CN106145626A - The manufacture method of a kind of glass cover-plate, glass cover-plate and mobile terminal - Google Patents

The manufacture method of a kind of glass cover-plate, glass cover-plate and mobile terminal Download PDF

Info

Publication number
CN106145626A
CN106145626A CN201610479378.3A CN201610479378A CN106145626A CN 106145626 A CN106145626 A CN 106145626A CN 201610479378 A CN201610479378 A CN 201610479378A CN 106145626 A CN106145626 A CN 106145626A
Authority
CN
China
Prior art keywords
glass substrate
double curved
curved glass
area
plate
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610479378.3A
Other languages
Chinese (zh)
Inventor
冷雪翔
谭小芳
林四亮
余锋
于脉军
吴晓楠
张维
王坤
朱华胜
莫博宇
戴乃仁
孙国栋
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Vivo Mobile Communication Co Ltd
Original Assignee
Vivo Mobile Communication Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Vivo Mobile Communication Co Ltd filed Critical Vivo Mobile Communication Co Ltd
Priority to CN201610479378.3A priority Critical patent/CN106145626A/en
Publication of CN106145626A publication Critical patent/CN106145626A/en
Pending legal-status Critical Current

Abstract

The invention provides the manufacture method of a kind of glass cover-plate, glass cover-plate and mobile terminal, relate to terminal manufacture technology field, solve existing glass cover-plate and be substantially plane or 2.5D, homogeneity is seriously difficult to the problem meeting people to high-quality appearance requirement.This manufacture method includes: cut pristine glass base material and hot-pressing processing, obtain double curved glass substrate, the double-edged edge of double curved glass substrate is cambered surface, and the cambered surface bending direction of the tow sides edge of double curved glass substrate is identical;Forming the first area being coated with the first predetermined color on the reverse side of double curved glass substrate, obtain double curved glass cover plate, first area is the region on double curved glass substrate in addition to predetermined middle window area and predetermined openings.The solution of the present invention defines the 3D double curved glass cover plate with particular color, novel and beautiful appearance, meets people's appearance requirement to glass cover-plate high-quality, and low cost of manufacture.

Description

The manufacture method of a kind of glass cover-plate, glass cover-plate and mobile terminal
Technical field
The present invention relates to terminal manufacture technology field, particularly relate to the manufacture method of a kind of glass cover-plate, glass cover-plate and Mobile terminal.
Background technology
Along with making rapid progress of consumer electronics product, the product competition of various brands is fierce, and consumer is for consumer electricity The requirement of sub-product is more and more higher, except hardware specification (such as processor, screen size and pixel, the network of electronic product Standard, camera pixel etc.), the appearance design of electronic product is valued the most very much by consumer.
As a example by TW cover plate in 3C Product, glass cover-plate in the market is substantially plane or 2.5D, homogeneity Change serious, lack novelty.The most existing glass cover-plate has been difficult to the appearance requirement meeting people to product high-quality.
Summary of the invention
The embodiment of the present invention provides the manufacture method of a kind of glass cover-plate, glass cover-plate and mobile terminal, existing to solve In technology, glass cover-plate is substantially plane or 2.5D, and homogeneity is serious, lacks novelty, it is difficult to meet people high to product The problem of the appearance requirement of quality.
First aspect, it is provided that the manufacture method of a kind of glass cover-plate, including:
Pristine glass base material is cut and hot-pressing processing, obtains double curved glass substrate, described double curved glass base The double-edged edge of plate is cambered surface, and the cambered surface of the tow sides edge of described double curved glass substrate is curved Qu Fangxiang is identical;
The reverse side of described double curved glass substrate is formed the first area being coated with the first predetermined color, obtains hyperbolic Surface glass cover plate, described first area be on described double curved glass substrate in the middle of predetermined in addition to window area and predetermined openings Region.
Second aspect, it is provided that a kind of glass cover-plate, the double-edged edge of described glass cover-plate is cambered surface, And the cambered surface bending direction of the tow sides edge of described glass cover-plate is identical;
Being formed with the first area being coated with the first predetermined color on the reverse side of described glass cover-plate, described first area is On described glass cover-plate in the middle of predetermined region in addition to window area and predetermined openings.
The third aspect, additionally provides a kind of mobile terminal, including glass cover-plate as above.
So, in the embodiment of the present invention, first pristine glass base material is cut and hot-pressing processing, obtain hyperboloid glass Glass substrate, the double-edged edge of this double curved glass substrate is cambered surface, and this double curved glass substrate is positive and negative The cambered surface bending direction of edge, two sides is identical;Then on the reverse side of double curved glass substrate formed be coated with first make a reservation for The first area of color (such as white), thus obtain double curved glass cover plate (the alternatively referred to as 3D hyperboloid with particular color Glass cover-plate), wherein first area is the district on double curved glass substrate in addition to predetermined middle window area and predetermined openings Territory.Made by brand-new technique and define the 3D double curved glass cover plate with particular color, novel in appearance, visual effect Good, meet people's appearance requirement to glass cover-plate high-quality, and low cost of manufacture, can be mass, widely should have Use prospect.Efficiently solving glass cover-plate in prior art and be substantially plane or 2.5D, homogeneity is serious, lacks novelty Property, it is difficult to meet people's problem to the appearance requirement of product high-quality.
Accompanying drawing explanation
In order to be illustrated more clearly that the technical scheme of the embodiment of the present invention, below will be in embodiment or description of the prior art The required accompanying drawing used is briefly described, it should be apparent that, the accompanying drawing in describing below is only some realities of the present invention Execute example, for those of ordinary skill in the art, on the premise of not paying creative work, it is also possible to attached according to these Figure obtains other accompanying drawing.
Fig. 1 is the flow chart of the manufacture method of glass cover-plate of the present invention;
Fig. 2 is the glass structure schematic diagram before and after the manufacture method CNC process of glass cover-plate of the present invention;
Fig. 3 is the operation chart that the manufacture method of glass cover-plate of the present invention is processed by hot pressing die;
Fig. 4 is the concrete applicating flow chart of the manufacture method of glass cover-plate of the present invention;
Fig. 5 is the structural representation of the glass cover-plate that the manufacture method of glass cover-plate of the present invention obtains.
Detailed description of the invention
Below in conjunction with the accompanying drawing in the embodiment of the present invention, the technical scheme in the embodiment of the present invention is carried out clear, complete Describe, it is clear that described embodiment is a part of embodiment of the present invention rather than whole embodiments wholely.Based on this Embodiment in bright, the every other enforcement that those of ordinary skill in the art are obtained under not making creative work premise Example, broadly falls into the scope of protection of the invention.
First embodiment
As it is shown in figure 1, the manufacture method of the glass cover-plate of the embodiment of the present invention, including:
Step 101, cuts and hot-pressing processing pristine glass base material, obtains double curved glass substrate, described hyperbolic The double-edged edge of surface glass substrate is cambered surface, and the tow sides edge of described double curved glass substrate Cambered surface bending direction identical.
Here, by pristine glass base material is cut and hot-pressing processing, obtained 3D double curved glass, used this 3D The glass cover-plate that double curved glass makes, has more attractive, novel appearance, and has more preferable visual effect.
Step 102, forms the first area being coated with the first predetermined color on the reverse side of described double curved glass substrate, Obtaining double curved glass cover plate, described first area is except making a reservation for middle window area and making a reservation on described double curved glass substrate Region outside perforate.
Here, by forming the first area of the first predetermined color on the reverse side of double curved glass substrate, had There is the 3D double curved glass cover plate of particular color.
First predetermined color can be such as white, pink, powder green, purple powder, rose gold etc..Specifically can be according to actual need Seek any one color of selection, in this no limit.
The manufacture method of the glass cover-plate of the embodiment of the present invention, is defined by brand-new technique making and has particular color 3D double curved glass cover plate, novel in appearance, good visual effect, meet people's appearance requirement to glass cover-plate high-quality, And low cost of manufacture, can be mass, be with a wide range of applications.Efficiently solve in prior art glass cover-plate the most all Being plane or 2.5D, homogeneity is serious, lacks novelty, it is difficult to meet people's asking the appearance requirement of product high-quality Topic.
Preferably, the step of above-mentioned steps 101 may include that
Step 1011, carries out cutting process to pristine glass base material, obtains the first stage glass of predefined size, reservation shape Glass base material.
Here, first pristine glass base material is carried out cutting process according to predefined size, reservation shape so that after cutting Glass baseplate matches with the size of terminal unit.
Step 1012, by hot pressing die set in advance, to described first stage glass base under the first predetermined temperature Material carries out hot pressing, obtains first stage double curved glass substrate.
Here, by hot pressing die set in advance, use uniform pressure to first stage glass under the first predetermined temperature Glass base material carries out hot pressing, can quickly obtain molding effect preferable double curved glass substrate.
Wherein, first stage glass baseplate progressively can be heated up, sequentially be heated to molten condition, then to molten The glass baseplate of state carries out hot pressing.
Step 1013, cools down described first stage double curved glass substrate, obtains second stage double curved glass Substrate.
Here, at high operating temperatures glass baseplate is carried out hot-forming after, need the double curved glass substrate that will obtain It is cooled to room temperature, so that double curved glass substrate to be further processed.
Wherein, first stage double curved glass substrate progressively can be cooled down, sequentially be cooled to room temperature.
Now, by cutting, the PROCESS FOR TREATMENT such as hot-forming, obtain molding effect preferable double curved glass substrate, Guarantee is provided for ensuing further process.
Concrete, in above-mentioned steps 1011, blanking can be first passed around, large stretch of pristine glass base material is cut into corresponding chi Very little little sheet glass;Then CNC (Computer Numerical Control, computer digital control machine tool) is used to process little The appearance profile of sheet glass and curved surface;As in figure 2 it is shown, little sheet glass 1 has obtained predefined size, preboarding after CNC processes The first stage glass baseplate 2 of shape.
The silver-colored steel that wearability can be used stronger due to CNC props up emery wheel and designs with gang tool, therefore to little sheet glass outside Shape profile, curved surface can be processed and formed at one time, and midway, without tool changing, improves yield rate and working (machining) efficiency.
Concrete, in above-mentioned steps 1012, hot pressing die can use graphite material, and the surface of graphite material is carried out height Precision polishes.The hot-die made due to graphite has a preferable heat conductivility, the most hot-forming soon, and the table of graphite material Face is through high accuracy polishing, it is ensured that the flatness of finished surface and smoothness.
Wherein, hot pressing die can include top board 3 and lower platen 4, and top board 3 is arranged on the top of lower platen 4.And upper pressure The lower surface of plate 3 forms first arc shape corresponding with the reverse side of double curved glass substrate, and the upper surface of lower platen 4 is formed The second arc shape answered with the vis-a-vis of double curved glass substrate.The additionally upper surface of top board 3 and the following table of lower platen 4 Face is respectively provided with having heaters 5.
During as it is shown on figure 3, above-mentioned steps 1012 carries out hot pressing by hot pressing die to first stage glass baseplate 2, can be first First first stage glass baseplate 2 is placed between the top board 3 of hot pressing die and lower platen 4, now first stage glass base Material 2 remains as flat shape;By heater 5, first stage glass baseplate 2 is progressively heated up again, make glass sequentially heat To molten condition;Then pressure applied above to top board 3 under the first predetermined temperature, make the lower surface of top board 3 with under press The upper surface of plate 4 is gripping into together under pressure, and now first stage glass baseplate 2 occurs modification;Finally by top board 3 Removing above lower platen 4, the double curved glass substrate taking out molding is progressively lowered the temperature.
Wherein general heat pressing process temperature is set between 720 DEG C-780 DEG C, and the first predetermined temperature refers to general hot pressing Technological temperature is arranged.
Further, above-mentioned steps 1012,1013 can include 11 following road molding procedure: the first step heats up, temperature 500 ℃;Second step heats up, temperature 550 DEG C;3rd step heats up, temperature 650 DEG C;4th step heats up, temperature 750 DEG C;5th step pressurization, Temperature 750 DEG C, pressure 20N/cm2;6th step pressurization, temperature 770 DEG C, pressure 30N/cm2;7th step pressurization, temperature 800 DEG C, Pressure 20N/cm2;8th step cooling, temperature 750 DEG C;9th step cooling, temperature 700 DEG C;Tenth step cooling, temperature 600 DEG C;The 11 step coolings, temperature 550 DEG C;May also include the cooling outside 4 step equipment below, be gradually cooled to room temperature, each step time is 90 seconds.
Now, cold by the material putting into hot pressing die is progressively heated up sequentially heating, progressively pressurization and favorable balance But, molding effect preferable double curved glass substrate has been obtained.
After obtaining double curved glass substrate, specific face can be formed by above-mentioned steps 102 at double curved glass substrate back side Color.Preferably, the step of above-mentioned steps 102 may include that
Step 1021, on the reverse side of described double curved glass substrate, protection is pasted in the region in addition to described first area Film.
Here, first pass through viscous in the region (such as predetermined middle window area and predetermined openings region) in addition to first area Pasting protective film, it is to avoid impact on these regions in processing procedure afterwards.
Step 1022, uses the first predetermined color ink to enter the reverse side of the described double curved glass substrate of bonding protective film After row spraying and baking process, the second predetermined color ink is used to spray and dry the reverse side of described double curved glass substrate Roasting process.
Here, first at whole even application the first predetermined color ink of reverse side of double curved glass substrate, such as white ink, After baking, more whole even application the second predetermined color ink of reverse side at double curved glass substrate, such as black ink, and carry out Baking.
Step 1023, removes and is pasted onto the protecting film on the reverse side of described double curved glass substrate, is formed at first and makes a reservation for The first area of the second predetermined color it is coated with in color.
Here, after being removed by the protecting film pasted, due to the bridging effect of protecting film, predetermined middle window area is with predetermined Opening area will not colour, therefore, it is possible to be formed on the first predetermined color the firstth district being coated with the second predetermined color Territory.
Now, the reverse side at double curved glass substrate defines specific color, thus has obtained having particular color 3D double curved glass cover plate, adds novelty, has beautified appearance.And by covering the on the first predetermined color ink Two predetermined color ink, obtain the second predetermined color ink as lid base oil ink, it is to avoid the first predetermined color printing opacity, further Ensure that the color effects formed on 3D double curved glass cover plate.And spray by pad pasting, ink, toast and striping, obtain The double curved glass substrate with particular color, technological process is short, efficiency is high, and technological effect is good, low cost.
It should be noted that for the coloring effect ensureing first area, the present invention can spray one the most respectively Determining the ink of thickness, thus improve color effects, often, the ink gross thickness finally given can control in 30 ± 5 μm.
Wherein, it has been mentioned hereinbefore that the first predetermined color can be such as white, pink, powder green, purple powder, rose gold Deng.Specifically can select any one color according to the actual requirements, in this no limit.
Second predetermined color covers on the first predetermined color, it is to avoid the first predetermined color printing opacity, therefore optional deeper Color, such as black, black-and-blue etc..Certainly, the second predetermined color selects also dependent on actual demand, does not makees at this Limit.
Wherein, before using particular color ink to whole even application of reverse side of double curved glass substrate, also can first basis The shape of double curved glass substrate makes corresponding spray finishing jig, then by spray finishing jig further need not spray to Regions shield.Spray distance typically uses 13cm, and toasts in process, and baking time is preferably 10 minutes, and baking temperature is preferred It it is 150 DEG C.
Wherein, it is preferred that described protecting film uses high temperature resistance polyester thin film.
Will be appreciated that high temperature resistance polyester thin film has another name called PET film, there is physical property, chemical property and the chi of excellence Very little stability, the transparency, recuperability, it is possible to realize predetermined middle window area and predetermined openings region are more preferably protected effect Really.Certainly, protecting film can also use the thin film of other materials to realize, and does not repeats them here.
In the embodiment of the present invention, in order to increase the appearance of glass cover-plate further, it is preferred that above-mentioned steps 102 Before step, described manufacture method can also include:
Step 103, forms the second area being coated with the 3rd predetermined color on the reverse side of described double curved glass substrate, Described second area is the region on described double curved glass substrate in addition to predetermined middle window area and predetermined openings, and institute State second area around described predetermined middle window area.
Here, second area can be by the lines of reservation shape around middle window area, to form specific lines.Should The lines of reservation shape such as lines or the lines etc. of lattice shape that can be rectilinear form.
Wherein the 3rd predetermined color selects also dependent on actual demand, as being black, blueness etc., does not limits at this Fixed.
It is different colours as the preferably the 3rd predetermined color and the first predetermined color.
Assuming that second area passes through the lines of rectilinear form around middle window area, and the 3rd predetermined color is black, Then second area shows as a black surround.
Now, by forming the second area being coated with the 3rd predetermined color on double curved glass substrate, it is possible to obtain There is the 3D double curved glass cover plate of specific lines (such as black surround), further increase novelty and the outward appearance effect of glass cover-plate Really.
Concrete, the step of above-mentioned steps 103 may include that
Step 1031, use the 3rd predetermined color photosensitive-ink to spray the reverse side of described double curved glass substrate, Cover and exposure-processed, form the second area being coated with the 3rd predetermined color.
Now, by the method for photosensitive-ink exposure imaging, it is possible to the reverse side at double curved glass substrate is formed has spy Determine the second area of lines, thus obtain the 3D double curved glass cover plate with specific lines, add novelty, outside having beautified See effect.
Concrete, step 1031 includes:
Step 10311, uses the 3rd predetermined color photosensitive-ink to spray the reverse side of described double curved glass substrate Process.
Here, corresponding spray finishing jig can be made according to the shape of double curved glass substrate, then be existed by spray finishing jig Whole even application the 3rd predetermined color photosensitive-ink of the reverse side of glass substrate, such as black photosensitive ink.
Step 10312, is carried out the described double curved glass substrate the 3rd predetermined color photosensitive-ink in addition to second area Cover.
Here, can use and cover the ink that needs are faded away by plate MASK, i.e. the 3rd predetermined color in addition to second area The carrying out of photosensitive-ink is covered, and stays the 3rd predetermined color photosensitive-ink of second area to be exposed.
Such as the photosensitive-ink of first area, middle window area and some position of opening can be covered.Shielded Ink can be eliminated by subsequent step.
Step 10313, uses ultraviolet to clean after being exposed processing to described double curved glass substrate, and formation is coated with The second area of the 3rd predetermined color.
Here, first ultraviolet is used to be exposed, through the effect of ultraviolet, second area double curved glass substrate Photosensitive-ink exposure curing, be attached to the surface of double curved glass substrate;Shielded region does not has illumination, thus the most solid Change.Then being carried out double curved glass substrate, after clear water rinses, the ink in shielded region can be faded away, only Leave the ink of second area, thus on double curved glass substrate, form the second area with specific lines.
Wherein, can use ultraviolet (UV) lamp that double curved glass substrate is exposed.
Now, by the method for photosensitive-ink exposure imaging, it is possible to the reverse side at double curved glass substrate is formed has spy Determine the second area of lines, thus obtain the 3D double curved glass cover plate with specific lines, add novelty, outside having beautified See effect.And the method precision of photosensitive-ink exposure imaging is the highest, it is very thin that lines can do, therefore, it is possible to formed finer Lines, thus further increase second area formed appearance.
Here, as a example by black photosensitive ink, after single exposure development, black ink thickness is about 3-5 μm, the most also The black surround thickness that can reach as required is to regulate the number of times that exposure imaging is carried out.
Further, before the step of above-mentioned steps 102, described manufacture method can also include:
Step 104, by the fused salt with the second predetermined temperature being pre-configured with, is carried out described double curved glass substrate Intensive treatment, the double curved glass substrate strengthened.
Here, by the high-temperature molten salt being pre-configured with, it is possible to the mechanism spread by ion changes the surface group of glass Become, and then improve the intensity of glass.Concrete, at a certain temperature glass is immersed in high-temperature molten salt, the sodium in glass Ion is intercoursed because of diffusion with the potassium ion in fused salt, produces " jammed " phenomenon, and making glass surface produce compression should Power such that it is able to improve the intensity of glass.
Now, by fused salt, glass is strengthened, add the intensity of glass cover-plate, improve the practicality of product.
Wherein fused salt material comprise the steps that KNO3, AL2O3, potassium silicate, kieselguhr and some other auxiliary agents (KNO3, AL2O3, Potassium silicate and diatomaceous component ratio are preferably 6:2:1:1).
The temperature of fused salt bathing pool, the i.e. second predetermined temperature can be: 380-550 DEG C, glass and the pure exchange of ion in fused salt Time is preferably at more than 4H.
To the embodiment of the present invention one implements flow process and is illustrated below below:
As shown in Figure 4, the manufacture method of the glass cover-plate of the embodiment of the present invention, including:
Step 201, after large stretch of pristine glass base material is cut into little sheet glass, uses CNC to process outside little sheet glass Shape profile and curved surface, obtained the first stage glass baseplate of predefined size, reservation shape;
Step 202, by hot pressing die set in advance, processes first stage glass baseplate through 11 road molding procedure Become double curved glass substrate;
Step 203, by the high-temperature molten salt being pre-configured with, carries out intensive treatment to double curved glass substrate;
Step 204, uses black photosensitive ink to spray, cover and at exposure the reverse side of double curved glass substrate Reason, forms the black surround around middle window area on the reverse side of double curved glass substrate;
Step 205, to the black surround region of reverse side of double curved glass substrate, predetermined middle window area and predetermined openings district Territory bonding protective film;
Step 206, uses white ink to spray the reverse side of double curved glass substrate and after baking process, uses black Color ink carries out spraying and baking process again, covers black ink on the white ink of double curved glass substrate;
Step 207, removes and is pasted onto the protecting film on the reverse side of double curved glass substrate, on double curved glass substrate Form the white portion covered at the bottom of black lid on reverse side, obtain final double curved glass cover plate.
Through the double curved glass cover plate that above-mentioned operation makes, as it is shown in figure 5, define spy on this double curved glass cover plate Fixed color (white portion 6) and lines (around the black surround 8 of middle window area 7).
To sum up, the manufacture method of the glass cover-plate of the embodiment of the present invention, defined by brand-new technique making and there is spy Determine the 3D double curved glass cover plate of color and lines, novel in appearance, good visual effect;Numerous consumer electronics products provide The effect of great differentiation and experience, meet people's appearance requirement to glass cover-plate high-quality;And low cost of manufacture, can Batch production, is with a wide range of applications.Efficiently solve glass cover-plate in prior art and be substantially plane or 2.5D, Homogeneity is serious, lacks novelty, it is difficult to meet people's problem to the appearance requirement of product high-quality.
Second embodiment
Embodiments providing a kind of glass cover-plate, the double-edged edge of described glass cover-plate is arc Face, and the cambered surface bending direction of the tow sides edge of described glass cover-plate is identical;
Being formed with the first area being coated with the first predetermined color on the reverse side of described glass cover-plate, described first area is On described glass cover-plate in the middle of predetermined region in addition to window area and predetermined openings.
The glass cover-plate of the embodiment of the present invention, for having the 3D double curved glass cover plate of particular color, novel in appearance, vision Effective;In numerous consumer electronics products, provide effect and the experience of great differentiation, meet people to glass cover The appearance requirement of plate hight quality;And low cost of manufacture, can be mass, be with a wide range of applications.Efficiently solve existing In technology, glass cover-plate is substantially plane or 2.5D, and homogeneity is serious, lacks novelty, it is difficult to meet people high to product The problem of the appearance requirement of quality.
It should be noted that the glass cover-plate of the embodiment of the present invention can be obtained by the manufacture method of above-mentioned glass cover-plate. Wherein, in the manufacture method embodiment of above-mentioned glass cover-plate, all implementations are all be applicable to the embodiment of this glass cover-plate, Also same technique effect can be reached.
3rd embodiment
Owing to the glass cover-plate of the embodiment of the present invention is applied to mobile terminal, therefore, the embodiment of the present invention additionally provides one Plant mobile terminal, including: the glass cover-plate as described in above-described embodiment.
The mobile terminal of the present invention can be such as the mobile electronic device such as mobile phone, panel computer.
Wherein, the described of above-mentioned glass cover-plate realizes embodiment all be applicable to the embodiment of this mobile terminal, also can reach To identical technique effect.
The above, the only detailed description of the invention of the present invention, but protection scope of the present invention is not limited thereto, and any Those familiar with the art, in the technical scope that the invention discloses, can readily occur in change or replace, should contain Cover within protection scope of the present invention.Therefore, protection scope of the present invention should be as the criterion with scope of the claims.

Claims (10)

1. the manufacture method of a glass cover-plate, it is characterised in that including:
Pristine glass base material is cut and hot-pressing processing, obtains double curved glass substrate, described double curved glass substrate Double-edged edge is cambered surface, and the cambered surface bending side of the tow sides edge of described double curved glass substrate To identical;
The reverse side of described double curved glass substrate is formed the first area being coated with the first predetermined color, obtains hyperboloid glass Glass cover plate, described first area is the district on described double curved glass substrate in addition to predetermined middle window area and predetermined openings Territory.
Manufacture method the most according to claim 1, it is characterised in that described pristine glass base material is cut and hot pressing Processing, the step obtaining double curved glass substrate includes:
Pristine glass base material is carried out cutting process, obtains the first stage glass baseplate of predefined size, reservation shape;
By hot pressing die set in advance, under the first predetermined temperature, described first stage glass baseplate is carried out hot pressing, To first stage double curved glass substrate;
Described first stage double curved glass substrate is cooled down, obtains second stage double curved glass substrate.
Manufacture method the most according to claim 1, it is characterised in that described on the reverse side of described double curved glass substrate The step forming the first area being coated with the first predetermined color includes:
The region bonding protective film in addition to described first area on the reverse side of described double curved glass substrate;
The first predetermined color ink is used to spray and toast the reverse side of the described double curved glass substrate of bonding protective film After process, use the second predetermined color ink to spray the reverse side of described double curved glass substrate and baking processes;
Remove and be pasted onto the protecting film on the reverse side of described double curved glass substrate, be formed on the first predetermined color and be coated with the The first area of two predetermined colors.
Manufacture method the most according to claim 3, it is characterised in that described protecting film uses high temperature resistance polyester thin film.
Manufacture method the most according to claim 1, it is characterised in that described on the reverse side of described double curved glass substrate Before forming the step of the first area being coated with the first predetermined color, described manufacture method also includes:
The reverse side of described double curved glass substrate is formed the second area being coated with the 3rd predetermined color, described second area For on described double curved glass substrate in the middle of predetermined region in addition to window area and predetermined openings, and described second area ring Around described predetermined middle window area.
Manufacture method the most according to claim 5, it is characterised in that described on the reverse side of described double curved glass substrate The step forming the second area being coated with the 3rd predetermined color includes:
The 3rd predetermined color photosensitive-ink is used to spray, cover and at exposure the reverse side of described double curved glass substrate Reason, forms the second area being coated with the 3rd predetermined color.
Manufacture method the most according to claim 6, it is characterised in that the described reverse side to described double curved glass substrate is adopted Carry out spraying, covering and exposure-processed by the 3rd predetermined color photosensitive-ink, form the secondth district being coated with the 3rd predetermined color The step in territory includes:
The 3rd predetermined color photosensitive-ink is used to carry out spray treatment the reverse side of described double curved glass substrate;
The described double curved glass substrate the 3rd predetermined color photosensitive-ink in addition to second area is covered;
Described double curved glass substrate uses ultraviolet clean after being exposed processing, is formed and be coated with the 3rd predetermined color Second area.
Manufacture method the most according to claim 1, it is characterised in that formed on the reverse side of described double curved glass substrate Before the step of the first area being coated with the first predetermined color, described manufacture method also includes:
According to the fused salt with the second predetermined temperature being pre-configured with, described double curved glass substrate is carried out intensive treatment, Double curved glass substrate to strengthening.
9. a glass cover-plate, it is characterised in that the double-edged edge of described glass cover-plate is cambered surface, and described The cambered surface bending direction of the tow sides edge of glass cover-plate is identical;
Being formed with the first area being coated with the first predetermined color on the reverse side of described glass cover-plate, described first area is described On glass cover-plate in the middle of predetermined region in addition to window area and predetermined openings.
10. a mobile terminal, it is characterised in that include glass cover-plate as claimed in claim 9.
CN201610479378.3A 2016-06-24 2016-06-24 The manufacture method of a kind of glass cover-plate, glass cover-plate and mobile terminal Pending CN106145626A (en)