CN105126255A - Health-care crystal/glass artware and preparation method thereof - Google Patents

Health-care crystal/glass artware and preparation method thereof Download PDF

Info

Publication number
CN105126255A
CN105126255A CN201510387853.XA CN201510387853A CN105126255A CN 105126255 A CN105126255 A CN 105126255A CN 201510387853 A CN201510387853 A CN 201510387853A CN 105126255 A CN105126255 A CN 105126255A
Authority
CN
China
Prior art keywords
crystal
glass
energy
mineral powder
ore
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510387853.XA
Other languages
Chinese (zh)
Inventor
周永富
赵东坤
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shitai Fuxing (beijing) Trading Co Ltd
Original Assignee
Shitai Fuxing (beijing) Trading Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shitai Fuxing (beijing) Trading Co Ltd filed Critical Shitai Fuxing (beijing) Trading Co Ltd
Priority to CN201510387853.XA priority Critical patent/CN105126255A/en
Publication of CN105126255A publication Critical patent/CN105126255A/en
Pending legal-status Critical Current

Abstract

The embodiment of the invention discloses health-care crystal/glass artware and a preparation method thereof. The health-care crystal/glass artware comprises a main body layer and an energy layer located at the inner side of the main body layer, wherein the main body layer is crystal or glass, energy mineral powder, which is formed by titanium dioxide with the mass fraction ranging from 10% to 15%, germanium ore with the mass fraction ranging from 5% to 15%, neodymium ore with the mass fraction ranging from 15% to 25%, lanthanum ore with the mass fraction ranging from 10% to 15%, cerium ore with the mass fraction ranging from 10% to 15% and rare earth with the mass fraction ranging from 25% to 35%, is naturally distributed in the energy layer; the energy layer is formed through adding the energy mineral powder to a high borosilicate glass tube acting as the crystal/glass main body layer; and then the high borosilicate glass tube is heated until the glass tube is softened so as to prepare the crystal/glass artware. According to the crystal/glass artware disclosed by the invention, 4um-16um far infrared light waves emitted by the energy mineral powder emits have such health-care effects as odor removing, bacterium fighting and inflammation eliminating for the human body and the environment in the daily life.

Description

A kind of crystal, Glass Craft and preparation method thereof of health care
Technical field
The present invention relates to crystal, Glass Craft, be specifically related to a kind of crystal, the Glass Craft with health-care effect.
Background technology
Crystal, Glass Craft are interior decorations, vehicle-mounted decoration, daily playing in part cannot lack, and demand is large.Along with the raising of people's living standard, to crystal, glass with to play the requirement of part also more and more higher.Although existing crystal, Glass Craft are beautiful, high-end, magnificent, decorate life and make people pleasing, and by shape, human acupoint stimulation is played to the effect playing part and harmonize the body.But, above-mentioned existing crystal, Glass Craft or only view and admire and decorative effect, or be only, by shape, certain massage effect is played to acupoint stimulation, to human body not significant health care.Therefore, the function making crystal, Glass Craft play health care to human body while having beautiful shape and outward appearance prepares the development prospect of functional health-care crystal, Glass Craft.
Far infrared has stronger penetration and radiant force, has significant temperature control effect and resonance effect, and it is easily absorbed by object and is converted into energy in object.After far infrared is absorbed by the body, hydrone in body can be made to produce resonance, make water molecule activation, strengthen its intermolecular adhesion, thus the biomacromolecules such as activation of protein, make biological cell be in the highest vibration level.Because biological cell produces resonance effect, far infrared heat energy can be delivered to the subcutaneous darker part of human body, following deep layer temperature rises, and the warm of generation is distributed from inside to outside.This action intensity, makes telangiectasis, blood circulation promoting, strengthens the metabolism between each tissue, increases the regeneration capacity of tissue, improves the immunocompetence of body, regulates the exaltation state of spirit, thus plays the effect of health care.
In order to prepare crystal, the Glass Craft with health care, the health-care effect of far infrared light wave effect of admiring and decorate with crystal, Glass Craft is combined by the present invention, provides a kind of crystal, Glass Craft and preparation method thereof with health-care effect.
Summary of the invention
A kind of crystal, the Glass Craft with health-care effect provided in the embodiment of the present invention can produce the far-infrared ray power light wave of 4um-16um, make people appreciate or play time reach the effect of health care simultaneously.
Crystal, the Glass Craft of a kind of health care provided in the embodiment of the present invention, comprise body layer and be positioned at the energy layer inside body layer, wherein, described body layer is crystal or glass, and in described energy layer, NATURAL DISTRIBUTION has energy mineral powder.
Preferably, above-mentioned crystal, Glass Craft, wherein said energy mineral powder is made up of each component of following mass fraction: titanium dioxide 10%-15%, germanium Ore 5%-15%, neodymium Ore 15%-25%, lanthanum Ore 10%-15%, cerium Ore 10%-15%, rare earth 25%-35%.
Preferably, above-mentioned crystal, Glass Craft, wherein said energy mineral powder is made up of each component of following mass fraction: titanium dioxide 15%, germanium Ore 10%, neodymium Ore 20%, lanthanum Ore 12%, cerium Ore 12%, rare earth 31%.
Preferably, above-mentioned crystal, Glass Craft also comprise color grains, and wherein said color grains is irregular to be distributed in body layer and energy layer.
Preferably, above-mentioned crystal, Glass Craft, wherein said color grains is selected from the one in stained glass particulates and colour crystal granule.
The preparation method of the above-mentioned crystal of any one, Glass Craft, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1000-2000 object energy mineral powder powder is for subsequent use;
(2) glass tubing is chosen as body layer, the energy mineral powder getting preparation in step (1) joins glass tubing, and glass tube is heated, the heating-up temperature making glass tube is 600 DEG C-1200 DEG C, makes energy mineral powder melt and automatically form the energy layer be positioned at inside glass body layer; Then heatable glass tube softens to glass tubing, is made into various difform Glass Craft.
Preferably, above-mentioned preparation method, wherein described in step (2), glass tubing is high-boron-silicon glass pipe.
The preparation method of the above-mentioned crystal of any one, Glass Craft, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1000-2000 object energy mineral powder powder is for subsequent use;
(2) crystal pipe is chosen as body layer, the energy mineral powder getting preparation in step (1) joins crystal pipe, and by the heating of crystal inside, the heating-up temperature making crystal pipe inside is 1000 DEG C-1200 DEG C, makes energy mineral powder melt and automatically form the energy layer be positioned at inside crystal body layer; Then heat crystal pipe to soften to crystal pipe, be made into various difform crystal works.
Preferably, the preparation method of above-mentioned two kinds, the energy mineral powder in wherein said step (2) also comprises stained glass particulates or colour crystal granule.
Preferably, the preparation method of above-mentioned two kinds, wherein, the particle diameter of the energy mineral powder powder in described step (1) is 1300-1800 order.
The present invention is by adding energy mineral powder in glass tubing or crystal pipe, the titanium in energy mineral powder, and germanium is as primary energy content, and neodymium Ore, lanthanum Ore, cerium Ore, rare earth, as auxiliary element, launches the far-infrared ray power light wave of 4um-16um.
The heat effect of the far infrared light wave that crystal of the present invention, Glass Craft are launched, by neurohumoral answer reaction, eliminate the pathological process of inflammation, originally the physiological equilibrium's state destroyed is restored, improve the resistance against diseases of local and whole body, have activated immune cell function, strengthen the phagocytic function of leukocyte and reticuloendothelial cell, reach the object that antiinflammatory is antibacterial.Far heat effect, makes skin temperature increase, sympathetic nerve decreased capacity, vaso-active substance is discharged, vasodilation, blood flow is accelerated, blood circulation improves, enhance histotrophic nutrition, enlivened tissue metabolism, improve cell oxygen-supplying amount, improve the blood supply oxygen condition of focal zone, strengthen cell regeneration ability, control the development of inflammation and make its localization, accelerating focus reparation.Far heat effect, improves microcirculation, establishes collateral circulation, enhances the stability of cell membrane, have adjusted the degree of depth of ion, facilitates the metabolism of noxious substance and the excretion of refuse, accelerates the absorption of oozing out material, cause disappearing of inflammation edema.
Relative to prior art, crystal of the present invention, Glass Craft, daily view and admire or play in, the far infrared light wave of transmitting serves human body and environment and eliminates the unusual smell and the health-care effect of anti-inflammation.
Accompanying drawing explanation
In order to be illustrated more clearly in the embodiment of the present invention or technical scheme of the prior art, be briefly described to the accompanying drawing used required in embodiment below, apparently, accompanying drawing in the following describes is only some embodiments of the present invention, for those of ordinary skill in the art, under the prerequisite not paying creative work, other accompanying drawing can also be obtained according to these accompanying drawings.
The infrared radiation wavelength of Fig. 1, embodiment of the present invention 1-5 crystal, Glass Craft detects collection of illustrative plates;
The crystal calabash of a kind of health care of Fig. 2, the embodiment of the present invention 1 preparation;
In figure: 1-crystal body layer; 2-energy layer; 3-color grains.
Detailed description of the invention
Below in conjunction with the embodiment of the present invention, carry out clear, complete description to the technical scheme in the embodiment of the present invention, obviously, described embodiment is only the present invention's part embodiment, instead of whole embodiments.Based on the embodiment in the present invention, those of ordinary skill in the art, not making the every other embodiment obtained under creative work prerequisite, belong to the scope of protection of the invention.
Embodiment 1
The crystal glass handicraft of a kind of health care provided in the embodiment of the present invention, comprise crystal body layer and be positioned at the energy layer inside crystal body layer, wherein, in described energy layer, NATURAL DISTRIBUTION has energy mineral powder, and described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 15%, germanium Ore 10%, neodymium Ore 20%, lanthanum Ore 12%, cerium Ore 12%, rare earth 31%.
The preparation method of the crystal works of the present embodiment, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1500 object energy mineral powder powder are for subsequent use;
(2) crystal pipe is chosen as crystal body layer, get the energy mineral powder 0.5g of preparation in step (1) and add colour crystal granule, mix homogeneously, subsequently mixture being joined thickness is 0.5cm-2cm, external diameter is the crystal pipe of 3cm-5cm, and by the heating of crystal pipe inside, make the heating-up temperature to 1100 DEG C of crystal pipe inside, make energy mineral powder melt and automatically form the energy layer be positioned at inside crystal body layer; Then heat crystal pipe to soften to crystal pipe, be made into lageniform crystal works, result as shown in Figure 2.In crystal calabash prepared by the present invention, energy layer 2 is positioned at the internal layer of crystal body layer 1, and the granule 3 that all irregular distribution is colored in energy layer and crystal glass body layer, both attractive in appearance have the effect with health care.
Embodiment 2
A kind of Glass Craft of health care, comprise glass body layer and be positioned at the energy layer inside glass body layer, wherein, in described energy layer, NATURAL DISTRIBUTION has energy mineral powder, and described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 13%, germanium Ore 5%, neodymium Ore 25%, lanthanum Ore 10%, cerium Ore 12%, rare earth 35%.
The preparation method of the Glass Craft of the present embodiment, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1800 object energy mineral powder powder are for subsequent use;
(2) high-boron-silicon glass pipe is chosen as glass body layer, get the energy mineral powder 0.5g of preparation in step (1) and add stained glass particulates, mix homogeneously, subsequently mixture being joined thickness is 0.5cm-2cm, external diameter is in the high-boron-silicon glass pipe of 3cm-5cm, and by the heating of high-boron-silicon glass pipe inside, the heating-up temperature making high-boron-silicon glass pipe inside is 800 DEG C, energy mineral powder is made to melt and automatically form the energy layer be positioned at inside glass body layer; Then heat high-boron-silicon glass pipe to soften to glass tubing, be made into lageniform crystal glass handicraft.
Embodiment 3
A kind of crystal works of health care, comprise crystal body layer and be positioned at the energy layer inside crystal body layer, wherein, in described energy layer, NATURAL DISTRIBUTION has energy mineral powder, and described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 10%, germanium Ore 10%, neodymium Ore 20%, lanthanum Ore 13%, cerium Ore 12%, rare earth 35%.
The preparation method of the crystal works of the present embodiment, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1300 object energy mineral powder powder are for subsequent use;
(2) crystal pipe is chosen as crystal body layer, it is 0.5cm-2cm that the energy mineral powder 0.5g getting preparation in step (1) joins thickness, external diameter is the crystal pipe of 3cm-5cm, and by the heating of crystal pipe inside, make the heating-up temperature to 1000 DEG C of crystal pipe inside, make energy mineral powder melt and automatically form the energy layer be positioned at inside crystal body layer; Then heat crystal pipe to soften to crystal pipe, make difform crystal glass handicraft as required.
Embodiment 4
A kind of Glass Craft of health care, comprise glass body layer and be positioned at the energy layer inside crystal glass body layer, wherein, in described energy layer, NATURAL DISTRIBUTION has energy mineral powder, and described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 15%, germanium Ore 15%, neodymium Ore 15%, lanthanum Ore 15%, cerium Ore 15%, rare earth 25%.
The preparation method of the Glass Craft of the present embodiment, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1000 object energy mineral powder powder are for subsequent use;
(2) high-boron-silicon glass pipe is chosen as glass body layer, it is 0.5cm-2cm that the energy mineral powder 0.5g getting preparation in step (1) joins thickness, external diameter is in the high-boron-silicon glass pipe of 3cm-5cm, and by the heating of high-boron-silicon glass pipe inside, the heating-up temperature making high-boron-silicon glass pipe inside is 600 DEG C, makes energy mineral powder melt and automatically form the energy layer be positioned at inside glass body layer; Then heat high-boron-silicon glass pipe to soften to glass tubing, make difform Glass Craft as required.
Embodiment 5
A kind of crystal works of health care, comprise crystal body layer and be positioned at the energy layer inside crystal body layer, wherein, in described energy layer, NATURAL DISTRIBUTION has energy mineral powder, and described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 15%, germanium Ore 14%, neodymium Ore 18%, lanthanum Ore 15%, cerium Ore 10%, rare earth 28%.
The preparation method of the crystal works of the present embodiment, comprises the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 2000 object energy mineral powder powder are for subsequent use;
(2) crystal pipe is chosen as crystal body layer, it is 0.5cm-2cm that the energy mineral powder 0.5g getting preparation in step (1) joins thickness, external diameter is the crystal pipe of 3cm-5cm, and by the heating of crystal pipe inside, make the heating-up temperature to 1200 DEG C of crystal pipe inside, make energy mineral powder melt and automatically form the energy layer be positioned at inside crystal body layer; Then heat crystal pipe to soften to crystal pipe, make difform crystal works as required.
According to GB/T7287-2008 " infrared radiation heater test method ", the crystal prepared above-described embodiment 1-5, Glass Craft carry out infrared radiation wavelength detection, as shown in Figure 1, crystal prepared by embodiment 1-5, Glass Craft all can produce the far-infrared ray power light wave of 4um-16um to result.
Crystal in the present embodiment 1-5, glass launch the far-infrared ray power light wave of 4um-16um in daily life, can play sterilization, the effect eliminated the unusual smell.
Prove through experiment, the crystal display within doors, glass goods of furniture for display rather than for use or play part launch far-infrared ray power light wave can appreciation while by reacting with the answer of human nerve body fluid, eliminate the pathological process of inflammation, originally the physiological equilibrium's state destroyed is restored, improve the resistance against diseases of local and whole body, have activated immune cell function, strengthen the phagocytic function of leukocyte and reticuloendothelial cell, reach the object that antiinflammatory is antibacterial.

Claims (10)

1. crystal, the Glass Craft of health care, is characterized in that, comprises body layer and be positioned at energy layer inside body layer, and wherein, described body layer is the one in crystal and glass, and in described energy layer, NATURAL DISTRIBUTION has energy mineral powder.
2. crystal according to claim 1, Glass Craft, it is characterized in that, described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 10%-15%, germanium Ore 5%-15%, neodymium Ore 15%-25%, lanthanum Ore 10%-15%, cerium Ore 10%-15%, rare earth 25%-35%.
3. crystal according to claim 2, Glass Craft, is characterized in that, described energy mineral powder is made up of each component of following mass fraction: titanium dioxide 15%, germanium Ore 10%, neodymium Ore 20%, lanthanum Ore 12%, cerium Ore 12%, rare earth 31%.
4. crystal according to claim 1, Glass Craft, is characterized in that, described crystal, Glass Craft also comprise color grains, and wherein said color grains is irregular to be distributed in body layer and energy layer.
5. crystal according to claim 4, Glass Craft, is characterized in that, described color grains is selected from the one in stained glass particulates and colour crystal granule.
6. the crystal according to any one of claim 2-5, a preparation method for Glass Craft, is characterized in that, comprise the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1000-2000 object energy mineral powder powder is for subsequent use;
(2) glass tubing is chosen as body layer, the energy mineral powder getting preparation in step (1) joins glass tubing, and glass tube is heated, the heating-up temperature making glass tube is 600 DEG C-1200 DEG C, makes energy mineral powder melt and automatically form the energy layer be positioned at inside glass body layer; Then heatable glass tube softens to glass tubing, is made into various difform Glass Craft.
7. preparation method according to claim 6, is characterized in that, described in step (2), glass tubing is high-boron-silicon glass pipe.
8. the crystal according to any one of claim 2-5, a preparation method for Glass Craft, is characterized in that, comprise the following steps:
(1) take raw material according to the mass fraction of each component of described energy mineral powder, mixed grinding is pulverized, and sieves, and selects particle diameter to be that 1000-2000 object energy mineral powder powder is for subsequent use;
(2) crystal pipe is chosen as body layer, the energy mineral powder getting preparation in step (1) joins crystal pipe, and by the heating of crystal inside, the heating-up temperature making crystal pipe inside is 1000 DEG C-1200 DEG C, makes energy mineral powder melt and automatically form the energy layer be positioned at inside crystal body layer; Then heat crystal pipe to soften to crystal pipe, be made into various difform crystal works.
9. the preparation method according to claim 6 or 8, is characterized in that, the energy mineral powder in described step (2) also comprises stained glass particulates or colour crystal granule.
10. the preparation method according to claim 6 or 8, is characterized in that, the particle diameter of the energy mineral powder powder in described step (1) is 1300-1800 order.
CN201510387853.XA 2015-07-03 2015-07-03 Health-care crystal/glass artware and preparation method thereof Pending CN105126255A (en)