CN107297065A - A kind of construction method of shuttlecock surface waterproofing paint - Google Patents

A kind of construction method of shuttlecock surface waterproofing paint Download PDF

Info

Publication number
CN107297065A
CN107297065A CN201710579135.1A CN201710579135A CN107297065A CN 107297065 A CN107297065 A CN 107297065A CN 201710579135 A CN201710579135 A CN 201710579135A CN 107297065 A CN107297065 A CN 107297065A
Authority
CN
China
Prior art keywords
shuttlecock
brush
temperature
paint
construction method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710579135.1A
Other languages
Chinese (zh)
Inventor
李方林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI HUA LING FEATHER PRODUCTS Co Ltd
Original Assignee
ANHUI HUA LING FEATHER PRODUCTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI HUA LING FEATHER PRODUCTS Co Ltd filed Critical ANHUI HUA LING FEATHER PRODUCTS Co Ltd
Priority to CN201710579135.1A priority Critical patent/CN107297065A/en
Publication of CN107297065A publication Critical patent/CN107297065A/en
Pending legal-status Critical Current

Abstract

The uniform brush first pass in shuttlecock surface is painted the invention discloses a kind of construction method of shuttlecock surface waterproofing paint, including with banister brush, and dries 8 12h, 30 40 DEG C of temperature;With banister brush to second time paint of the uniform brush in shuttlecock surface, and dry 6 8h, 35 45 DEG C of temperature;With banister brush to the paint of the uniform brush in shuttlecock surface the 3rd time, and dry 4 6h, the step such as 25 35 DEG C of temperature.The present invention provides a kind of construction method of shuttlecock surface waterproofing paint; the simple science of construction method; pass through the different temperature and time of three secondary controls; paint application in shuttlecock surface-stable, will not fall off; it can effectively protect shuttlecock not encroached on by rainwater, sweat etc., effectively protect shuttlecock.

Description

A kind of construction method of shuttlecock surface waterproofing paint
Technical field
The present invention relates to shuttlecock processing technique field, more particularly to a kind of construction party of shuttlecock surface waterproofing paint Method.
Background technology
Shuttlecock is an indoor and outdoor motion taken into account.According to the number participated in, singles and doubles can be divided into, and Emerging 3V3 rules.
Shuttlecock can typically receive the infringement of the water quality such as rainwater, sweat in use, once shuttlecock Using effect will be had a strong impact on by getting wet, and reduce its service life.
People can typically coat some on shuttlecock surface has the paint of water resistance, can effectively protect feather Ball feather, the present invention proposes a kind of construction method of shuttlecock surface waterproofing paint.
The content of the invention
To overcome above-mentioned deficiency, the present invention provides the construction method and its construction party of a kind of shuttlecock surface waterproofing paint Method.
The present invention takes following technical scheme to realize:A kind of construction method of shuttlecock surface waterproofing paint, Comprise the following steps:
The impurity such as the dust a. carried using brush cleaning shuttlecock surface;
B. shuttlecock is soaked using 5% physiological saline;
C. the shuttlecock rinsed repeatedly after immersion using distilled water;
D. the shuttlecock after distilled water cleaning is dried;
E. shuttlecock surface is arranged, makes its surfacing;
F. the uniform brush first pass in shuttlecock surface is painted with banister brush, and dries 8-12h, 30-40 DEG C of temperature;
G. with banister brush to second time paint of the uniform brush in shuttlecock surface, and 6-8h, 35-45 DEG C of temperature are dried;
H. with banister brush to the 3rd time paint of the uniform brush in shuttlecock surface, and 4-6h, 25-35 DEG C of temperature are dried;
I. shuttlecock surface is arranged again, makes its surfacing;
J. one layer of beeswax, air drying are uniformly applied to shuttlecock surface with banister brush.
Specifically, step f. banister brush is painted to the uniform brush first pass in shuttlecock surface, and dries 10h, temperature 35℃。
Specifically, step g. banister brush is to second time paint of the uniform brush in shuttlecock surface, and dries 7h, temperature 40 ℃。
Specifically, step h. banister brush is to the 3rd time paint of the uniform brush in shuttlecock surface, and dries 5h, temperature 30 ℃。
In summary the invention has the advantages that:The present invention provides a kind of applying for shuttlecock surface waterproofing paint Work method, the simple science of construction method, by the different temperature and time of three secondary controls, paint application is on shuttlecock surface Stablize, will not fall off, can effectively protect shuttlecock not encroached on by rainwater, sweat etc., effectively protect shuttlecock plumage Hair.
Embodiment
To be easy to understand the technical means, the inventive features, the objects and the advantages of the present invention, with reference to Embodiment, is expanded on further the present invention.
A kind of construction method of shuttlecock surface waterproofing paint of embodiment 1
A kind of construction method of shuttlecock surface waterproofing paint, comprises the following steps:
The impurity such as the dust a. carried using brush cleaning shuttlecock surface;
B. shuttlecock is soaked using 5% physiological saline;
C. the shuttlecock rinsed repeatedly after immersion using distilled water;
D. the shuttlecock after distilled water cleaning is dried;
E. shuttlecock surface is arranged, makes its surfacing;
F. the uniform brush first pass in shuttlecock surface is painted with banister brush, and dries 8-12h, 30-40 DEG C of temperature;
G. with banister brush to second time paint of the uniform brush in shuttlecock surface, and 6-8h, 35-45 DEG C of temperature are dried;
H. with banister brush to the 3rd time paint of the uniform brush in shuttlecock surface, and 4-6h, 25-35 DEG C of temperature are dried;
I. shuttlecock surface is arranged again, makes its surfacing;
J. one layer of beeswax, air drying are uniformly applied to shuttlecock surface with banister brush.
As the priority scheme of the present invention, step f. banister brush of the present invention is to the uniform brush first pass in shuttlecock surface Paint, and dry 10h, 35 DEG C of temperature.
As the priority scheme of the present invention, step g. banister brush of the present invention is to the uniform brush in shuttlecock surface second time Paint, and dry 7h, 40 DEG C of temperature.
As the priority scheme of the present invention, step h. banister brush of the present invention is to the uniform brush in shuttlecock surface the 3rd time Paint, and dry 5h, 30 DEG C of temperature.
It is obvious to a person skilled in the art that the invention is not restricted to the details of above-mentioned one exemplary embodiment, Er Qie In the case of without departing substantially from spirit or essential attributes of the invention, the present invention can be realized in other specific forms.Therefore, no matter From the point of view of which point, embodiment all should be regarded as exemplary, and be nonrestrictive, the scope of the present invention is by appended power Profit is required rather than described above is limited, it is intended that all in the implication and scope of the equivalency of claim by falling Change is included in the present invention.
Moreover, it will be appreciated that although the present specification is described in terms of embodiments, not each embodiment is only wrapped Containing an independent technical scheme, this narrating mode of specification is only that for clarity, those skilled in the art should Using specification as an entirety, the technical solutions in the various embodiments may also be suitably combined, forms those skilled in the art It may be appreciated other embodiment.

Claims (4)

1. a kind of construction method of shuttlecock surface waterproofing paint, it is characterised in that:Comprise the following steps:
The impurity such as the dust a. carried using brush cleaning shuttlecock surface;
B. shuttlecock is soaked using 5% physiological saline;
C. the shuttlecock rinsed repeatedly after immersion using distilled water;
D. the shuttlecock after distilled water cleaning is dried;
E. shuttlecock surface is arranged, makes its surfacing;
F. the uniform brush first pass in shuttlecock surface is painted with banister brush, and dries 8-12h, 30-40 DEG C of temperature;
G. with banister brush to second time paint of the uniform brush in shuttlecock surface, and 6-8h, 35-45 DEG C of temperature are dried;
H. with banister brush to the 3rd time paint of the uniform brush in shuttlecock surface, and 4-6h, 25-35 DEG C of temperature are dried;
I. shuttlecock surface is arranged again, makes its surfacing;
J. one layer of beeswax, air drying are uniformly applied to shuttlecock surface with banister brush.
2. a kind of construction method of shuttlecock surface waterproofing paint according to claim 1, it is characterised in that:Step f. The uniform brush first pass in shuttlecock surface is painted with banister brush, and dries 10h, 35 DEG C of temperature.
3. a kind of construction method of shuttlecock surface waterproofing paint according to claim 1, it is characterised in that:Step g. With banister brush to second time paint of the uniform brush in shuttlecock surface, and dry 7h, 40 DEG C of temperature.
4. a kind of construction method of shuttlecock surface waterproofing paint according to claim 1, it is characterised in that:Step h. With banister brush to the 3rd time paint of the uniform brush in shuttlecock surface, and dry 5h, 30 DEG C of temperature.
CN201710579135.1A 2017-07-17 2017-07-17 A kind of construction method of shuttlecock surface waterproofing paint Pending CN107297065A (en)