CN107377341A - A kind of brushing technique of long and thin metal tubing inside coating - Google Patents

A kind of brushing technique of long and thin metal tubing inside coating Download PDF

Info

Publication number
CN107377341A
CN107377341A CN201710789229.1A CN201710789229A CN107377341A CN 107377341 A CN107377341 A CN 107377341A CN 201710789229 A CN201710789229 A CN 201710789229A CN 107377341 A CN107377341 A CN 107377341A
Authority
CN
China
Prior art keywords
coating
metal tube
glueballs
flexible
brushing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710789229.1A
Other languages
Chinese (zh)
Inventor
刘春晓
修立杰
丁帅
武鹏波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201710789229.1A priority Critical patent/CN107377341A/en
Publication of CN107377341A publication Critical patent/CN107377341A/en
Pending legal-status Critical Current

Abstract

The invention belongs to field of surface engineering technique, more particularly to a kind of brushing technique of long and thin metal tubing inside coating.The brushing technique of the present invention can adapt to the bigger long and thin metal tubing of major diameter, under air pressure promotion, ensure that the brushing thickness of long and thin metal tubing inwall is uniform, the problem of being not in holiday and scratch, make tubing long-term stable operation in caustic acid liquid medium or low-level oxidation environment, effectively prevent metal pipe-wall from corroding, while ensure that managing interior medium is not contaminated.

Description

A kind of brushing technique of long and thin metal tubing inside coating
Technical field
The invention belongs to field of surface engineering technique, more particularly to a kind of painter of long and thin metal tubing inside coating Skill.
Background technology
In energy industry, cooling tower is to provide the important equipment of low-temperature receiver.Recirculated water is during indirect air cooling tower cooler There is certain corrosiveness to heated surface bundle, corrosion product causes circulating water quality problem and etching problem more and more tighter again Weight, eventually affects the safe operation of unit.In order to solve this problem, it is badly in need of a kind of reliable tube bank inner wall anti-corrosive process.
At present, in the coating process on surface, most common technique is surface spraying and dip-coating.Through experiment, in internal diameter φ On 25mm and following relatively slender tube material inwall, spraying and dip-coating can not reach quality requirement, tube wall occur along journey coating The problem of brushing uneven thickness, subregion holiday and coating raw material waste.It is traditional on internal diameter φ 6mm slender tube material Surface spraying and dip-coating can not construct.
The content of the invention
The present invention is directed to above-mentioned the shortcomings of the prior art, there is provided a kind of painter of long and thin metal tubing inside coating Skill.
The technical scheme that the present invention solves above-mentioned technical problem is as follows:A kind of painter of long and thin metal tubing inside coating Skill, step are as follows:
(1) flexible glueballs or piston brush are filled into metal tube to be coated, utilize compressed air or vacuum driving flexible glue Ball or piston brush advance, and remove the particulate matter and anvil cinder of inner wall of metal tube;
(2) according to metal tube length, coating content needed for inner wall of metal tube brushing is calculated;
(3) using injecting device make closing fluid column, will flexible glueballs be filled into injecting device, inject coating, then will apply In material brush push-in injecting device, make to form sealing paint fluid column between paint brush and flexible glueballs;
(4) injecting device front end is docked with metal tube one end, injecting device rear end access compressed air;Promoted using compressed air Paint brush, coating fluid column is extruded, coating is extruded into paint brush bristle periphery, before compressed air promotes paint brush and flexible glueballs During entering, coating is uniformly brushed in inner wall of metal tube;
(5) set in the metal tube other end exit recycling bin, recovery brush after flexible glueballs, paint brush and remaining Coating.
The beneficial effects of the invention are as follows:The brushing technique of the present invention can adapt to the bigger long and thin metal tubing of major diameter, Under air pressure promotion, ensure that the brushing thickness of long and thin metal tubing inwall is uniform, the problem of being not in holiday and scratch, make pipe Material long-term stable operation in caustic acid liquid medium or low-level oxidation environment, effectively prevents metal pipe-wall from corroding, while ensure to manage Interior medium is not contaminated.
On the basis of above-mentioned technical proposal, the present invention can also do following improvement.
Further, the coating content injected in step (3) is 1.2-1.4 times of coating content needed for calculating in step (2).
Beneficial effect using above-mentioned further scheme is that filling coating content is slightly larger than filling amount of calculation, to ensure metal Pipe internal surface is all brushed.
Further, can also be vacuumized in flexible glueballs one end in metal tube, pull flexible glueballs, coating fluid column and Paint brush, inner wall of metal tube is brushed.
Further, the front-end and back-end of coating fluid column use flexible glueballs, and coating can be in straight length and turnaround section Deng being brushed in complicated metal pipe.
Brief description of the drawings
Fig. 1 is the brushing schematic diagram of the present invention;
In figure, 1, compressed air;2nd, paint brush;3rd, bristle;4th, coating fluid column;5th, flexible glueballs;6th, metal tube;7th, inject Device.
Embodiment
The principle and feature of the present invention are described below in conjunction with example, the given examples are served only to explain the present invention, and It is non-to be used to limit the scope of the present invention.
Embodiment 1
A kind of brushing technique of long and thin metal tubing inside coating, step are as follows:
(1) flexible glueballs 5 is filled into metal tube 6 to be coated, promotes flexible glueballs to advance using compressed air 1, remove The particulate matter and anvil cinder of inner wall of metal tube;
(2) according to metal tube length, coating content needed for inner wall of metal tube brushing is calculated;
(3) using injecting device 7 make closing fluid column, will flexible glueballs be filled into injecting device, inject coating, then will apply In material brush push-in injecting device, make to form sealing paint fluid column 4 between paint brush and flexible glueballs;The coating content of injection is step (2) 1.2-1.4 times of coating content needed for being calculated in;
(4) injecting device front end is docked with metal tube one end, injecting device rear end access compressed air;Promoted using compressed air Paint brush 2, coating fluid column is extruded, coating is extruded into the periphery of paint brush bristle 3, and compressed air promotes paint brush and flexible glueballs During advance, coating is uniformly brushed in inner wall of metal tube;
(5) set in the metal tube other end exit recycling bin, recovery brush after flexible glueballs, paint brush and remaining Coating.
The foregoing is only presently preferred embodiments of the present invention, be not intended to limit the invention, it is all the present invention spirit and Within principle, any modification, equivalent substitution and improvements made etc., it should be included in the scope of the protection.

Claims (2)

1. a kind of brushing technique of long and thin metal tubing inside coating, it is characterised in that step is as follows:
(1) flexible glueballs or piston brush are filled into metal tube to be coated, using compressed air or vacuum driving flexibility glueballs or Piston brush advances, and removes the particulate matter and anvil cinder of inner wall of metal tube;
(2) according to metal tube length, coating content needed for inner wall of metal tube brushing is calculated;
(3) make closing fluid column using injecting device, will flexible glueballs be filled into injecting device, inject coating, then by paint brush It is pushed into injecting device, makes to form sealing paint fluid column between paint brush and flexible glueballs;
(4) injecting device front end is docked with metal tube one end, injecting device rear end access compressed air;Coating is promoted using compressed air Brush, coating fluid column is extruded, coating is extruded into paint brush bristle periphery, and compressed air promotes paint brush and flexible glueballs to advance Cheng Zhong, coating are uniformly brushed in inner wall of metal tube;
(5) recycling bin, flexible glueballs, paint brush and remaining painting after recovery brushing are set in metal tube other end exit Material.
2. brushing technique according to claim 1, it is characterised in that the coating content of injection is in step (2) in step (3) 1.2-1.4 times of coating content needed for calculating.
CN201710789229.1A 2017-09-05 2017-09-05 A kind of brushing technique of long and thin metal tubing inside coating Pending CN107377341A (en)