then propose that a kind of welded type lengthens screw tap and its processing method.
The present invention adopts the technical scheme that to solve the above problems:Screw tap of the present invention includes screw tap main body and spreading Bar, the rear end of screw tap main body and the front end of extension bar connect.
Processing method of the present invention comprises the following steps that:
Step 1: thread cone main body and extension bar;
Step 2: the groove of milling screw tap main body, cutting parameter are:Milling cutter rotating speed is 200r/min, amount of feeding 0.15mm/ R, cutting depth 3mm;
Step 3: the square tail of milling extension bar, cutting parameter are:Rotating speed is 200r/min, amount of feeding 0.25mm/r, is cut Depth is 2mm;
Step 4: screw tap main body is heat-treated to HRC63~66;
Step 5: extension bar is heat-treated to HRC43~48;
It is Step 6: screw tap main body and extension bar soldering is integral;Screw tap main body and extension bar are welded on high frequency furnace apparatus Connect one;During welding, solder flux is put at solder bond face, 720~750 DEG C of welding temperature, treats that solder melts full of weldering completely After connecing faying face, stove tempering destressing is put back to, 400 DEG C of temperature, 2 hours is incubated, is then air-cooled to normal temperature, complete welding Process;
Step 7: grind screw tap main center hole;
Step 8: grinding screw tap main body anterior angle is accurate;
Step 9: it is cylindrical in cylindrical grinding machine extension bar, it is ground screw tap body outer diameter;
Step 10: in the spade milling machine tool grinding screw tap main body left end cutting conical surface and its relief angle;
Step 11: in the 60 ° of tooth forms and pitch diameter of thread size of threader grinding screw tap main body, wherein in a cone directly Footpath is 10.45mm, a diameter of 10.783mm in plug tap, a diameter of 10.943mm in third hand tap;
Step 12: pincers worker prints figure number, welded type lengthens screw tap completion of processing.
The beneficial effects of the invention are as follows:The screw tap pattern of the present invention is attacked by original two and is improved to three and attacks pattern, rational distribution Allowance, substantially prolongs screw tap service life, service life is enhanced about more than once, and the screw tap uses welding structure type Formula, screw tap and extension bar are welded using soldering pattern, reduce screw tap manufacturing cost.Meanwhile it have developed the welded type and add The processing method of long screw tap, the screw tap accuracy of manufacture is effectively ensured.
Brief description of the drawings
Fig. 1 is the front view of the present invention;
Fig. 2 is Fig. 1 left view;
Fig. 3 be in Fig. 1 A-A to sectional view.
Embodiment
Embodiment one:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds Long screw tap includes screw tap main body 1 and extension bar 2, and the rear end of screw tap main body 1 is connected with the front end of extension bar 2.
Embodiment two:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds The front end of the screw tap main body 1 of long screw tap is along the circumferential direction provided with a cone 1-1, plug tap 1-2 and third hand tap 1-3.Other compositions and connection Relation is identical with embodiment one.
Embodiment three:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds The front end face of the extension bar 2 of long screw tap is provided with mounting hole 2-1, and the rear end of screw tap main body 1 is inserted into mounting hole 2-1.Other groups Into and annexation it is identical with embodiment one.
Embodiment four:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds The rear end of the extension bar 2 of long screw tap is provided with square tail 2-2, and square tail 2-2 cross section is square.It is other composition and annexation with Embodiment one is identical.
Embodiment five:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds Long screw tap processing method comprises the following steps that:
Step 1: thread cone main body 1 and extension bar 2;
Step 2: the groove of milling screw tap main body 1, cutting parameter are:Milling cutter rotating speed is 200r/min, and the amount of feeding is 0.15mm/r, cutting depth 3mm;
Step 3: 12.5 × 12.5mm square tail 2-3 of milling extension bar 2, cutting parameter are:Rotating speed is 200r/min, feeding Measure as 0.25mm/r, cutting depth 2mm;
Step 4: screw tap main body 1 is heat-treated to HRC63~66;
Step 5: extension bar 2 is heat-treated to HRC43~48;
It is Step 6: screw tap main body 1 and the soldering of extension bar 2 is integral;By screw tap main body 1 and extension bar 2 in high frequency furnace apparatus It is upper welded;During welding, solder flux is put at solder bond face, 720~750 DEG C of welding temperature, treats that solder melts completely and fill Behind full solder bond face, stove tempering destressing is put back to, 400 DEG C of temperature, 2 hours is incubated, is then air-cooled to normal temperature, complete Welding sequence;
Step 7: center lapping;
Step 8: the anterior angle of grinding screw tap main body 1 is accurate;
Step 9:, grinding screw tap main body 1 external diameter cylindrical in cylindrical grinding machine extension bar 2;
Step 10: in the left end cutting conical surface of spade milling machine tool grinding screw tap main body 1 and its relief angle;
Step 11: the 60 ° of tooth forms and pitch diameter of thread size of screw tap main body 1 are ground in threader, wherein a cone 1-1 In a diameter of 10.45mm, a diameter of 10.943mm in a diameter of 10.783mm in plug tap 1-2, third hand tap 1-3;
Step 12: pincers worker prints figure number, welded type lengthens screw tap completion of processing.
Alignment≤0.2mm after being welded in present embodiment in step 6;Solder flux is by 105 copper sheets, sodium tetraborate powder constituent.
Embodiment six:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds Long screw tap processing method, it is characterised in that:The both ends centering of step 1 plug tap main body 1, the overall diameter of screw tap main body 1 are high-volume 0.5-0.6mm, the middle diameter of screw tap main body 1 is high-volume 0.6-0.7mm.
The present embodiment plug tap bar Φ cylindrical high-volume 0.6-0.7mm of 16mm, right-hand member centering, Φ 9mm endoporus press silk Bore Φ 9mm cylindrical handles gap 0.05-0.08mm;Cutting parameter is:Rotating speed 500r/min, amount of feeding 0.25mm/r, cutting depth 1.5mm。
Embodiment seven:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds Screw tap main body 1 is heat-treated to the method for HRC63~6 in the step of long screw tap processing method four is:First preheat 550 DEG C two small When, then put 850 DEG C of moderate oven and heat 16 minutes, then put 1240 DEG C of high temperature furnace and heat 8 minutes, then put 600 DEG C of insulations of constant-temperature oven 16 minutes, it is finally putting into 550 DEG C of tempering furnace and is tempered 2 times, every time 2 hours.
Embodiment eight:Illustrate present embodiment with reference to Fig. 1 to Fig. 3, a kind of welded type described in present embodiment adds Extension bar 2 is heat-treated to the method for HRC43~48 in the step of long screw tap processing method five is:First in moderate oven 820-840 DEG C heating 30 minutes, be then placed in tank and be cooled to 300-400 DEG C, the time is about 20~30 minutes, is placed into cold in oil groove But to normal temperature, it is finally putting into 340 DEG C of tempering furnace and is tempered 2 hours.
The above described is only a preferred embodiment of the present invention, any formal limitation not is made to the present invention, though So the present invention is disclosed above with preferred embodiment, but is not limited to the present invention, any to be familiar with this professional technology people Member, without departing from the scope of the present invention, when the technology contents using the disclosure above make a little change or modification For the equivalent embodiment of equivalent variations, as long as be without departing from technical solution of the present invention content, according to the technical spirit of the present invention, Within the spirit and principles in the present invention, any simple modification, equivalent substitution and improvement for being made to above example etc., still Belong within the protection domain of technical solution of the present invention.

Claims (8)

1. a kind of welded type lengthens screw tap, it is characterised in that:A kind of welded type, which lengthens screw tap, to be included screw tap main body (1) and connects Stock (2), the rear end of screw tap main body (1) are connected with the front end of extension bar (2).
2. a kind of welded type lengthens screw tap according to claim 1, it is characterised in that:The front end of screw tap main body (1) is circumferentially Direction is provided with a cone (1-1), plug tap (1-2) and third hand tap (1-3).
3. a kind of welded type lengthens screw tap according to claim 1, it is characterised in that:The front end face of extension bar (2) is provided with peace Fill hole (2-1), the rear end of screw tap main body (1) is inserted into mounting hole (2-1).
4. a kind of welded type lengthens screw tap according to claim 1, it is characterised in that:The rear end of extension bar (2) is provided with square tail (2-2), the cross section of square tail (2-2) is square.
A kind of 5. processing method of screw tap described in claim 1, it is characterised in that:A kind of welded type lengthens screw tap processing side Method comprises the following steps that:
Step 1: thread cone main body (1) and extension bar (2);
Step 2: the groove of milling screw tap main body (1), cutting parameter are:Milling cutter rotating speed is 200r/min, amount of feeding 0.15mm/ R, cutting depth 3mm;
Step 3: 12.5 × 12.5mm square tails (2-3) of milling extension bar (2), cutting parameter are:Rotating speed is 200r/min, feeding Measure as 0.25mm/r, cutting depth 2mm;
Step 4: screw tap main body (1) is heat-treated to HRC63~66;
Step 5: extension bar (2) is heat-treated to HRC43~48;
It is Step 6: screw tap main body (1) and extension bar (2) soldering is integral;By screw tap main body (1) and extension bar (2) in coreless induction furnace It is welded in equipment;During welding, solder flux is put at solder bond face, 720~750 DEG C of welding temperature, treats that solder melts completely Change after being full of solder bond face, put back to stove tempering destressing, 400 DEG C of temperature, be incubated 2 hours, be then air-cooled to normal temperature, Complete welding sequence;
Step 7: center lapping;
Step 8: grinding screw tap main body (1) anterior angle is accurate;
Step 9: it is cylindrical in cylindrical grinding machine extension bar (2), it is ground screw tap main body (1) external diameter;
Step 10: in spade milling machine tool grinding screw tap main body (1) left end cutting conical surface and its relief angle;
Step 11: in the 60 ° of tooth forms and pitch diameter of thread size of threader grinding screw tap main body (1), wherein one bores (1-1) In a diameter of 10.45mm, a diameter of 10.783mm in plug tap (1-2), a diameter of 10.943mm in third hand tap (1-3);
Step 12: pincers worker prints figure number, welded type lengthens screw tap completion of processing.
6. a kind of welded type lengthens screw tap processing method according to claim 5, it is characterised in that:Step 1 plug tap main body (1) both ends centering, screw tap main body (1) overall diameter are high-volume 0.5-0.6mm, and the middle diameter of screw tap main body (1) is high-volume 0.6-0.7mm。
7. a kind of welded type lengthens screw tap processing method according to claim 5, it is characterised in that:By screw tap master in step 4 The method that body (1) is heat-treated to HRC63~6 is:First preheat 550 DEG C two hours, then put 850 DEG C of moderate oven and heat 16 minutes, 1240 DEG C of high temperature furnace is put again to heat 8 minutes, then puts 600 DEG C of constant-temperature oven and is incubated 16 minutes, is finally putting into 550 DEG C of tempering 2 of tempering furnace It is secondary, 2 hours every time.
8. a kind of welded type lengthens screw tap processing method according to claim 5, it is characterised in that:By extension bar in step 5 (2) being heat-treated to the method for HRC43~48 is:First in the heating 30 minutes of 820-840 DEG C of moderate oven, it is then placed in tank and cools down To 300-400 DEG C, the time is about 20~30 minutes, places into and normal temperature is cooled in oil groove, is finally putting into 340 DEG C of tempering of tempering furnace 2 hours.
CN201710702453.2A 2017-08-16 2017-08-16 A kind of welded type lengthens screw tap and its processing method Pending CN107414217A (en)