- stainless steel
- shell
- solid shell
- half side
- welded
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Links
Images
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B23—MACHINE TOOLS; METAL-WORKING NOT OTHERWISE PROVIDED FOR
- B23P—METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS
- B23P15/00—Making specific metal objects by operations not covered by a single other subclass or a group in this subclass
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Moulds For Moulding Plastics Or The Like (AREA)
- Heat Treatment Of Articles (AREA)
- Arc Welding In General (AREA)
Abstract
The invention discloses a casting method of a solid stainless steel ice roller, which comprises the steps of respectively casting a stainless steel solid shell or a hollow shell with the left half and the right half of the shell by using a die. If the half solid shell is cast, the pipeline of the half solid shell is a section of a single cavity, so the half solid shell can be cast in a traditional way, and then the left and right 2 stainless steel half solid shells are spliced and welded together. And finally, grinding and polishing the welded semi-finished product. If the half hollow shell is cast, the prepared stainless steel pipe which is coiled off is welded with the upper connector and the lower connector of the left half stainless steel shell which is cast previously, and then the left and the right half stainless steel shells are welded together. Then, a metal with a melting point lower than that of stainless steel is poured into the welded semi-finished product from the upper reserved opening. And after cooling, welding and plugging the reserved opening by using a corresponding stainless steel filling piece. And finally, grinding and polishing the welded semi-finished product.
Description
Technical Field
The invention relates to the field of casting, in particular to a casting method of a solid stainless steel ice roller.
Background
At present, a casting method of a solid stainless steel ice roller does not exist. The solid stainless steel bottle opening ice-suppression device of the inventor, Chengling in Wu, 2016, 05, 04, application No. 201610287946X introduces a method that a coiled stainless steel pipe is pre-embedded in a casting die, and then molten steel is poured to be combined with the stainless steel pipe. The problem that exists is that pre-buried stainless steel pipe can be scalded by the molten steel of watering and become warp, probably blocks up the pipeline, causes the finished product to scrap.
Disclosure of Invention
In order to overcome the defects of the prior art, the invention provides a casting method of a solid stainless steel ice roller.
The technical scheme adopted by the invention for realizing the purpose is as follows: firstly, casting 2 half stainless steel solid shells or hollow shells on the left and right sides by using a mould respectively. If the half solid shell is cast, the pipeline of the half solid shell is a section of a single cavity, so the half solid shell can be cast in a traditional way, and then the left and right 2 stainless steel half solid shells are spliced and welded together. When a half solid shell is cast, the left shell and the right shell are respectively cast, the pipeline position of the left shell is slightly higher, and a small section of the pipeline of the splicing surface protrudes. The pipeline position of the right shell is slightly lower, and the pipeline of the splicing surface is recessed into a small section. The left and right 2 half solid shells are just welded after being connected in a concave-convex way during assembly and welding. And finally, grinding and polishing the welded semi-finished product to obtain a finished product.
If the half hollow shell is cast, the prepared stainless steel pipe which is coiled off is welded with the upper connector and the lower connector of the left half stainless steel shell which is cast previously, and then the left and the right half stainless steel shells are welded together. Then, a metal with a melting point lower than that of stainless steel is poured into the welded semi-finished product from the upper reserved opening. And after cooling, welding and plugging the reserved opening by using a corresponding stainless steel filling piece. And finally, grinding and polishing the welded semi-finished product to obtain a finished product.
The invention has the advantages of practicality and effectiveness, and the pipeline in the solid stainless steel ice roller can not be blocked to cause the scrapping of the whole finished product.
Drawings
The invention is further described with reference to the following figures and implementations. FIG. 1 is a schematic of the present invention. Fig. 2 is a schematic view showing the concave-convex connection of the pipes of the left and right housings.
Detailed Description
In fig. 1, a stainless steel hollow shell (1) or a solid shell (1) with left and right halves of the shell being respectively cast by a die. If the half solid shell (1) is cast, the pipeline (2) of the half solid shell (1) is a section of a single cavity, so that the half solid shell can be cast in a traditional mode, and then the left and right 2 stainless steel half solid shells (1) are assembled and welded together. When a half solid shell (1) is cast, the left shell and the right shell are respectively cast, the pipeline position of the left shell is slightly higher, and the pipeline of the splicing surface protrudes out of a small section (3). The pipeline of the right shell is slightly lower, and the pipeline of the splicing surface is recessed into a small section (4). The left and right 2 half solid shells are just welded after being connected in a concave-convex way during assembly and welding. And finally, grinding and polishing the welded semi-finished product to obtain a finished product.
If the half hollow shell is cast, the stainless steel pipe (2) which is prepared in advance and is coiled is welded with the upper interface and the lower interface of the left half stainless steel shell (1) which is cast previously, and then the left and the right half stainless steel shells (1) are welded together. Then, a metal with a melting point lower than that of stainless steel is poured into the welded semi-finished product from the upper reserved opening. And after cooling, welding and plugging the reserved opening by using a corresponding stainless steel filling piece. And finally, grinding and polishing the welded semi-finished product to obtain a finished product.
The above description is only a preferred embodiment of the present invention, and is not intended to limit the present invention in any way, and any simple modification, equivalent change and modification made to the above embodiment according to the technical spirit of the present invention are within the scope of the technical solution of the present invention without departing from the content of the present invention.
Claims (1)
1. A casting method of a solid stainless steel ice roller is characterized by comprising the following process steps:
firstly, respectively casting a stainless steel solid shell on the left half side and a stainless steel solid shell on the right half side by using a mould, wherein a pipeline of the stainless steel solid shell on the left half side and a pipeline of the stainless steel solid shell on the right half side are both a section of independent cavity; when the stainless steel solid shell on the left half side and the stainless steel solid shell on the right half side are respectively cast, the pipeline position of the stainless steel solid shell on the left half side is slightly higher than that of the stainless steel solid shell on the right half side, and a small section of pipeline on the splicing surface of the stainless steel solid shell on the left half side protrudes; the pipeline position of the stainless steel solid shell on the right half side is slightly lower than that of the stainless steel solid shell on the left half side, and the pipeline on the splicing surface of the stainless steel solid shell on the right half side is recessed into a small section;
secondly, the stainless steel solid shell on the left half side and the stainless steel solid shell on the right half side are connected in a concave-convex manner, assembled and welded into a whole;
and thirdly, grinding and polishing the welded semi-finished product to obtain a finished product.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610309678.7A CN107363469B (en) | 2016-05-11 | 2016-05-11 | Casting method of solid stainless steel ice roller |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201610309678.7A CN107363469B (en) | 2016-05-11 | 2016-05-11 | Casting method of solid stainless steel ice roller |
Publications (2)
Publication Number | Publication Date |
---|---|
CN107363469A CN107363469A (en) | 2017-11-21 |
CN107363469B true CN107363469B (en) | 2022-01-04 |
Family
ID=60304474
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201610309678.7A Active CN107363469B (en) | 2016-05-11 | 2016-05-11 | Casting method of solid stainless steel ice roller |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN107363469B (en) |
Family Cites Families (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN2141537Y (en) * | 1992-10-30 | 1993-09-01 | 周益人 | Ice cooling device |
JP4401680B2 (en) * | 2003-05-12 | 2010-01-20 | 川崎重工業株式会社 | Body frame of motorcycle |
CN201575219U (en) * | 2009-10-18 | 2010-09-08 | 林惠良 | Stainless steel sensor faucet |
CN102109278B (en) * | 2010-12-15 | 2013-07-10 | 中国瑞林工程技术有限公司 | Method for manufacturing cooling water jacket and cooling water jacket for high temperature furnace |
CN202191130U (en) * | 2011-09-06 | 2012-04-18 | 侯攀 | Quick icing wine pourer |
CN203375785U (en) * | 2013-06-06 | 2014-01-01 | 周银春 | Iced container |
CN203687487U (en) * | 2013-12-27 | 2014-07-02 | 任天碧 | Rapid icing device |
CN205119598U (en) * | 2015-10-19 | 2016-03-30 | 王玉璐 | Puck is used to fast cold drink material |
-
2016
- 2016-05-11 CN CN201610309678.7A patent/CN107363469B/en active Active
Also Published As
Publication number | Publication date |
---|---|
CN107363469A (en) | 2017-11-21 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP5662556B2 (en) | Method and apparatus for manufacturing a bi-material sleeve and sleeve manufactured thereby | |
CN103736974A (en) | One-step molding method for long and thin hole in casting | |
CN102266934A (en) | Method for manufacturing preburied pipeline type mould | |
CN104923732A (en) | Method for casting titanium or titanium alloy casting with special-shaped inner hole | |
CN107363469B (en) | Casting method of solid stainless steel ice roller | |
CN104043783B (en) | Small-bore high pound level valve body core for cast | |
CN104259406A (en) | Sand core support for exhausting pipe | |
CN103611920A (en) | Casting-in method of steel pipe in casting | |
CN103934306B (en) | Manufacturing method for steel-made welded tilted three-way pipe | |
CN103170576A (en) | Technology for casting thick-wall steel casting with thin and long inner hole | |
CN202490914U (en) | Chill structure at casting circular hole position | |
CN103909254A (en) | Casting pouring device | |
CN205393465U (en) | Foundry goods elongated hole shaping psammitolite structure | |
CN105563035A (en) | Machining technology of machine shell cooling water way | |
CN204770593U (en) | Spiral water channel psammitolite structure | |
CN103028705A (en) | Sand mould used for blind tube casting | |
CN105397031A (en) | Method for lengthening casting feeding channel | |
CN102248130B (en) | Manufacturing process of core assembly for butterfly valve body | |
CN104923733A (en) | Casting method of titanium or titanium alloy casting having special-shaped inner hole | |
FR3023196B1 (en) | IMPROVED TURBOMACHINE HOLLOW DAWN MOLDING PROCESS | |
JP2015174140A5 (en) | ||
CN202087779U (en) | Elongated hole sand core | |
CN202845700U (en) | Lateral-casting type casting system | |
CN202207772U (en) | Sand mould structure | |
CN207127237U (en) | Triple-valve body electroslag smelting casting shaped device |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
PB01 | Publication | ||
PB01 | Publication | ||
SE01 | Entry into force of request for substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
TA01 | Transfer of patent application right |
Effective date of registration: 20211214 Address after: 272000 Jining Economic Development Zone, Jining City, Shandong Province (Jiacheng Road, west of Jixu Expressway and north of Huixiang Road) Applicant after: Jining Economic Development Zone Hongyu metal products Co.,Ltd. Address before: No. 304, building 24, Jinying community, Kaifu District, Changsha City, Hunan Province Applicant before: Wu Huilin |
|
TA01 | Transfer of patent application right | ||
GR01 | Patent grant | ||
GR01 | Patent grant |