CN105315740A - Antitarnish paint - Google Patents

Antitarnish paint Download PDF

Info

Publication number
CN105315740A
CN105315740A CN201410378794.5A CN201410378794A CN105315740A CN 105315740 A CN105315740 A CN 105315740A CN 201410378794 A CN201410378794 A CN 201410378794A CN 105315740 A CN105315740 A CN 105315740A
Authority
CN
China
Prior art keywords
parts
paint
antitarnish
acrylic acid
resin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410378794.5A
Other languages
Chinese (zh)
Inventor
张崇亮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin Xinlihua Color Material Co Ltd
Original Assignee
Tianjin Xinlihua Color Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin Xinlihua Color Material Co Ltd filed Critical Tianjin Xinlihua Color Material Co Ltd
Priority to CN201410378794.5A priority Critical patent/CN105315740A/en
Publication of CN105315740A publication Critical patent/CN105315740A/en
Pending legal-status Critical Current

Abstract

The invention provides antitarnish paint and belongs to the technical field of chemical engineering. The antitarnish paint is prepared from the following raw materials in parts by mass: 20-40 parts of a paint component, 30-50 parts of a mixture of anti-yellowing resin and acrylic acid, 5-10 parts of solidification glue, 5-10 parts of zeolite powder and 5-10 parts of water soluble resin, optimally 25 parts of the paint component, 36 parts of the mixture of anti-yellowing resin and acrylic acid, 6 parts of the solidification glue, 6 parts of the zeolite powder and 6 parts of the water soluble resin, wherein the mass ratio of the anti-yellowing resin and the acrylic acid is 1:3. By taking the mixture of anti-yellowing resin and acrylic acid as a main component of the antitarnish paint, the antitarnish paint has good antioxidant and antitarnish effects and is free of any heavy metal additives. The antitarnish paint provided by the invention is green and environmental-friendly, non-toxic and odorless, free of environmental pollution and harmless to human body.

Description

A kind of Anti-tarnishing paint
Technical field
The present invention relates to chemical technology field, specifically a kind of Anti-tarnishing paint.
Background technology
Paint is that one firmly can cover body surface, plays protection, decoration, mark and the chemical mixture coating of other special purposes.In family's process of assembling, the situation of coating color-changing can be met with.Originally be the varnish of clear, colorless or extremely light yellow, after variable color, just become pale brown or black; Colored paint also has the phenomenon of variable color, and main manifestations is that the colored paint that color is shallow darkens.For these problems, improve although some paint product has made some, the Anti-tarnish property of paint is improved, and with the addition of some heavy metal additives, this causes huge injury to human body undoubtedly.
Summary of the invention
The problem to be solved in the present invention is: overcome the deficiencies in the prior art, a kind of effect with good anti-oxidant and Anti-tarnishing is provided, and do not add any heavy metal additive, environmental protection, nonpoisonous and tasteless, nonpollution environment, the Anti-tarnishing of personal fanout free region to be painted.
For solving the problems of the technologies described above, the technical solution used in the present invention is: a kind of Anti-tarnishing paint, is prepared from by the raw material of following mass fraction: paint component 20-40 part, anti-yellowing resin and acrylic acid mixture 30-50 part, freezing plastic 5-10 part, zeolite powder 5-10 part, water soluble resin 5-10 part.
Further, the mass fraction of described raw material the best is: 36 parts, paint component 25 parts, anti-yellowing resin and acrylic acid mixture, freezing plastic 6 parts, zeolite powder 6 parts, water soluble resin 6 parts.
Further, anti-yellowing resin and acrylic acid mass ratio are 1:3.
The advantage that the present invention has and positively effect are:
(1) the present invention's main ingredient of painting as Anti-tarnishing using anti-yellowing resin and acrylic acid mixture, has the effect of good anti-oxidant and Anti-tarnishing.
(2) the present invention does not add any heavy metal additive, environmental protection, nonpoisonous and tasteless, nonpollution environment, to personal fanout free region.
Embodiment
A kind of Anti-tarnishing paint, is prepared from by the raw material of following mass fraction: paint component 20-40 part, anti-yellowing resin and acrylic acid mixture 30-50 part, freezing plastic 5-10 part, zeolite powder 5-10 part, water soluble resin 5-10 part.
The mass fraction of described raw material the best is: 36 parts, paint component 25 parts, anti-yellowing resin and acrylic acid mixture, freezing plastic 6 parts, zeolite powder 6 parts, water soluble resin 6 parts.
Anti-yellowing resin and acrylic acid mass ratio are 1:3.
A kind of Anti-tarnishing paint of the present invention, the mass fraction of each raw material the best is: 36 parts, paint component 25 parts, anti-yellowing resin and acrylic acid mixture, freezing plastic 6 parts, zeolite powder 6 parts, water soluble resin 6 parts.Wherein anti-yellowing resin and acrylic acid mass ratio are 1:3.Before using, first will clear up the surface dust on wall or furniture, with thicker sand paper, polishing wall, increases bond area.Then Anti-tarnishing paint is added brushing on the wall of polishing, general brushing 2-3 time, after brushing 5-10 minute can be completely dry.Long-time solarization also can not variable color or fade in the sun.
The main ingredient that the present invention paints using anti-yellowing resin and acrylic acid mixture as Anti-tarnishing, there is the effect of good anti-oxidant and Anti-tarnishing, and do not add any heavy metal additive, environmental protection of the present invention, nonpoisonous and tasteless, nonpollution environment, to personal fanout free region.
Above embodiments of the invention have been described in detail, but described content being only specific examples of the present invention, can not being considered to for limiting practical range of the present invention.All equalizations done according to the present patent application scope change and improve, and all should still belong within patent covering scope of the present invention.

Claims (3)

1. Anti-tarnishing paint, is characterized in that: be prepared from by the raw material of following mass fraction: paint component 20-40 part, anti-yellowing resin and acrylic acid mixture 30-50 part, freezing plastic 5-10 part, zeolite powder 5-10 part, water soluble resin 5-10 part.
2. a kind of Anti-tarnishing paint according to claim 1, is characterized in that: the mass fraction of described raw material the best is: 36 parts, paint component 25 parts, anti-yellowing resin and acrylic acid mixture, freezing plastic 6 parts, zeolite powder 6 parts, water soluble resin 6 parts.
3. a kind of Anti-tarnishing paint according to claim 1, is characterized in that: anti-yellowing resin and acrylic acid mass ratio are 1:3.
CN201410378794.5A 2014-07-31 2014-07-31 Antitarnish paint Pending CN105315740A (en)