CN106514069A - Device inhibiting welding defects of small-diameter aluminum alloy guiding pipe - Google Patents

Device inhibiting welding defects of small-diameter aluminum alloy guiding pipe Download PDF

Info

Publication number
CN106514069A
CN106514069A CN201611108072.3A CN201611108072A CN106514069A CN 106514069 A CN106514069 A CN 106514069A CN 201611108072 A CN201611108072 A CN 201611108072A CN 106514069 A CN106514069 A CN 106514069A
Authority
CN
China
Prior art keywords
aluminum alloy
diameter aluminum
inner support
minor diameter
suppressing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201611108072.3A
Other languages
Chinese (zh)
Inventor
贾洪德
杨修东
贺斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Aerospace Equipments Manufacturer Co Ltd
Original Assignee
Shanghai Aerospace Equipments Manufacturer Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Aerospace Equipments Manufacturer Co Ltd filed Critical Shanghai Aerospace Equipments Manufacturer Co Ltd
Priority to CN201611108072.3A priority Critical patent/CN106514069A/en
Publication of CN106514069A publication Critical patent/CN106514069A/en
Pending legal-status Critical Current

Abstract

The invention provides a device inhibiting welding defects of a small-diameter aluminum alloy guiding pipe. The device inhibiting the welding defects of the small-diameter aluminum alloy guiding pipe can be applied to welding of small-diameter aluminum alloy guiding pipes of a spacecraft or in other fields.

Description

A kind of device for suppressing minor diameter aluminum alloy conduit weld defect
Technical field
The present invention relates to a kind of auxiliary welding equipment, in particular, it is related to a kind of suppression minor diameter aluminum alloy conduit The device of weld defect.
Background technology
Minor diameter aluminum alloy conduit is generally light-wall pipe, the method that argon tungsten-arc welding is adopted its butt welding more.Due to size Limit, the typically no support in workpiece back, while welding condition scope is narrower, therefore easily form weld blowhole, lack of penetration With the defect such as misalignment.
The content of the invention
The present invention will improve minor diameter aluminum alloy conduit assemble welding, increase welding condition scope, suppress welding to lack Fall into and occur.
It is critical only that for the present invention increase inner support in conduit welding position.
The material for making inner support is the fluorine-containing activating agent that aluminum alloy melting weldering can be used;The general ratio of inner support diameter is led The little 0.1-0.3mm of bore, is advisable with being positioned over formation tight fit during guide pipe inner hole;The thickness of inner support is greater than weld seam width Degree, is advisable with 4-5mm;Immediately below conduit docking location, whole circle circular arc weldering bakie is opened up on inner support is cylindrical, bakie width is welded Degree is not more than 0.5mm less than weld width 1-2mm, depth;Open up on inner support is cylindrical several gas vents connection weldering bakies with The external world, gas vent are circumferentially generally 1mm or so, are radially not more than 0.5mm.
The inner support as made by above-mentioned condition, in assemble welding pair in be placed in catheter interior, can fit in welding process Work as high current, in making the uniform heavy bakie with weldering of weldering leakage.Can be carried out using the method such as solid, liquid, gas pair of interior support after the completion of welding Cleaning.
The beneficial effects of the present invention is:
1) increased inner support to improve assembling effect, reduce misalignment defect and produce to being increased constraint by weldering conduit.
2) weldering bakie is formed with inner support, molten metal can be formed and be supported, therefore electricity can be suitably increased when welding Stream, contributes to the gas effusion in molten bath, reduces the generation of gas hole defect, while the formation for welding leakage can reduce incomplete penetration defect Generation.
3) inner support is made up of the fluorine-containing activating agent that Welded can be used, and the metal that high temperature is contacted during welding melts Liquid, can be reacted with hydrogen therein and form hydrogen fluoride discharge, contribute to eliminating weld blowhole.
4) inner support weldering bakie is provided with gas vent, discharges can the gas that heated up by weld heating in weldering bakie, just Well shape in weld seam back.
Description of the drawings
Fig. 1 is that a kind of operation principle of the device of suppression minor diameter aluminum alloy conduit weld defect that the present invention is provided is illustrated Figure.
Fig. 2 is a kind of schematic cross-section of the device of suppression minor diameter aluminum alloy conduit weld defect that the present invention is provided.
Specific embodiment
Embodiment of the present invention is illustrated below in conjunction with the accompanying drawings, in accompanying drawing 1:1 be conduit A, 2 be conduit B, 3 be inner support, 4 To weld bakie, 5 is gas vent.
Specific embodiment is as follows:
1) activating agent that can be used using Welded makes the inner support 3 in accompanying drawing 1, and diameter is typically little than catheter diameter 0.1-0.3mm;Width is more than weld width 4-5mm;4 width of weldering bakie is less than weld width 1-2mm, and depth is not more than 0.5mm, For circular arc;Open up gas vent 5 some, gas vent 5 is circumferential to be generally 1mm or so, is radially not more than 0.5mm.
2) conduit A1 and conduit B2 interfaces make perpendicular cuts face, and conduit A1, conduit B2 and inner support 3 are pressed accompanying drawing 1 Shown centered assembling.
3) preliminary filling protective gas inside dummy pipe is welded, then starts welding.
4) inner support 3 is removed after the completion of welding, the method such as solid, liquid, gas may be used individually or jointly during removing, is removed Method is illustrated:As hard thing is tapped, gases at high pressure, liquid extrusion etc..
After removing inner support 3, as needed catheter interior is cleared up.

Claims (5)

1. a kind of device for suppressing minor diameter aluminum alloy conduit weld defect, it is characterised in that described device is and guide pipe inner hole Close-fitting inner support is formed, whole lap welding bakie is opened up on the inner support is cylindrical, be further opened with the inner support is cylindrical Several gas vents, the gas vent connect the weldering bakie.
2. a kind of as described in claim 1 device for suppressing minor diameter aluminum alloy conduit weld defect, it is characterised in that institute State inner support to be made up of the fluorine-containing activating agent that can be used for aluminum alloy melting weldering.
3. a kind of as described in claim 2 device for suppressing minor diameter aluminum alloy conduit weld defect, it is characterised in that institute The thickness for stating inner support is more than weld width.
4. a kind of as described in claim 1 device for suppressing minor diameter aluminum alloy conduit weld defect, it is characterised in that institute State weldering bakie width and be less than weld width.
5. a kind of as described in claim 1 device for suppressing minor diameter aluminum alloy conduit weld defect, it is characterised in that institute It is circular arc to state weldering bakie.
CN201611108072.3A 2016-12-06 2016-12-06 Device inhibiting welding defects of small-diameter aluminum alloy guiding pipe Pending CN106514069A (en)