CN107189480A - Add the composite of ramulus mori fiber - Google Patents

Add the composite of ramulus mori fiber Download PDF

Info

Publication number
CN107189480A
CN107189480A CN201710372856.5A CN201710372856A CN107189480A CN 107189480 A CN107189480 A CN 107189480A CN 201710372856 A CN201710372856 A CN 201710372856A CN 107189480 A CN107189480 A CN 107189480A
Authority
CN
China
Prior art keywords
ramulus mori
mori fiber
composite
fiber
lubricant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710372856.5A
Other languages
Chinese (zh)
Inventor
陈海银
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201710372856.5A priority Critical patent/CN107189480A/en
Publication of CN107189480A publication Critical patent/CN107189480A/en
Pending legal-status Critical Current

Abstract

The invention discloses a kind of composite for adding ramulus mori fiber, including ramulus mori fiber, waste plastic, compatilizer, lubricant, toughener, nano-particle, the weight proportion of each component is:Ramulus mori fiber 15~20%, waste plastic 50~60%, inorganic nano-particle 10~20%, compatilizer 8~12%, lubricant 5~8%, toughener 2~4%;Further improvement is that:Lubricant is stearic acid or atoleine.Energy scale of the invention utilizes ramulus mori fiber, waste plastic, environmental protection.

Description

Add the composite of ramulus mori fiber
Technical field
The present invention relates to a kind of polymer composite, particularly a kind of PVC composites.
Background technology
In in the past few decades, by wood materials(Such as wood powder, cellulose fibre)With farming raw material(Such as jute, Rice husk, flax, hemp etc.)The natural organic filler constituted has begun to infiltration thermoplasticity finishing material market.Natural plants Fiber (Natural Vegetable Fibers, NVF) is to store resource the abundantest in the world, is given birth to every year in nature The total amount of cellulose can be up to hundred billion tons in the long NVF existed, considerably beyond the earth on existing petroleum total reserve.But my god Right string does not form scale utilization, and ramulus mori fiber is exactly one kind therein, and a large amount of ramulus mori fibers go out of use, and not only cause The wasting of resources, also result in serious environmental pollution.
The content of the invention
The present invention in view of the shortcomings of the prior art, proposes a kind of energy scale using the addition ramulus mori fiber of ramulus mori fiber Composite.
The present invention is achieved through the following technical solutions technical goal.
The composite of ramulus mori fiber is added, it is theed improvement is that:Including ramulus mori fiber, waste plastic, compatilizer, profit Lubrication prescription, toughener, nano-particle, the weight proportion of each component is:Ramulus mori fiber 15~20%, waste plastic 50~60%, nothing Machine nano-particle 10~20%, compatilizer 8~12%, lubricant 5~8%, toughener 2~4%.
Further improvement is that:The lubricant is stearic acid or atoleine.
The present invention compared with prior art, has the positive effect that:
1st, energy scale utilizes ramulus mori fiber.
2nd, inorganic nano-particle is added, the mechanical property of the present invention is remarkably improved.
3rd, using waste plastic, turn waste into wealth, while reducing environmental pollution.
4th, lubricant is stearic acid or atoleine, is conducive to shaping.
Embodiment
With reference to embodiment, the invention will be further described.
Embodiment:
Add the composite of ramulus mori fiber, including ramulus mori fiber, waste plastic, compatilizer, lubricant, toughener, nanoparticle Son, the weight proportion of each component is:Ramulus mori fiber 15~20%, waste plastic 50~60%, inorganic nano-particle 10~20%, Compatilizer 8~12%, lubricant 5~8%, toughener 2~4%.
In the present embodiment, lubricant is stearic acid or atoleine.

Claims (2)

1. a kind of composite for adding ramulus mori fiber, it is characterised in that:Including ramulus mori fiber, waste plastic, compatilizer, lubrication Agent, toughener, nano-particle, the weight proportion of each component is:Ramulus mori fiber 15~20%, waste plastic 50~60% is inorganic Nano-particle 10~20%, compatilizer 8~12%, lubricant 5~8%, toughener 2~4%.
2. the composite of addition ramulus mori fiber according to claim 1, it is characterised in that:The lubricant is stearic acid Or atoleine.
CN201710372856.5A 2017-05-24 2017-05-24 Add the composite of ramulus mori fiber Pending CN107189480A (en)