CN106480715A - A kind of weaving rust remover and preparation method thereof - Google Patents
A kind of weaving rust remover and preparation method thereof Download PDFInfo
- Publication number
- CN106480715A CN106480715A CN201510545318.2A CN201510545318A CN106480715A CN 106480715 A CN106480715 A CN 106480715A CN 201510545318 A CN201510545318 A CN 201510545318A CN 106480715 A CN106480715 A CN 106480715A
- Authority
- CN
- China
- Prior art keywords
- textile
- deionized water
- mixed
- acid
- mass fraction
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a kind of textile rust remover and preparation method thereof, is made up of oxalic acid, citric acid, acetic acid, natrium nitrosum, alcoxylates, ammonium hydrogen carbonate, ammonium benzoate, second methylcellulose, tertiary sodium phosphate, triethanolamine, ethanol, acetone and deionized water;It is an advantage of the current invention that:Product of the present invention is solution, it is easy to be encased in container as needed, need rust cleaning part to only need to taking-up for textile surface to be cleaned, for the textile for needing batch rust cleaning, textile then directly can be soaked, rinsed using deionized water repeatedly, with good rust cleaning effect, and do not damage textile surface;The preparation process is simple of the present invention, with low cost, be suitable for factory mode under production.
Description
Technical field
The present invention relates to textile processing techniques field, and in particular to a kind of weaving rust remover and preparation method thereof.
Background technology
Textile is widely used at present in people's daily life.Textile is commonly used to make various products, to meet the needs of people.During processing or use, due to the frequent and various metallic weapon of meeting and tool contact, its surface is possible to produce iron rust textile.If carrying out processing of rust removing not in time, its use can be affected.And in general family or textile processing, due to can not find a good rust remover, the way that a lot of people take some very wrong, useful washing powder, liquid detergent go cleaning, useful banana skin, toothpaste cleaning, then using washing or machine cleaning, so not only do not reach preferably rust cleaning effect yet, the textile life-span can be allowed on the contrary to reduce, cause more broadly to injure textile surface.
Content of the invention
Present invention aims to the deficiencies in the prior art, now provide and a kind of can effectively remove textile rust remover of rusty stain and preparation method thereof.
For achieving the above object, the technical scheme is that:A kind of weaving rust remover, its innovative point are:It is made up of oxalic acid, citric acid, acetic acid, natrium nitrosum, alcoxylates, ammonium hydrogen carbonate, ammonium benzoate, second methylcellulose, tertiary sodium phosphate, triethanolamine, ethanol, acetone and deionized water;Described oxalic acid 10-15 part, citric acid 20-30 part, acetic acid 3-5 part, natrium nitrosum 5-10 part, alcoxylates 6-10 part, ammonium hydrogen carbonate 3-8 part, ammonium benzoate 10-20 part, second methylcellulose 2-5 part, tertiary sodium phosphate 1-3 part, triethanolamine 1-5 part, ethanol 60-80 part, acetone 6-15 part and deionized water 180-250 part.
Further, the alcoxylates are propylene oxide.
It is another object of the present invention to disclosing a kind of preparation method of weaving rust remover, its innovative point is:Comprise the following steps:
(1)By the ethyl cellulose of above-mentioned mass fraction and ethanol, acetone mixing, acquisition component A solution for standby is uniformly mixed;
(2)The oxalic acid of above-mentioned mass fraction, citric acid, acetic acid are mixed, add the deionized water of above-mentioned mass fraction, after being uniformly mixed, the tertiary sodium phosphate of the above-mentioned mass fraction of addition, triethanolamine, ammonium hydrogen carbonate, benzoic acid ammonia, stir and mix acquisition B component solution for standby;
(3)Remaining ingredient is mixed, is stirred, obtain C component solution standby;
(4)By step(1), step(2)And step(3)Obtained A, B, C component solution mixed, be thoroughly mixed, after filtration, obtained solution is this product.
Beneficial effects of the present invention are as follows:Product of the present invention is solution, it is easy to be encased in container as needed, need rust cleaning part to only need to taking-up for textile surface to be cleaned, for the textile for needing batch rust cleaning, textile then directly can be soaked, rinsed using deionized water repeatedly, with good rust cleaning effect, and do not damage textile surface;The preparation process is simple of the present invention, with low cost, be suitable for factory mode under production.
Specific embodiment
Hereinafter embodiments of the present invention are illustrated by particular specific embodiment, the content that those skilled in the art can be disclosed by this specification understands other advantages of the present invention and effect easily.
Embodiment 1
A kind of weaving rust remover, is made up of oxalic acid, citric acid, acetic acid, natrium nitrosum, alcoxylates, ammonium hydrogen carbonate, ammonium benzoate, second methylcellulose, tertiary sodium phosphate, triethanolamine, ethanol, acetone and deionized water;10 parts of oxalic acid, 20 parts of citric acid, 3 parts of acetic acid, 5 parts of natrium nitrosum, 6 parts of alcoxylates, 3 parts of ammonium hydrogen carbonate, 10 parts of ammonium benzoate, 2 parts of second methylcellulose, 1 part of tertiary sodium phosphate, 1 part of triethanolamine, 60 parts of ethanol, acetone 6-15 part and 180 parts of deionized water.
A kind of preparation method of weaving rust remover, comprises the following steps:
(1)By the ethyl cellulose of above-mentioned mass fraction and ethanol, acetone mixing, acquisition component A solution for standby is uniformly mixed;
(2)The oxalic acid of above-mentioned mass fraction, citric acid, acetic acid are mixed, add the deionized water of above-mentioned mass fraction, after being uniformly mixed, the tertiary sodium phosphate of the above-mentioned mass fraction of addition, triethanolamine, ammonium hydrogen carbonate, benzoic acid ammonia, stir and mix acquisition B component solution for standby;
(3)Remaining ingredient is mixed, is stirred, obtain C component solution standby;
(4)By step(1), step(2)And step(3)Obtained A, B, C component solution mixed, be thoroughly mixed, after filtration, obtained solution is this product.
Embodiment 2
A kind of weaving rust remover, is made up of oxalic acid, citric acid, acetic acid, natrium nitrosum, alcoxylates, ammonium hydrogen carbonate, ammonium benzoate, second methylcellulose, tertiary sodium phosphate, triethanolamine, ethanol, acetone and deionized water;15 parts of oxalic acid, 30 parts of citric acid, 5 parts of acetic acid, 10 parts of natrium nitrosum, 10 parts of alcoxylates, 8 parts of ammonium hydrogen carbonate, 20 parts of ammonium benzoate, 5 parts of second methylcellulose, 3 parts of tertiary sodium phosphate, 5 parts of triethanolamine, 80 parts of ethanol, 15 parts of acetone and 250 parts of deionized water.
A kind of preparation method of weaving rust remover, comprises the following steps:
(5)By the ethyl cellulose of above-mentioned mass fraction and ethanol, acetone mixing, acquisition component A solution for standby is uniformly mixed;
(6)The oxalic acid of above-mentioned mass fraction, citric acid, acetic acid are mixed, add the deionized water of above-mentioned mass fraction, after being uniformly mixed, the tertiary sodium phosphate of the above-mentioned mass fraction of addition, triethanolamine, ammonium hydrogen carbonate, benzoic acid ammonia, stir and mix acquisition B component solution for standby;
(7)Remaining ingredient is mixed, is stirred, obtain C component solution standby;
(8)By step(5), step(6)And step(7)Obtained A, B, C component solution mixed, be thoroughly mixed, after filtration, obtained solution is this product.
Embodiment 3
A kind of weaving rust remover, is made up of oxalic acid, citric acid, acetic acid, natrium nitrosum, alcoxylates, ammonium hydrogen carbonate, ammonium benzoate, second methylcellulose, tertiary sodium phosphate, triethanolamine, ethanol, acetone and deionized water;13 parts of oxalic acid, 25 parts of citric acid, 4 parts of acetic acid, 7 parts of natrium nitrosum, 8 parts of alcoxylates, 4 parts of ammonium hydrogen carbonate, 15 parts of ammonium benzoate, 3 parts of second methylcellulose, 2 parts of tertiary sodium phosphate, 3 parts of triethanolamine, 70 parts of ethanol, 10 parts of acetone and 220 parts of deionized water.
A kind of preparation method of weaving rust remover, comprises the following steps:
(9)By the ethyl cellulose of above-mentioned mass fraction and ethanol, acetone mixing, acquisition component A solution for standby is uniformly mixed;
(10)The oxalic acid of above-mentioned mass fraction, citric acid, acetic acid are mixed, add the deionized water of above-mentioned mass fraction, after being uniformly mixed, the tertiary sodium phosphate of the above-mentioned mass fraction of addition, triethanolamine, ammonium hydrogen carbonate, benzoic acid ammonia, stir and mix acquisition B component solution for standby;
(11)Remaining ingredient is mixed, is stirred, obtain C component solution standby;
(12)By step(9), step(10)And step(11)Obtained A, B, C component solution mixed, be thoroughly mixed, after filtration, obtained solution is this product.
Product of the present invention is solution, it is easy to be encased in container as needed, need rust cleaning part to only need to taking-up for textile surface to be cleaned, for the textile for needing batch rust cleaning, textile then directly can be soaked, rinsed using deionized water repeatedly, with good rust cleaning effect, and do not damage textile surface;The preparation process is simple of the present invention, with low cost, be suitable for factory mode under production.
Above-described embodiment is presently preferred embodiments of the present invention; it is not the restriction to technical solution of the present invention; as long as without the technical scheme that creative work can be realized on the basis of above-described embodiment, it is regarded as falling in the rights protection scope of patent of the present invention.
Claims (3)
1. a kind of weaving rust remover, it is characterised in that:It is made up of oxalic acid, citric acid, acetic acid, natrium nitrosum, alcoxylates, ammonium hydrogen carbonate, ammonium benzoate, second methylcellulose, tertiary sodium phosphate, triethanolamine, ethanol, acetone and deionized water;Described oxalic acid 10-15 part, citric acid 20-30 part, acetic acid 3-5 part, natrium nitrosum 5-10 part, alcoxylates 6-10 part, ammonium hydrogen carbonate 3-8 part, ammonium benzoate 10-20 part, second methylcellulose 2-5 part, tertiary sodium phosphate 1-3 part, triethanolamine 1-5 part, ethanol 60-80 part, acetone 6-15 part and deionized water 180-250 part.
2. a kind of weaving rust remover according to claim 1, it is characterised in that:The alcoxylates are propylene oxide.
3. a kind of weaving rust remover preparation method, it is characterised in that:Comprise the following steps:
(1)By the ethyl cellulose of above-mentioned mass fraction and ethanol, acetone mixing, acquisition component A solution for standby is uniformly mixed;
(2)The oxalic acid of above-mentioned mass fraction, citric acid, acetic acid are mixed, add the deionized water of above-mentioned mass fraction, after being uniformly mixed, the tertiary sodium phosphate of the above-mentioned mass fraction of addition, triethanolamine, ammonium hydrogen carbonate, benzoic acid ammonia, stir and mix acquisition B component solution for standby;
(3)Remaining ingredient is mixed, is stirred, obtain C component solution standby;
(4)By step(1), step(2)And step(3)Obtained A, B, C component solution mixed, be thoroughly mixed, after filtration, obtained solution is this product.