CN106190083A - The preparation method of petroleum crude oil thinner - Google Patents

The preparation method of petroleum crude oil thinner Download PDF

Info

Publication number
CN106190083A
CN106190083A CN201610515180.6A CN201610515180A CN106190083A CN 106190083 A CN106190083 A CN 106190083A CN 201610515180 A CN201610515180 A CN 201610515180A CN 106190083 A CN106190083 A CN 106190083A
Authority
CN
China
Prior art keywords
parts
crude oil
petroleum crude
preparation
added
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610515180.6A
Other languages
Chinese (zh)
Inventor
贺昶明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Sichuan Xingzhi Zhihui Intellectual Property Operation Co Ltd
Original Assignee
Sichuan Xingzhi Zhihui Intellectual Property Operation Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Sichuan Xingzhi Zhihui Intellectual Property Operation Co Ltd filed Critical Sichuan Xingzhi Zhihui Intellectual Property Operation Co Ltd
Priority to CN201610515180.6A priority Critical patent/CN106190083A/en
Publication of CN106190083A publication Critical patent/CN106190083A/en
Pending legal-status Critical Current

Abstract

The invention discloses the preparation method of petroleum crude oil thinner, the viscosity break ratio solving existing petroleum crude oil thinner is undesirable, especially on paraffin content without impact, causes exploiting the problem being difficult to.The present invention includes: step one, be added to the water mix homogeneously by 2 (3,4 dihydroxy phenyl) ethamine, lignin;Step 2, heating, and in heating process, it is added sequentially carbon tetrachloride, o-tert-butylphenol, polyisobutene succinimide, methyl formate, poly alkyl alcohol ethylene oxide ether sulfates ester and sodium hydroxide, mix homogeneously;Step 3, added after, reach 60~80 DEG C in temperature and keep at least 2h;Step 4, dried below 100 DEG C.The present invention has a viscosity break ratio being effectively increased petroleum crude oil, and effectively reduces the advantages such as paraffin content in crude oil.

Description

The preparation method of petroleum crude oil thinner
Technical field
The present invention relates to a kind of thinner, be specifically related to the preparation method of petroleum crude oil thinner.
Background technology
In viscous crude, light constituent content is low, and asphalitine and gum level are higher, and straight-chain hydrocarbons content is few, thus causes major part thick Oil has high viscosity and highdensity characteristic, exploits and transport extremely difficult.At present, commonly use both at home and abroad during thickened oil recovery Fall sticking method have heating, mixing light oil method, upgrading fall glutinous and the glutinous method of chemical agent fall.Breast is added when thick oil steam drive Changing visbreaking agent, be a kind of newer the Technology of Heavy Oil Recovery, the key component of reducing viscosity by emulsification agent is surfactant, by reducing oil Water interfacial tension, makes the viscous crude in stratum be changed into the emulsified state with water as foreign minister from water in oil emulsified state, makes viscous crude Viscosity is greatly lowered, and recovery ratio significantly improves.
The viscosity break ratio of existing petroleum crude oil thinner is undesirable, especially on paraffin content without impact, causes exploiting being difficult to Problem.
Summary of the invention
The technical problem to be solved is: the viscosity break ratio of existing petroleum crude oil thinner is undesirable, the most right Paraffin content, without impact, causes exploiting the problem being difficult to, it is provided that solve the preparation method of the petroleum crude oil thinner of the problems referred to above.
The present invention is achieved through the following technical solutions:
The preparation method of petroleum crude oil thinner, including:
Step one, be added to the water mix homogeneously by 2-(3,4-dihydroxy phenyl) ethamine, lignin;
Step 2, heating, and in heating process, it is added sequentially carbon tetrachloride, o-tert-butylphenol, polyisobutylene succinyl Asia Amine, methyl formate, poly alkyl alcohol ethylene oxide ether sulfates ester and sodium hydroxide, mix homogeneously;
Step 3, added after, reach 60~80 DEG C in temperature and keep at least 2h;
Step 4, dried below 100 DEG C;
The weight portion of above-mentioned each component is: 2-(3,4-dihydroxy phenyl) ethamine 5~8 parts, polyisobutene succinimide 10~ 15 parts, methyl formate 5~8 parts, poly alkyl alcohol ethylene oxide ether sulfates ester 10~15 parts, o-tert-butylphenol 3~6 parts, wooden Element 5~8 parts, carbon tetrachloride 2~4 parts, sodium hydroxide 1~2 parts.
Further, described 2-(3,4-dihydroxy phenyl) ethamine 6~7 parts, polyisobutene succinimide 13~15 parts, Methyl formate 5~6 parts, poly alkyl alcohol ethylene oxide ether sulfates ester 12~14 parts, o-tert-butylphenol 5~6 parts, lignin 7~8 Part, carbon tetrachloride 2~3 parts, sodium hydroxide 1~2 parts.
Further, 7 parts of described 2-(3,4-dihydroxy phenyl) ethamine, polyisobutene succinimide 13 parts, formic acid Methyl ester 5 parts, poly alkyl alcohol ethylene oxide ether sulfates ester 13 parts, o-tert-butylphenol 6 parts, lignin 7 parts, carbon tetrachloride 2 parts, hydrogen Sodium oxide 2 parts.
The present invention compared with prior art, has such advantages as and beneficial effect:
The present invention, by each constituent and the optimization of proportioning, effectively makes the thinner of the present invention be effectively increased the fall of petroleum crude oil Viscous rate, and effectively reduce the paraffin content in crude oil.
Detailed description of the invention
For making the object, technical solutions and advantages of the present invention clearer, below in conjunction with embodiment, the present invention is made Further describing in detail, the exemplary embodiment of the present invention and explanation thereof are only used for explaining the present invention, are not intended as this The restriction of invention.
Embodiment
The preparation method of petroleum crude oil thinner, including:
Step one, be added to the water mix homogeneously by 2-(3,4-dihydroxy phenyl) ethamine, lignin;
Step 2, heating, and in heating process, it is added sequentially carbon tetrachloride, o-tert-butylphenol, polyisobutylene succinyl Asia Amine, methyl formate, poly alkyl alcohol ethylene oxide ether sulfates ester and sodium hydroxide, mix homogeneously;
Step 3, added after, reach 60~80 DEG C in temperature and keep at least 2h;
Step 4, dried below 100 DEG C;
The weight portion of above-mentioned each component is: 2-(3,4-dihydroxy phenyl) ethamine 5~8 parts, polyisobutene succinimide 10~ 15 parts, methyl formate 5~8 parts, poly alkyl alcohol ethylene oxide ether sulfates ester 10~15 parts, o-tert-butylphenol 3~6 parts, wooden Element 5~8 parts, carbon tetrachloride 2~4 parts, sodium hydroxide 1~2 parts.
In the present embodiment, the concrete parts by weight of each constituent are as shown in table 1.
Table 1
The thinner of the material composition of weight portion in above-mentioned table 1 is carried out viscosity break ratio and the performance test of paraffin content slip, contains Wax amount slip refer to former paraffin content and add after the difference of paraffin content divided by the percentage value of former paraffin content, this test result such as table Shown in 2.
Table 2
By the test data of above-mentioned table 2, the data in present example 1-example 3 show: proportioning of the present invention, effectively increase Adding viscosity break ratio and the paraffin content slip of the present invention, effect is the most notable.
Above-described detailed description of the invention, has been carried out the purpose of the present invention, technical scheme and beneficial effect further Describe in detail, be it should be understood that the detailed description of the invention that the foregoing is only the present invention, be not intended to limit the present invention Protection domain, all within the spirit and principles in the present invention, any modification, equivalent substitution and improvement etc. done, all should comprise Within protection scope of the present invention.

Claims (3)

1. the preparation method of petroleum crude oil thinner, it is characterised in that including:
Step one, be added to the water mix homogeneously by 2-(3,4-dihydroxy phenyl) ethamine, lignin;
Step 2, heating, and in heating process, it is added sequentially carbon tetrachloride, o-tert-butylphenol, polyisobutylene succinyl Asia Amine, methyl formate, poly alkyl alcohol ethylene oxide ether sulfates ester and sodium hydroxide, mix homogeneously;
Step 3, added after, reach 60~80 DEG C in temperature and keep at least 2h;
Step 4, dried below 100 DEG C;
The weight portion of above-mentioned each component is: 2-(3,4-dihydroxy phenyl) ethamine 5~8 parts, polyisobutene succinimide 10~ 15 parts, methyl formate 5~8 parts, poly alkyl alcohol ethylene oxide ether sulfates ester 10~15 parts, o-tert-butylphenol 3~6 parts, wooden Element 5~8 parts, carbon tetrachloride 2~4 parts, sodium hydroxide 1~2 parts.
The preparation method of petroleum crude oil thinner the most according to claim 1, it is characterised in that described 2-(3,4-bis- Hydroxy phenyl) ethamine 6~7 parts, polyisobutene succinimide 13~15 parts, methyl formate 5~6 parts, poly alkyl alcohol epoxy second Alkane ether sulfuric ester 12~14 parts, o-tert-butylphenol 5~6 parts, lignin 7~8 parts, carbon tetrachloride 2~3 parts, sodium hydroxide 1~ 2 parts.
The preparation method of petroleum crude oil thinner the most according to claim 1, it is characterised in that described 2-(3,4-bis- Hydroxy phenyl) 7 parts of ethamine, polyisobutene succinimide 13 parts, methyl formate 5 parts, poly alkyl alcohol ethylene oxide ether sulfates ester 13 parts, o-tert-butylphenol 6 parts, lignin 7 parts, carbon tetrachloride 2 parts, sodium hydroxide 2 parts.
CN201610515180.6A 2016-07-04 2016-07-04 The preparation method of petroleum crude oil thinner Pending CN106190083A (en)