CN106217713B - A kind of mobile phone shell and preparation method thereof - Google Patents

A kind of mobile phone shell and preparation method thereof Download PDF

Info

Publication number
CN106217713B
CN106217713B CN201610625226.XA CN201610625226A CN106217713B CN 106217713 B CN106217713 B CN 106217713B CN 201610625226 A CN201610625226 A CN 201610625226A CN 106217713 B CN106217713 B CN 106217713B
Authority
CN
China
Prior art keywords
mobile phone
phone shell
rubber
preparation
hole
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201610625226.XA
Other languages
Chinese (zh)
Other versions
CN106217713A (en
Inventor
田妍基
王向春
田瑜基
马腾飞
吴先辉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Ningde Vocational and Technical College
Original Assignee
Ningde Vocational and Technical College
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ningde Vocational and Technical College filed Critical Ningde Vocational and Technical College
Priority to CN201610625226.XA priority Critical patent/CN106217713B/en
Publication of CN106217713A publication Critical patent/CN106217713A/en
Application granted granted Critical
Publication of CN106217713B publication Critical patent/CN106217713B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of mobile phone shells and preparation method thereof, mobile phone shell of the invention is rubber to be added in rubber solvent naphtha to add alkali grain after dissolution, mobile phone shell mold is injected, vulcanizing treatment is carried out to rubber, is finally smeared made from acid reagent at the mobile phone shell back side.The application method of mobile phone shell of the invention is that mobile phone shell is pressed in smooth object surface, air in the subsequent hole of mobile phone shell can partially be discharged, since rubber is bonded closely with body surface, air can not flow freely into hole again, the air pressure in hole is caused to be less than external atmosphere pressure, so the atmospheric pressure of mobile phone front can be by mobile phone shell pressure on a surface of an.Mobile phone shell produced by the present invention can not only function well as the effect of protection mobile phone, but also can liberate both hands, have multifunctionality.

Description

A kind of mobile phone shell and preparation method thereof
Technical field
The invention belongs to rubber mobile phone shell fields, and in particular to a kind of mobile phone shell and preparation method thereof.
Background technique
From last century the nineties, cell-phone cover or mobile phone shell start by the opportunity that mobile phone is reduced weight it is gradually prevailing, Its type also with mobile phone brand and function increase and in diversification, point have leather by quality, silica gel, cloth, duroplasts is soft Plastics, knitting wool, the product such as silk are other, and then have the difference of straight panel and flip lid by type point.It is limited by type, cell-phone cover is fitted Also different with classification, bar phone can usually use the other cell-phone cover of universal class, and slide phone and clamshell phone then often can only Select leather sheath.
Phone housing is no longer simple utility goods till now.With popularizing for mobile phone, almost each is chased after It asks the user of fashion to be intended to possess a unique mobile phone, gradually shows the one of individual character at them to mobile phone beauty Kind mode.In order to cater to this trend, mobile phone protective cover manufacturer is proposed that many workmanships are more superior, and colour image is more again Unique product, this makes the type more diversification of mobile phone protective cover.
Generalization, universalness in China, with various middle and high end mobile phones using crowd, it is seen that the development of global cell-phone cover Prospect, so that the manufacturer of cell-phone cover emerges as emerging rapidly in large numbersBamboo shoots after a spring rain.These companies produce cell-phone cover with a variety of materials, Also focus on beauty, individual character and the quality of cell-phone cover, the diversification of cell-phone cover simultaneously, diversification emerges one after another.
For existing phone housing mostly based on plastic material, design has all kinds of individualized patterns above in the market, but in addition to Protective effect when mobile phone is fallen, almost without other more utility functions.In daily life, people need in many occasions Mobile phone is fixed on a place to liberate both hands, when our rests in bed, it is desirable to which mobile phone is capable of fixing in headpiece Upper broadcasting video;When one section of video of self-timer being needed to upload to social networks when staying alone, it is desirable to which mobile phone can be just facing to oneself It fixes on the wall;Want to be directly anchored to mobile phone directly to play study course on vanity mirror when makeup;When shaving against mirror It wishes to for mobile phone being fixed on mirror and watches ball match;When needing and when friend's self-timer together needs mobile phone sticker building over there It builds on object;Mobile phone need to be placed directly against on equipment and be recorded when body-building;It needs on mobile phone sticker cabinet while to watch when cooking Menu study course etc..
Summary of the invention
In order to achieve this goal, the purpose of the present invention is to provide a kind of mobile phone shells and preparation method thereof.
A kind of technical solution of the invention is: a kind of mobile phone shell, and depth is equal to the thickness of mobile phone, and edge extends inwardly 1~2 millimeter, by mobile phone package in order to avoid mobile phone is deviate from, when needing to take out mobile phone, an angular outside of mobile phone shell is blocked with finger It moves, mobile phone can be detached from mobile phone shell.
Further, mobile phone shell is made of special rubber, and this material is the addition alkali grain system in rubber material It forms, the weight proportion of rubber and alkali grain is 80:20, and common alkali grain is calcium carbonate, magnesia, zinc oxide Deng.
Further, in the present invention there are many production methods of special rubber, principle is first by rubber and alkalinity Grain is fused together, and is fabricated to the shape of needs, and after special rubber is cooling, chemistry occurs using chemical solvent and alkali grain Partial alkaline grain dissolution will appear many holes in special rubber, chemical solvent is usually glacial acetic acid or third by reaction Acid, the reaction time 8~10 minutes.
Further, alkali grain will accomplish macroscopic size, and particle diameter is 0.2~0.3mm, undersized Words, the hole worked it out is smaller, and the dust being easy in absorption air causes the adsorption capacity of mobile phone shell to weaken.
Further, the surface that the inside of mobile phone shell is contacted with mobile phone is smooth, no hole, at the back side of mobile phone shell, distribution There is the dissolved hole of various alkali grains.
Further, application method of the invention is, after mobile phone is packed into mobile phone shell, when needing to liberate both hands, by hand Casing is attached on the object with smooth surface.
The present invention will be further described in detail with reference to the accompanying drawings and detailed description.
Detailed description of the invention
Fig. 1 is positive structure schematic of the invention;
Fig. 2 is structure schematic diagram of the invention;
Fig. 3 is the schematic diagram of the section structure of the invention.
Fig. 4 is using renderings of the invention.
In figure: 1- mobile phone shell;2- mobile phone;A- hole.
Specific embodiment
As shown in Figs 1-4, a kind of mobile phone shell, depth are equal to the thickness of mobile phone, and edge extends 1~2 millimeter inwardly, will Mobile phone package, when needing to take out mobile phone, is moved, mobile phone is in order to avoid mobile phone is deviate from the angular outside that finger blocks mobile phone shell Mobile phone shell can be detached from.
Further, the material of mobile phone shell uses special rubber, and this material is that alkali grain is added in rubber material It is made, the weight proportion of rubber and alkali grain is 80:20, and common alkali grain is calcium carbonate, magnesia, zinc oxide Deng.
Further, in the present invention there are many production methods of special rubber, principle is first by rubber and alkalinity Grain is fused together, and is fabricated to the shape of needs, and after special rubber is cooling, chemistry occurs using chemical solvent and alkali grain Partial alkaline grain dissolution will appear many holes by reaction in special rubber.Chemical solvent is usually glacial acetic acid or third Acid, the reaction time 8~10 minutes.Air meeting portion when mobile phone shell is pressed in smooth object surface, in the subsequent hole of mobile phone shell Divide discharge, since rubber is bonded closely with body surface, air can not flow freely into hole again, and the air pressure in hole is caused to be less than External atmosphere pressure, so the atmospheric pressure of mobile phone front can be by mobile phone shell pressure on a surface of an.
Embodiment 1
By taking 5.5 inches of screen mobile phone shells as an example, a kind of preparation method of mobile phone shell:
(1) mold of mobile phone shell is made according to the size characteristic of mobile phone using metal material 3Cr2W8V steel, mold is divided into Upper die and lower die, after upper and lower mould is combined, internal void shape is exactly the shape of mobile phone shell, and mobile phone shell is long by 158~ 160mm, wide 78~80mm, high 6~7mm, 0.8~1mm of shell thickness;
(2) 30g rubber is put into 300 DEG C of heating in rubber solvent naphtha 100ml until being completely dissolved, calcium carbonate granule is added It is stirred evenly after 7.5g, is then injected into mold and is cooled to room temperature;
(3) after the rubber solvent naphtha volatilization in rubber, vulcanizing treatment is carried out to rubber, increases its surface hardness extremely 80HRB;
(4) acid reagent glacial acetic acid 300ml is smeared at the mobile phone shell back side, by the macroscopic calcium carbonate in the mobile phone shell back side Grain dissolution, forms small holes, then rinsed well with 1L pure water.
Further, the diameter of alkali grain is 0.3mm, and if undersized, the hole worked it out is smaller, is easy absorption Dust in air causes the adsorption capacity of mobile phone shell to weaken.
Further, the surface that the inside of mobile phone shell is contacted with mobile phone is smooth, no hole, at the back side of mobile phone shell, distribution There is the dissolved hole of various calcium carbonate granules.
Further, application method of the invention is, after mobile phone is packed into mobile phone shell, when needing to liberate both hands, by hand Casing is attached on the object with smooth surface, such as marble, ceramic tile, mirror, glass, smooth metal etc..
Embodiment 2
By taking 4.3 inches of screen mobile phone shells as an example, a kind of preparation method of mobile phone shell:
(1) mold of mobile phone shell is made according to the size characteristic of mobile phone using metal material 5CrMnMo steel, mold is divided into Upper die and lower die, after upper and lower mould is combined, internal void shape is exactly the shape of mobile phone shell, and mobile phone shell is long by 93~ 95mm, wide 53~56mm, high 6~7mm, 0.8~1mm of shell thickness;
(2) 23.2g rubber is put into 300 DEG C of heating in rubber solvent naphtha 100ml until being completely dissolved, zinc oxide is added It is stirred evenly after grain 5.8g, is then injected into mold and is cooled to room temperature;
(3) vulcanizing treatment is carried out to rubber, increases its surface hardness to 85HRB;
(4) acid reagent propionic acid 250ml is smeared at the mobile phone shell back side, by the macroscopic Zinc oxide particles in the mobile phone shell back side Dissolution forms small holes, then is rinsed well with 1L pure water.
Further, the diameter of Zinc oxide particles is 0.2mm, and if undersized, the hole worked it out is smaller, is easy to inhale Dust in attached air causes the adsorption capacity of mobile phone shell to weaken.
Further, the surface that the inside of mobile phone shell is contacted with mobile phone is smooth, no hole, at the back side of mobile phone shell, distribution There is the dissolved hole of various Zinc oxide particles.
Further, application method of the invention is, after mobile phone is packed into mobile phone shell, when needing to liberate both hands, by hand Casing is attached on the object with smooth surface, such as marble, ceramic tile, mirror, glass, smooth metal etc..
Embodiment 3
By taking 4.3 inches of screen mobile phone shells as an example, a kind of preparation method of mobile phone shell:
(1) mold of mobile phone shell is made according to the size characteristic of mobile phone using metal material 5CrMnMo steel, mold is divided into Upper die and lower die, after upper and lower mould is combined, internal void shape is exactly the shape of mobile phone shell, and mobile phone shell is long by 93~ 95mm, wide 53~56mm, high 6~7mm, 0.8~1mm of shell thickness;
(2) 23.2g rubber is put into 300 DEG C of heating in rubber solvent naphtha 100ml until being completely dissolved, magnesia is added It is stirred evenly after grain 5.8g, is then injected into mold and is cooled to room temperature;
(3) vulcanizing treatment is carried out to rubber, increases its surface hardness to 85HRB;
(4) acid reagent propionic acid 250ml is smeared at the mobile phone shell back side, by the macroscopic magnesium oxide particle in the mobile phone shell back side Dissolution forms small holes, then is rinsed well with 1L pure water.
Further, the diameter of magnesium oxide particle is 0.2mm, and if undersized, the hole worked it out is smaller, is easy to inhale Dust in attached air causes the adsorption capacity of mobile phone shell to weaken.
Further, the surface that the inside of mobile phone shell is contacted with mobile phone is smooth, no hole, at the back side of mobile phone shell, distribution There is the dissolved hole of various magnesium oxide particles.
Further, application method of the invention is, after mobile phone is packed into mobile phone shell, when needing to liberate both hands, by hand Casing is attached on the object with smooth surface, such as marble, ceramic tile, mirror, glass, smooth metal etc..
The foregoing is merely presently preferred embodiments of the present invention, all equivalent changes done according to scope of the present invention patent with Modification, is all covered by the present invention.

Claims (4)

1. a kind of preparation method of mobile phone shell, which is characterized in that specifically includes the following steps:
(1) 300 DEG C of heating in 100ml rubber solvent naphtha are added until being completely dissolved in 23.2-30g rubber, 5.8-7.5g is added It is stirred evenly after alkali grain, is then injected into mobile phone shell mold and is cooled to room temperature;
(2) after the rubber solvent naphtha volatilization in rubber, vulcanizing treatment is carried out to rubber, increase its surface hardness to 80~ 85HRB;
(3) acid reagent 250-300ml is smeared at the mobile phone shell back side, the reaction time 8~10 minutes, forms small holes, then use 1L Pure water is rinsed well;
The diameter of alkali grain in the step (1) is 0.2-0.3mm;
The surface that the inside of mobile phone shell obtained is contacted with mobile phone is smooth, no hole, and at the back side of mobile phone shell, various alkali are distributed with Hole after property grain dissolution;
Application method are as follows: after mobile phone is packed into mobile phone shell, when needing to liberate both hands, mobile phone shell is attached to smooth surface On object.
2. the preparation method of mobile phone shell according to claim 1, which is characterized in that the alkali grain in the step (1) For one kind of calcium carbonate, magnesia, zinc oxide.
3. the preparation method of mobile phone shell according to claim 1, which is characterized in that the acid reagent in the step (3) For glacial acetic acid or propionic acid.
4. mobile phone shell made from a kind of preparation method as described in claim 1-3 is any.
CN201610625226.XA 2016-08-03 2016-08-03 A kind of mobile phone shell and preparation method thereof Active CN106217713B (en)