CN106009683A - High-toughness silica gel strip used for windscreen wipers, and manufacturing method thereof - Google Patents

High-toughness silica gel strip used for windscreen wipers, and manufacturing method thereof Download PDF

Info

Publication number
CN106009683A
CN106009683A CN201610634130.XA CN201610634130A CN106009683A CN 106009683 A CN106009683 A CN 106009683A CN 201610634130 A CN201610634130 A CN 201610634130A CN 106009683 A CN106009683 A CN 106009683A
Authority
CN
China
Prior art keywords
silica gel
gel strip
white carbon
high tenacity
wiper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610634130.XA
Other languages
Chinese (zh)
Inventor
陆耀明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiaxing Yi Xia Auto Parts Technology Co Ltd
Original Assignee
Jiaxing Yi Xia Auto Parts Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiaxing Yi Xia Auto Parts Technology Co Ltd filed Critical Jiaxing Yi Xia Auto Parts Technology Co Ltd
Priority to CN201610634130.XA priority Critical patent/CN106009683A/en
Publication of CN106009683A publication Critical patent/CN106009683A/en
Pending legal-status Critical Current

Abstract

The invention provides a high-toughness silica gel strip used for windscreen wipers. The silica gel strip comprises, by mass, 60-70% of silica gel, 8-12% of white carbon black, 4-6% of silicone oil, 5-8% of polytetrafluoroethylene, 5-10% of diisooctyl phthalate, 2-3% of diisooctyl adipate, 2-3% of tributyl(1-ethoxyvinyl)tin, 1-3% of carbon black and 2-3% of dicumyl peroxide. The invention also provides a manufacturing method of the high-toughness silica gel strip used for windscreen wipers. The silica gel strip made through the method has the advantages of good toughness, strong corrosion resistance, good flexibility, effective wiping of glass, difficulty in ageing, and long service life.

Description

High tenacity wiper silica gel strip and manufacture method thereof
Technical field
The present invention relates to auto parts machinery field, be specifically related to high tenacity wiper silica gel strip and manufacture method thereof.
Background technology
Wiper is widely used on the glass of the vehicles such as automobile, train, electric car, the engineering machine of some There are also installed wiper on tool such as crane, and most important in wiper be exactly windscreen wiper bar.Due to windscreen wiper Directly and glass contact, this scraping article of will praying for rain has good toughness, shape stability and corrosion resistance to bar, because of The production of this windscreen wiper bar is of crucial importance.Existing windscreen wiper bar major part is made up of rubber, toughness, shape stability and Corrosion resistance is poor, and particularly pliability is poor so that windscreen wiper bar is inadequate with the laminating degree of glass, causes Cannot be clean by glass scraper, affect the visual field of the driver, bring potential safety hazard, it is impossible to meet the demand in market. The service life of existing wiper rubber bar is shorter, mainly relevant with sun direct projection, especially with rain erosion Being being exposed to the sun of the sun in summer, ultraviolet is relatively strong, owing to ultra-violet bands is easily absorbed (ultraviolet one by rubber The energy (E=h ν) of photon is close with carbon carbon covalency), promote rubber carbon-carbon bond accelerated ageing to rupture, show Carrying out surface checking, product strength reduces, hardness enhancing etc., and then causes wiper rubber bar to use.
Summary of the invention
The technical problem to be solved is to provide high tenacity wiper silica gel strip and manufacturer thereof Method, the silica gel strip good toughness manufactured, corrosion resistance is strong, and pliability is good, it is possible to effectively by glass scraper Totally, and being difficult to aging, service life is long.
For solving above-mentioned existing technical problem, the present invention uses following scheme: high tenacity wiper silica gel Bar, by mass fraction be the silica gel of 60-70%, the white carbon of 8-12%, the silicone oil of 4-6%, poly-the four of 5-8% Fluorothene, the diisooctyl phthalate of 5-10%, the adipic acid di-isooctyl of 2-3%, three fourths of 2-3% Base (1-ethoxy ethylene) stannum, the white carbon black of 1-3%, the cumyl peroxide composition of 2-3%.
As preferably, described high tenacity wiper silica gel strip by the silica gel that mass fraction is 60%, 12% White carbon, the silicone oil of 6%, the politef of 5%, the diisooctyl phthalate of 5%, the two of 3% Acid di-isooctyl, tributyl (1-ethoxy ethylene) stannum of 3%, the white carbon black of 3%, the peroxidating diisopropyl of 3% Benzene forms.
As preferably, described high tenacity wiper silica gel strip by the silica gel that mass fraction is 65%, 10% White carbon, the silicone oil of 5%, the politef of 6%, the diisooctyl phthalate of 6%, the two of 2% Acid di-isooctyl, tributyl (1-ethoxy ethylene) stannum of 3%, the white carbon black of 1%, the peroxidating diisopropyl of 2% Benzene forms.
As preferably, described high tenacity wiper silica gel strip by the silica gel that mass fraction is 70%, 8% white White carbon black, the silicone oil of 4%, the politef of 5%, the diisooctyl phthalate of 5%, the adipic acid of 2% Di-isooctyl, tributyl (1-ethoxy ethylene) stannum of 2%, the white carbon black of 2%, the cumyl peroxide of 2% Composition.
The manufacture method of high tenacity wiper silica gel strip, comprises the following steps:
Step one: raw material mixes: by silica gel, white carbon, silicone oil, politef, phthalic acid Di-isooctyl, white carbon black, cumyl peroxide stir, and then proceed to stirring, in whipping process first Add adipic acid di-isooctyl, add tributyl (1-ethoxy ethylene) stannum afterwards, stir, formed Silica gel strip blank;
Step 2: by extruded for the silica gel strip blank in step one;
Step 3: silica gel strip blank extruded in step 2 is put in drying baker, 500-600 degree Carrying out drying and shaping under high temperature, product is made.
Beneficial effect:
The present invention uses technique scheme to provide high tenacity wiper silica gel strip and manufacture method thereof, manufactures Silica gel strip good toughness out, corrosion resistance is strong, and pliability is good, it is possible to effectively that glass scraper is clean, and And it being difficult to aging, service life is long.
Detailed description of the invention
Embodiment one:
High tenacity wiper silica gel strip, by silica gel that mass fraction is 60%, the white carbon of 12%, 6% Silicone oil, the politef of 5%, the diisooctyl phthalate of 5%, the adipic acid di-isooctyl of 3%, Tributyl (1-ethoxy ethylene) stannum of 3%, the white carbon black of 3%, the cumyl peroxide composition of 3%.
The manufacture method of high tenacity wiper silica gel strip, comprises the following steps:
Step one: raw material mixes: by silica gel, white carbon, silicone oil, politef, phthalic acid Di-isooctyl, white carbon black, cumyl peroxide stir, and then proceed to stirring, in whipping process first Add adipic acid di-isooctyl, add tributyl (1-ethoxy ethylene) stannum afterwards, stir, formed Silica gel strip blank;
Step 2: by extruded for the silica gel strip blank in step one;
Step 3: silica gel strip blank extruded in step 2 is put in drying baker, 500-600 degree Carrying out drying and shaping under high temperature, product is made.
The use of silica gel so that silica gel strip pliability is good, stickiness is good;Add white carbon and white carbon black, strengthen The abrasion-proof and refractory performance of silica gel strip;Cumyl peroxide further increases the wear-resisting and waterproof of silica gel strip Can, and add smoothness;Add politef, improve antiacid alkali resistant ability;Adipic acid two Different monooctyl ester can improve service life effective against oxidation;Tributyl (1-ethoxy ethylene) stannum is effectively prevented from Silica gel strip is aging so that the silica gel strip good toughness that manufactures, and corrosion resistance is strong, and pliability is good, it is possible to Effectively that glass scraper is clean, and it is difficult to aging, service life is long.
Embodiment two:
High tenacity wiper silica gel strip, by silica gel that mass fraction is 65%, the white carbon of 10%, 5% Silicone oil, the politef of 6%, the diisooctyl phthalate of 6%, the adipic acid di-isooctyl of 2%, Tributyl (1-ethoxy ethylene) stannum of 3%, the white carbon black of 1%, the cumyl peroxide composition of 2%.
Compared with embodiment one, adding the consumption of silica gel, pliability increases, and is more easy to glass scraper clean.
Embodiment three:
High tenacity wiper silica gel strip, described high tenacity wiper silica gel strip is 70% by mass fraction Silica gel, the white carbon of 8%, the silicone oil of 4%, the politef of 5%, the diisooctyl phthalate of 5%, The adipic acid di-isooctyl of 2%, tributyl (1-ethoxy ethylene) stannum of 2%, the white carbon black of 2%, the mistake of 2% Oxidation diisopropylbenzene (DIPB) composition.
Compared with above-mentioned two embodiment, silica gel consumption is most, and pliability is best.
Specific embodiment described herein is only to present invention spirit explanation for example.Belonging to the present invention Described specific embodiment can be made various amendment or supplements or adopt by those skilled in the art Substitute by similar mode, but without departing from the spirit of the present invention or surmount appended claims and determined The scope of justice.

Claims (5)

1. high tenacity wiper silica gel strip, it is characterised in that: it is the silica gel of 60-70%, 8-12% by mass fraction White carbon, the silicone oil of 4-6%, the politef of 5-8%, the diisooctyl phthalate of 5-10%, The adipic acid di-isooctyl of 2-3%, tributyl (1-ethoxy ethylene) stannum of 2-3%, the white carbon black of 1-3%, The cumyl peroxide composition of 2-3%.
High tenacity wiper silica gel strip the most according to claim 1, it is characterised in that: described high tenacity rain Curette silica gel strip by the silica gel that mass fraction is 60%, the white carbon of 12%, the silicone oil of 6%, 5% poly- Tetrafluoroethene, the diisooctyl phthalate of 5%, the adipic acid di-isooctyl of 3%, the tributyl of 3% (1-ethoxy ethylene) stannum, the white carbon black of 3%, the cumyl peroxide composition of 3%.
High tenacity wiper silica gel strip the most according to claim 1, it is characterised in that: described high tenacity rain Curette silica gel strip by the silica gel that mass fraction is 65%, the white carbon of 10%, the silicone oil of 5%, 6% poly- Tetrafluoroethene, the diisooctyl phthalate of 6%, the adipic acid di-isooctyl of 2%, the tributyl of 3% (1-ethoxy ethylene) stannum, the white carbon black of 1%, the cumyl peroxide composition of 2%.
High tenacity wiper silica gel strip the most according to claim 1, it is characterised in that: described high tenacity rain Curette silica gel strip by the silica gel that mass fraction is 70%, the white carbon of 8%, the silicone oil of 4%, 5% poly- Tetrafluoroethene, the diisooctyl phthalate of 5%, the adipic acid di-isooctyl of 2%, the tributyl of 2% (1-ethoxy ethylene) stannum, the white carbon black of 2%, the cumyl peroxide composition of 2%.
5. the manufacture method of high tenacity wiper silica gel strip as claimed in claim 1, it is characterised in that: include Following steps:
Step one: raw material mixes: by silica gel, white carbon, silicone oil, politef, phthalic acid Di-isooctyl, white carbon black, cumyl peroxide stir, and then proceed to stirring, in whipping process first Add adipic acid di-isooctyl, add tributyl (1-ethoxy ethylene) stannum afterwards, stir, formed Silica gel strip blank;
Step 2: by extruded for the silica gel strip blank in step one;
Step 3: silica gel strip blank extruded in step 2 is put in drying baker, 500-600 degree Carrying out drying and shaping under high temperature, product is made.
CN201610634130.XA 2016-08-03 2016-08-03 High-toughness silica gel strip used for windscreen wipers, and manufacturing method thereof Pending CN106009683A (en)