CN105540534A - Nanotube nano-particle composite material - Google Patents
Nanotube nano-particle composite material Download PDFInfo
- Publication number
- CN105540534A CN105540534A CN201510905409.2A CN201510905409A CN105540534A CN 105540534 A CN105540534 A CN 105540534A CN 201510905409 A CN201510905409 A CN 201510905409A CN 105540534 A CN105540534 A CN 105540534A
- Authority
- CN
- China
- Prior art keywords
- nanotube
- nano
- vertical
- tortuous
- tube
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a nanotube nano-particle composite material, comprising horizontal central nanotubes, and horizontal zigzag nanotubes, nano-particles, vertical zigzag nanotubes, and vertical central nanotubes. The plurality of horizontal central nanotubes and the plurality of vertical central nanotubes are woven into a net structure. The horizontal central nanotube traverses through the horizontal zigzag nanotube. The point of intersection of the horizontal central nanotube and the horizontal zigzag nanotube is provided with the nano-particle. The vertical central nanotube passes longitudinally through the vertical zigzag nanotube. The point of intersection of the vertical central nanotube and the vertical zigzag nanotube is provided with the nano-particle. Beneficial effects of the material are that the material has relatively large shrinkage, and satisfies requirements of people on shrinkage nanotube nano-particle composite materials.
Description
Technical field
The present invention relates to composite equipment technical field, be specially a kind of nano-tube nano particulate composite.
Background technology
Nanotube has great specific area, and excellent machinery and photoelectric properties etc., be widely used in the preparation of composite.Nano particle itself has the excellent specific properties such as great specific area and photocatalysis, but nano particle itself is easily reunited.So, by nanoparticulate dispersed in carbon nano tube surface, prepare the focus that nano-tube nano particulate composite becomes research.And existing nano-tube nano particulate composite is mostly not contractile, the demand of people for shrinkage nano-tube nano particulate composite can not be met.
Summary of the invention
The invention provides a kind of nano-tube nano particulate composite, Main Function is to provide one and has inotropic nano-tube nano particulate composite, meet the demand of people for shrinkage nano-tube nano particulate composite, considerably increase the scope of application of nano-tube nano particulate composite, very practical.
For solving the problem, the embodiment of the present application provides a kind of nano-tube nano particulate composite, comprise horizontal centre nanotube, also comprise the tortuous nanotube of level, nano particle, vertical tortuous nanotube and vertical center nanotube, described multiple horizontal centre nanotube and multiple vertical centers nanotube are woven into network structure, described horizontal centre nanotube crosses through the tortuous nanotube of level, the point of intersection of described horizontal centre nanotube and the tortuous nanotube of level is provided with nano particle, described vertical center nanotube is vertical is perforated through vertical tortuous nanotube, the point of intersection of described vertical center nanotube and vertical tortuous nanotube is provided with nano particle.
As the preferred embodiment of this programme, a part at least one nanotube is coated on wherein by each nano particle described.
As the preferred embodiment of this programme, the length of described horizontal centre nanotube and vertical center nanotube is at least the twice of the tortuous nanotube of level and vertical tortuous nanotube respectively.
As the preferred embodiment of this programme, described nano tube structure comprises at least one nanotube bundle, and the part surface of two adjacent nanotubes in nanotube bundle is wrapped up by least one nano particle.
The one or more technical schemes provided in the embodiment of the present application, at least there is following technique effect or advantage: provide one and there is inotropic nano-tube nano particulate composite, meet the demand of people for shrinkage nano-tube nano particulate composite, considerably increase the scope of application of nano-tube nano particulate composite, very practical.
Accompanying drawing explanation
In order to be illustrated more clearly in the embodiment of the present invention or technical scheme of the prior art, be briefly described to the accompanying drawing used required in embodiment or description of the prior art below, apparently, accompanying drawing in the following describes is only some embodiments of the present invention, for those of ordinary skill in the art, under the prerequisite not paying creative work, other accompanying drawing can also be obtained according to these accompanying drawings.
Fig. 1 is the structural representation of the embodiment of the present application;
In figure: 1 horizontal centre nanotube, 2 levels tortuous nanotube, 3 nano particles, 4 vertical tortuous nanotubes and 5 vertical center nanotubes.
Detailed description of the invention
The invention provides a kind of nano-tube nano particulate composite, Main Function is to provide one and has inotropic nano-tube nano particulate composite, meet the demand of people for shrinkage nano-tube nano particulate composite, considerably increase the scope of application of nano-tube nano particulate composite, very practical.
In order to better understand technique scheme, below in conjunction with Figure of description and concrete embodiment, technique scheme is described in detail.
Refer to shown in Fig. 1, a kind of nano-tube nano particulate composite, comprises horizontal centre nanotube 1, also comprises the tortuous nanotube 2 of level, nano particle 3, vertical tortuous nanotube 4 and vertical center nanotube 5.
Wherein, in actual applications, described multiple horizontal centre nanotube 1 is woven into network structure with multiple vertical centers nanotube 5, thus adds the intensity of nano-tube nano particulate composite to a certain extent.
Wherein, in actual applications, described horizontal centre nanotube 1 crosses through the tortuous nanotube 2 of level, the tortuous nanotube 2 of level has retractility, thus the tortuous nanotube 2 of level can be pulled to slide on horizontal centre nanotube 1, described horizontal centre nanotube 1 is provided with nano particle 3 with the point of intersection of the tortuous nanotube 2 of level.
Wherein, in actual applications, described vertical center nanotube 5 is vertical is perforated through vertical tortuous nanotube 4, vertical tortuous nanotube 4 has retractility, can slide on vertical center nanotube 5 by pulling vertical tortuous nanotube 4, described vertical center nanotube 5 is provided with nano particle 3 with the point of intersection of vertical tortuous nanotube 4.
Wherein, in actual applications, a part at least one nanotube is coated on wherein by each nano particle 3 described, the length of described horizontal centre nanotube 1 and vertical center nanotube 5 is at least the twice of the tortuous nanotube 2 of level and vertical tortuous nanotube 4 respectively, thus nano-tube nano particulate composite can be extended to more than twice, there is good retractility, meet the demand of people for shrinkage nano-tube nano particulate composite, considerably increase the scope of application of nano-tube nano particulate composite, described nano tube structure comprises at least one nanotube bundle, and the part surface of two adjacent nanotubes in nanotube bundle is wrapped up by least one nano particle 3.
To those skilled in the art, obviously the invention is not restricted to the details of above-mentioned one exemplary embodiment, and when not deviating from spirit of the present invention or essential characteristic, the present invention can be realized in other specific forms.Therefore, no matter from which point, all should embodiment be regarded as exemplary, and be nonrestrictive, scope of the present invention is limited by claims instead of above-mentioned explanation, therefore all changes be intended in the implication of the equivalency by dropping on claim and scope are included in the present invention, any Reference numeral in claim should be considered as the claim involved by limiting.
The above; be only the present invention's preferably detailed description of the invention; but protection scope of the present invention is not limited thereto; anyly be familiar with those skilled in the art in the technical scope that the present invention discloses; be equal to according to technical scheme of the present invention and inventive concept thereof and replace or change, all should be encompassed within protection scope of the present invention.
Claims (4)
1. a nano-tube nano particulate composite, comprise horizontal centre nanotube (1), it is characterized in that: also comprise the tortuous nanotube (2) of level, nano particle (3), vertical tortuous nanotube (4) and vertical center nanotube (5), described multiple horizontal centre nanotube (1) and multiple vertical center nanotube (5) are woven into network structure, described horizontal centre nanotube (1) is crossed through the tortuous nanotube (2) of level, described horizontal centre nanotube (1) is provided with nano particle (3) with the point of intersection of the tortuous nanotube (2) of level, described vertical center nanotube (5) is vertical is perforated through vertical tortuous nanotube (4), described vertical center nanotube (5) is provided with nano particle (3) with the point of intersection of vertical tortuous nanotube (4).
2. a kind of nano-tube nano particulate composite according to claim 1, is characterized in that: a part at least one nanotube is coated on wherein by described each nano particle (3).
3. a kind of nano-tube nano particulate composite according to claim 1, is characterized in that: the length at described horizontal centre nanotube (1) and vertical center nanotube (5) is at least the twice of the tortuous nanotube (2) of level and vertical tortuous nanotube (4) respectively.
4. a kind of nano-tube nano particulate composite according to claim 1, it is characterized in that: described nano tube structure comprises at least one nanotube bundle, and the part surface of two adjacent nanotubes in nanotube bundle is wrapped up by least one nano particle (3).