CN107309615B - A kind of nontoxic inside door powder coating methods - Google Patents

A kind of nontoxic inside door powder coating methods Download PDF

Info

Publication number
CN107309615B
CN107309615B CN201710629156.XA CN201710629156A CN107309615B CN 107309615 B CN107309615 B CN 107309615B CN 201710629156 A CN201710629156 A CN 201710629156A CN 107309615 B CN107309615 B CN 107309615B
Authority
CN
China
Prior art keywords
keel
health
door leaf
powder spray
environment temperature
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201710629156.XA
Other languages
Chinese (zh)
Other versions
CN107309615A (en
Inventor
李颖辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Intelligent Home Furnishing Dongyirisheng Technology Co Ltd
Original Assignee
Intelligent Home Furnishing Dongyirisheng Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Intelligent Home Furnishing Dongyirisheng Technology Co Ltd filed Critical Intelligent Home Furnishing Dongyirisheng Technology Co Ltd
Priority to CN201710629156.XA priority Critical patent/CN107309615B/en
Publication of CN107309615A publication Critical patent/CN107309615A/en
Application granted granted Critical
Publication of CN107309615B publication Critical patent/CN107309615B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention provides a kind of nontoxic inside door powder coating methods, characterized by the following steps: blanking;Code keel;Health;Fixed thickness sanding;Punching;Hot pressing is compound;Pressure maintaining health;Door leaf production line;Powder spray;Punching;Powder spray;Mating, trial assembly manually forms trial assembly;Outseam is inlayed;Health;Mating inspection declaration;It is packaged;Storage.The processes such as the present invention is using compound, the multiple health of reasonable hot pressing, powder spray, and outseam is inlayed are realized nontoxic after the inside door powder spray processed.

Description

A kind of nontoxic inside door powder coating methods
Technical field
The present invention relates to a kind of inside door production method, a kind of specifically nontoxic inside door powder coating methods.
Background technique
For inside door in production, existing inside door surface forming method, which will be slow, releases noxious material, distributes in the room, Human body is caused greatly to damage, pole is not environmentally.
Summary of the invention
The present invention provides a kind of nontoxic inside door powder coating methods to be made to produce the purpose is to solve prior art disadvantage Inside door asepsis environment-protecting.
The technical solution adopted by the present invention to solve the technical problems is:
A kind of nontoxic inside door powder coating methods, characterized by the following steps:
A: blanking: use sizing saw machine or hand saw blanking: keel use LVL;6A panel is using plain density board;Keel double open Ventilating groove;
B: code keel: artificial code keel: in transom and centre keel stitching portion gluing, transom and centre keel junction are applied Glue is simultaneously fixed with flat nail;
C: health: after code keel, horizontal piles up progress health in 8 hours;
D: thickness fixed thickness sanding: is confined to keel with contact calibrating machine;
E: punching: manual electric drill or machining center make a call to 3 carryings ventholes door leaf both ends are each, carry venthole be located at it is imperial At bone and keel neutral gear;
F: hot pressing is compound: being pressed panel and keel with automatic heating crimping, glue-spread: 120g/ ㎡, pressure: 0.7kg/ cm2, temperature: 85 DEG C ± 5 DEG C, hot pressing time: 6-7min;The open hour of glue: should be in 1.5min at 25 DEG C of environment temperature > Pressurized-heated is carried out, whens environment temperature≤25 DEG C should carry out Pressurized-heated in 3min;
G: pressure maintaining health: horizontal, which is piled up, after hot pressing carries out health: conditioned time 48 in the case of 20 DEG C of operating environment temperature > Hour, conditioned time 24 hours in the case of operating environment temperature≤20 DEG C;
H: door leaf production line: with numerical control door leaf four while saw carry out door leaf it is net while, scale, groove milling, then mend poly-putty base;
I: powder spray powder spray: is carried out with powder spray line;
J: lockhole, hinge hole punching: are beaten to door leaf with digital control perforating machine;
K: powder spray powder spray: is carried out with powder spray line;
L: mating, trial assembly manually forms trial assembly;
M: outseam is inlayed: manually being inlayed lines, glass, door leaf and is inlayed;
N: health: outseam inlays rear straight stacking and carries out health: health in the case of 10 DEG C≤operating environment temperature≤35 DEG C Time 12 hours;Conditioned time 24 hours in the case of 10 DEG C of 0 DEG C≤operating environment temperature <;
O: mating inspection declaration: lining, set line, the mating inspection of door leaf;
P: be packaged: baling press requires to pack according to PS Package Specification;
Q: storage.
The invention has the beneficial effects that:
The processes such as the present invention is using compound, the multiple health of reasonable hot pressing, powder spray, and outseam is inlayed, realize processing It is nontoxic after inside door powder spray out.
Specific embodiment
The present invention is a kind of nontoxic inside door powder coating methods, characterized by the following steps:
A: blanking: use sizing saw machine or hand saw blanking: keel use LVL;6A panel is using plain density board;Keel double open Ventilating groove, when groove depth 7mm, size≤1000mm, open 3;5 are opened when size > 1000mm;
B: code keel: artificial code keel: in transom and centre keel stitching portion gluing 3052, glue-spread: 20g/ fan, horizontal dragon Bone and centre keel junction gluing are simultaneously fixed with flat nail;
C: health: after code keel, horizontal piles up progress health in 8 hours;
D: fixed thickness sanding: thickness is confined to keel with contact calibrating machine, 38 ± 0.2mm of precision uses abrasive band 40#/80#;
E: punching: manual electric drill or machining center make a call to 3 carrying ventholes door leaf both ends are each, and each carrying venthole is straight Diameter 12mm carries venthole and is located at keel and keel neutral gear;
F: hot pressing is compound: panel and keel pressed with automatic heating crimping, glue-type number: 3052, and glue-spread: 120g/ ㎡, pressure It is strong: 0.7kg/cm2, temperature: 85 DEG C ± 5 DEG C, hot pressing time: 6-7min;The open hour of glue: should be at 25 DEG C of environment temperature > Carry out Pressurized-heated in 1.5min, whens environment temperature≤25 DEG C should carry out Pressurized-heated in 3min, there is honeycomb paper filling;
G: pressure maintaining health: horizontal, which is piled up, after hot pressing carries out health: conditioned time 48 in the case of 20 DEG C of operating environment temperature > Hour, conditioned time 24 hours in the case of operating environment temperature≤20 DEG C, when health, whole plate thickness cannot be less than 18mm, above Whole plate adds pressure maintaining square pressure maintaining, and pressure maintaining square is no less than three and uniformly places;
H: door leaf production line: with numerical control door leaf four while saw carry out door leaf it is net while, scale, (two long side of door leaf facet is fallen for groove milling R2 fillet inserts the formula hinge door leaf side fillet of falling R2), then mend poly-putty base;
I: powder spray powder spray: is carried out with powder spray line;
J: lockhole, hinge hole punching: are beaten to door leaf with digital control perforating machine;
K: powder spray powder spray: is carried out with powder spray line;
L: mating, trial assembly manually forms trial assembly (lining, set line, door leaf are mating);
M: outseam is inlayed: manually being inlayed lines, glass, door leaf and is inlayed;Lines bonding: the coating of glass cement strip, hot melt adhesive Dotted fixed lines, glass door are fixed with rummy promise fastener fixing lines and glass cement, after glue coating before the deadline Lines are mounted on door leaf, the open hour of summer hot melt adhesive are 80 seconds, and winter is 50 seconds, and summer forbids being applied with fan blow-through The glass cement of cloth avoids glass cement surface solid, influences adhesive tension;
N: health: outseam inlays rear straight stacking and carries out health: health in the case of 10 DEG C≤operating environment temperature≤35 DEG C Time 12 hours;Conditioned time 24 hours in the case of 10 DEG C of 0 DEG C≤operating environment temperature <;
O: mating inspection declaration: lining, set line, the mating inspection of door leaf;
P: be packaged: baling press requires to pack according to PS Package Specification;
Q: storage.
Each embodiment in this specification is described in a progressive manner, the highlights of each of the examples are with other The difference of embodiment, the same or similar parts in each embodiment may refer to each other.To the upper of the disclosed embodiments It states bright, enables those skilled in the art to implement or use the present invention.Various modifications to these embodiments are to ability Will be apparent for the professional technician in domain, the general principles defined herein can not depart from it is of the invention In the case where spirit or scope, realize in other embodiments.Therefore, the present invention be not intended to be limited to it is shown in this article these Embodiment, and it is to fit to the widest scope consistent with the principles and novel features disclosed herein.

Claims (1)

1. a kind of nontoxic inside door powder coating methods, characterized by the following steps:
A: blanking: use sizing saw machine or hand saw blanking: keel use LVL;6A panel is using plain density board;Keel double open is ventilative Slot;
B: code keel: artificial code keel: in transom and centre keel stitching portion gluing, transom and centre keel junction gluing are simultaneously It is fixed with flat nail;
C: health: after code keel, horizontal piles up progress health in 8 hours;
D: thickness fixed thickness sanding: is confined to keel with contact calibrating machine;
E: punching: manual electric drill or machining center make a call to 3 carryings ventholes door leaf both ends are each, carry venthole be located at keel and At keel neutral gear;
F: hot pressing is compound: being pressed panel and keel with automatic heating crimping, glue-spread: 120g/ ㎡, pressure: 0.7kg/cm2, temperature Degree: 85 DEG C ± 5 DEG C, hot pressing time: 6-7min;The open hour of glue: should be added in 1.5min at 25 DEG C of environment temperature > Pressure heating, whens environment temperature≤25 DEG C, should carry out Pressurized-heated in 3min;
G: pressure maintaining health: horizontal, which is piled up, after hot pressing carries out health: conditioned time 48 hours in the case of 20 DEG C of operating environment temperature >, Conditioned time 24 hours in the case of operating environment temperature≤20 DEG C;
H: door leaf production line: with numerical control door leaf four while saw carry out door leaf it is net while, scale, groove milling, then mend poly-putty base;
I: powder spray powder spray: is carried out with powder spray line;
J: lockhole, hinge hole punching: are beaten to door leaf with digital control perforating machine;
K: powder spray powder spray: is carried out with powder spray line;
L: mating, trial assembly manually forms trial assembly;
M: outseam is inlayed: manually being inlayed lines, glass, door leaf and is inlayed;
N: health: outseam inlays rear straight stacking and carries out health: conditioned time in the case of 10 DEG C≤operating environment temperature≤35 DEG C 12 hours;Conditioned time 24 hours in the case of 10 DEG C of 0 DEG C≤operating environment temperature <;
O: mating inspection declaration: lining, set line, the mating inspection of door leaf;
P: be packaged: baling press requires to pack according to PS Package Specification;
Q: storage.
CN201710629156.XA 2017-07-28 2017-07-28 A kind of nontoxic inside door powder coating methods Active CN107309615B (en)