CN107383969A - Based on the environment protection oil paint for improving glossiness - Google Patents

Based on the environment protection oil paint for improving glossiness Download PDF

Info

Publication number
CN107383969A
CN107383969A CN201710751183.4A CN201710751183A CN107383969A CN 107383969 A CN107383969 A CN 107383969A CN 201710751183 A CN201710751183 A CN 201710751183A CN 107383969 A CN107383969 A CN 107383969A
Authority
CN
China
Prior art keywords
weight
parts
environment protection
protection oil
oil paint
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710751183.4A
Other languages
Chinese (zh)
Inventor
李睿阳
倪念英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chengdu Ruixin Mitt Mstar Technology Ltd
Original Assignee
Chengdu Ruixin Mitt Mstar Technology Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chengdu Ruixin Mitt Mstar Technology Ltd filed Critical Chengdu Ruixin Mitt Mstar Technology Ltd
Priority to CN201710751183.4A priority Critical patent/CN107383969A/en
Publication of CN107383969A publication Critical patent/CN107383969A/en
Pending legal-status Critical Current

Abstract

The invention discloses based on the environment protection oil paint for improving glossiness, including following parts by weight of component:The parts by weight of maleic anhydride 10 15, the parts by weight of phthalic anhydride 8 16, the parts by weight of ethylene glycol 10 12, the parts by weight of hydroquinones 58, the parts by weight of polyester resin 15 20, the parts by weight of turpentine oil 6 10, the parts by weight of stearic acid 10 15, the parts by weight of titanium dioxide 12 18.Environment protection oil paint of the present invention has the advantages of volatilization is small, and taste is small, meanwhile, by adding the stearic acid and titanium dioxide of certain component, its glossiness is improved under conditions of especially performance itself is not influenceed.

Description

Based on the environment protection oil paint for improving glossiness
Technical field
The present invention relates to paint preparing technical field, and in particular to based on the environment protection oil paint for improving glossiness.
Background technology
Environment protection oil paint refers to the performance indications of painting, safety index on the premise of respective product standard is met.Symbol Close the painting for the technical requirements that National Environmental famous special product proposes.Be applied to body surface can be formed with protection, decoration or The general name of a kind of liquid or solid material of the solid coated film of property.
According to the use range of our house ornamentation lives, we have three regions by common paint:Wall paint, woodcare paint, metal Paint.
No matter being used for what field, the harmful substance such as formaldehyde, toluene, benzene in environment protection oil paint must be controlled in rational model In enclosing, meanwhile, attractive in appearance in order to ensure environment protection oil paint, in addition to the color of paint itself, the photochromism of paint is also to influence An important factor for its is attractive in appearance, existing environment protection oil paint, although with less harmful substance, glossiness is poor.
The content of the invention
It is an object of the invention to provide based on the environment protection oil paint for improving glossiness, the glossiness for solving existing paint is bad The problem of.
The present invention is achieved through the following technical solutions:
Based on the environment protection oil paint for improving glossiness, including following parts by weight of component:
Maleic anhydride 10-15 parts by weight, phthalic anhydride 8-16 parts by weight, ethylene glycol 10-12 parts by weight, to benzene Diphenol 5-8 parts by weight, polyester resin 15-20 parts by weight, turpentine oil 6-10 parts by weight, stearic acid 10-15 parts by weight, titanium dioxide 12-18 parts by weight.
Based on the environment protection oil paint for improving glossiness, it is made up of following parts by weight of component:
Maleic anhydride 10-15 parts by weight, phthalic anhydride 8-16 parts by weight, ethylene glycol 10-12 parts by weight, to benzene Diphenol 5-8 parts by weight, polyester resin 15-20 parts by weight, turpentine oil 6-10 parts by weight, stearic acid 10-15 parts by weight, titanium dioxide 12-18 parts by weight.
Component of the present invention is prior art.
Environment protection oil paint of the present invention has the advantages of volatilization is small, and taste is small, meanwhile, by adding the hard of certain component Resin acid and titanium dioxide, its glossiness is improved under conditions of especially performance itself is not influenceed.
Further, in addition to limonene 10-12 parts by weight.
The limonene has certain fragrance, can reduce the taste of paint, is allowed to taste and is easier to receive.
Further, in addition to glutinous rice flour 5-8 parts by weight.
The glutinous rice flour has certain viscosity, and especially uniform viscous can be improved by adding appropriate glutinous rice flour Property.
The present invention compared with prior art, has the following advantages and advantages:
Environment protection oil paint of the present invention has the advantages of volatilization is small, and taste is small, meanwhile, by adding the hard of certain component Resin acid and titanium dioxide, its glossiness is improved under conditions of especially performance itself is not influenceed.
Embodiment
For the object, technical solutions and advantages of the present invention are more clearly understood, with reference to embodiment, the present invention is made Further to describe in detail, exemplary embodiment of the invention and its explanation are only used for explaining the present invention, are not intended as to this The restriction of invention.
Embodiment 1:
Based on the environment protection oil paint for improving glossiness, it is made up of following parts by weight of component:
The parts by weight of maleic anhydride 10, the parts by weight of phthalic anhydride 8, the parts by weight of ethylene glycol 10, the weight of hydroquinones 5 Part, the parts by weight of polyester resin 15, the parts by weight of turpentine oil 6, the parts by weight of stearic acid 10, the parts by weight of titanium dioxide 12.
Embodiment 2:
Based on the environment protection oil paint for improving glossiness, it is made up of following parts by weight of component:
The parts by weight of maleic anhydride 15, the parts by weight of phthalic anhydride 16, the parts by weight of ethylene glycol 12, the weight of hydroquinones 8 Measure part, the parts by weight of polyester resin 20, the parts by weight of turpentine oil 10, the parts by weight of stearic acid 15, the parts by weight of titanium dioxide 18.
Embodiment 3:
Based on the environment protection oil paint for improving glossiness, it is made up of following parts by weight of component:
The parts by weight of maleic anhydride 12, the parts by weight of phthalic anhydride 14, the parts by weight of ethylene glycol 11, the weight of hydroquinones 6 Measure part, the parts by weight of polyester resin 18, the parts by weight of turpentine oil 8, the parts by weight of stearic acid 12, the parts by weight of titanium dioxide 15.
Embodiment 4:
Based on the environment protection oil paint for improving glossiness, it is made up of following parts by weight of component:
The parts by weight of maleic anhydride 12, the parts by weight of phthalic anhydride 14, the parts by weight of ethylene glycol 11, the weight of hydroquinones 6 Measure part, the parts by weight of polyester resin 18, the parts by weight of turpentine oil 8, the parts by weight of stearic acid 12, the parts by weight of titanium dioxide 15, the weight of limonene 10 Part is measured, includes the parts by weight of glutinous rice flour 5.
Embodiment 5:
Based on the environment protection oil paint for improving glossiness, it is made up of following parts by weight of component:
The parts by weight of maleic anhydride 12, the parts by weight of phthalic anhydride 14, the parts by weight of ethylene glycol 11, the weight of hydroquinones 6 Measure part, the parts by weight of polyester resin 18, the parts by weight of turpentine oil 8, the parts by weight of stearic acid 12, the parts by weight of titanium dioxide 15, the weight of limonene 12 Part is measured, includes the parts by weight of glutinous rice flour 8.
Paint described in embodiment 1 to embodiment 5 is used for interior decoration, the glossiness painted after use is apparently higher than now Some paint.
Above-described embodiment, the purpose of the present invention, technical scheme and beneficial effect are carried out further Describe in detail, should be understood that the embodiment that the foregoing is only the present invention, be not intended to limit the present invention Protection domain, within the spirit and principles of the invention, any modification, equivalent substitution and improvements done etc., all should include Within protection scope of the present invention.

Claims (4)

1. based on the environment protection oil paint for improving glossiness, it is characterised in that including following parts by weight of component:
Maleic anhydride 10-15 parts by weight, phthalic anhydride 8-16 parts by weight, ethylene glycol 10-12 parts by weight, hydroquinones 5-8 parts by weight, polyester resin 15-20 parts by weight, turpentine oil 6-10 parts by weight, stearic acid 10-15 parts by weight, titanium dioxide 12-18 Parts by weight.
2. based on the environment protection oil paint for improving glossiness, it is characterised in that be made up of following parts by weight of component:
Maleic anhydride 10-15 parts by weight, phthalic anhydride 8-16 parts by weight, ethylene glycol 10-12 parts by weight, hydroquinones 5-8 parts by weight, polyester resin 15-20 parts by weight, turpentine oil 6-10 parts by weight, stearic acid 10-15 parts by weight, titanium dioxide 12-18 Parts by weight.
It is 3. according to claim 1 based on the environment protection oil paint for improving glossiness, it is characterised in that also including limonene 10- 12 parts by weight.
It is 4. according to claim 1 based on the environment protection oil paint for improving glossiness, it is characterised in that also including glutinous rice flour 5-8 Parts by weight.
CN201710751183.4A 2017-08-28 2017-08-28 Based on the environment protection oil paint for improving glossiness Pending CN107383969A (en)