CN105149588A - Preparation method of novel stainless steel glasses slingshot compartment - Google Patents

Preparation method of novel stainless steel glasses slingshot compartment Download PDF

Info

Publication number
CN105149588A
CN105149588A CN201510661145.0A CN201510661145A CN105149588A CN 105149588 A CN105149588 A CN 105149588A CN 201510661145 A CN201510661145 A CN 201510661145A CN 105149588 A CN105149588 A CN 105149588A
Authority
CN
China
Prior art keywords
slingshot
stainless steel
grinding
box
slingshot box
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510661145.0A
Other languages
Chinese (zh)
Inventor
林建和
谢智忠
孙文龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510661145.0A priority Critical patent/CN105149588A/en
Publication of CN105149588A publication Critical patent/CN105149588A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method of a novel stainless steel glasses slingshot compartment. The preparation method of the novel stainless steel glasses slingshot compartment is characterized by comprising the steps of material preparing, forming, chemical reaction degreasing, final forming, magnetic decontamination grinding and shaping. According to the technical scheme, by means of the stainless steel powder metallurgy, casting is conducted directly, a series of problems such as mildewing and oxidation caused in the production process of glasses and earpiece sleeves can be avoided, production technology processes are reduced, and the production efficiency is greatly improved.

Description

Preparation method of novel stainless steel glasses slingshot box
Technical Field
The invention belongs to a preparation method of a novel stainless steel glasses slingshot box.
Background
All slingshots on the market at present have the defects that the cupronickel material does not meet the market requirements for production requirements, environmental protection requirements and welding requirements, the product adopts high-quality imported stainless steel raw materials without problems for environmental protection and welding, the cupronickel double-tooth welding needs high-quality silver sheets, the product adopts laser welding but has low price, then the electroplated slingshot foot wires need to be protected, and the product can cause oxidation and mildew in case of bruising or throwing off an electroplated layer, the product is electroplated by environment-friendly nickel, and can not cause oxidation and mildew in case of bruising because the product is made of stainless steel, furthermore, the spectacle industry needs to develop mechanization, and the mechanization process can be influenced according to the current structure; the same stainless steel material greatly improves the mechanical operation for welding and processing procedures.
Disclosure of Invention
The invention aims to solve the technical problem of providing a preparation method of a novel stainless steel slingshot box for glasses.
The technical scheme adopted by the invention for solving the technical problems is as follows:
a preparation method of a novel stainless steel glasses slingshot box is characterized by comprising the following steps:
the method comprises the following steps: adding 80-90% of plastic into stainless steel powder, mixing, adding 10-20% of plastic adhesive, heating to 150-200 ℃ in an internal mixer, banburying, dissolving, and preparing into granular feed;
step two: the prepared materials are put into an injection molding machine to be heated to 150-200 ℃ and then injected into a mold of a slingshot box product of a corresponding style for molding;
step three: putting the slingshot box of the corresponding style into a degreasing catalytic furnace, heating to 100-150 ℃, and degreasing through chemical reaction;
step four: putting the degreased slingshot box product into a high-temperature vacuum sintering furnace, slowly heating to 1300-1400 ℃, sintering for 8-15 hours, and finally forming a product with a relative slingshot box style;
step five: and step four, performing decontamination grinding by multiple magnetic forces, and shaping.
Preferably, the step two of the preparation method of the novel stainless steel spectacle slingshot box is subjected to trimming treatment after molding.
Further, preferably, the step three of the preparation method of the slingshot box of the novel stainless steel glasses is protected by nitrogen in the degreasing process.
Further, preferably, the grinding and shaping in step five of the method for preparing the slingshot box of the novel stainless steel glasses further comprises:
the method comprises the following steps: aligning the thick capillary holes of the slingshot boxes through the arrangement plates to the slingshot boxes, and roughly polishing and peeling the slingshot boxes through the polishing disc;
step two: severe coarse pores generated by the slingshot box are subjected to sanding by a disc machine to remove surface pores;
step three: grinding the slingshot box by using a 6 x 6 circle coarse grinding machine;
step four: grinding the slingshot box by a flow type finishing machine with 4-4 round grinding materials;
step five: grinding the slingshot box by using a flow type finishing machine with 3 x 3 round thin materials;
step five: grinding the slingshot box by using a walnut grain polishing material for a flow type polishing machine.
After the scheme is adopted, the stainless steel powder is directly cast, so that a series of problems such as mildew, oxidation and the like caused in the production process of the glasses and the glasses foot sleeves can be avoided, the production process flow is reduced, and the production efficiency is greatly improved.
Additional features and advantages of the invention will be set forth in the description which follows, and in part will be obvious from the description, or may be learned by practice of the invention. The objectives and other advantages of the invention will be realized and attained by the structure particularly pointed out in the written description and claims hereof as well as the appended drawings.
Drawings
The present invention will be described in detail below with reference to the accompanying drawings so that the above advantages of the present invention will be more apparent. Wherein,
fig. 1 is a schematic diagram of the slingshot box of the novel stainless steel spectacle slingshot box manufacturing method of the present invention.
Detailed Description
The following detailed description of the embodiments of the present invention will be provided with reference to the drawings and examples, so that how to apply the technical means to solve the technical problems and achieve the technical effects can be fully understood and implemented. It should be noted that, as long as there is no conflict, the embodiments and the features of the embodiments of the present invention may be combined with each other, and the technical solutions formed are within the scope of the present invention.
A preparation method of a novel stainless steel glasses slingshot box is characterized by comprising the following steps:
the method comprises the following steps: adding 80-90% of plastic into stainless steel powder, mixing, adding 10-20% of plastic adhesive, heating to 150-200 ℃ in an internal mixer, banburying, dissolving, and preparing into granular feed;
step two: the prepared materials are put into an injection molding machine to be heated to 150-200 ℃ and then injected into a mold of a slingshot box product of a corresponding style for molding;
step three: putting the slingshot box of the corresponding style into a degreasing catalytic furnace, heating to 100-150 ℃, and degreasing through chemical reaction;
step four: putting the degreased slingshot box product into a high-temperature vacuum sintering furnace, slowly heating to 1300-1400 ℃, sintering for 8-15 hours, and finally forming a product with a relative slingshot box style;
step five: and step four, performing decontamination grinding by multiple magnetic forces, and shaping.
Preferably, the step two of the preparation method of the novel stainless steel spectacle slingshot box is subjected to trimming treatment after molding.
Further, preferably, the step three of the preparation method of the slingshot box of the novel stainless steel glasses is protected by nitrogen in the degreasing process.
Further, preferably, the grinding and shaping in step five of the method for preparing the slingshot box of the novel stainless steel glasses further comprises:
the method comprises the following steps: aligning the thick capillary holes of the slingshot boxes through the arrangement plates to the slingshot boxes, and roughly polishing and peeling the slingshot boxes through the polishing disc;
step two: severe coarse pores generated by the slingshot box are subjected to sanding by a disc machine to remove surface pores;
step three: grinding the slingshot box by using a 6 x 6 circle coarse grinding machine;
step four: grinding the slingshot box by a flow type finishing machine with 4-4 round grinding materials;
step five: grinding the slingshot box by using a flow type finishing machine with 3 x 3 round thin materials;
step five: grinding the slingshot box by using a walnut grain polishing material for a flow type polishing machine.
After the scheme is adopted, the stainless steel powder is directly cast, so that a series of problems such as mildew, oxidation and the like caused in the production process of the glasses and the glasses foot sleeves can be avoided, the production process flow is reduced, and the production efficiency is greatly improved.
Finally, it should be noted that: although the present invention has been described in detail with reference to the foregoing embodiments, it will be apparent to those skilled in the art that changes may be made in the embodiments and/or equivalents thereof without departing from the spirit and scope of the invention. Any modification, equivalent replacement, or improvement made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims (4)

1. A preparation method of a novel stainless steel glasses slingshot box is characterized by comprising the following steps:
the method comprises the following steps: adding 80-90% of plastic into stainless steel powder, mixing, adding 10-20% of plastic adhesive, heating to 150-200 ℃ in an internal mixer, banburying, dissolving, and preparing into granular feed;
step two: the prepared materials are put into an injection molding machine to be heated to 150-200 ℃ and then injected into a mold of a slingshot box product of a corresponding style for molding;
step three: putting the slingshot box of the corresponding style into a degreasing catalytic furnace, heating to 100-150 ℃, and degreasing through chemical reaction;
step four: putting the degreased slingshot box product into a high-temperature vacuum sintering furnace, slowly heating to 1300-1400 ℃, sintering for 8-15 hours, and finally forming a product with a relative slingshot box style;
step five: and step four, performing decontamination grinding by multiple magnetic forces, and shaping.
2. The method for preparing the slingshot box of the novel stainless steel glasses as claimed in claim 1, wherein the second step is to perform edging treatment after molding.
3. The method for preparing the slingshot box of the novel stainless steel glasses according to claim 1, wherein the third step is to protect with nitrogen gas in the degreasing process.
4. The method for preparing a new stainless steel spectacle slingshot box of claim 1, wherein the grinding and shaping in step five further comprises:
the method comprises the following steps: aligning the thick capillary holes of the slingshot boxes through the arrangement plates to the slingshot boxes, and roughly polishing and peeling the slingshot boxes through the polishing disc;
step two: severe coarse pores generated by the slingshot box are subjected to sanding by a disc machine to remove surface pores;
step three: grinding the slingshot box by using a 6 x 6 circle coarse grinding machine;
step four: grinding the slingshot box by a flow type finishing machine with 4-4 round grinding materials;
step five: grinding the slingshot box by using a flow type finishing machine with 3 x 3 round thin materials;
step five: grinding the slingshot box by using a walnut grain polishing material for a flow type polishing machine.
CN201510661145.0A 2015-10-15 2015-10-15 Preparation method of novel stainless steel glasses slingshot compartment Pending CN105149588A (en)