- Publication number
- CN106422222A CN106422222A CN201510488299.4A CN201510488299A CN106422222A CN 106422222 A CN106422222 A CN 106422222A CN 201510488299 A CN201510488299 A CN 201510488299A CN 106422222 A CN106422222 A CN 106422222A
- Authority
- CN
- China
- Prior art keywords
- die
- ice hockey
- die cavity
- water
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to an improved ice hockey manufacturing method. The method comprises steps of first manufacturing a modular die assembly forming a spherical die cavity, evenly painting an oil film with a freezing point higher than water and incompatible with water on a die cavity surface of each assembly in a modular die, injecting water into the die cavity, conducting low-temperature treatment to the modular die filled with water to freeze water in the die cavity, and at last dismantling the modular die after the water in the die cavity is fully frozen, and achieving an ice hockey. The improved ice hockey manufacturing method is advantageous in that improvements are made for an ice hockey manufacturing via a die in the prior art, and adhesion between the surface after the formation of the ice hockey and a die cavity surface of the die can be prevented, so ice hockey surface damage and crack due to the adhesion between the ice hockey surface and the die cavity surface of the die during the manufacturing process can be solved; and the ice hockey surface can be maintained to be tidy and smooth.
Description
Technical field
The present invention relates to a kind of ice hockey manufacture method, especially a kind of modified form ice hockey manufacture method.
Background technology
The making of ice hockey is carried out generally by mould at present, spherical die cavity with water filling port is formed by mould matched moulds, then fill water into die cavity and the mould after water filling is made K cryogenic treatment so that water freezing in die cavity, remove mould after the water in die cavity freezes completely, the icicle being formed because of water filling port on ice hockey that will be obtained is repaiied and removed.But adopt in this way make ice hockey during, may be because the reason mould itself material and because the water in die cavity can expand after icing, water in die cavity is easily cohered with die cavity face after icing, thus easily causing ice hockey surface fracture, fragmentation during removing mould, form hollow, and have a strong impact on the type quality of ice hockey.
Therefore, be just badly in need of developing a kind of readily removable except and the modified form ice hockey manufacture method that will not cohere, through retrieval, do not find the same or analogous technical scheme with the present invention.
Content of the invention
The technical problem to be solved in the present invention be provide a kind of readily removable except and the modified form ice hockey manufacture method that will not cohere.
For solving above-mentioned technical problem, the technical scheme is that:A kind of modified form ice hockey manufacture method, its innovative point is:Its step is as follows:
1)First, make the die assembly forming spherical die cavity for combination;
2)Again one layer of higher than water and immiscible with water oil film of freezing point is equably brushed in the die cavity face of each assembly of sectional die;
3)Then, combination die is formed a spherical die cavity;
4)Then, fill water into die cavity and the sectional die after water filling is made K cryogenic treatment so that water freezing in die cavity;
5)Finally, remove sectional die after the water in die cavity freezes completely and ice hockey is obtained.
Further, described oil film adopts butter or Oleum Arachidis hypogaeae semen or olive oil.
It is an advantage of the current invention that:The present invention be directed to using the improvement of Mold Making ice hockey method at present, in manufacturing process, " flexible separate layer " is formed by the die cavity face that rationally and cleverly means make mould in existing ice hockey, cohered with the die cavity face stoping with avoid surface and mould after ice hockey molding, thus efficiently solve there is the problem of ice hockey surface fracture, fragmentation it is ensured that the ice hockey surface made is complete and bright and clean when being cohered and led to remove mould with ice hockey surface is easy with the die cavity face of mould in manufacturing process existing for the method for Mold Making ice hockey at present.
Specific embodiment
A kind of modified form ice hockey manufacture method, its step is as follows:First, make the die assembly forming spherical die cavity for combination;Again one layer of higher than water and immiscible with water oil film of freezing point is equably brushed in the die cavity face of each assembly of sectional die;Then, combination die is formed a spherical die cavity;Then, fill water into die cavity and the sectional die after water filling is made K cryogenic treatment so that water freezing in die cavity;Finally, remove sectional die after the water in die cavity freezes completely and ice hockey is obtained;The oil film of technical solution of the present invention adopts butter or Oleum Arachidis hypogaeae semen or olive oil.
The present invention be directed to using the improvement of Mold Making ice hockey method at present, in manufacturing process, " flexible separate layer " is formed by the die cavity face that rationally and cleverly means make mould in existing ice hockey, cohered with the die cavity face stoping with avoid surface and mould after ice hockey molding, thus efficiently solve there is the problem of ice hockey surface fracture, fragmentation it is ensured that the ice hockey surface made is complete and bright and clean when being cohered and led to remove mould with ice hockey surface is easy with the die cavity face of mould in manufacturing process existing for the method for Mold Making ice hockey at present.
Ultimate principle and the principal character of the present invention have been shown and described above.It should be understood by those skilled in the art that; the present invention is not restricted to the described embodiments; merely illustrating the principles of the invention described in above-described embodiment and description; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements both fall within scope of the claimed invention.Claimed scope is by appending claims and its equivalent thereof.
Claims (2)
1. a kind of modified form ice hockey manufacture method it is characterised in that:Its step is as follows:
First, make the die assembly forming spherical die cavity for combination;
Again one layer of higher than water and immiscible with water oil film of freezing point is equably brushed in the die cavity face of each assembly of sectional die;
Then, combination die is formed a spherical die cavity;
Then, fill water into die cavity and the sectional die after water filling is made K cryogenic treatment so that water freezing in die cavity;
Finally, remove sectional die after the water in die cavity freezes completely and ice hockey is obtained.
2. a kind of modified form ice hockey manufacture method according to claim 1 it is characterised in that:Described oil film adopts butter or Oleum Arachidis hypogaeae semen or olive oil.