CN105618504B - A kind of microchannel aluminium flat conduit extrusion die - Google Patents

A kind of microchannel aluminium flat conduit extrusion die Download PDF

Info

Publication number
CN105618504B
CN105618504B CN201610190309.0A CN201610190309A CN105618504B CN 105618504 B CN105618504 B CN 105618504B CN 201610190309 A CN201610190309 A CN 201610190309A CN 105618504 B CN105618504 B CN 105618504B
Authority
CN
China
Prior art keywords
die
radiator
aluminium flat
flat conduit
extrusion die
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201610190309.0A
Other languages
Chinese (zh)
Other versions
CN105618504A (en
Inventor
周秋芳
梅小明
刘小稻
房荣胜
石宇凡
崔韬
薛云
陈�峰
周俞
郭宏林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Yangzhou Rise-Al Composite Metal Material Co Ltd
Original Assignee
Yangzhou Rise-Al Composite Metal Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Yangzhou Rise-Al Composite Metal Material Co Ltd filed Critical Yangzhou Rise-Al Composite Metal Material Co Ltd
Priority to CN201610190309.0A priority Critical patent/CN105618504B/en
Publication of CN105618504A publication Critical patent/CN105618504A/en
Application granted granted Critical
Publication of CN105618504B publication Critical patent/CN105618504B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of microchannel aluminium flat conduit extrusion die; including modular ring connected in order, die-cushion and die sleeve; upper die and lower die are provided with die sleeve; two pits are provided with one side of the die-cushion towards die sleeve; radiator is equipped with pit; air admission hole and venthole are provided with modular ring, air admission hole connects with the air inlet of radiator, and venthole connects with the gas outlet of radiator.The present invention solves the deficiency in terms of aluminium flat conduit Extrusion Die Design in the prior art, there is provided a kind of microchannel aluminium flat conduit extrusion die, its good heat dissipation effect, service life length, is advantageous to improve extrusion speed, so as to improve aluminium flat conduit yield.

Description

A kind of microchannel aluminium flat conduit extrusion die
Technical field
The present invention relates to a kind of extrusion die, especially a kind of aluminium flat conduit extrusion die.
Background technology
The cross-sectional area of microchannel aluminium flat conduit is very small, typically in 10mm2Left and right, therefore even if using porous extruding, Its extrusion ratio still can be considerably beyond the extrusion ratio of traditional 8~50 times of aluminium extrusion specification, and reaches 500 times or so, so big Extrusion ratio, it can such as be talked without yield at all according to traditional extrusion speed, extrude the product in the past, because mould temperature rise is too high And temperature can not be lowered, therefore the method used is generally the speed for lowering extruding, reduces to 50m/min, so causes Result be production loss 28.47%.Therefore extrusion speed must be just improved if improving yield, from traditional 50m/ Min brings up to 70m/min, but so high extrusion speed can make the temperature of mould rise to more than 610 DEG C, makes common heat Make mould steel and be in tempering and annealed condition, it will quickly because losing the life-span without hardness.
The content of the invention
Present invention aim to address the deficiency in terms of aluminium flat conduit Extrusion Die Design in the prior art, there is provided a kind of micro- logical Road aluminium flat conduit extrusion die, its good heat dissipation effect, service life length, be advantageous to improve extrusion speed, so as to improve aluminium flat conduit production Amount.
Technical scheme
A kind of microchannel aluminium flat conduit extrusion die, including modular ring connected in order, die-cushion and die sleeve, die sleeve is interior to be provided with upper mould With lower mould, two pits are provided with one side of the die-cushion towards die sleeve, radiator is equipped with pit, air inlet is provided with modular ring Hole and venthole, air admission hole connect with the air inlet of radiator, and venthole connects with the gas outlet of radiator.
Further, the radiator is fine copper radiator.The heat conductivility of fine copper is high, and it can be rapidly the heat of mould Amount is delivered in whole radiator.
Further, the radiator includes the gas channel of vertical and horizontal, and radiating effect is more preferable.
In use, simultaneously toward the freeze-drying air that 0.2~0.3MPA pressure is constantly poured in air admission hole, the gas being filled with The heat in fine copper radiator can be taken away rapidly, so circulation, among mould can be made to be maintained at 560 DEG C~580 DEG C of temperature, Reach the purpose of crushing failure at high speed.
Beneficial effect:The microchannel aluminium flat conduit structure of extrusion of the present invention is simple, easy to operate, good heat dissipation effect, makes With long lifespan, be advantageous to improve extrusion speed, so as to improve aluminium flat conduit yield.
Brief description of the drawings
Fig. 1 is the structural representation of microchannel aluminium flat conduit extrusion die of the present invention;
Fig. 2 is the A-A direction views of die-cushion in Fig. 1;
Wherein, 1- modular rings, 2- die-cushions, 3- die sleeves, the upper moulds of 4-, mould under 5-, 6- radiators, 7- air admission holes, 8- ventholes.
Embodiment
The invention will be further described with reference to the accompanying drawings and examples.
Fig. 1 be microchannel aluminium flat conduit extrusion die of the present invention structural representation, Fig. 2 be Fig. 1 in die-cushion A-A to regarding Figure, as shown, a kind of microchannel aluminium flat conduit extrusion die, including modular ring 1 connected in order, die-cushion 2 and die sleeve 3, set in die sleeve 3 There are upper mould 4 and lower mould 5, two pits are provided with one side of the die-cushion 2 towards die sleeve 3, radiator 6 are equipped with pit, in mould Ring 1 is provided with air admission hole 7 and venthole 8, and air admission hole 7 connects with the air inlet of radiator 6, the outlet of venthole 8 and radiator 6 Mouth connection, radiator 6 is fine copper radiator, includes the gas channel of vertical and horizontal.
In use, simultaneously toward the freeze-drying air that 0.2~0.3MPA pressure is constantly poured in air admission hole, the gas being filled with The heat in fine copper radiator can be taken away rapidly, so circulation, among mould can be made to be maintained at 560 DEG C~580 DEG C of temperature, Reach the purpose of crushing failure at high speed.
The microchannel aluminium flat conduit structure of extrusion of the present invention is simple, easy to operate, good heat dissipation effect, service life length, Be advantageous to improve extrusion speed, so as to improve aluminium flat conduit yield.

Claims (3)

  1. Be provided with 1. a kind of microchannel aluminium flat conduit extrusion die, including modular ring connected in order, die-cushion and die sleeve, in die sleeve upper mould and Lower mould, it is characterised in that two pits are provided with one side of the die-cushion towards die sleeve, radiator are equipped with pit, in modular ring Air admission hole and venthole are provided with, air admission hole connects with the air inlet of radiator, and venthole connects with the gas outlet of radiator.
  2. 2. microchannel aluminium flat conduit extrusion die as claimed in claim 1, it is characterised in that the radiator radiates for fine copper Device.
  3. 3. microchannel aluminium flat conduit extrusion die as claimed in claim 1, it is characterised in that the radiator includes longitudinal direction and horizontal stroke To gas channel.
CN201610190309.0A 2016-03-30 2016-03-30 A kind of microchannel aluminium flat conduit extrusion die Active CN105618504B (en)