CN105290057A - Method and device for removing welding slag generated after grinding of inner welding joint of spiral welding pipe - Google Patents
Method and device for removing welding slag generated after grinding of inner welding joint of spiral welding pipe Download PDFInfo
- Publication number
- CN105290057A CN105290057A CN201510738557.XA CN201510738557A CN105290057A CN 105290057 A CN105290057 A CN 105290057A CN 201510738557 A CN201510738557 A CN 201510738557A CN 105290057 A CN105290057 A CN 105290057A
- Authority
- CN
- China
- Prior art keywords
- wire brush
- sharpening machine
- weld
- rotating shaft
- outside weld
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a method and device for removing welding slag generated after grinding of an inner welding joint of a spiral welding pipe. The device for removing the welding slag comprises a steel wire brush and a steel wire brush through shaft. One end of the steel wire brush through shaft is fixedly connected with the shaft end of a rotary shaft of an outer welding joint grinder through threads, the inner ring of the steel wire brush is fixedly connected with the steel wire brush through shaft through a long key, and the rotary shaft of the outer welding joint grinder can drive the steel wire brush to rotate through the steel wire brush through shaft. The shaft end of the steel wire brush is fixed through a locknut. As the steel wire brush is detachably installed on the outer welding joint grinder, the residual welding slag generated after the inner welding joint is ground can be electrically removed, installation and use are convenient, one device has dual purposes, the utilization rate of existing equipment is increased, and the labor intensity of field staff is reduced.
Description
Technical field
The present invention relates to spiral submerged welded pipe postwelding scarfing cinder technical field, particularly relate to welding slag sweep-out method and deslagging device after the reconditioning of a kind of spiral welded pipe inside weld.
Background technology
At present, the inside weld of spiral submerged welded pipe generally adopts inside weld sharpening machine to carry out welding seam grinding, its operation principle utilizes abrasive band reconditioning pipe end weld seam, because fuel factor during reconditioning and strenuous exercise make metal waste residue produce magnetization, is adsorbed on end of spirial welded pipe inwall; Operating personnel make cleaning equipment by hand process usually, cannot thoroughly remove magnetic metal waste residue, and cause in next operation and flat head chamfering operation, the tiny waste residue of metal enters in chamfering machine cutter head, causes the damage that cutter head is regular.In addition, manual slagging-off operation can increase the labour intensity of operating personnel, and the metallic dust flown upward also can become the healthy hidden danger of operating personnel.
Summary of the invention
The invention provides welding slag sweep-out method and deslagging device after the reconditioning of a kind of spiral welded pipe inside weld, by the electronic cleaning of remaining welding slag after welding seam grinding machine outside removably being installed wire brush and realizing internal welding seam grinding, and it is easy to install, dual-use, improve the utilization rate of existing equipment, reduce the labour intensity of Field Force.
In order to achieve the above object, the present invention realizes by the following technical solutions:
Welding slag sweep-out method after the reconditioning of spiral welded pipe inside weld, comprises the steps:
1) spiral welded pipe weld seam shaping after, inside weld adopts inside weld sharpening machine reconditioning weld seam to qualified;
2) grinding wheel being arranged on outside weld sharpening machine rotating shaft axle head is unloaded, wire brush is installed; Wire brush is fixedly connected with the rotating shaft of outside weld sharpening machine by wire brush axis, and can with outside weld sharpening machine axis of rotation;
3) start outside weld sharpening machine, wire brush rotates under rotating shaft drives, and wire brush removes welding slag while the movement of spiral welded pipe inside weld;
4) different according to steel pipe caliber, the height of wire brush adjusts by outside weld sharpening machine vertical guide rail;
5) when needs carry out outside weld reconditioning, wire brush and wire brush axis entirety are disassembled from outside weld sharpening machine rotating shaft axle head, reinstalls grinding wheel.
For realizing the deslagging device of welding slag sweep-out method after the reconditioning of spiral welded pipe inside weld, comprise wire brush and wire brush axis, described wire brush axis one end is fixedly connected with by screw thread with outside weld sharpening machine rotating shaft axle head, wire brush inner ring is fixedly connected with wire brush axis by long key, and the rotating shaft of outside weld sharpening machine drives wire brush to rotate by wire brush axis; Wire brush axle head is fixed by locking nut.
Compared with prior art, the invention has the beneficial effects as follows:
1) the present invention is by the Automatic clearance of remaining welding slag after welding seam grinding machine outside removably being installed wire brush and realizing internal welding seam grinding, and described deslagging device reasonable in design is easy to operate;
2) wire brush and wire brush axis adopt key type of attachment, are fixedly connected with reliable, and can transmitting torque;
3) wire brush axis and outside weld sharpening machine rotating shaft axle head are by thread connection, convenient to disassembly;
4) dual-use is achieved, when steel pipe needs outside weld reconditioning, can integral demounting wire brush axis, directly outside weld grinding wheel is installed, realizes outside weld reconditioning function, improve the utilization rate of existing equipment.
5) avoid manual operation, reduce the labour intensity of Field Force, eliminate healthy hidden danger.
Accompanying drawing explanation
Fig. 1 is the structural representation of deslagging device of the present invention.
Fig. 2 is the structural representation of wire brush axis of the present invention.
In figure: 1. long key 6. locking nut of outside weld sharpening machine 2. outside weld sharpening machine rotating shaft 3. wire brush axis 31. internal thread hole 32. keyway 33. external thread of shaft end 4. wire brush 5.
Detailed description of the invention
Below in conjunction with accompanying drawing, the specific embodiment of the present invention is described further:
Seeing Fig. 1, is the structural representation of deslagging device of the present invention.Welding slag sweep-out method after spiral welded pipe inside weld of the present invention reconditioning, comprises the steps:
1) spiral welded pipe weld seam shaping after, inside weld adopts inside weld sharpening machine reconditioning weld seam to qualified;
2) grinding wheel being arranged on outside weld sharpening machine rotating shaft 2 axle head is unloaded, wire brush 4 is installed; Wire brush 4 is fixedly connected with outside weld sharpening machine rotating shaft 2 by wire brush axis 3, and can rotate with outside weld sharpening machine rotating shaft 2;
3) start outside weld sharpening machine 1, wire brush 4 rotates under rotating shaft 2 drives, and wire brush 4 removes welding slag while the movement of spiral welded pipe inside weld;
4) different according to steel pipe caliber, the height of wire brush 4 adjusts by outside weld sharpening machine 1 vertical guide rail;
5) when needs carry out outside weld reconditioning, wire brush 4 and wire brush axis 3 entirety are disassembled from outside weld sharpening machine rotating shaft 2 axle head, reinstalls grinding wheel.
For realizing the deslagging device of welding slag sweep-out method after the reconditioning of spiral welded pipe inside weld, comprise wire brush 4 and wire brush axis 3, described wire brush axis 3 one end is fixedly connected with by screw thread with outside weld sharpening machine rotating shaft 2 axle head, wire brush 4 inner ring is fixedly connected with wire brush axis 3 by long key 5, and outside weld sharpening machine rotating shaft 2 drives wire brush 4 to rotate by wire brush axis 3; Wire brush 4 axle head is fixed by locking nut 6.
Following examples are implemented under premised on technical solution of the present invention, give detailed embodiment and concrete operating process, but protection scope of the present invention are not limited to following embodiment.In following embodiment, method therefor is conventional method if no special instructions.
[embodiment]
As shown in Figure 2, welding seam grinding machine rotating shaft outside 2 axle head installs a wire brush axis 3, wire brush axis 3 one end processing M27*1.5mm internal thread hole 31 is connected with the external screw thread processed for installing grinding wheel original on outside weld welding seam grinding machine rotating shaft 2 axle head, the external screw thread 33 of opposite side axle head processing M27*1.5mm, fixes the axial location of wire brush 4 by locking nut 6; Wire brush axis 3 is multidiameter form, and multidiameter end face is used for the axial location inside wire brush 4.Wire brush axis 3 offers elongated keyway 32 vertically, fixes wire brush 4 and transmitting torque by long key 5.Different according to steel pipe caliber, the upper-lower position of wire brush 4 adjusts by outside weld sharpening machine 1 vertical guide rail.
In the present embodiment, outside weld sharpening machine 1 is outsourcing finished product, wire brush axis 3 and outside weld sharpening machine rotating shaft 2 are threaded connection, the size of the internal thread hole 31 on wire brush axis 3 and outside weld sharpening machine rotating shaft 2 end adapted for installing the external screw thread size of repairing grit wheel originally, can ensure installation accuracy.
Wire brush axis 3 is multidiameter, and mid portion is for installing wire brush 4, and mid portion is processed with elongated keyway 32, is located inside wire brush 4 by multidiameter end face, and outside is locked by locking nut 6.
During work, wire brush 4 is removed by the welding slag of drive to steel pipe inner wall of outside weld sharpening machine rotating shaft 2, and because pipe diameter size is different, the height of wire brush 4 is controlled by vertical guide rail original on outside weld sharpening machine 1.When needs carry out outside weld reconditioning, directly can remove wire brush axis 3 axle head and be threaded, wire brush 4 and wire brush axis 3 entirety are unloaded.
The present invention is ensureing under the prerequisite that original outside weld sharpening machine 1 function is constant, achieve the function of metal waste residue after the reconditioning of electronic removing spiral steel pipe inside weld, spoil removing rate is higher than processing manually, and welding slag can be avoided the adverse effect of subsequent handling equipment, reliable guarantee is provided to the maintaining of apparatus for production line.
The above; be only the present invention's preferably detailed description of the invention; but protection scope of the present invention is not limited thereto; anyly be familiar with those skilled in the art in the technical scope that the present invention discloses; be equal to according to technical scheme of the present invention and inventive concept thereof and replace or change, all should be encompassed within protection scope of the present invention.
Claims (2)
1. welding slag sweep-out method after the reconditioning of spiral welded pipe inside weld, is characterized in that, comprise the steps:
1) spiral welded pipe weld seam shaping after, inside weld adopts inside weld sharpening machine reconditioning weld seam to qualified;
2) grinding wheel being arranged on outside weld sharpening machine rotating shaft axle head is unloaded, wire brush is installed; Wire brush is fixedly connected with the rotating shaft of outside weld sharpening machine by wire brush axis, and can with outside weld sharpening machine axis of rotation;
3) start outside weld sharpening machine, wire brush rotates under rotating shaft drives, and wire brush removes welding slag while the movement of spiral welded pipe inwall;
4) different according to steel pipe caliber, the height of wire brush adjusts by outside weld sharpening machine vertical guide rail;
5) when needs carry out outside weld reconditioning, wire brush and wire brush axis entirety are disassembled from outside weld sharpening machine rotating shaft axle head, reinstalls grinding wheel.
2. for realizing the deslagging device of welding slag sweep-out method after spiral welded pipe inside weld according to claim 1 reconditioning, it is characterized in that, comprise wire brush and wire brush axis, described wire brush axis one end is fixedly connected with by screw thread with outside weld sharpening machine rotating shaft axle head, wire brush inner ring is fixedly connected with wire brush axis by long key, and the rotating shaft of outside weld sharpening machine drives wire brush to rotate by wire brush axis; Wire brush axle head is fixed by locking nut.