CN106432850A - Rubber material for making gloves - Google Patents
Rubber material for making gloves Download PDFInfo
- Publication number
- CN106432850A CN106432850A CN201610776031.5A CN201610776031A CN106432850A CN 106432850 A CN106432850 A CN 106432850A CN 201610776031 A CN201610776031 A CN 201610776031A CN 106432850 A CN106432850 A CN 106432850A
- Authority
- CN
- China
- Prior art keywords
- parts
- rubber
- styrene
- butadiene
- natural rubber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a rubber material for making gloves. The material is prepared, by weight, from the following materials: 10-40 parts of epoxidized natural rubber, 5-25 parts of chlorinated natural rubber, 5-30 parts of styrene-butadiene rubber, 5-25 parts of epoxidized soybean oil, 2-10 parts of acrylic polyurethane, 2-8 parts of styrene-butadiene latex, 1-5 parts of curing agent, 1-5 parts of dithiocarbamate and 0.5-3 parts of zinc oxide. According to the materials of the rubber material, the epoxidized natural rubber increases the anti-moisture and anti-aging properties of the material. The lignin rubber additive can increase the anti-friction property of the rubber. The rubber material has the advantage of having a good anti-friction property, good waterproof property and high temperature resistance.
Description
Technical field
The present invention relates to a kind of elastomeric material for making glove, belong to rubber and its product technique field.
Background technology
The rubber of early stage is taken from the latex of the plants such as rubber tree, russian dandelion, and that makes after processing has elasticity, insulation
Property, the material of impermeable water and air.Synthetic rubber is then obtained by the aggregated reaction of various monomers.Rubber is widely used in work
Industry or life each side, such as automobile tire, electric wire, insulant, ball stationery sports goods, toy, rubber glovess, locomotorium
Material dispensing etc..The a large amount of use of rubber also creates a lot of waste rubber products.Scrap rubber be six big solid-state regenerated resources it
One, its harmless resource utilization recycles and is always the important topic that countries in the world are actively studied.
Content of the invention
It is an object of the invention to provide the rubber for making glove that a kind of oil resistivity is good, wearability is good, water proofing property is good
Glue material.
Technical scheme is as follows:A kind of elastomeric material for making glove, by the raw material of following mass fraction
Preparation:Epoxy natural rubber 10-40 part, chlorinated natural rubber 5-25 part, butadiene-styrene rubber rubber 5-30 part, epoxy soybean oil 5-25
Part, acroleic acid polyurethane 2-10 part, styrene-butadiene latex 2-8 part, firming agent 1-5 part, dithiocar-bamate 1-5 part, zinc oxide
0.5-3 part.
Preferably, the described elastomeric material for making glove, by the raw material preparation of following mass fraction:Epoxidation is natural
35 parts of rubber, 85 parts of chlorinated natural rubber, 30 parts of butadiene-styrene rubber rubber, 12 parts of epoxy soybean oil, 8 parts of acroleic acid polyurethane, butylbenzene
4 parts of latex, 4 parts of firming agent, 1 part of dithiocar-bamate, 0.5 part of zinc oxide.
Preferably, the described elastomeric material for making glove, by the raw material preparation of following mass fraction:Epoxidation is natural
17 parts of rubber, 23 parts of chlorinated natural rubber, 18 parts of butadiene-styrene rubber rubber, 20 parts of epoxy soybean oil, acroleic acid polyurethane 2-10 part, fourth
8 parts of benzene latex, 2 parts of firming agent, 2 parts of dithiocar-bamate, 2.5 parts of zinc oxide.
Preferably, the described elastomeric material for making glove, by the raw material preparation of following mass fraction:Epoxidation is natural
24 parts of rubber, 16 parts of chlorinated natural rubber, 20 parts of butadiene-styrene rubber rubber, 18 parts of epoxy soybean oil, acroleic acid polyurethane 2-10 part, fourth
5 parts of benzene latex, 2.5 parts of firming agent, 3 parts of dithiocar-bamate, 1.5 parts of zinc oxide.
In its constitutive material of elastomeric material of the present invention, epoxy natural rubber increased material waterproof anti ageing property,
Lignin rubber chemicals can increase the wearability of rubber;The elastomeric material for making glove of the present invention has wearability
Good, water proofing property is good, resistant to elevated temperatures feature.
Specific embodiment
Below by embodiment, the present invention is described in further details, these embodiments are only used for the present invention is described, and
Do not limit the scope of the invention.
A kind of elastomeric material for making glove of embodiment 1, by the raw material preparation of following mass fraction:Epoxidation is natural
35 parts of rubber, 85 parts of chlorinated natural rubber, 30 parts of butadiene-styrene rubber rubber, 12 parts of epoxy soybean oil, 8 parts of acroleic acid polyurethane, butylbenzene
4 parts of latex, 4 parts of firming agent, 1 part of dithiocar-bamate, 0.5 part of zinc oxide.
A kind of elastomeric material for making glove of embodiment 2, by the raw material preparation of following mass fraction:Epoxidation is natural
17 parts of rubber, 23 parts of chlorinated natural rubber, 18 parts of butadiene-styrene rubber rubber, 20 parts of epoxy soybean oil, acroleic acid polyurethane 2-10 part, fourth
8 parts of benzene latex, 2 parts of firming agent, 2 parts of dithiocar-bamate, 2.5 parts of zinc oxide.
A kind of elastomeric material for making glove of embodiment 3, by the raw material preparation of following mass fraction:Epoxidation is natural
24 parts of rubber, 16 parts of chlorinated natural rubber, 20 parts of butadiene-styrene rubber rubber, 18 parts of epoxy soybean oil, acroleic acid polyurethane 2-10 part, fourth
5 parts of benzene latex, 2.5 parts of firming agent, 3 parts of dithiocar-bamate, 1.5 parts of zinc oxide.
Claims (4)
1. a kind of elastomeric material for making glove it is characterised in that:Raw material preparation by following mass fraction:Epoxidation sky
So rubber 10-40 part, chlorinated natural rubber 5-25 part, butadiene-styrene rubber rubber 5-30 part, epoxy soybean oil 5-25 part, poly- ammonia of acrylic acid
Ester 2-10 part, styrene-butadiene latex 2-8 part, firming agent 1-5 part, dithiocar-bamate 1-5 part, zinc oxide 0.5-3 part.
2. the elastomeric material for making glove according to claim 1 it is characterised in that:Former by following mass fraction
Material preparation:35 parts of epoxy natural rubber, 85 parts of chlorinated natural rubber, 30 parts of butadiene-styrene rubber rubber, 12 parts of epoxy soybean oil, propylene
8 parts of sour polyurethane, 4 parts of styrene-butadiene latex, 4 parts of firming agent, 1 part of dithiocar-bamate, 0.5 part of zinc oxide.
3. the elastomeric material for making glove according to claim 1 it is characterised in that:Former by following mass fraction
Material preparation:17 parts of epoxy natural rubber, 23 parts of chlorinated natural rubber, 18 parts of butadiene-styrene rubber rubber, 20 parts of epoxy soybean oil, propylene
Sour polyurethane 2-10 part, 8 parts of styrene-butadiene latex, 2 parts of firming agent, 2 parts of dithiocar-bamate, 2.5 parts of zinc oxide.
4. the elastomeric material for making glove according to claim 1 it is characterised in that:Former by following mass fraction
Material preparation:24 parts of epoxy natural rubber, 16 parts of chlorinated natural rubber, 20 parts of butadiene-styrene rubber rubber, 18 parts of epoxy soybean oil, propylene
Sour polyurethane 2-10 part, 5 parts of styrene-butadiene latex, 2.5 parts of firming agent, 3 parts of dithiocar-bamate, 1.5 parts of zinc oxide.