CN106818253A - A kind of garden saw - Google Patents
A kind of garden saw Download PDFInfo
- Publication number
- CN106818253A CN106818253A CN201710081051.5A CN201710081051A CN106818253A CN 106818253 A CN106818253 A CN 106818253A CN 201710081051 A CN201710081051 A CN 201710081051A CN 106818253 A CN106818253 A CN 106818253A
- Authority
- CN
- China
- Prior art keywords
- parts
- saw
- handheld division
- antiskid glue
- glue sleeve
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
The present invention discloses a kind of garden saw, including Handheld Division, saw body and saw blade, the Handheld Division includes handle and fixed column, the handle is integrated setting with fixed column, antiskid glue sleeve is arranged with the handle, the end of the fixed column is provided with movable post, the right-hand member of the movable post is provided with nut and is threadedly coupled therewith, the saw body is weldingly fixed on the left end of Handheld Division, the saw body includes the kink of 45 ° of body and downward bending, the left end of the saw blade is fixed with saw body stud, right-hand member is fixed with Handheld Division stud, the antiskid glue sleeve is made up of the material of following weight portion, including rubber powder, water-and acrylate emulsion, hygroscopic heating fibers, acrylic fiber, white carbon, silica flour, talcum powder, pulverized limestone, chlorinated paraffin, aluminium hydroxide, antimony oxide, xylenylphosphate, dimethylbenzene, silicone oil and titanate esters;This kind of garden saw simple structure, it is easy to use, while antiskid glue sleeve has the advantages that soft, anti-skidding and is difficult hardening.
Description
Technical field
The present invention relates to a kind of garden saw.
Background technology
At present, the tree strain of Chinese garden planting is more, therefore many nutrients can be consumed when branch is too big, unnecessary bough
Bar is cut, and will reduce consumption, is conducive to tree to grow tall, in order that ornamental trees are beautiful and clean, it is more good-looking, often will be to trees branch
Bar is pruned, and trees will grow many branches every year in planting process, if do not pruned, unnecessary branch will it is more long more
It is long, it is more long closeer, therefore be frequently necessary to prune branch, when fruit tree catches pest and disease damage, cut off the bough fallen ill
Bar, can reduce the destruction of insect pest, and present people's pollard is particularly larger thicker branch, typically all big with common gardens
Scissors, this gardens shear is not easy to larger, the thicker branch of shearing compared with suitable for shearing thinner branch, if want to cut
Cut larger, thicker branch to have to amputate the branch for wanting to remove with saw, saw blade installs inconvenient in the prior art, so
Brought some inconvenience to gardener author.
Garden saw is a kind of instrument for being usually used in gardens, is mainly used in cutting branch, and existing garden saw includes power saws
With saw manually, the operation principle of power saws is that saw blade of the motor by gear-box drive installation on reciprocating lever moves reciprocatingly,
Reciprocating cutting motion can be done to branch.But when saw blade does with respect to branch and moves back and forth at a high speed, if branch is not fixed,
Frictional force can be such that workpiece is produced with the reciprocating motion of saw blade acutely to shake or wave, so as to bring the inconvenience in cutting.Cause
During gardens tree strain is pruned, people are used mostly manual saw for this.
But, although existing manual garden saw can facilitate being pruned to less tree branch, due to it
Complex structure, is difficult to change saw blade, does not have skidproof effect, have impact on the efficiency of gardens branch pruning.
The content of the invention
In view of this, it is easy to use it is an object of the present invention to provide a kind of simple structure, at the same antiskid glue sleeve have it is soft,
The garden saw of advantage that is anti-skidding and being difficult hardening.
In order to solve the above-mentioned technical problem, the technical scheme is that:
A kind of garden saw, including Handheld Division, saw body and saw blade, the Handheld Division include handle and fixed column, the handle
Setting is integrated with fixed column, antiskid glue sleeve is arranged with the handle, the end of the fixed column is provided with movable post, described
The right-hand member of movable post is provided with nut and is threadedly coupled therewith, and the saw body is weldingly fixed on the left end of Handheld Division, the saw body bag
The kink of 45 ° of body and downward bending is included, left end and the saw body stud of the saw blade are fixed, right-hand member is consolidated with Handheld Division stud
Fixed, the antiskid glue sleeve is made up of the material of following weight portion, including rubber powder 100-130 parts, water-and acrylate emulsion 20-
40 parts, hygroscopic heating fibers 15-23 parts, acrylic fiber 14-20 parts, white carbon 13-17 parts, silica flour 16-20 parts, talcum powder
10-18 parts, pulverized limestone 17-25 parts, chlorinated paraffin 6-10 parts, aluminium hydroxide 10-14 parts, antimony oxide 11-15 parts, di(2-ethylhexyl)phosphate
13-19 parts, dimethylbenzene 5-7 parts, silicone oil 11-17 parts and titanate esters 13-15 parts of toluene ester.
Further, the antiskid glue sleeve is made up of the material of following weight portion, including 130 parts of rubber powder, aqueous acrylamide
20 parts of acid esters emulsion, 15 parts of hygroscopic heating fibers, 14 parts of acrylic fiber, 13 parts of white carbon, 16 parts of silica flour, 10 parts of talcum powder,
17 parts of pulverized limestone, 6 parts of chlorinated paraffin, 10 parts of aluminium hydroxide, 11 parts of antimony oxide, 13 parts of xylenylphosphate, dimethylbenzene 5
13 parts of part, 11 parts of silicone oil and titanate esters.
Further, the antiskid glue sleeve is made up of the material of following weight portion, including 100 parts of rubber powder, aqueous acrylamide
40 parts of acid esters emulsion, 23 parts of hygroscopic heating fibers, 20 parts of acrylic fiber, 17 parts of white carbon, 20 parts of silica flour, 18 parts of talcum powder,
25 parts of pulverized limestone, 10 parts of chlorinated paraffin, 14 parts of aluminium hydroxide, 15 parts of antimony oxide, 19 parts of xylenylphosphate, dimethylbenzene 7
15 parts of part, 17 parts of silicone oil and titanate esters.
Further, the antiskid glue sleeve is made up of the material of following weight portion, including 115 parts of rubber powder, aqueous acrylamide
30 parts of acid esters emulsion, 19 parts of hygroscopic heating fibers, 17 parts of acrylic fiber, 15 parts of white carbon, 18 parts of silica flour, 14 parts of talcum powder,
21 parts of pulverized limestone, 8 parts of chlorinated paraffin, 12 parts of aluminium hydroxide, 13 parts of antimony oxide, 16 parts of xylenylphosphate, dimethylbenzene 6
14 parts of part, 14 parts of silicone oil and titanate esters.
The invention solves the problems that another technical problem be that a kind of preparation method of antiskid glue sleeve is provided, comprise the following steps:
1) rubber powder 100-130 parts is taken, 20-40 parts and dimethylbenzene 5-7 parts of water-and acrylate emulsion is put into banbury
Mixing, speed change refining is carried out by 160-220 DEG C of temperature, and mixed glue solution is obtained, standby;
2) white carbon 13-17 parts, silica flour 16-20 parts, talcum powder 10-18 parts and pulverized limestone 17-25 parts is taken by simple
Mixing, the filler that then will be mixed to get ground 2-3 times repeatedly with grinder so that filler is made powder, then will
Powdered filler carries out sub-sieve by the screen cloth of 50 mesh, collects the powder below 50 mesh, standby;
3) by step 2) obtained in pulverulent filler be put into mixer, then compare 1 by the weight with pulverulent filler:2
Addition water, while starting mixer, is mixed powder filler with water with the rotating speed of 60r/min, and slurries are obtained, standby;
4) by step 3) obtained in slurries and chlorinated paraffin 6-10 parts, aluminium hydroxide 10-14 parts, antimony oxide 11-
15 parts, xylenylphosphate 13-19 parts, silicone oil 11-17 parts and titanate esters 13-15 parts are added to step 1) obtained in compound
It is interior, then drive banbury inversely to plasticate, the temperature of banbury is controlled for 200-240 DEG C, and the rotating speed of banbury is 30r/
Min, refined so that slurry is well mixed with compound by the high temperature of 10 minutes, and elastomeric compound is obtained, standby;
5) hygroscopic heating fibers 15-23 parts and acrylic fiber 14-20 part are taken by the prepared fiber mesh cloth of braider, and by fibre
Dimension screen cloth is cut into suitable length and width, and embryo cloth is obtained, standby;
6) dumping mouthful of banbury is connected with the feeding mouth of extruder, the elastomeric compound in banbury is defeated to extruder
It is interior, elastomeric compound is carried out by extruder then to be expressed into embryo cloth, cooling is then stood, gum cover blank is obtained, it is standby;
7) by step 6) surface of obtained gum cover blank carries out hot pressing after cooling so that and the surface of gum cover blank forms anti-
Sliding line, obtains final product.
The technology of the present invention effect major embodiment is in the following areas:Due to garden saw simple structure, saw blade can be convenient for changing,
Simultaneously by rubber powder, water-and acrylate emulsion, hygroscopic heating fibers, acrylic fiber, white carbon, silica flour, talcum powder, lime
Powder, chlorinated paraffin, aluminium hydroxide, antimony oxide, xylenylphosphate, dimethylbenzene, silicone oil and skid-proof rubber obtained in titanate esters
Set, can not only reduce the rubber sleeve caused by perspiration influences the use of garden saw, while antiskid glue sleeve is hard using being difficult in long-time
Change.
Brief description of the drawings
Fig. 1 is a kind of overall structure diagram of garden saw of the invention;
Fig. 2 is the stud and nut structure figure of a kind of garden saw of the invention.
Specific embodiment
Below in conjunction with accompanying drawing 1-2, specific embodiment of the invention is described in further detail, so that technical solution of the present invention
It is more readily understood and grasps.
Embodiment 1
A kind of garden saw, including Handheld Division 1, saw body 2 and saw blade 3, the Handheld Division 1 include handle 4 and fixed column 6, institute
State handle 4 and be integrated setting with fixed column 6, antiskid glue sleeve 5 is arranged with the handle 4, do not changed hands when user-friendly
Sliding, the end of the fixed column 6 is provided with movable post 7, and the right-hand member of the movable post 7 is provided with nut 8 and is threadedly coupled therewith, energy
Enough that saw blade 3 is securely fixed on Handheld Division 1 and saw body 2, the saw body 2 is weldingly fixed on the left end of Handheld Division 1, the saw
Body 2 includes the kink of 45 ° of body and downward bending, and left end and the stud of saw body 2 of the saw blade 3 are fixed, right-hand member and Handheld Division 1
Stud is fixed, and the antiskid glue sleeve 5 is made up of the material of following weight portion, including 130 parts of rubber powder, water-and acrylate emulsion
20 parts, 15 parts of hygroscopic heating fibers, 14 parts of acrylic fiber, 13 parts of white carbon, 16 parts of silica flour, 10 parts of talcum powder, pulverized limestone 17
Part, 6 parts of chlorinated paraffin, 10 parts of aluminium hydroxide, 11 parts of antimony oxide, 13 parts of xylenylphosphate, 5 parts of dimethylbenzene, silicone oil 11
13 parts of part and titanate esters.
A kind of preparation method of antiskid glue sleeve, comprises the following steps:
1) 5 parts of 130 parts of rubber powder, 20 parts of water-and acrylate emulsion and dimethylbenzene are taken and is put into mixing in banbury, passed through
160 DEG C of temperature carries out speed change refining, and mixed glue solution is obtained, standby;
2) 17 parts of 13 parts of white carbon, 16 parts of silica flour, 10 parts of talcum powder and pulverized limestone are taken by simple mixing, then will
The filler being mixed to get is ground 2 times repeatedly with grinder so that filler is made powder, then passes through powdered filler
The screen cloth of 50 mesh carries out sub-sieve, collects the powder below 50 mesh, standby;
3) by step 2) obtained in pulverulent filler be put into mixer, then compare 1 by the weight with pulverulent filler:2
Addition water, while starting mixer, is mixed powder filler with water with the rotating speed of 60r/min, and slurries are obtained, standby;
4) by step 3) obtained in slurries and 6 parts of chlorinated paraffin, 10 parts of aluminium hydroxide, 11 parts of antimony oxide, phosphoric acid
13 parts of 13 parts of diformazan phenyl ester, 11 parts of silicone oil and titanate esters are added to step 1) obtained in compound, then drive banbury inverse
To plasticating, the temperature of banbury is controlled for 200 DEG C, and the rotating speed of banbury is 30r/min, is refined by the high temperature of 10 minutes,
So that slurry is well mixed with compound, elastomeric compound is obtained, it is standby;
5) 14 parts of 15 parts of hygroscopic heating fibers and acrylic fiber are taken fiber mesh cloth is obtained by braider, and by fiber mesh cloth
Suitable length and width are cut into, embryo cloth is obtained, it is standby;
6) dumping mouthful of banbury is connected with the feeding mouth of extruder, the elastomeric compound in banbury is defeated to extruder
It is interior, elastomeric compound is carried out by extruder then to be expressed into embryo cloth, cooling is then stood, gum cover blank is obtained, it is standby;
7) by step 6) surface of obtained gum cover blank carries out hot pressing after cooling so that and the surface of gum cover blank forms anti-
Sliding line, obtains final product.
Embodiment 2
A kind of garden saw, including Handheld Division 1, saw body 2 and saw blade 3, the Handheld Division 1 include handle 4 and fixed column 6, institute
State handle 4 and be integrated setting with fixed column 6, antiskid glue sleeve 5 is arranged with the handle 4, do not changed hands when user-friendly
Sliding, the end of the fixed column 6 is provided with movable post 7, and the right-hand member of the movable post 7 is provided with nut 8 and is threadedly coupled therewith, energy
Enough that saw blade 3 is securely fixed on Handheld Division 1 and saw body 2, the saw body 2 is weldingly fixed on the left end of Handheld Division 1, the saw
Body 2 includes the kink of 45 ° of body and downward bending, and left end and the stud of saw body 2 of the saw blade 3 are fixed, right-hand member and Handheld Division 1
Stud is fixed, and the antiskid glue sleeve 5 is made up of the material of following weight portion, including 100 parts of rubber powder, water-and acrylate emulsion
40 parts, 23 parts of hygroscopic heating fibers, 20 parts of acrylic fiber, 17 parts of white carbon, 20 parts of silica flour, 18 parts of talcum powder, pulverized limestone 25
Part, 10 parts of chlorinated paraffin, 14 parts of aluminium hydroxide, 15 parts of antimony oxide, 19 parts of xylenylphosphate, 7 parts of dimethylbenzene, silicone oil 17
15 parts of part and titanate esters.
A kind of preparation method of antiskid glue sleeve, comprises the following steps:
1) 7 parts of 100 parts of rubber powder, 40 parts of water-and acrylate emulsion and dimethylbenzene are taken and is put into mixing in banbury, passed through
220 DEG C of temperature carries out speed change refining, and mixed glue solution is obtained, standby;
2) 25 parts of 17 parts of white carbon, 20 parts of silica flour, 18 parts of talcum powder and pulverized limestone are taken by simple mixing, then will
The filler being mixed to get is ground 3 times repeatedly with grinder so that filler is made powder, then passes through powdered filler
The screen cloth of 50 mesh carries out sub-sieve, collects the powder below 50 mesh, standby;
3) by step 2) obtained in pulverulent filler be put into mixer, then compare 1 by the weight with pulverulent filler:2
Addition water, while starting mixer, is mixed powder filler with water with the rotating speed of 60r/min, and slurries are obtained, standby;
4) by step 3) obtained in slurries and 10 parts of chlorinated paraffin, 14 parts of aluminium hydroxide, 15 parts of antimony oxide, phosphoric acid
15 parts of 19 parts of diformazan phenyl ester, 17 parts of silicone oil and titanate esters are added to step 1) obtained in compound, then drive banbury inverse
To plasticating, the temperature of banbury is controlled for 240 DEG C, and the rotating speed of banbury is 30r/min, is refined by the high temperature of 10 minutes,
So that slurry is well mixed with compound, elastomeric compound is obtained, it is standby;
5) 20 parts of 23 parts of hygroscopic heating fibers and acrylic fiber are taken fiber mesh cloth is obtained by braider, and by fiber mesh cloth
Suitable length and width are cut into, embryo cloth is obtained, it is standby;
6) dumping mouthful of banbury is connected with the feeding mouth of extruder, the elastomeric compound in banbury is defeated to extruder
It is interior, elastomeric compound is carried out by extruder then to be expressed into embryo cloth, cooling is then stood, gum cover blank is obtained, it is standby;
7) by step 6) surface of obtained gum cover blank carries out hot pressing after cooling so that and the surface of gum cover blank forms anti-
Sliding line, obtains final product.
Embodiment 3
A kind of garden saw, including Handheld Division 1, saw body 2 and saw blade 3, the Handheld Division 1 include handle 4 and fixed column 6, institute
State handle 4 and be integrated setting with fixed column 6, antiskid glue sleeve 5 is arranged with the handle 4, do not changed hands when user-friendly
Sliding, the end of the fixed column 6 is provided with movable post 7, and the right-hand member of the movable post 7 is provided with nut 8 and is threadedly coupled therewith, energy
Enough that saw blade 3 is securely fixed on Handheld Division 1 and saw body 2, the saw body 2 is weldingly fixed on the left end of Handheld Division 1, the saw
Body 2 includes the kink of 45 ° of body and downward bending, and left end and the stud of saw body 2 of the saw blade 3 are fixed, right-hand member and Handheld Division 1
Stud is fixed, and the antiskid glue sleeve 5 is made up of the material of following weight portion, including 115 parts of rubber powder, water-and acrylate emulsion
30 parts, 19 parts of hygroscopic heating fibers, 17 parts of acrylic fiber, 15 parts of white carbon, 18 parts of silica flour, 14 parts of talcum powder, pulverized limestone 21
Part, 8 parts of chlorinated paraffin, 12 parts of aluminium hydroxide, 13 parts of antimony oxide, 16 parts of xylenylphosphate, 6 parts of dimethylbenzene, silicone oil 14
14 parts of part and titanate esters.
A kind of preparation method of antiskid glue sleeve, comprises the following steps:
1) 6 parts of 115 parts of rubber powder, 30 parts of water-and acrylate emulsion and dimethylbenzene are taken and is put into mixing in banbury, passed through
190 DEG C of temperature carries out speed change refining, and mixed glue solution is obtained, standby;
2) 21 parts of 15 parts of white carbon, 18 parts of silica flour, 14 parts of talcum powder and pulverized limestone are taken by simple mixing, then will
The filler being mixed to get is ground 3 times repeatedly with grinder so that filler is made powder, then passes through powdered filler
The screen cloth of 50 mesh carries out sub-sieve, collects the powder below 50 mesh, standby;
3) by step 2) obtained in pulverulent filler be put into mixer, then compare 1 by the weight with pulverulent filler:2
Addition water, while starting mixer, is mixed powder filler with water with the rotating speed of 60r/min, and slurries are obtained, standby;
4) by step 3) obtained in slurries and 8 parts of chlorinated paraffin, 12 parts of aluminium hydroxide, 13 parts of antimony oxide, phosphoric acid
14 parts of 16 parts of diformazan phenyl ester, 14 parts of silicone oil and titanate esters are added to step 1) obtained in compound, then drive banbury inverse
To plasticating, the temperature of banbury is controlled for 220 DEG C, and the rotating speed of banbury is 30r/min, is refined by the high temperature of 10 minutes,
So that slurry is well mixed with compound, elastomeric compound is obtained, it is standby;
5) 17 parts of 19 parts of hygroscopic heating fibers and acrylic fiber are taken fiber mesh cloth is obtained by braider, and by fiber mesh cloth
Suitable length and width are cut into, embryo cloth is obtained, it is standby;
6) dumping mouthful of banbury is connected with the feeding mouth of extruder, the elastomeric compound in banbury is defeated to extruder
It is interior, elastomeric compound is carried out by extruder then to be expressed into embryo cloth, cooling is then stood, gum cover blank is obtained, it is standby;
7) by step 6) surface of obtained gum cover blank carries out hot pressing after cooling so that and the surface of gum cover blank forms anti-
Sliding line, obtains final product.
Experimental example
Experimental subjects:Using propylene is fine, the plastics that are made of polytrifluorochloroethylene, polytetrafluoroethylene (PTFE), PPSU and polyamide
Set is contrasted with the antiskid glue sleeve of the application.
Requirement of experiment:The modeling that above-mentioned propylene is fine, polytrifluorochloroethylene, polytetrafluoroethylene (PTFE), PPSU and polyamide are made
The consistency of thickness of the antiskid glue sleeve of material set and the application, and area is consistent.
Experimental technique:By to propylene is fine, the modeling that is made of polytrifluorochloroethylene, polytetrafluoroethylene (PTFE), PPSU and polyamide
The skid-proof rubber jacking of material set and the application carries out the modulus of elasticity in static bending, shrinkage factor test and durability degree test, in this experimental example
In, durability degree test includes the test such as ageing-resistant performance, heat-resisting and resistance to low temperature.
Concrete outcome is as shown in the table:
With reference to upper table, the data of different rubber gained under identical experimental technique are contrasted, one kind of the invention is anti-skidding
The test data of gum cover is above the various plastic sheaths for contrasting, therefore, embody antiskid glue sleeve intensity of the invention greatly, no
Easy aging and good weatherability, performance is more stablized.
The technology of the present invention effect major embodiment is in the following areas:Due to garden saw simple structure, saw blade can be convenient for changing,
Simultaneously by rubber powder, water-and acrylate emulsion, hygroscopic heating fibers, acrylic fiber, white carbon, silica flour, talcum powder, lime
Powder, chlorinated paraffin, aluminium hydroxide, antimony oxide, xylenylphosphate, dimethylbenzene, silicone oil and skid-proof rubber obtained in titanate esters
Set, can not only reduce the rubber sleeve caused by perspiration influences the use of garden saw, while antiskid glue sleeve is hard using being difficult in long-time
Change.
Certainly, it is more than representative instance of the invention, in addition, the present invention can also have other various specific implementations
The technical scheme that mode, all use equivalents or equivalent transformation are formed, all falls within the scope of protection of present invention.
Claims (4)
1. a kind of garden saw, including Handheld Division, saw body and saw blade, the Handheld Division include handle and fixed column, the handle with
Fixed column is integrated setting, and antiskid glue sleeve is arranged with the handle, and the end of the fixed column is provided with movable post, the work
The right-hand member of dynamic post is provided with nut and is threadedly coupled therewith, and the saw body is weldingly fixed on the left end of Handheld Division, and the saw body includes
The kink of 45 ° of body and downward bending, left end and the saw body stud of the saw blade are fixed, and right-hand member is fixed with Handheld Division stud,
It is characterized in that:The antiskid glue sleeve is made up of the material of following weight portion, including rubber powder 100-130 parts, water soluble acrylic acid
20-40 parts of ester emulsion, hygroscopic heating fibers 15-23 parts, acrylic fiber 14-20 parts, white carbon 13-17 parts, silica flour 16-20
Part, talcum powder 10-18 parts, pulverized limestone 17-25 parts, chlorinated paraffin 6-10 parts, aluminium hydroxide 10-14 parts, antimony oxide 11-15
Part, xylenylphosphate 13-19 parts, dimethylbenzene 5-7 parts, silicone oil 11-17 parts and titanate esters 13-15 parts.
2. a kind of garden saw as claimed in claim 1, it is characterised in that:The antiskid glue sleeve by following weight portion material system
Into, including 130 parts of rubber powder, 20 parts of water-and acrylate emulsion, 15 parts of hygroscopic heating fibers, 14 parts of acrylic fiber, white carbon
13 parts, 16 parts of silica flour, 10 parts of talcum powder, 17 parts of pulverized limestone, 6 parts of chlorinated paraffin, 10 parts of aluminium hydroxide, antimony oxide 11
Part, 13 parts of xylenylphosphate, 5 parts of dimethylbenzene, 11 parts of silicone oil and 13 parts of titanate esters.
3. a kind of garden saw as claimed in claim 1, it is characterised in that:The antiskid glue sleeve by following weight portion material system
Into, including 100 parts of rubber powder, 40 parts of water-and acrylate emulsion, 23 parts of hygroscopic heating fibers, 20 parts of acrylic fiber, white carbon
17 parts, 20 parts of silica flour, 18 parts of talcum powder, 25 parts of pulverized limestone, 10 parts of chlorinated paraffin, 14 parts of aluminium hydroxide, antimony oxide 15
Part, 19 parts of xylenylphosphate, 7 parts of dimethylbenzene, 17 parts of silicone oil and 15 parts of titanate esters.
4. a kind of garden saw as claimed in claim 1, it is characterised in that:The antiskid glue sleeve by following weight portion material system
Into, including 115 parts of rubber powder, 30 parts of water-and acrylate emulsion, 19 parts of hygroscopic heating fibers, 17 parts of acrylic fiber, white carbon
15 parts, 18 parts of silica flour, 14 parts of talcum powder, 21 parts of pulverized limestone, 8 parts of chlorinated paraffin, 12 parts of aluminium hydroxide, antimony oxide 13
Part, 16 parts of xylenylphosphate, 6 parts of dimethylbenzene, 14 parts of silicone oil and 14 parts of titanate esters.