CN106881230A - A kind of industrial lacquer spraying technique and its operating system - Google Patents
A kind of industrial lacquer spraying technique and its operating system Download PDFInfo
- Publication number
- CN106881230A CN106881230A CN201710278990.9A CN201710278990A CN106881230A CN 106881230 A CN106881230 A CN 106881230A CN 201710278990 A CN201710278990 A CN 201710278990A CN 106881230 A CN106881230 A CN 106881230A
- Authority
- CN
- China
- Prior art keywords
- workshop section
- paint
- treatment
- finish paint
- station
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The present invention relates to lacquering technologies field, and in particular to a kind of industrial lacquer spraying technique and its operating system, the operating system includes the pretreatment system, prime treatment system and the finish paint processing system that are sequentially connected;The pretreatment system includes being sequentially connected workpiece upper part mouthful and preheating workshop section;The prime treatment system includes the basecoat paint station, the first microwave drying workshop section, priming paint polishing station and the second microwave drying workshop section that are sequentially connected;The finish paint processing system includes finish paint upper part mouth, finish paint spray station, the 3rd microwave drying workshop section and the finish paint lower part mouthful that are sequentially connected.Operating system simple structure of the invention, working environment takes up an area small, reduce operation cost, staff's positioning work, it is to avoid the repeated multiple times caused production safety problem of walking up and down of staff, it is combined with lacquer spraying technique, the production cycle is shortened, production efficiency is improve, energy consumption is reduced, environmental protection and energy saving, it is adaptable to the field such as furniture, electronics, automobile, ship, machine-building.
Description
Technical field
The present invention relates to lacquering technologies field, and in particular to a kind of industrial lacquer spraying technique and its operating system.
Background technology
In existing lacquer spraying technique flow, often using large area wire body and the production technology and form of construction work of highly energy-consuming,
Also fail to accomplish smart, short, small design, cause worker workload and walk the increase of momentum, staff is concentrated
Formula works and manages, and environment takes up an area greatly, and energy consumption is big, reduces the working security of staff, extends the production cycle, increases
Add production and operation cost, increased the operated pressure of enterprise, be unfavorable for the long-run development and environmentally friendly development of enterprise.
In addition, existing lacquer spraying technique flow is poor to the temperature and time control of each processing step, cause obtained spray
The lacquer painting of lacquerer's part is not smooth enough, not smooth enough, not uniform enough, and aesthetics ground, total quality is poor.
The content of the invention
In order to overcome shortcoming and defect present in prior art, make it is an object of the invention to provide a kind of industry spray painting
Industry system, the operating system simple structure, working environment takes up an area small, reduction operation cost, and staff's positioning work is shortened
Production cycle, production efficiency is improve, reduce energy consumption, environmental protection and energy saving.
Another object of the present invention is to provide a kind of industrial lacquer spraying technique, the lacquer spraying technique flow is simple, by strict
Control each operation, and strict control each operation treatment temperature, be combined with spray painting operation system, shorten the production cycle,
Environmental protection and energy saving, obtained painting workpieces have preferably planarization, slickness and uniformity, and quality is good, and aesthetics is good.
The purpose of the present invention is achieved through the following technical solutions:A kind of industrial spray painting operation system, including be sequentially connected
Pretreatment system, prime treatment system and finish paint processing system;The pretreatment system include being sequentially connected workpiece upper part mouthful and
Preheating workshop section;The prime treatment system includes the basecoat paint station, the first microwave drying workshop section, the priming paint polishing that are sequentially connected
Station and the second microwave drying workshop section;The finish paint processing system include be sequentially connected finish paint upper part mouth, finish paint spray station,
3rd microwave drying workshop section and finish paint lower part mouthful.
Industrial spray painting operation system of the invention is by setting pretreatment system, prime treatment system and finish paint processing system
System, can be such that industrial lacquer spraying technique carries out in order, and the industrial spray painting operation system architecture is simple, be easy to maintenance, and use
Wire body operating type, working environment takes up an area small, staff's positioning work, it is to avoid repeated multiple times the walking up and down of staff causes
Production safety problem, shorten the production cycle, improve production efficiency, reduce energy consumption, reduce operation cost, environmental protection
Energy-conservation.Wherein, the basecoat paint station includes at least two spray stations;The priming paint polishing station includes at least four dozens
Grinder position.
Further, the workpiece upper part mouthful includes the first workpiece upper part mouthful being sequentially connected and second workpiece upper part mouthful,
The input of the second workpiece upper part mouthful be connected with the output end of the first workpiece upper part mouthful, second workpiece upper part mouth it is defeated
Go out end to be connected with the input of the preheating workshop section.
The present invention can make workpiece to be painted by setting the first workpiece upper part being sequentially connected mouthful and second workpiece upper part mouthful
Intersect upper part in the first workpiece upper part mouthful and second workpiece upper part mouthful, in order alternately upper part, the upper of paint spraying system can be improved
Part speed, and then the operating efficiency of paint spraying system is improved, shorten the production cycle, save production cost.
Further, the first normal temperature levelling is also included between the basecoat paint station and the first microwave drying workshop section
Workshop section, the input of the first normal temperature levelling workshop section is connected with the output end of basecoat paint station, the first normal temperature levelling workshop section
Output end be connected with the input of the first microwave drying workshop section.
The present invention is simple to operate by setting the first normal temperature levelling workshop section, improves the orderly of industrial spray painting operation system
Property, operating efficiency and work quality, and normal temperature levelling treatment can be in order carried out to the workpiece after spray-applied primer, make obtained spray painting
Workpiece has smooth, smooth, uniform priming paint, the carrying out for being easy to following process to process, and improves the quality of processing workpiece, shortens life
In the product cycle, save production cost.
Further, the first heating cure is also included between the first microwave drying workshop section and priming paint polishing station
Workshop section, the input of the first heating cure workshop section is connected with the output end of the first microwave drying workshop section, the first heating
The output end for solidifying workshop section is connected with the input of priming paint polishing station.
The present invention is simple to operate by setting the first heating cure workshop section, improves the orderly of industrial spray painting operation system
Property, operating efficiency and work quality, and heating cure can be in order carried out to the workpiece after microwave drying, make obtained painting workpieces
With stability priming paint face high, the carrying out for being easy to following process to process is improved the quality of processing workpiece, shortens the production cycle,
Save production cost.
Further, also color work is repaiied including priming paint between the priming paint polishing station and the second microwave drying workshop section
Position, the input that the priming paint repaiies color station is connected with the output end of priming paint polishing station, and priming paint repaiies the output of color station
End is connected with the input of the second microwave drying workshop section.
The present invention repaiies color workpiece by setting priming paint, simple to operate, improves order, the work of industrial spray painting operation system
Make efficiency and work quality, and refine color can be carried out to the priming paint after polishing, make obtained workpiece have preferably aesthetics and
Quality higher, the carrying out for being easy to following process to process shortens the production cycle, saves production cost.
Further, priming color grinder position, the second microwave drying work are also included after the second microwave drying workshop section
The output end of section is connected with the input of priming color grinder position.
The present invention is simple to operate by increasing priming color grinder position after the tail end workshop section of prime treatment system, improves
The order of industrial spray painting operation system, operating efficiency and work quality, and color can be carried out to the dried priming paint of secondary microwave
Mill treatment, makes obtained workpiece have preferably aesthetics and quality higher, and the carrying out for being easy to following process to process shortens life
In the product cycle, save production cost.Wherein, the priming color grinder position includes at least three color grinders position.
Further, the second normal temperature levelling is also included between the finish paint spray station and the 3rd microwave drying workshop section
Workshop section, the input of the second normal temperature levelling workshop section is connected with the output end of the finish paint spray station, the second normal temperature levelling
The output end of workshop section is connected with the input of the 3rd microwave drying workshop section.
The present invention is simple to operate by setting the second normal temperature levelling workshop section, improves the orderly of industrial spray painting operation system
Property, operating efficiency and work quality, and normal temperature levelling treatment can be in order carried out to the workpiece after spray paint, make obtained spray painting
Workpiece has smooth, smooth, uniform finish paint, the carrying out for being easy to following process to process, and improves the quality of processing workpiece, shortens life
In the product cycle, save production cost.
Further, be sequentially connected second is also included between the 3rd microwave drying workshop section and the finish paint lower part mouthful
Heating cure workshop section and finish paint repair color station, and the input of the second heating cure workshop section is defeated with the 3rd microwave drying workshop section
Go out end connection, the input that the output end of the second heating cure workshop section repaiies color station with the finish paint is connected, and finish paint repaiies color station
The input of output end and finish paint lower part mouthful be connected.
Color station is repaiied by the second heating cure workshop section and finish paint that the present invention is set, simple to operate, improves industry spray painting and makees
The order of industry system, operating efficiency and work quality, make the workpiece after microwave drying carry out heating cure treatment and face in order
Paint repaiies color treatment, obtained painting workpieces is had smooth, smooth, uniform finish paint, improves the quality of processing workpiece, shortens
Production cycle, save production cost.
Another object of the present invention is achieved through the following technical solutions:A kind of industrial lacquer spraying technique, comprises the following steps:
A, the pre-heat treatment:The pre-heat treatment of workpiece will be carried out in each workpiece upper part to be painted to preheating workshop section;
B, prime treatment:Workpiece to be painted after step A the pre-heat treatments is carried out into basecoat paint treatment successively, at priming paint levelling
Reason, microwave water lift dried process, priming paint heating cure treatment, priming paint grinding process, a priming paint are repaiied color treatment, secondary microwave and are carried
Water dried process and priming color mill are processed, and priming paint finished work-piece is obtained;
C, finish paint treatment:By this finished work-piece of priming paint obtained in step B carry out successively finish paint spray treatment, finish paint levelling treatment,
Finish paint microwave water lift dried process, finish paint heating cure treatment and finish paint repair color treatment, and lower part is obtained painting workpieces finished product.
Lacquer spraying technique flow of the invention is simple, by each operation of strict control, is combined with spray painting operation system, contracts
Short production cycle, environmental protection and energy saving, obtained painting workpieces have preferably planarization, slickness, uniformity and aesthetics, matter
Measure.
Wherein, the step A carries out the pre-heat treatment using common hot blast;In the step B, the treatment of priming paint levelling treatment
Temperature is 20-30 DEG C, and one time the treatment temperature of microwave water lift dried process is 30-50 DEG C, the treatment of priming paint heating cure treatment
Temperature is 30-40 DEG C;In the step C, the treatment temperature of finish paint levelling treatment is 20-30 DEG C, finish paint heating cure treatment
Treatment temperature is 30-40 DEG C.
The priming paint levelling treatment temperature that the present invention passes through strict rate-determining steps B, makes obtained painting workpieces have smooth, light
Sliding, uniform priming paint;Microwave water lift dried process temperature of strict rate-determining steps B, can enter to the moisture in workpiece priming paint
Row sufficiently drying, it is preferred that microwave drying is carried out using profit all-in-one;The priming paint heating cure treatment temperature of strict control B
Degree, improves the stability of priming paint, and the priming paint for making workpiece is unlikely to deform in follow-up process, not easy to wear;Strict control
The finish paint levelling treatment temperature of step C, makes obtained painting workpieces have smooth, smooth, uniform finish paint;Strict rate-determining steps
The finish paint heating cure treatment temperature of C, improves the stability of finish paint, makes the finish paint of workpiece not variable in follow-up process
It is shape, not easy to wear.
The beneficial effects of the present invention are:Operating system simple structure of the invention, working environment takes up an area small, reduction operation
Cost, staff's positioning work, shortens the production cycle, improves production efficiency, reduces energy consumption, environmental protection and energy saving,
Suitable for fields such as furniture, automobile, ship, machine-building.
Lacquer spraying technique flow of the invention is simple, by each operation of strict control, and the strictly treatment of control each operation
Temperature, is combined with spray painting operation system, shortens production cycle, environmental protection and energy saving, and obtained painting workpieces have preferably puts down
Whole property, slickness, uniformity and aesthetics, quality are good.
Brief description of the drawings
Fig. 1 is system structure diagram of the invention.
Reference is:1-pretreatment system, 11-workpiece upper part mouth, the 111-the first workpiece upper part mouthful, 112-the second
Workpiece upper part mouthful, 12-preheating workshop section, 2-prime treatment system, 21-basecoat paint station, the 211-the first normal temperature levelling work
Section, the 22-the first microwave drying workshop section, the 221-the first heating cure workshop section, 23-priming paint polishing station, 231-priming paint repair color
Station, the 24-the second microwave drying workshop section, 241-priming color grinder position, 3-finish paint processing system, 31-finish paint upper part mouthful,
32-finish paint spray station, the 321-the second normal temperature levelling workshop section, the 33-the three microwave drying workshop section, the 331-the second heating cure
Color station, 34-finish paint lower part mouthful are repaiied by workshop section, 332-finish paint.
Specific embodiment
For the ease of the understanding of those skilled in the art, with reference to embodiment and accompanying drawing, 1 couple of present invention makees further
Illustrate, the content that implementation method is referred to not limitation of the invention.
Embodiment 1
See Fig. 1, a kind of industrial paint spraying system, including pretreatment system 1, prime treatment system 2 and the finish paint treatment being sequentially connected
System 3;The pretreatment system 1 includes the workpiece upper part mouthful 11 being sequentially connected and preheating workshop section 12;The prime treatment system 2
Including the basecoat paint station 21, the polishing microwave drying of station 23 and second of the first microwave drying workshop section 22, priming paint that are sequentially connected
Workshop section 24;The finish paint processing system 3 includes that the finish paint upper part mouthful 31, finish paint spray station 32 being sequentially connected, the 3rd microwave are done
Dry workshop section 33 and finish paint lower part mouthful 34.
The workpiece upper part mouthful 11 includes the first workpiece upper part mouthful 111 being sequentially connected and second workpiece upper part mouthful 112, institute
The input for stating second workpiece upper part mouthful 112 is connected with the output end of the first workpiece upper part mouthful 111, second workpiece upper part mouthful
112 output end is connected with the input of the preheating workshop section 12.
Also include the first normal temperature levelling workshop section between the basecoat paint station 21 and the first microwave drying workshop section 22
211, the input of the first normal temperature levelling workshop section 211 is connected with the output end of basecoat paint station 21, the first normal temperature levelling
The output end of workshop section 211 is connected with the input of the first microwave drying workshop section 22.
Also include the first heating cure workshop section between the first microwave drying workshop section 22 and priming paint polishing station 23
221, the input of the first heating cure workshop section 221 is connected with the output end of the first microwave drying workshop section 22, and first
The output end of heating cure workshop section 221 is connected with the input of priming paint polishing station 23.
Color station 231 also is repaiied including priming paint between the priming paint polishing station 23 and the second microwave drying workshop section 24,
The input that the priming paint repaiies color station 231 is connected with the output end of priming paint polishing station 23, and priming paint repaiies color station 231
Output end is connected with the input of the second microwave drying workshop section 24.
Priming color grinder position 241, the second microwave drying workshop section 24 are also included after the second microwave drying workshop section 24
The input of output end and the priming color grinder position 241 be connected.
Also include the second normal temperature levelling workshop section between the finish paint spray station 32 and the 3rd microwave drying workshop section 33
321, the input of the second normal temperature levelling workshop section 321 is connected with the output end of the finish paint spray station 32, the second normal temperature
The output end of levelling workshop section 321 is connected with the input of the 3rd microwave drying workshop section 33.
Also include the second heating being sequentially connected between the 3rd microwave drying workshop section 33 and the finish paint lower part mouthful 34
Solidification workshop section 331 and finish paint repair color station 332, the input and the 3rd microwave drying work of the second heating cure workshop section 331
The output end connection of section 33, output end and the finish paint of the second heating cure workshop section 331 repair the input company of color station 332
Connect, the output end that finish paint repaiies color station 332 is connected with the input of finish paint lower part mouthful 34.
Embodiment 2
The present embodiment is with the difference of above-described embodiment 1:
A kind of industrial lacquer spraying technique, comprises the following steps:
A, the pre-heat treatment:The pre-heat treatment of workpiece will be carried out in each workpiece upper part to be painted to preheating workshop section;
B, prime treatment:Workpiece to be painted after step A the pre-heat treatments is carried out into basecoat paint treatment successively, at priming paint levelling
Reason, microwave water lift dried process, priming paint heating cure treatment, priming paint grinding process, a priming paint are repaiied color treatment, secondary microwave and are carried
Water dried process and priming color mill are processed, and priming paint finished work-piece is obtained;
C, finish paint treatment:By this finished work-piece of priming paint obtained in step B carry out successively finish paint spray treatment, finish paint levelling treatment,
Finish paint microwave water lift dried process, finish paint heating cure treatment and finish paint repair color treatment, and lower part is obtained painting workpieces finished product.
The step A carries out the pre-heat treatment using common hot blast;In the step B, the treatment temperature of priming paint levelling treatment
It it is 20 DEG C, one time the treatment temperature of microwave water lift dried process is 30 DEG C, the treatment temperature of priming paint heating cure treatment is 30 DEG C;
In the step C, the treatment temperature of finish paint levelling treatment is 20 DEG C, and the treatment temperature of finish paint heating cure treatment is 30 DEG C.
Embodiment 3
The present embodiment is with the difference of above-described embodiment 1:
In the step B, the treatment temperature of priming paint levelling treatment is 22 DEG C, and the treatment temperature of a microwave water lift dried process is
35 DEG C, the treatment temperature of priming paint heating cure treatment is 32 DEG C;
In the step C, the treatment temperature of finish paint levelling treatment is 22 DEG C, and the treatment temperature of finish paint heating cure treatment is 32
℃。
Embodiment 4
The present embodiment is with the difference of above-described embodiment 1:
In the step B, the treatment temperature of priming paint levelling treatment is 25 DEG C, and the treatment temperature of a microwave water lift dried process is
40 DEG C, the treatment temperature of priming paint heating cure treatment is 35 DEG C;
In the step C, the treatment temperature of finish paint levelling treatment is 25 DEG C, and the treatment temperature of finish paint heating cure treatment is 35
℃。
Embodiment 5
The present embodiment is with the difference of above-described embodiment 1:
In the step B, the treatment temperature of priming paint levelling treatment is 28 DEG C, and the treatment temperature of a microwave water lift dried process is
45 DEG C, the treatment temperature of priming paint heating cure treatment is 38 DEG C;
In the step C, the treatment temperature of finish paint levelling treatment is 28 DEG C, and the treatment temperature of finish paint heating cure treatment is 38
℃。
Embodiment 6
The present embodiment is with the difference of above-described embodiment 1:
In the step B, the treatment temperature of priming paint levelling treatment is 30 DEG C, and the treatment temperature of a microwave water lift dried process is
50 DEG C, the treatment temperature of priming paint heating cure treatment is 40 DEG C;
In the step C, the treatment temperature of finish paint levelling treatment is 30 DEG C, and the treatment temperature of finish paint heating cure treatment is 40
℃。
Above-described embodiment is the present invention preferably implementation, and in addition, the present invention can be realized with other manner,
Any obvious replacement is within protection scope of the present invention on the premise of not departing from present inventive concept.
Claims (10)
1. a kind of industrial spray painting operation system, it is characterised in that:Including be sequentially connected pretreatment system, prime treatment system and
Finish paint processing system;The pretreatment system includes being sequentially connected workpiece upper part mouthful and preheating workshop section;The prime treatment system
Including the basecoat paint station, the first microwave drying workshop section, priming paint polishing station and the second microwave drying workshop section that are sequentially connected;Institute
Under stating finish paint processing system and including the finish paint upper part mouth, finish paint spray station, the 3rd microwave drying workshop section and the finish paint that are sequentially connected
Part mouthful.
2. a kind of industrial spray painting operation system according to claim 1, it is characterised in that:The workpiece upper part mouthful include according to
The first workpiece upper part mouthful and second workpiece upper part mouthful of secondary connection, the input and first work of the second workpiece upper part mouthful
The output end connection of part upper part mouthful, the output end of second workpiece upper part mouthful is connected with the input of the preheating workshop section.
3. a kind of industrial spray painting operation system according to claim 1, it is characterised in that:The basecoat paint station and institute
Stating also includes the first normal temperature levelling workshop section, the input of the first normal temperature levelling workshop section and bottom between the first microwave drying workshop section
The output end connection of spray station is painted, the output end of the first normal temperature levelling workshop section connects with the input of the first microwave drying workshop section
Connect.
4. a kind of industrial spray painting operation system according to claim 1, it is characterised in that:The first microwave drying workshop section
Also include the first heating cure workshop section, the input of the first heating cure workshop section and institute between priming paint polishing station
State the output end connection of the first microwave drying workshop section, the output end of the first heating cure workshop section and the input of priming paint polishing station
Connection.
5. a kind of industrial spray painting operation system according to claim 1, it is characterised in that:Priming paint polishing station and the institute
State and also repair color station including priming paint between the second microwave drying workshop section, the priming paint repaiies the input of color station and the priming paint is beaten
The output end connection of grinder position, the output end that priming paint repaiies color station is connected with the input of the second microwave drying workshop section.
6. a kind of industrial spray painting operation system according to claim 1, it is characterised in that:The second microwave drying workshop section
Priming color grinder position is also included afterwards, and the output end of the second microwave drying workshop section connects with the input of priming color grinder position
Connect.
7. a kind of industrial spray painting operation system according to claim 1, it is characterised in that:The finish paint spray station and institute
Stating also includes the second normal temperature levelling workshop section, the input of the second normal temperature levelling workshop section and institute between the 3rd microwave drying workshop section
The output end connection of finish paint spray station is stated, the output end of the second normal temperature levelling workshop section is defeated with the 3rd microwave drying workshop section
Enter end connection.
8. a kind of industrial paint spraying system according to claim 1, it is characterised in that:The 3rd microwave drying workshop section and institute
State and also include that the second heating cure workshop section being sequentially connected and finish paint repair color station between finish paint lower part mouthful, second heating is solid
The input of chemical industry section is connected with the output end of the 3rd microwave drying workshop section, output end and the face of the second heating cure workshop section
Paint repaiies the input connection of color station, and the output end that finish paint repaiies color station is connected with the input of finish paint lower part mouthful.
9. the industrial lacquer spraying technique of the industrial spray painting operation system described in a kind of application claim 1-8, it is characterised in that:Including
Following steps:
A, the pre-heat treatment:The pre-heat treatment of workpiece will be carried out in each workpiece upper part to be painted to preheating workshop section;
B, prime treatment:Workpiece to be painted after step A the pre-heat treatments is carried out into basecoat paint treatment successively, at priming paint levelling
Reason, microwave water lift dried process, priming paint heating cure treatment, priming paint grinding process, a priming paint are repaiied color treatment, secondary microwave and are carried
Water dried process and priming color mill are processed, and priming paint finished work-piece is obtained;
C, finish paint treatment:By this finished work-piece of priming paint obtained in step B carry out successively finish paint spray treatment, finish paint levelling treatment,
Finish paint microwave water lift dried process, finish paint heating cure treatment and finish paint repair color treatment, and lower part is obtained painting workpieces finished product.
10. a kind of industrial lacquer spraying technique according to claim 9, it is characterised in that:The step A is entered using common hot blast
Row the pre-heat treatment;In the step B, the treatment temperature of priming paint levelling treatment is 20-30 DEG C, microwave water lift dried process
Treatment temperature is 30-50 DEG C, and the treatment temperature of priming paint heating cure treatment is 30-40 DEG C;In the step C, at finish paint levelling
The treatment temperature of reason is 20-30 DEG C, and the treatment temperature of finish paint heating cure treatment is 30-40 DEG C.