CN107337368A - Cold-application tar pavement asphalt diluent - Google Patents

Cold-application tar pavement asphalt diluent Download PDF

Info

Publication number
CN107337368A
CN107337368A CN201610272647.9A CN201610272647A CN107337368A CN 107337368 A CN107337368 A CN 107337368A CN 201610272647 A CN201610272647 A CN 201610272647A CN 107337368 A CN107337368 A CN 107337368A
Authority
CN
China
Prior art keywords
pitch
diluent
construction
parts
weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610272647.9A
Other languages
Chinese (zh)
Inventor
宋学忠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201610272647.9A priority Critical patent/CN107337368A/en
Publication of CN107337368A publication Critical patent/CN107337368A/en
Pending legal-status Critical Current

Abstract

Cold-application tar pavement asphalt diluent of the present invention, the diluent is dichloromethane, the pitch diluent of 40 50 parts by weight poured into the pitch of 50 60 parts by weight after stirring after being diluted, mix directly can be carried out to building stones at normal temperatures using the pitch after being diluted, the stone after mix can carry out construction of paving the way at normal temperatures;Pass through the technical program, pitch and building stones need not be heated, and can be paved the way at the construction field (site) in mix, be not in expense material, the work period is not by temperature limiting, substantially increase efficiency of construction and construction cost, construction quality is effectively guaranteed, every Construction index meets relevant national standard and various performance requirements, constructs no longer by seasonal effect, also no longer by it is southern it is different with northern surface temperature limited, open new invention for paving the way for asphalt surface.

Description

Cold-application tar pavement asphalt diluent
Technical field
The present invention relates to a kind of diluent, more particularly to a kind of cold-application tar pavement asphalt diluent.
Background technology
In the prior art asphalt surface when paving the way, it is necessary to which will pave the way used main material pitch and building stones are heated separately to approach Mix is carried out at 200 DEG C, stone temperature cannot be below 160 DEG C when paving the way, and when stone is less than 150 DEG C when paving the way, stone will All scrap and can not use again, so as to cause short construction period of paving the way, climate change or seasonal variations also directly influence construction effect Fruit and quality, and need the larger energy to be heated pitch and building stones, mass energy is consumed, while also in mix Surrounding enviroment are caused with pollution.
The content of the invention
In view of this, it is a primary object of the present invention to provide a kind of cold-application tar pavement asphalt diluent, by the technical program, After diluent is added in pitch, the pitch after resulting dilution, mix directly can be carried out with building stones at normal temperatures, after mix Stone can carry out construction of paving the way at normal temperatures, pitch and building stones need not be heated, and can be spread at the construction field (site) in mix Road, efficiency of construction and construction cost are substantially increased, be effectively guaranteed construction quality, opened newly for paving the way for asphalt surface Invention.
In order to achieve the above object, the technical proposal of the invention is realized in this way:A kind of cold-application tar pavement asphalt diluent, The diluent is dichloromethane, the diluent of 40-50 parts by weight is poured into the pitch of 50-60 parts by weight after stirring and obtained Pitch after to dilution, mix directly can be carried out to building stones at normal temperatures using the pitch after being diluted, the stone after mix can be Construction of paving the way is carried out under normal temperature.
As further technical scheme, the diluent by 50-80 parts by weight dichloromethane and the chloroethene of 20-50 parts by weight three Alkene mixes.
It is using the beneficial effect after above-mentioned technical proposal:A kind of cold-application tar pavement asphalt diluent, by the technical program, After diluent is added in pitch, the pitch after resulting dilution, mix directly can be carried out with building stones at normal temperatures, after mix Stone can carry out construction of paving the way at normal temperatures, pitch and building stones need not be heated, and can be spread at the construction field (site) in mix Road, be not in expense material, the work period is not substantially increased efficiency of construction and construction cost by temperature limiting, effective to ensure Construction quality, every Construction index meet relevant national standard and various performance requirements, and construction is no longer by seasonal effect, also not Again by it is southern it is different with northern surface temperature limited, open new invention for paving the way for asphalt surface.
Embodiment
The technical scheme in the present invention is described in further detail below in conjunction with specific embodiment.
Cold-application tar pavement asphalt diluent of the present invention, the diluent is dichloromethane, by the dilute of 40-50 parts by weight Release agent pour into the pitch of 50-60 parts by weight stir after diluted after pitch, can be direct using the pitch after being diluted Mix is carried out to building stones at normal temperatures, the stone after mix can carry out construction of paving the way at normal temperatures.
As further embodiment, the diluent by 50-80 parts by weight dichloromethane and the chloroethene of 20-50 parts by weight three Alkene mixes.
Embodiment one
Diluent uses dichloromethane, the dichloromethane of 50 parts by weight is poured into the pitch of 50 parts by weight after stirring and obtained Pitch after dilution, after carrying out mix by the pitch after the dilution of 6 parts by weight and the stone material of 100 parts by weight, it is adapted to carry out in the winter time Pave the way construction.
Embodiment two
Diluent uses dichloromethane, the dichloromethane of 40 parts by weight is poured into the pitch of 60 parts by weight after stirring and obtained Pitch after dilution, after carrying out mix by the pitch after the dilution of 6 parts by weight and the stone material of 100 parts by weight, it is adapted to carry out in summer Pave the way construction.
Embodiment three
Diluent is mixed by the dichloromethane and 20 parts by weight trichloro ethylenes of 80 parts by weight, by 50 parts by weight after mixing Dichloromethane and trichloro ethylene are poured into the pitch of 50 parts by weight stir after diluted after pitch, it is dilute by 6 parts by weight After the stone material of pitch and 100 parts by weight after releasing carries out mix, by increasing, trichloro ethylene can effectively simultaneously appropriate extension be paved the way The haulage time of middle mix and activity duration, while extending the hardening time on road surface, for generally, road surface is adjacent Be combineding with each other for aspect creates condition.
Example IV
Diluent is mixed by the dichloromethane and 50 parts by weight trichloro ethylenes of 50 parts by weight, by 50 parts by weight after mixing Dichloromethane and trichloro ethylene are poured into the pitch of 50 parts by weight stir after diluted after pitch, it is dilute by 6 parts by weight , can be effectively bright by increasing, increasing the content of trichloro ethylene after the stone material of pitch and 100 parts by weight after releasing carries out mix Aobvious extension pave the way middle mix haulage time and the activity duration, while also effectively extend road surface hardening time, be In particular cases, the mutual strong bonded between the multilayer asphalt surface of particular/special requirement creates advantage, is carried for road surface waterproof Relatively reliable guarantee is supplied.
It is described above, it is only the preferable possible embodiments of the present invention, is not limited to protection scope of the present invention.

Claims (2)

1. a kind of cold-application tar pavement asphalt diluent, it is characterised in that the diluent is dichloromethane, by 40-50 weight Part diluent pour into the pitch of 50-60 parts by weight stir after diluted after pitch, utilize the pitch after being diluted Mix directly can be carried out to building stones at normal temperatures, the stone after mix can carry out construction of paving the way at normal temperatures.
2. cold-application tar pavement asphalt diluent according to claim 1, it is characterised in that the diluent is by 50-80 The dichloromethane and 20-50 parts by weight trichloro ethylenes of parts by weight mix.
CN201610272647.9A 2016-04-29 2016-04-29 Cold-application tar pavement asphalt diluent Pending CN107337368A (en)