CN106564100A - Gluing method for solid combined cylinder and products thereof - Google Patents
Gluing method for solid combined cylinder and products thereof Download PDFInfo
- Publication number
- CN106564100A CN106564100A CN201610986280.7A CN201610986280A CN106564100A CN 106564100 A CN106564100 A CN 106564100A CN 201610986280 A CN201610986280 A CN 201610986280A CN 106564100 A CN106564100 A CN 106564100A
- Authority
- CN
- China
- Prior art keywords
- length
- square column
- cylinder
- arc
- integrated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a gluing method for solid combined cylinders and products thereof. The gluing method comprises the following steps that the diameter and height of the solid combined cylinder are determined according to requirements; the size and length of a middle square pillar and the number and length of integrated arc-shaped unit bodies are determined according to the diameter and height of the solid combined cylinder; the number of layers and size of laminated plates for being combined into an integrated plate are chosen according to the determined size and length of the middle square pillar and the determined number and length of the integrated arc-shaped unit bodies, the length of the laminated plates is equal to the length of the integrated arc-shaped unit bodies, the chosen laminated plates are coated with an adhesive for gluing, then pressurization, solidification and aging are conducted, and thus the integrated plate is obtained; polishing and milling are conducted on the integrated plate, so that the multiple arc-shaped unit bodies are obtained, and then the multiple arc-shaped unit bodies are combined with the middle square pillar for forming a circle, so that the required solid cylinder is obtained.
Description
Technical field
The present invention relates to a kind of gluing method of cylinder, more particularly to a kind of gluing method of solid cylinder, belong to building
Technical field.
Background technology
Timber is a kind of graceful natural material of fine quality, sense organ, with beautiful decorative pattern, gloss and color, size
It is stable, the ratio of strength to weight is high, easy to process, the advantages of be easy to maintenance, become one of widest raw material of purposes, by every profession and trade green grass or young crops
Look at, with the development and people's living standard continuous improvement of national economy, the demand of timber is increasingly increased.
At present, China's Forest Resources add denudation and the guarantor in later stage of wildwood resource early stage with, based on small dimension wood
Shield, timber supply and demand contradiction are serious, and especially the big footpath level timber resources of high-quality is deficient.Meanwhile, for the protection to wildwood, country
The pressure of the demand of interests and International Environmental Protection tissue, timber export state go into overdrive to protect the national forest reserves, limit and
Reduce big footpath level, the outlet of precious timber.
So, the characteristics of domestic wood supply it is:Small dimension wood is more, and big-diameter wood is little;Low-quality material is more, and good material is few.And build
Industry often needs the column of big footpath level again, is to solve this contradiction, starts to occur in that integrated timber on market, and integrated timber is exactly to use sheet material
Or scantlings press the parallel direction of the wood fiber, in the timber-work of thickness, width and length direction gluing, integrated timber can profit
With thinnings, small dimension wood and processing clout, it is to save timber to improve one of effective means of timber utilization rate.
The content of the invention
The present invention is directed to the deficiency such as little existing cylindrical material footpath level, length limited, easy to crack, there is provided a kind of solid combination cylinder
Gluing method and products thereof.
The technical scheme that the present invention solves above-mentioned technical problem is as follows:
A kind of gluing method of solid combination cylinder, it is characterised in that comprise the steps:
1) diameter and height of solid combination cylinder are determined as requested;
2) according to step 1) solid combination cylinder diameter and height determine in the middle of the size of square column, length and arc
Length of the length of the size of integrated unit body, length, the square column and arc cell cube for solid cylinder;
3) according to step 2) determined by the length of square column and arc cell cube, size Selection synthesize the laminate of integrated sheet material
The number of plies and size, the length of laminate is the length of square column and integrated unit body, and the laminate coated with adhesive for choosing is entered
Row bonding, then carries out pressurizeing, solidifies, display and obtain integrated sheet material;
4) to step 3) in gained integrated timber carry out scraping, the processing of milling type, obtain square column and the outer face of any surface finish
For several cell cubes of circular arc, but the outer face of cell cube can be spliced into circle, inner face can be spliced into rectangle and side that
This is spliced to form cylinder;
5) by step 4) in gained square column, some arc cell cubes spliced, circular arc outer end faces outwardly, unit side
Face is spliced each other, interior junction and square column carry out splicing to obtain solid combination cylinder.
Further, there is an angle for 90 ° and two sides with two angles of circular arc opposite side in the cell cube
Length, depending on the parameter with specific reference to the diameter and process equipment of solid cylinder.
Further, step 3) in the number of integrated unit body be at least 4.
Further, step 3) number of plies of la m is at least 5 layers, with specific reference to the thickness and solid cylinder of material plate
Radius determines.
The beneficial effect of method that the present invention is provided is:
1) utilization small diameter grade timber that can be effective and reasonable, produces big footpath level cylinder, improves the extra price of small diameter grade timber
Value;
2) integrated processing, is effectively reduced cracking and the deformation of cylinder;
3) the footpath level of cylinder obtained by is larger, uniform specification, attractive in appearance, and can mass production;
4) concentric reducer of log is solved, the problem of length limited can carry out any spreading as needed;
5) integrated optimization, the cylinder good stability of the dimension of gained, intensity are high.
The present invention is also claimed the product obtained by said method.
Description of the drawings
Fig. 1 square column structure schematic diagrams used by the present invention;
Fig. 2 is arc Unit agent structure schematic diagram used by embodiment 1;
Fig. 3 is 2 unit therefor body structural representation of embodiment;
Fig. 4 is 3 unit therefor body structural representation of embodiment;
Fig. 5 is 1 gained solid cylinder structural representation of embodiment;
Fig. 6 is 2 gained solid cylinder structural representation of embodiment;
Fig. 7 is 3 gained solid cylinder structural representation of embodiment;
In Fig. 1~7,1, square column;2nd, cell cube;3rd, solid cylinder.
Specific embodiment
The principle and feature of the present invention are described below in conjunction with example, example is served only for explaining the present invention, and
It is non-for limiting the scope of the present invention.
Embodiment 1:
As a example by producing a diameter of 450mm, the arbitrary cylinder of length, the size that is combined into of middle square column 1 is 200*200mm,
The size of material plate is 42*205mm, and 5 blocks of sheet materials of middle square column need carry out applying glue spelling and are pressed into 210*205mm, then scrape into
Required sectional dimension 200*200mm (as shown in Figure 1);Cell cube 2 needs the sheet material applying glue spelling of 3 pieces of 42*160mm to be pressed into square
Tee section timber 126*160mm, the arc cell cube required for being then processed into by four-side planing type, wherein being right angle
90 ° (as shown in Figure 2), the long 125mm of two side a lines that right angle is located, another length of side 100mm, the radian of circular arc is 45 °,
The length of circular arc is 176.625mm;Then applying glue, spells circle square column and 8 cell cube combinations, and the cylinder 3 required for obtaining is (such as
Shown in Fig. 5).
Embodiment 2:
As a example by producing a diameter of 450mm, the arbitrary cylinder of length, the size that is combined into of middle square column 1 is 200*200mm,
The size of material plate is 42*205mm, and 5 blocks of sheet materials of middle square column need carry out applying glue spelling and are pressed into 210*205mm, then scrape into
Required sectional dimension 200*200mm (as shown in Figure 1);Cell cube 2 needs the sheet material applying glue spelling of 3 pieces of 42*320mm to be pressed into square
Tee section timber 126*320mm, the cell cube (as shown in Figure 3) required for being then processed into by four-side planing type, arc list
The radian of first body 2 is 90 °, is highly 125mm, and two length of sides are respectively 83.6mm, then applying glue, square column and 4 cell cubes
Circle is spelled in combination, the cylinder 3 (as shown in Figure 6) required for obtaining.
Embodiment 3:
As a example by producing the arbitrary cylinder of a diameter of 350mm length, the size that is combined into of middle square column 1 is 200*200mm, former
The size of flitch material is 42*245mm, and 5 blocks of sheet materials of middle square column need carry out applying glue and spell pressure, then scrape into required section chi
Very little 200*200mm (as shown in Figure 1);Cell cube 2 needs the sheet material applying glue spelling of 2 pieces of 42*245mm to be pressed into square-section timber 84*
245mm, is then processed into required cell cube (as shown in Figure 4) by four-side planing type, and the radian of arc cell cube is
90 °, arc length is 274.75mm, and cell cube is highly 75mm, and base length is 243.6mm;Then applying glue, square column and 4
Circle is spelled in individual arc cell cube combination, the cylinder 3 (as shown in Figure 7) required for obtaining.
The foregoing is only presently preferred embodiments of the present invention, not to limit the present invention, all spirit in the present invention and
Within principle, any modification, equivalent substitution and improvements made etc. should be included within the scope of the present invention.
Claims (5)
1. a kind of gluing method of solid combination cylinder, it is characterised in that comprise the steps:
1) diameter and height of solid combination cylinder are determined as requested;
2) according to step 1) solid combination cylinder diameter and height determine in the middle of the size of square column, length and collection camber
Length of the length of the size of cell cube, length, the square column and arc cell cube for solid cylinder;
3) according to step 2) determined by the length of square column and arc cell cube, size Selection synthesize integrated sheet material laminate layer
Number and size, the length of laminate are the length of square column and integrated unit body, and the laminate coated with adhesive for choosing is glued
Knot, then carries out pressurizeing, solidifies, display and obtain integrated timber;
4) to step 3) in gained integrated timber carry out scraping, the processing of milling type, the square column and outer face for obtaining any surface finish is arc
Several cell cubes of shape, the outer face of cell cube can be spliced into that circle, inner face can be spliced into rectangle and side can be spelled each other
Connect to form cylinder;
5) by step 4) in gained square column, some arc cell cubes spliced, circular arc outer end faces outwardly, unit body side surface that
This splicing, interior junction and square column carry out splicing to obtain solid combination cylinder.
2. the gluing method of solid combination cylinder according to claim 1, it is characterised in that with circular arc in the cell cube
There is an angle in two angles of opposite side for 90 ° and two side edge lengths.
3. the gluing method of solid combination cylinder according to claim 1, it is characterised in that the step 3) in integrated list
The number of first body is at least 4.
4. the gluing method of solid combination cylinder according to claim 1, it is characterised in that step 3) la m the number of plies
It is at least 5 layers.
5. the solid combination cylinder obtained by the gluing method any one of Claims 1 to 4.