A kind of mouse
Technical field
The present invention is specifically related to a kind of mouse.
Background technology
Mouse is a kind of computer input apparatus be in daily use, and it can position the vernier on current screen, and by button and roller devices to vernier screen elements through position operate.A outstanding mouse first want outward appearance beautiful, use comfortable and applicable user's hand-type, different users then should select according to the actual conditions of oneself.The people of many frequent use mouses can find that the carpal bone of oneself is given prominence to, and the sensation of ache often can appear in finger and wrist, and this just illustrates that the design of its mouse does not embody the design philosophy that people-oriented.
Along with the development of science and technology, universal and the application of computing machine, the accessory of computing machine is also more and more exquisite, as the accessory mouse that computing machine is important, also experienced by the development of a very long time, from original mouse, mechanical mouse, optical mouse, optical machine mouse optical mouse by now again, the change of each product design is all be more suitable for people use mouse to produce.Current mouse product is mainly in the majority with the roller type mouse or optical mouse that are flat on desktop, and the size of producing each mouse is fixing mostly, specially do not produce mouse according to the size of the hand of actual persons, just produce the certain mouse of size with the mould of a standard.When people are when using mouse, for the people that palm is larger, what usually can cause because mouse is too little holding is uncomfortable; hand is easily ached, also or when child use mouse time, usually can feeling mouse too large; seem painstaking especially according to mouse button, use extremely inconvenient.
Current mouse is on the market in order to better improve the comfort of user, and mouse profile is designed to streamlined with the hand of the user that better fits, but such design but causes mouse to be not easy to carry, and obviously there is defect.
Summary of the invention
The technical problem to be solved in the present invention is to provide one and is beneficial to and carries, the mouse of easy to use and comfortable feel.
For solving the problem, the present invention adopts following technical scheme:
A kind of mouse, comprise mouse main body, described mouse main body comprises interlayer, lower interlayer and soft rubber cushion, described upper interlayer is connected with lower interlayer, roller is provided with above described upper interlayer, smooth seat, laser mark and battery case is provided with bottom described lower interlayer, described smooth seat is provided with more than one, described laser mark is in the centre of smooth seat, described laser mark inside is provided with laser head, described battery case is positioned at below laser target, and described soft rubber cushion is fixed on interlayer and lower interlayer is inner, and described soft rubber cushion is that elasticity is arranged.
Further, described mouse main body is provided with smooth layer, is conducive to palm and contacts with mouse main body more comfortable, avoid the service condition because of frictional influence mouse.
Further, described roller two ends are provided with thin layer, and when pointing with roller contact, the bacterium of hand and foreign material cannot be attached on roller, are conducive to the health keeping mouse.
Further, between described upper interlayer and lower interlayer, be provided with jacking block, be conducive to supporting interlayer and lower interlayer, bounce-back can be avoided and affect mouse and normally use.
Further, described smooth seat is provided with four, and smooth seat is distributed in the corner bottom lower interlayer, is conducive to balance support and facility of sliding.
Further, described battery case is provided with capping, battery can be covered and protect.
Further, described soft rubber cushion is provided with groove, when being conducive to soft rubber cushion extruding, can has living space accommodation because extruding produces distortion.
A kind of preparation method of soft rubber cushion, be made up of the material of following parts by weight proportioning: comprise synthetic rubber 20-30 part, vinyl cyanide-benzene second 20-30 part, glass microballoon 13-16 part, paraffinic base rubber oil 9-13 part, matrix pitch 8-13 part, talcum powder 5-15 part, silane coupling agent 4-7 part, hydroxy silicon oil 5-15 part, latex 11-16 part, carbon black 6-9 part, modification infusorial earth 11-16 part, magnesium hydroxide 8-13 part, aluminium hydroxide 4-8 part, levelling agent 2-4 part and hardening agent 8-13 part, comprise the following steps:
1) get synthetic rubber 20-30 part and latex 11-16 part adds smelting furnace, by high temperature, synthetic rubber is become glue with latex, for subsequent use;
2) get glass microballoon 13-16 part and be milled into powder, stir in homo-mixer and add silane coupling agent 4-7 part, obtained modified glass hollow powder, for subsequent use;
3) by step 2) obtained modified glass hollow powder adds step 1) in, and by continuing heating, modified glass hollow powder and glue are merged, and obtain and mix plastic cement liquid, for subsequent use;
4) get vinyl cyanide-benzene second 20-30 part, carbon black 6-9 part, modification infusorial earth 11-16 part, matrix pitch 8-13 part and talcum powder 5-15 part and grind to form broken end by muller, then stirred by stirring machine, the obtained filler mixed, for subsequent use;
5) magnesium hydroxide 8-13 part, aluminium hydroxide 4-8 part, paraffinic base rubber oil 9-13 part and hydroxy silicon oil 5-15 part blend step 4 is got) obtained mixed fillers adds step 3 to) in, and stirred down by homo-mixer, make it even by high-speed stirred, mixed glue solution is thickness more, for subsequent use;
6) levelling agent 2-4 part and hardening agent 8-13 part interpolation step 5 is got) in, by heating, make additive and epoxy glue liquid phase fusion reaction, obtained plastic material, for subsequent use;
7) by step 6) obtained plastic cement liquid puts into injection machine, carries out mold injection, the demoulding after cooling, obtained plastic mold by injection machine, for subsequent use;
8) by step 7) obtained plastic mold through the operation of polishing corner angle and surface lacquer, to obtain final product.
The invention has the beneficial effects as follows: owing to being provided with upper interlayer and lower interlayer; can be folded by upper interlayer and lower interlayer and fix on computers; be conducive to carrying, owing to being provided with smooth seat, can be convenient to slide; owing to being provided with battery case; can battery be loaded, be conducive to mouse and use, owing to being provided with soft rubber cushion; mouse and protection calculation machine can be protected by soft rubber cushion, avoid being pressed from both sides bad.
Accompanying drawing explanation
Fig. 1 is the one-piece construction schematic diagram of a kind of mouse of the present invention.
Fig. 2 is the structural representation bottom the lower interlayer of a kind of mouse of the present invention.
Embodiment
Embodiment one:
Consult shown in Fig. 1-2, a kind of mouse, comprise mouse main body 1, described mouse main body 1 comprises interlayer 2, lower interlayer 3 and soft rubber cushion 4, described upper interlayer 2 is connected with lower interlayer 3, roller 5 is provided with above described upper interlayer 2, smooth seat 6 is provided with bottom described lower interlayer 3, laser mark 7 and battery case 9, described smooth seat 6 is provided with more than one, described laser mark 7 is positioned at the centre of smooth seat 6, described laser mark 7 inside is provided with laser head 8, described battery case 9 is positioned at the below of laser mark 7, described soft rubber cushion 4 is fixed on interlayer 2 and lower interlayer 3 is inner, described soft rubber cushion 4 is elasticity setting.
Described mouse main body 1 is provided with smooth layer, is conducive to palm and contacts with mouse main body more comfortable, avoid the service condition because of frictional influence mouse.
Described roller 5 two ends are provided with thin layer (not shown), and when pointing with roller contact, the bacterium of hand and foreign material cannot be attached on roller, are conducive to the health keeping mouse.
Be provided with jacking block (not shown) between described upper interlayer 2 and lower interlayer 3, be conducive to supporting interlayer and lower interlayer, bounce-back can be avoided and affect mouse and normally use.
Described smooth seat 6 is provided with four, and smooth seat is distributed in the corner bottom lower interlayer, is conducive to balance support and facility of sliding.
Described battery case 9 is provided with capping, battery can be covered and protect.
Described soft rubber cushion 4 is provided with groove, when being conducive to soft rubber cushion extruding, can has living space accommodation because extruding produces distortion.
A kind of preparation method of soft rubber cushion, be made up of the material of following parts by weight proportioning: comprise synthetic rubber 30 parts, vinyl cyanide-benzene second 20 parts, glass microballoon 13 parts, paraffinic base rubber oil 9 parts, matrix pitch 8 parts, talcum powder 5 parts, silane coupling agent 4 parts, hydroxy silicon oil 5 parts, latex 11 parts, carbon black 6 parts, modification infusorial earth 11 parts, magnesium hydroxide 8 parts, aluminium hydroxide 4 parts, levelling agent 2 parts and 8 parts, hardening agent, comprise the following steps:
1) get synthetic rubber 30 parts and add smelting furnace with latex 11 parts, by high temperature, synthetic rubber is become glue with latex, for subsequent use;
2) get glass microballoon 13 parts and be milled into powder, stir in homo-mixer and add silane coupling agent 4-7 part, obtained modified glass hollow powder, for subsequent use;
3) by step 2) obtained modified glass hollow powder adds step 1) in, and by continuing heating, modified glass hollow powder and glue are merged, and obtain and mix plastic cement liquid, for subsequent use;
4) get vinyl cyanide-benzene second 20 parts, carbon black 6 parts, modification infusorial earth 11 parts, matrix pitch 8 parts and talcum powder 5 parts and grind to form broken end by muller, then stirred by stirring machine, the obtained filler mixed, for subsequent use;
5) magnesium hydroxide 8 parts, aluminium hydroxide 4 parts, paraffinic base rubber oil 9 parts and hydroxy silicon oil 5 parts of blend steps 4 are got) obtained mixed fillers adds step 3 to) in, and stirred down by homo-mixer, make it even by high-speed stirred, mixed glue solution is thickness more, for subsequent use;
6) levelling agent 2 parts and 8 parts, hardening agent interpolation step 5 is got) in, by heating, make additive and epoxy glue liquid phase fusion reaction, obtained plastic material, for subsequent use;
7) by step 6) obtained plastic cement liquid puts into injection machine, carries out mold injection, the demoulding after cooling, obtained plastic mold by injection machine, for subsequent use;
8) by step 7) obtained plastic mold through the operation of polishing corner angle and surface lacquer, to obtain final product.
Embodiment two:
Consult shown in Fig. 1-2, a kind of mouse, comprise mouse main body 1, described mouse main body 1 comprises interlayer 2, lower interlayer 3 and soft rubber cushion 4, described upper interlayer 2 is connected with lower interlayer 3, roller 5 is provided with above described upper interlayer 2, smooth seat 6 is provided with bottom described lower interlayer 3, laser mark 7 and battery case 9, described smooth seat 6 is provided with more than one, described laser mark 7 is positioned at the centre of smooth seat 6, described laser mark 7 inside is provided with laser head 8, described battery case 9 is positioned at the below of laser mark 7, described soft rubber cushion 4 is fixed on interlayer 2 and lower interlayer 3 is inner, described soft rubber cushion 4 is elasticity setting.
Described mouse main body 1 is provided with smooth layer, is conducive to palm and contacts with mouse main body more comfortable, avoid the service condition because of frictional influence mouse.
Described roller 5 two ends are provided with thin layer (not shown), and when pointing with roller contact, the bacterium of hand and foreign material cannot be attached on roller, are conducive to the health keeping mouse.
Be provided with jacking block (not shown) between described upper interlayer 2 and lower interlayer 3, be conducive to supporting interlayer and lower interlayer, bounce-back can be avoided and affect mouse and normally use.
Described smooth seat 6 is provided with four, and smooth seat is distributed in the corner bottom lower interlayer, is conducive to balance support and facility of sliding.
Described battery case 9 is provided with capping, battery can be covered and protect.
Described soft rubber cushion 4 is provided with groove, when being conducive to soft rubber cushion extruding, can has living space accommodation because extruding produces distortion.
A kind of preparation method of soft rubber cushion, be made up of the material of following parts by weight proportioning: comprise synthetic rubber 20 parts, vinyl cyanide-benzene second 30 parts, glass microballoon 16 parts, paraffinic base rubber oil 13 parts, matrix pitch 13 parts, talcum powder 5 parts, silane coupling agent 7 parts, hydroxy silicon oil 15 parts, latex 16 parts, carbon black 9 parts, modification infusorial earth 16 parts, magnesium hydroxide 13 parts, aluminium hydroxide 8 parts, levelling agent 4 parts and 13 parts, hardening agent, comprise the following steps:
1) get synthetic rubber 20 parts and add smelting furnace with latex 16 parts, by high temperature, synthetic rubber is become glue with latex, for subsequent use;
2) get glass microballoon 16 parts and be milled into powder, stir in homo-mixer and add silane coupling agent 7 parts, obtained modified glass hollow powder, for subsequent use;
3) by step 2) obtained modified glass hollow powder adds step 1) in, and by continuing heating, modified glass hollow powder and glue are merged, and obtain and mix plastic cement liquid, for subsequent use;
4) get vinyl cyanide-benzene second 30 parts, carbon black 9 parts, modification infusorial earth 16 parts, matrix pitch 13 parts and talcum powder 15 parts and grind to form broken end by muller, then stirred by stirring machine, the obtained filler mixed, for subsequent use;
5) magnesium hydroxide 13 parts, aluminium hydroxide 8 parts, paraffinic base rubber oil 13 parts and hydroxy silicon oil 15 parts of blend steps 4 are got) obtained mixed fillers adds step 3 to) in, and stirred down by homo-mixer, make it even by high-speed stirred, mixed glue solution is thickness more, for subsequent use;
6) levelling agent 4 parts and 13 parts, hardening agent interpolation step 5 is got) in, by heating, make additive and epoxy glue liquid phase fusion reaction, obtained plastic material, for subsequent use;
7) by step 6) obtained plastic cement liquid puts into injection machine, carries out mold injection, the demoulding after cooling, obtained plastic mold by injection machine, for subsequent use;
8) by step 7) obtained plastic mold through the operation of polishing corner angle and surface lacquer, to obtain final product.
Embodiment three:
Consult shown in Fig. 1-2, a kind of mouse, comprise mouse main body 1, described mouse main body 1 comprises interlayer 2, lower interlayer 3 and soft rubber cushion 4, described upper interlayer 2 is connected with lower interlayer 3, roller 5 is provided with above described upper interlayer 2, smooth seat 6 is provided with bottom described lower interlayer 3, laser mark 7 and battery case 9, described smooth seat 6 is provided with more than one, described laser mark 7 is positioned at the centre of smooth seat 6, described laser mark 7 inside is provided with laser head 8, described battery case 9 is positioned at the below of laser mark 7, described soft rubber cushion 4 is fixed on interlayer 2 and lower interlayer 3 is inner, described soft rubber cushion 4 is elasticity setting.
Described mouse main body 1 is provided with smooth layer, is conducive to palm and contacts with mouse main body more comfortable, avoid the service condition because of frictional influence mouse.
Described roller 5 two ends are provided with thin layer (not shown), and when pointing with roller contact, the bacterium of hand and foreign material cannot be attached on roller, are conducive to the health keeping mouse.
Be provided with jacking block (not shown) between described upper interlayer 2 and lower interlayer 3, be conducive to supporting interlayer and lower interlayer, bounce-back can be avoided and affect mouse and normally use.
Described smooth seat 6 is provided with four, and smooth seat is distributed in the corner bottom lower interlayer, is conducive to balance support and facility of sliding.
Described battery case 9 is provided with capping, battery can be covered and protect.
Described soft rubber cushion 4 is provided with groove, when being conducive to soft rubber cushion extruding, can has living space accommodation because extruding produces distortion.
A kind of preparation method of soft rubber cushion, be made up of the material of following parts by weight proportioning: comprise synthetic rubber 25 parts, vinyl cyanide-benzene second 25 parts, glass microballoon 15 parts, paraffinic base rubber oil 11 parts, matrix pitch 11 parts, talcum powder 10 parts, silane coupling agent 6 parts, hydroxy silicon oil 10 parts, latex 13 parts, carbon black 8 parts, modification infusorial earth 14 parts, magnesium hydroxide 12 parts, aluminium hydroxide 6 parts, levelling agent 3 parts and 10 parts, hardening agent, comprise the following steps:
1) get synthetic rubber 25 parts and add smelting furnace with latex 13 parts, by high temperature, synthetic rubber is become glue with latex, for subsequent use;
2) get glass microballoon 15 parts and be milled into powder, stir in homo-mixer and add silane coupling agent 6 parts, obtained modified glass hollow powder, for subsequent use;
3) by step 2) obtained modified glass hollow powder adds step 1) in, and by continuing heating, modified glass hollow powder and glue are merged, and obtain and mix plastic cement liquid, for subsequent use;
4) get vinyl cyanide-benzene second 25 parts, carbon black 8 parts, modification infusorial earth 14 parts, matrix pitch 11 parts and talcum powder 10 parts and grind to form broken end by muller, then stirred by stirring machine, the obtained filler mixed, for subsequent use;
5) magnesium hydroxide 12 parts, aluminium hydroxide 6 parts, paraffinic base rubber oil 11 parts and hydroxy silicon oil 10 parts of blend steps 4 are got) obtained mixed fillers adds step 3 to) in, and stirred down by homo-mixer, make it even by high-speed stirred, mixed glue solution is thickness more, for subsequent use;
6) levelling agent 3 parts and 10 parts, hardening agent interpolation step 5 is got) in, by heating, make additive and epoxy glue liquid phase fusion reaction, obtained plastic material, for subsequent use;
7) by step 6) obtained plastic cement liquid puts into injection machine, carries out mold injection, the demoulding after cooling, obtained plastic mold by injection machine, for subsequent use;
8) by step 7) obtained plastic mold through the operation of polishing corner angle and surface lacquer, to obtain final product.
Experimental example:
Choose common plastics with special plastics compared with plastic cushion of the present invention, and according to pliability, elasticity and crushing strength foundation as a comparison, analyze the situation of three groups of plastic stents, and draw best plastic stent.
With common plastics be control group one, special plastics for control group two and plastics of the present invention are for control group three, concrete data are as shown in the table:
Contrast three groups of materials, the effect obtaining plastics of the present invention is best, has that pliability is good, good springiness and the good advantage of crush resistance strength compared with two groups of control groups.
The invention has the beneficial effects as follows: owing to being provided with upper interlayer and lower interlayer; can be folded by upper interlayer and lower interlayer and fix on computers; be conducive to carrying, owing to being provided with smooth seat, can be convenient to slide; owing to being provided with battery case; can battery be loaded, be conducive to mouse and use, owing to being provided with soft rubber cushion; mouse and protection calculation machine can be protected by soft rubber cushion, avoid being pressed from both sides bad.
The above, be only the specific embodiment of the present invention, but protection scope of the present invention is not limited thereto, and any change of expecting without creative work or replacement, all should be encompassed in protection scope of the present invention.