CN105344810B - A kind of container roof plate rolling die - Google Patents
A kind of container roof plate rolling die Download PDFInfo
- Publication number
- CN105344810B CN105344810B CN201510765809.8A CN201510765809A CN105344810B CN 105344810 B CN105344810 B CN 105344810B CN 201510765809 A CN201510765809 A CN 201510765809A CN 105344810 B CN105344810 B CN 105344810B
- Authority
- CN
- China
- Prior art keywords
- groove
- convex block
- roof plate
- rolling die
- formpiston
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The invention discloses a kind of container roof plate rolling dies, the rolling die, it include intermeshing former and formpiston, the former is equipped at least one groove, the groove is around the periphery of former, the groove includes starting point and end, and the starting point is not overlapped with end;The formpiston is equipped at least one convex block, and for the convex block around the periphery of formpiston, the convex block includes head end and end, and the head end is not overlapped with end;The groove and convex block correspond.The present invention carries out roll-in by two intermeshing molds, since the field of conjugate action of mold is not a plane, when the groove of former is engaged with the convex block of formpiston, the blind wave of container roof plate can be processed, when the convex block of the groove of former and formpiston is out of mesh, it is equivalent to the side at the blind wave both ends of container roof plate.Roll-in production is carried out using mold of the invention, the production efficiency of container roof plate can be greatly improved.
Description
Technical field
The present invention relates to the roll-forming molds of a kind of rolling die, especially container roof plate.
Background technique
In reality production, such as color steel tile, container side plate, because cross sectional shape continuously standardizes, general use is rolled into
Shape production is divided into life after the forming of coil of strip material continuous rolling two kinds of veneer rolling formation after cutting to length or coiled strip cutting to length
Produce high-efficient, energy saving, saving labour, convenient for automated production.But for cross sectional shape it is not continuous workpiece,
Such as container roof plate, since it is that blind wave crest plate (has a recessed portion, all round closure structure is shown in attached among container roof plate
Fig. 1), because cross sectional shape is discontinuous, and the groove depth changes, and is unfavorable for continuous rolling forming, so as to cause in actual production
In, container roof plate is substantially using press mold compression moulding, and cause production efficiency low, waste of energy, inconvenient shape
At continuous production processes.
Summary of the invention
The technical problem to be solved by the present invention is a kind of novel rolling die is provided, so that container roof plate can be carried out
Continuous roll-in production.
The solution that the present invention solves its technical problem is: a kind of container roof plate rolling die, the rolling die,
It include intermeshing former and formpiston, the former is equipped at least one groove, and the groove is around the outer of former
Week, the groove include starting point and end, and the starting point is not overlapped with end;The formpiston is equipped at least one
A convex block, for the convex block around the periphery of formpiston, the convex block includes head end and end, and the head end is not weighed with end
It closes;The groove and convex block correspond.
As a further improvement of the above technical scheme, the starting point of the groove and end are transition and both sides
Fillet is fallen;The head end of the convex block and end are transition and fillet of having leaned now to one side, then to the other.
As a further improvement of the above technical scheme, the roller die has multiple groups, and the multiple groups rolling die is located at
Same level, multiple groups rolling die are rear in one line from going to;The depth of the multiple groups groove is gradually increased from after going to;Institute
The height for stating multiple groups convex block is gradually increased from after going to.
The beneficial effects of the present invention are: the present invention carries out roll-in by two intermeshing molds, due to nibbling for mold
Conjunction face is not a plane, when the groove of former is engaged with the convex block of formpiston, so that it may process container roof plate
Blind wave is equivalent to the side at the blind wave both ends of container roof plate when the convex block of the groove of former and formpiston is out of mesh.Using this
The mold of invention carries out roll-in production, can greatly improve the production efficiency of container roof plate.The present invention is used for the roll-in of blind wave
Molding.
Detailed description of the invention
To describe the technical solutions in the embodiments of the present invention more clearly, make required in being described below to embodiment
Attached drawing is briefly described.Obviously, described attached drawing is a part of the embodiments of the present invention, rather than is all implemented
Example, those skilled in the art without creative efforts, can also be obtained according to these attached drawings other designs
Scheme and attached drawing.
Fig. 1 is existing container roof plate schematic diagram;
Fig. 2 is front view of the invention;
Fig. 3 is perspective view of the invention.
Specific embodiment
It is carried out below with reference to technical effect of the embodiment and attached drawing to design of the invention, specific structure and generation clear
Chu is fully described by, to be completely understood by the purpose of the present invention, feature and effect.Obviously, described embodiment is this hair
Bright a part of the embodiment, rather than whole embodiments, based on the embodiment of the present invention, those skilled in the art are not being paid
Other embodiments obtained, belong to the scope of protection of the invention under the premise of creative work.In addition, be previously mentioned in text
All connection/connection relationships not singly refer to that component directly connects, and referring to can be added deduct according to specific implementation situation by adding
Few couple auxiliary, to form more preferably coupling structure.Each technical characteristic in the invention, in not conflicting conflict
Under the premise of can be with combination of interactions.
Referring to Fig. 2~Fig. 3, a kind of container roof plate rolling die, the rolling die includes intermeshing former
1 is equipped at least one groove 11 with formpiston 2, the former 1, and the groove 11 is around the periphery of former 1, the groove 11
It include starting point and end, the starting point is not overlapped with end;The formpiston 2 is equipped at least one convex block 21,
The convex block 21 includes head end and end around the periphery of formpiston 2, the convex block 21, and the head end is not overlapped with end;
The groove 11 is corresponded with convex block 21.Multiple tracks groove is processed on former by mach method, then also by
Mach method processes multiple convex blocks on formpiston so that each convex block can mesh together with groove, when former 1 with
When formpiston 2 rotates, the two remains close contact.It, will be in the surface roll of steel plate when steel plate is by former 1 and formpiston 2
Closed pit, i.e. blind wave needed for container roof plate together are extruded, it only need to be by the length of the groove of former 1 and the convex block of formpiston 2
Degree is arranged to the equal length with blind wave.
It is further used as preferred embodiment, the starting point of the groove 11 is transition with end and leans now to one side, then to the other
Fillet;The head end of the convex block 21 and end are transition and fillet of having leaned now to one side, then to the other.In order to enable the blind wave of roll-forming
Both ends it is rounder and more smooth, the starting of the groove and convex block and terminate the transition processing all deepened using gradual change, and both sides are equal
The case where having fallen fillet, not only having extended the service life of mold but also reduced steel plate cracking.
It is further used as preferred embodiment, the roller die has multiple groups, and the multiple groups rolling die is located at same
Horizontal plane, multiple groups rolling die are rear in one line from going to;The depth of the multiple groups groove 11 is gradually increased from after going to;It is described
The height of multiple groups convex block 21 is gradually increased from after going to.Since the blind depth of convolution degree of container roof plate is larger, although as long as theoretically
The depth of groove be equal to blind wave needed for depth can a roll-forming, it is contemplated that the stress condition and steel of mold
The factor of the elongation percentage of plate etc., the molding of blind wave can be divided into multiple roll-in and carry out, and the groove for the mold that roll-in each time uses is deep
Degree increases with the equal equal proportion of convex block depth, so that the depth of the blind wave after roll-in also gradually increases, makes after eventually passing through repeatedly
The depth for obtaining blind wave meets design requirement.Certainly, the number of roll-in can be according to the hardness of mold, the elongation of steel plate and blind wave
Size carry out adaptability adjustment.
Better embodiment of the invention is illustrated above, but the invention is not limited to the implementation
Example, those skilled in the art can also make various equivalent modifications on the premise of without prejudice to spirit of the invention or replace
It changes, these equivalent variation or replacement are all included in the scope defined by the claims of the present application.
Claims (3)
1. a kind of container roof plate rolling die, it is characterised in that: roller of the rolling die for the blind wave of container roof plate
It is molded;The rolling die, includes intermeshing former (1) and formpiston (2), and the former (1) is equipped at least one
A groove (11), for the groove (11) around the periphery of former (1), the groove (11) includes starting point and end,
The starting point is not overlapped with end;The formpiston (2) be equipped at least one convex block (21), the convex block (21) around
The periphery of formpiston (2), the convex block (21) includes head end and end, and the head end is not overlapped with end;The groove (11)
It is corresponded with convex block (21);The blind waves of the difference of every group of rolling die while the same container roof plate of roll-in;The groove (11)
Starting point and end be transition;The head end of the convex block (21) and end are transition.
2. container roof plate rolling die according to claim 1, it is characterised in that: the starting point of the groove (11) with
End has been leaned now to one side, then to the other fillet;The head end of the convex block (21) and end have been leaned now to one side, then to the other fillet.
3. container roof plate rolling die according to claim 1, it is characterised in that: the roller die has multiple groups, institute
It states multiple groups rolling die and is located at same level, multiple groups rolling die is rear in one line from going to;The multiple groups rolling die
The depth of groove (11) is gradually increased from after going to;The height of the convex block (21) of the multiple groups rolling die gradually increases from after going to
Add.