CN106291858B - The preparation method of lens module - Google Patents

The preparation method of lens module Download PDF

Info

Publication number
CN106291858B
CN106291858B CN201610766414.4A CN201610766414A CN106291858B CN 106291858 B CN106291858 B CN 106291858B CN 201610766414 A CN201610766414 A CN 201610766414A CN 106291858 B CN106291858 B CN 106291858B
Authority
CN
China
Prior art keywords
mirror plate
glue
plate layers
lens
spacer shims
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201610766414.4A
Other languages
Chinese (zh)
Other versions
CN106291858A (en
Inventor
王娇娇
廖敏智
王辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Howell Electronics Technology (shanghai) Co Ltd
Original Assignee
Howell Electronics Technology (shanghai) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Howell Electronics Technology (shanghai) Co Ltd filed Critical Howell Electronics Technology (shanghai) Co Ltd
Priority to CN201610766414.4A priority Critical patent/CN106291858B/en
Publication of CN106291858A publication Critical patent/CN106291858A/en
Application granted granted Critical
Publication of CN106291858B publication Critical patent/CN106291858B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

Present invention discloses a kind of preparation methods of lens module, it include: that will pass through the first glue sticking between first mirror plate layers and spacer shims, the second glue sticking will be passed through between the spacer shims and the second mirror plate layers, first mirror plate layers, spacer shims and the second mirror plate layers are stacked into lens module, wherein, first glue or/and the second glue are that can dissociate glue;The lens module is tested, if test result is undesirable, glue, which can be dissociated, described in can making under given conditions loses viscosity, separate the lens module, so as to adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, such as focus parameter etc., stacking is re-started using the glue that dissociates, the lens module after doing over again is formed, until the test result meets the requirements.It can quickly and easily adjust and discharge of the coke away from parameter and the preferable lens module of optical quality, save the time, reduce cost.

Description

The preparation method of lens module
Technical field
The present invention relates to zoom lens manufacturing fields, more particularly to a kind of preparation method of lens module.
Background technique
Lens module generally comprises the first mirror plate layers, the second mirror plate layers and is located at first mirror plate layers and the second mirror The components such as the spacer shims of lamella.At product development initial stage, needs to carry out a large amount of focal length parameter and the correlation of optical quality is real Test, can not rapid pin focusing related process tested and adjusted, can only be verified, be wasted many valuable by large-tonnage product Development time, development cost are high.
Summary of the invention
The object of the present invention is to provide a kind of preparation methods of lens module, can rapidly be directed to and not meet test It is required that product carry out focal length adjusting, save the time, reduce cost.
In order to solve the above technical problems, the present invention provides a kind of preparation method of lens module, comprising:
First mirror plate layers, spacer shims and the second mirror plate layers are provided;
Will between first mirror plate layers and spacer shims by the first glue sticking, by the spacer shims and the second mirror plate layers it Between by the second glue sticking, first mirror plate layers, spacer shims and the second mirror plate layers are stacked into lens module, wherein described First glue or/and the second glue are that can dissociate glue;
The lens module is tested, judges whether test result meets the requirements, is wanted if test result is not met It asks, then carries out rework operation, until test result meets the requirements;
The rework operation includes:
Glue can be dissociated described in making under given conditions and loses viscosity, separate the lens module;
The matching degree between first mirror plate layers, spacer shims and the second mirror plate layers is adjusted, dissociates glue weight using described It is newly stacked, forms the lens module after doing over again.
Further, when first glue, which is, to dissociate glue, first mirror plate layers, spacer shims and the second eyeglass are adjusted The process of matching degree between layer includes: the thickness for adjusting first glue and/or the shape of first mirror plate layers;When described Second glue is when can dissociate glue, to adjust the process packet of the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers It includes: the thickness of adjustment second glue and/or the shape of second mirror plate layers;When first glue and second glue are When can dissociate glue, the process for adjusting the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers includes: adjustment institute State the thickness of the first glue, the thickness of second glue, the thickness of the spacer shims, the shape of first mirror plate layers and described It is one or several in the shape of two mirror plate layers.
Further, the spacer shims include through-hole, first mirror plate layers include the first transparent conducting glass substrate and First lens, second mirror plate layers include the second transparent conducting glass substrate and the second lens, first lens and second Lens are corresponding with the through-hole.
Further, first mirror plate layers and the second mirror plate layers are single-surface mirror lamella, and first lens are located at institute Side of first transparent conducting glass substrate towards the spacer shims is stated, second lens are located at the second electrically conducting transparent glass Side of the glass substrate towards the spacer shims;Or, first mirror plate layers and the second mirror plate layers are Double sided mirror lamella, described One lens include a pair of first sub-lens, and a pair of first sub-lens are located at first transparent conducting glass substrate face Deviate from the side of the spacer shims, second lens to the side of the spacer shims and first transparent conducting glass substrate Including a pair of second sub-lens, a pair of second sub-lens are located at second transparent conducting glass substrate towards described The side of spacer shims and second transparent conducting glass substrate deviate from the side of the spacer shims.
Further, the process for adjusting the shape of first mirror plate layers includes: to adjust the shape of first lens;It adjusts The process of the shape of whole second mirror plate layers includes: to adjust the shape of second lens.
Further, the glue that dissociates is hydrolysis glue, the water environment that the specified conditions are 80 DEG C or more.
Further, first by first glue coated in the side of first mirror plate layers towards the spacer shims, and/ Or, first glue is first coated in side of the spacer shims towards first mirror plate layers, then by first mirror plate layers Pass through first glue sticking between spacer shims;Second glue is first coated in second mirror plate layers towards the gap The side of piece, and/or, second glue is first coated in side of the spacer shims towards second mirror plate layers, then by institute It states between the second mirror plate layers and spacer shims through second glue sticking.
Further, the thickness for dissociating glue is more than or equal to 5 μm.
Further, the test includes modulation transfer function test, depth of field test and spatial frequency response test.
Further, the spacer shims include through-hole, first mirror plate layers include the first transparent conducting glass substrate and First lens, second mirror plate layers include the second transparent conducting glass substrate and the second lens, first lens and second Lens are corresponding with the through-hole.
Compared with prior art, the preparation method of lens module provided by the invention has the advantage that
In the preparation method of the lens module, the first gluing will be passed through between first mirror plate layers and spacer shims It connects, the second glue sticking will be passed through between the spacer shims and the second mirror plate layers, by first mirror plate layers, spacer shims and the second mirror Lamella is stacked into lens module, wherein first glue or/and the second glue are that can dissociate glue;The lens module is surveyed Examination, if test result is undesirable, can make under given conditions it is described can dissociate glue and lose viscosity, make the camera lens mould Group separation, so as to adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, such as focuses parameter Deng re-starting stacking using the glue that dissociates, form the lens module after doing over again, until the test result conforms to It asks.It can quickly and easily adjust and discharge of the coke away from parameter and the preferable lens module of optical quality, save the time, reduce cost.
Detailed description of the invention
Fig. 1 is the flow chart of the preparation method of lens module in first embodiment of the invention;
Fig. 2 to Fig. 7 is the schematic diagram of device architecture in the preparation method of the lens module of first embodiment of the invention;
Fig. 8 is the flow chart of the preparation method of lens module in second embodiment of the invention;
Fig. 9 to Figure 13 is the schematic diagram of device architecture in the preparation method of the lens module of second embodiment of the invention;
Figure 14 is the flow chart of the preparation method of lens module in third embodiment of the invention;
Figure 15 to Figure 19 is the schematic diagram of device architecture in the preparation method of the lens module of third embodiment of the invention.
Specific embodiment
Existing time of product development is long, and development cost is high.Inventor to the prior art (technology known for inventor, But not for well known to others skilled in the art) the study found that existing lens module is during the preparation process, generally need First mirror plate layers, spacer shims, the second mirror plate layers are passed sequentially through into disposable glue sticking, are assembled into lens module, Then the lens module is tested again.Disposable glue is generally ultraviolet glue or hot-setting adhesive, can not be lossless after bonding Wound remove.So after lens module group assembling, first mirror plate layers, spacer shims, the second mirror plate layers just can not again into Row separation.If the result of test is undesirable, need to prepare first mirror plate layers, spacer shims, the second eyeglass again Layer, and be again bonded together first mirror plate layers, spacer shims, the second mirror plate layers, increase development cost and period.
Inventor furthers investigate discovery, and the reason for causing the result of test undesirable is mainly first eyeglass Matching degree between layer, spacer shims and the second mirror plate layers is bad, for example, between first mirror plate layers and the second mirror plate layers between The shape of lens away from improper or described first mirror plate layers and the second mirror plate layers is improper, causes each in the lens module It is mismatched between a element.If the spacing between first mirror plate layers and the second mirror plate layers is adjustable, and first eyeglass The shape of layer and the lens of the second mirror plate layers, then can be by adjusting between first mirror plate layers and the second mirror plate layers Away from, and the shape of the lens of first mirror plate layers and the second mirror plate layers is adjusted, so that test result meets the requirements, save exploitation Cost and period.Inventor further study show that, if carried out between first mirror plate layers, spacer shims, the second mirror plate layers The glue of bonding is that can dissociate glue, then when the result of test is undesirable, can make described can dissociate glue under given conditions Viscosity is lost, separates the lens module, so as to readjust first mirror plate layers, spacer shims and the second mirror plate layers Between matching degree.
According to the studies above, the present invention provides a kind of preparation method of lens module, includes the following steps:
First mirror plate layers, spacer shims and the second mirror plate layers are provided;
Will between first mirror plate layers and spacer shims by the first glue sticking, by the spacer shims and the second mirror plate layers it Between by the second glue sticking, first mirror plate layers, spacer shims and the second mirror plate layers are stacked into lens module, wherein described First glue or/and the second glue are that can dissociate glue;
The lens module is tested, judges whether test result meets the requirements, is wanted if test result is not met It asks, then carries out rework operation, until test result meets the requirements;
The rework operation includes:
Glue can be dissociated described in making under given conditions and loses viscosity, separate the lens module;
The matching degree between first mirror plate layers, spacer shims and the second mirror plate layers is adjusted, dissociates glue weight using described It is newly stacked, forms the lens module after doing over again.
In the rework operation, can make under given conditions it is described can dissociate glue and lose viscosity, make the camera lens mould Group separation, so as to adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, such as focuses parameter Deng re-starting stacking using the glue that dissociates, form the lens module after doing over again, until the test result conforms to It asks.It can quickly and easily adjust and discharge of the coke away from parameter and the preferable lens module of optical quality, save the time, reduce cost.
It is described in more detail below in conjunction with preparation method of the schematic diagram to lens module of the invention, wherein indicating The preferred embodiment of the present invention, it should be appreciated that those skilled in the art can modify invention described herein, and still real Existing advantageous effects of the invention.Therefore, following description should be understood as the widely known of those skilled in the art, and simultaneously Not as limitation of the present invention.
For clarity, not describing whole features of practical embodiments.In the following description, it is not described in detail well known function And structure, because they can make the present invention chaotic due to unnecessary details.It will be understood that opening in any practical embodiments In hair, it is necessary to make a large amount of implementation details to realize the specific objective of developer, such as according to related system or related business Limitation, changes into another embodiment by one embodiment.Additionally, it should think that this development may be complicated and expend Time, but to those skilled in the art it is only routine work.
The present invention is more specifically described by way of example referring to attached drawing in the following passage.It is wanted according to following explanation and right Book is sought, advantages and features of the invention will become apparent from.It should be noted that attached drawing is all made of very simplified form and using non- Accurately ratio, only for the purpose of facilitating and clarifying the purpose of the embodiments of the invention.
The several embodiments for being exemplified below the preparation method of the lens module are answered with clearly illustrating the contents of the present invention When it is clear that, the contents of the present invention are not restricted to following embodiment, other pass through the routine of those of ordinary skill in the art The improvement of technological means is also within thought range of the invention.
First embodiment
In the present embodiment, it please refers to Fig. 1-Fig. 7 and illustrates the first embodiment of the present invention, wherein Fig. 1 is the present invention The flow chart of the preparation method of lens module in first embodiment;Fig. 2 to Fig. 7 is the lens module of first embodiment of the invention The schematic diagram of device architecture in preparation method.
Firstly, as shown in Fig. 2, providing the first mirror plate layers 100, spacer shims 300, the second mirror plate layers 200, wherein described the One mirror plate layers 100 are used for providing the first lens, second mirror plate layers 200 for providing the second lens, the spacer shims 300 In protection first lens and the second lens.In the present embodiment, the spacer shims 300 include through-hole 310, first mirror Lamella 100 includes the first transparent conducting glass substrate 110 and the first lens 120, and second mirror plate layers 200 include second transparent Conducting glass substrate 210 and the second lens 220, first lens 120 and the second lens 220 are opposite with the through-hole 310 It answers.The thickness of first transparent conducting glass substrate 110 is more than or equal to 100 μm, second transparent conducting glass substrate 210 Thickness be more than or equal to 100 μm.
Specifically, as shown in Fig. 2, first mirror plate layers 100 and the second mirror plate layers 200 are single-surface mirror lamella, that is, institute It states the first lens 120 and is located at side of first transparent conducting glass substrate 110 towards the spacer shims 300, described second Lens 220 are located at side of second transparent conducting glass substrate 210 towards the spacer shims 300.In Fig. 2, described One lens 120 are concavees lens, and second lens 220 are that convex lens in other embodiments can be with first lens 120 be convex lens, and second lens 220 are concavees lens.
Preferably, first carrying out dispensing before stacking first mirror plate layers 100, spacer shims 300, the second mirror plate layers 200 Technique first exists as shown in figure 3, first applying the first glue 410 towards the side of the spacer shims 300 in first mirror plate layers 100 Second mirror plate layers 200 apply the second glue 510, in the present embodiment, first glue towards the side of the spacer shims 300 410 is can dissociate glue, and the glue that dissociates can lose viscosity under given conditions, preferably, the glue that dissociates is hydrolysis glue, The glue that dissociates can lose viscosity in 80 DEG C or more of water environment, be dissociated with can be convenient.Wherein, described to dissociate Glue is not limited to hydrolyze glue, as long as can lose viscosity under given conditions, within thought range of the invention.
Then, as shown in figure 4, being stacked, described the will be passed through between first mirror plate layers 100 and spacer shims 300 One glue 410 bonding will be bonded between the spacer shims 300 and the second mirror plate layers 200 by second glue 510, by described the One mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 are stacked into lens module, wherein first glue 410 is that can dissociate Glue is dissociated preferably, the thickness H1 for dissociating glue is more than or equal to 5 μm with facilitating.
Then, the lens module of stacking is tested, preferably, the test is optic test, including modulation Transmission function tests (Modulation Transfer Function), depth of field test (depth of focus) and space frequency Rate response test (Spatial Frequency Response).
If test result is undesirable, rework operation is carried out, the rework operation includes:
It is lost as shown in figure 5, glue (being in the present embodiment first glue 410) can be dissociated described in making under given conditions Viscosity separates the lens module, specifically, in the present embodiment, the lens module can be placed in 80 DEG C or more Water environment in, then first glue 410 dissociates, and first mirror plate layers 100 and spacer shims 300 separate;
Then, the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 is adjusted, is passed through First glue 410 again bonds together first mirror plate layers 100 and spacer shims 300, forms the camera lens mould after doing over again Group.Preferably, the thickness of adjustment first glue 410, adjusts first mirror plate layers 100 and the second mirror plate layers in which can be convenient The distance between 200, so as to adjust the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200, To find the optimum distance between first mirror plate layers 100 and the second mirror plate layers 200.As shown in fig. 6, in first mirror Lamella 100 applies first glue 410 towards the side of the spacer shims 300, first glue 410 apply with a thickness of H2, Then described as shown in fig. 7, first mirror plate layers 100 and spacer shims 300 are bonded together by first glue 410 The distance between first mirror plate layers 100 and the second mirror plate layers 200 are changed.
In addition, the step of adjusting the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 It can also include: the shape for adjusting first mirror plate layers 100, specifically, adjustable in the present embodiment described first is saturating The shape of first lens 112 on bright conducting glass substrate 111, to find the shape of most suitable first lens 112.
Later, and to the lens module after doing over again test is re-started, if test result is undesirable, then carried out The rework operation, until test result meets the requirements.
Then, subsequent technique is carried out, such as the lens module such as is bonded with sensor, and be packaged at the works Skill, this be it will be appreciated by those skilled in the art that, therefore not to repeat here.It is described to dissociate glue quilt in structure after encapsulation It is encapsulated in the inside of structure, is generally not under the specified conditions and (will not be corroded by 80 DEG C or more of water), it is described Glue, which can be dissociated, to be dissociated, the stable structure of the lens module.
In the present embodiment, glue can be dissociated described in making under given conditions and loses viscosity, separate the lens module, from And adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, such as focus parameter etc., use institute Glue can be dissociated by, which stating, re-starts stacking, forms the lens module after doing over again, until the test result meets the requirements.It is finding most During good matching degree, first mirror plate layers brought are not damaged, can also continue to using.
Second embodiment
Please refer to Fig. 8-Figure 13, wherein Fig. 8 is the process of the preparation method of lens module in second embodiment of the invention Figure;Fig. 9 to Figure 13 is the schematic diagram of device architecture in the preparation method of the lens module of second embodiment of the invention.In Fig. 9-figure In 13, reference label indicates statement component same as the first embodiment identical with Fig. 2-Fig. 7.The second embodiment The preparation method of preparation method and the first embodiment is essentially identical, and difference is: second glue 510 is that can dissociate Glue.
As shown in figure 9, first being carried out before stacking first mirror plate layers 100, spacer shims 300, the second mirror plate layers 200 Gluing process first applies the first glue 410 towards the side of the spacer shims 300 in first mirror plate layers 100, first described the Two mirror plate layers 200 apply the second glue 510 towards the side of the spacer shims 300, and in the present embodiment, second glue 510 is Glue can be dissociated, the glue that dissociates can lose viscosity under given conditions, preferably, the glue that dissociates is hydrolysis glue, it is described Glue can be dissociated can lose viscosity in 80 DEG C or more of water environment, be dissociated with can be convenient.Wherein, described to dissociate glue simultaneously It is not limited to hydrolysis glue, as long as viscosity can be lost under given conditions, within thought range of the invention.
Then, as shown in Figure 10, stacked, described the will be passed through between first mirror plate layers 100 and spacer shims 300 One glue 410 bonding will be bonded between the spacer shims 300 and the second mirror plate layers 200 by second glue 510, by described the One mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 are stacked into lens module, wherein second glue 510 is that can dissociate Glue is dissociated preferably, the thickness H3 for dissociating glue is more than or equal to 5 μm with facilitating.
Then, the lens module of stacking is tested, preferably, the test is optic test, including modulation Transmission function tests (Modulation Transfer Function), depth of field test (depth of focus) and space frequency Rate response test (Spatial Frequency Response).
If test result is undesirable, rework operation is carried out, the rework operation includes:
As shown in figure 11, glue (being in the present embodiment second glue 510) mistake can be dissociated described in making under given conditions Vanishing viscosity separates the lens module, specifically, in the present embodiment, the lens module can be placed in 80 DEG C with On water environment in, then second glue 510 dissociates, and second mirror plate layers 200 and spacer shims 300 separate;
Then, the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 is adjusted, is passed through Second glue 510 again bonds together second mirror plate layers 200 and spacer shims 300, forms the camera lens mould after doing over again Group.Preferably, the thickness of adjustment second glue 510, adjusts first mirror plate layers 100 and the second mirror plate layers in which can be convenient The distance between 200, so as to adjust the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200, To find the optimum distance between first mirror plate layers 100 and the second mirror plate layers 200.As shown in figure 12, in the gap Piece 300 applies second glue 510 towards the side of second mirror plate layers 200, second glue 510 apply with a thickness of Then as shown in figure 13 H4 is bonded together second mirror plate layers 200 and spacer shims 300 by second glue 510, The distance between first mirror plate layers 100 and the second mirror plate layers 200 are changed.
In addition, the step of adjusting the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 It can also include: the shape for adjusting second mirror plate layers 200, specifically, adjustable in the present embodiment described second is saturating The shape of second lens 212 on bright conducting glass substrate 211, to find the shape of most suitable second lens 212.
Later, and to the lens module after doing over again test is re-started, if test result is undesirable, then carried out The rework operation, until test result meets the requirements.
In the present embodiment, glue can be dissociated described in making under given conditions and loses viscosity, separate the lens module, from And adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, such as focus parameter etc., use institute Glue can be dissociated by, which stating, re-starts stacking, forms the lens module after doing over again, until the test result meets the requirements.It is finding most During good matching degree, first mirror plate layers brought are not damaged, can also continue to using.
3rd embodiment
Please refer to Fig. 8-Figure 13, wherein Fig. 8 is the process of the preparation method of lens module in second embodiment of the invention Figure;Fig. 9 to Figure 13 is the schematic diagram of device architecture in the preparation method of the lens module of second embodiment of the invention.In Fig. 9-figure In 13, reference label indicates statement component same as the first embodiment identical with Fig. 2-Fig. 7.The second embodiment The preparation method of preparation method and the first embodiment is essentially identical, and difference is: first glue 410 and described second Glue 510 is that can dissociate glue.
As shown in figure 15, it before stacking first mirror plate layers 100, spacer shims 300, the second mirror plate layers 200, first carries out Gluing process first applies the first glue 410 towards the side of the spacer shims 300 in first mirror plate layers 100, first described the Two mirror plate layers 200 apply the second glue 510, in the present embodiment, 410 He of the first glue towards the side of the spacer shims 300 Second glue 510 is that can dissociate glue, and the glue that dissociates can lose viscosity under given conditions, preferably, described solve It is hydrolysis glue from glue, the glue that dissociates can lose viscosity in 80 DEG C or more of water environment, be dissociated with can be convenient.Its In, the glue that dissociates is not limited to hydrolyze glue, as long as can lose viscosity under given conditions, in thought model of the invention Within enclosing.
Then, as shown in figure 16, stacked, described the will be passed through between first mirror plate layers 100 and spacer shims 300 One glue 410 bonding will be bonded between the spacer shims 300 and the second mirror plate layers 200 by second glue 510, by described the One mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 are stacked into lens module, wherein the spacer shims 300 with a thickness of H5。
Then, the lens module of stacking is tested, preferably, the test is optic test, including modulation Transmission function tests (Modulation Transfer Function), depth of field test (depth of focus) and space frequency Rate response test (Spatial Frequency Response).
If test result is undesirable, rework operation is carried out, the rework operation includes:
As shown in figure 17, can dissociate glue described in making under given conditions (is in the present embodiment first glue 410 and institute State the second glue 510) viscosity is lost, the lens module is separated, specifically, in the present embodiment, it can be by the camera lens mould Group is placed in 80 DEG C or more of water environment, then first glue 410 and second glue 510 dissociation, first mirror plate layers 100 and spacer shims 300 separate, second mirror plate layers 200 and spacer shims 300 separate;
Then, the matching degree between first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 is adjusted, is passed through Second glue 510 again bonds together second mirror plate layers 200 and spacer shims 300, forms the camera lens mould after doing over again Group.Preferably, in the present embodiment, adjusting the thickness of the spacer shims 300, first mirror plate layers are adjusted with can be convenient 100 and second the distance between the mirror plate layers 200, so as to adjust first mirror plate layers 100, spacer shims 300 and the second mirror plate layers Matching degree between 200, to find the optimum distance between first mirror plate layers 100 and the second mirror plate layers 200.Such as Figure 18 It is shown, second glue 510 is applied towards the side of second mirror plate layers 200 in the spacer shims 300, in first mirror Lamella 100 applies first glue 410 towards the side of the spacer shims 300, then as shown in figure 19, by first eyeglass Layer 100 and spacer shims 300 are bonded together by first glue 410, and second mirror plate layers 200 and spacer shims 300 are led to It crosses second glue 510 to bond together, the distance between first mirror plate layers 100 and the second mirror plate layers 200 are changed.
Later, and to the lens module after doing over again test is re-started, if test result is undesirable, then carried out The rework operation, until test result meets the requirements.
In the present embodiment, glue can be dissociated described in making under given conditions and loses viscosity, separate the lens module, from And adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, such as focus parameter etc., use institute Glue can be dissociated by, which stating, re-starts stacking, forms the lens module after doing over again, until the test result meets the requirements.It is finding most During good matching degree, first mirror plate layers brought are not damaged, can also continue to using.
It in the third embodiment, can also be by adjusting first glue 410 and/or described in the rework operation The thickness of second glue 510, to adjust the distance between first mirror plate layers 100 and the second mirror plate layers 200, also of the invention Within thought range.
In addition, adjusting first mirror plate layers 100, spacer shims 300 and the second mirror plate layers 200 in the rework operation Between matching degree the step of can also include: the shape for adjusting first mirror plate layers 100 and/or second mirror plate layers 200 Shape, specifically, on first transparent conducting glass substrate 111 adjustable in the present embodiment the first lens 112 shape, Or the shape of the second lens 212 on second transparent conducting glass substrate 211 is adjusted, to find most suitable described first The shape of lens 112 and/or second lens 212.
Presently preferred embodiments of the present invention as described above, still, the present invention is not limited to contents disclosed above, such as:
First mirror plate layers and the second mirror plate layers can also be Double sided mirror lamella, and first lens include a pair of the One sub-lens, a pair of first sub-lens are located at one of first transparent conducting glass substrate towards the spacer shims Side and first transparent conducting glass substrate deviate from the side of the spacer shims, and second lens include that the second son of a pair is saturating Mirror, a pair of second sub-lens are located at side and institute of second transparent conducting glass substrate towards the spacer shims State the side that the second transparent conducting glass substrate deviates from the spacer shims;
In addition, first glue can also be coated in side of the spacer shims towards first mirror plate layers, or, described First glue is coated in side and the spacer shims of first mirror plate layers towards the spacer shims towards first mirror simultaneously The side of lamella;Also, second glue can also be coated in side of the spacer shims towards second mirror plate layers, or, Second glue is coated in side of second mirror plate layers towards the spacer shims and the spacer shims towards described the simultaneously The side of two mirror plate layers.
Obviously, various changes and modifications can be made to the invention without departing from essence of the invention by those skilled in the art Mind and range.In this way, if these modifications and changes of the present invention belongs to the range of the claims in the present invention and its equivalent technologies Within, then the present invention is also intended to include these modifications and variations.

Claims (10)

1. a kind of preparation method of lens module characterized by comprising
First mirror plate layers, spacer shims and the second mirror plate layers are provided;
, by the first glue sticking, it will will lead between the spacer shims and the second mirror plate layers between first mirror plate layers and spacer shims The second glue sticking is crossed, first mirror plate layers, spacer shims and the second mirror plate layers are stacked into lens module, wherein described first Glue or/and the second glue are that can dissociate glue;
The lens module is tested, judges whether test result meets the requirements, if test result is undesirable, Rework operation is carried out, until test result meets the requirements;
The rework operation includes:
Glue can be dissociated described in making under given conditions and loses viscosity, separate the lens module;
Adjust the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers, using it is described dissociate glue again into Row stacks, and forms the lens module after doing over again.
2. the preparation method of lens module as described in claim 1, which is characterized in that when first glue is that can dissociate glue When, the process for adjusting the matching degree between first mirror plate layers, spacer shims and the second mirror plate layers includes: adjustment first glue Thickness and/or first mirror plate layers shape;When second glue, which is, to dissociate glue, adjustment first mirror plate layers, The process of matching degree between spacer shims and the second mirror plate layers includes: the thickness and/or second mirror for adjusting second glue The shape of lamella;When first glue and second glue are that can dissociate glue, adjust first mirror plate layers, spacer shims and The process of matching degree between second mirror plate layers include: the thickness for adjusting first glue, the thickness of second glue, it is described between It is one or several in the shape of the thickness of feeler, the shape of first mirror plate layers and second mirror plate layers.
3. the preparation method of lens module as claimed in claim 2, which is characterized in that the spacer shims include through-hole, described First mirror plate layers include the first transparent conducting glass substrate and the first lens, and second mirror plate layers include the second electrically conducting transparent glass Glass substrate and the second lens, first lens and the second lens are corresponding with the through-hole.
4. the preparation method of lens module as claimed in claim 3, which is characterized in that first mirror plate layers and the second eyeglass Layer is single-surface mirror lamella, and first lens are located at one of first transparent conducting glass substrate towards the spacer shims Side, second lens are located at the side of second transparent conducting glass substrate towards the spacer shims;Or, first mirror Lamella and the second mirror plate layers are Double sided mirror lamella, and first lens include a pair of first sub-lens, a pair of first son Lens are located at side and the first electrically conducting transparent glass of first transparent conducting glass substrate towards the spacer shims Glass substrate deviates from the side of the spacer shims, and second lens include a pair of second sub-lens, a pair of second sub-lens It is located at side and the second transparent conducting glass base of second transparent conducting glass substrate towards the spacer shims Side of the backboard from the spacer shims.
5. the preparation method of lens module as claimed in claim 3, which is characterized in that the shape of adjustment first mirror plate layers Process include: to adjust the shape of first lens;The process for adjusting the shape of second mirror plate layers includes: described in adjustment The shape of second lens.
6. the preparation method of lens module as described in claim 1, which is characterized in that the glue that dissociates is hydrolysis glue, institute State the water environment that specified conditions are 80 DEG C or more.
7. the preparation method of lens module as described in claim 1, which is characterized in that first by first glue coated in described Side of first mirror plate layers towards the spacer shims, and/or, first by first glue coated in the spacer shims towards described the The side of one mirror plate layers, then first glue sticking will be passed through between first mirror plate layers and spacer shims;First by described second Glue is coated in the side of second mirror plate layers towards the spacer shims, and/or, second glue is first coated in the gap Side of the piece towards second mirror plate layers, then second glue sticking will be passed through between second mirror plate layers and spacer shims.
8. the preparation method of lens module as described in claim 1, which is characterized in that the thickness for dissociating glue be greater than etc. In 5 μm.
9. the preparation method of lens module as described in claim 1, which is characterized in that the test includes modulation transfer function Test, depth of field test and spatial frequency response test.
10. the preparation method of lens module as described in claim 1, which is characterized in that the spacer shims include through-hole, described First mirror plate layers include the first transparent conducting glass substrate and the first lens, and second mirror plate layers include the second electrically conducting transparent glass Glass substrate and the second lens, first lens and the second lens are corresponding with the through-hole.
CN201610766414.4A 2016-08-30 2016-08-30 The preparation method of lens module Active CN106291858B (en)