CN104999849B - 3d打印的树脂画、制备其的设备和方法 - Google Patents

3d打印的树脂画、制备其的设备和方法 Download PDF

Info

Publication number
CN104999849B
CN104999849B CN201510448510.XA CN201510448510A CN104999849B CN 104999849 B CN104999849 B CN 104999849B CN 201510448510 A CN201510448510 A CN 201510448510A CN 104999849 B CN104999849 B CN 104999849B
Authority
CN
China
Prior art keywords
printing
matrix
printer
pigment
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201510448510.XA
Other languages
English (en)
Other versions
CN104999849A (zh
Inventor
朱巍
祝孔涛
赵耀
段云涛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510448510.XA priority Critical patent/CN104999849B/zh
Publication of CN104999849A publication Critical patent/CN104999849A/zh
Application granted granted Critical
Publication of CN104999849B publication Critical patent/CN104999849B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种3D打印的树脂画、及制备其的设备和方法,3D打印的树脂画包括透明材料经3D打印制成的基体、嵌设在基体内的颜料经3D打印制成的画体;制备树脂画的设备包括模具和3D打印机,3D打印机上安装有基体墨盒和颜料墨盒,基体墨盒内盛装有透明材质的基体墨,颜料墨盒内盛装有颜料制成的颜料墨;模具具有一开口向上的容纳腔室,3D打印机的打印区域设有固定模具的底部的夹具;3D打印机包括模型存储单元,模型存储单元内存储有3D模型的数据。本发明的有益效果为:提高生产效率,降低作品的成本;提高了树脂画的表现力;缩短固化时间,提高了作业效率,缩减了制备成本。

Description

3D打印的树脂画、制备其的设备和方法
技术领域
本发明涉及艺术品制备技术领域,具体涉及一种3D打印的树脂画、制备其的设备和方法。
背景技术
树脂只是一种载体,用来模拟水的形态然后绘制成画,因此树脂画看起来特别逼真,另,由于逐层绘画,更有层次感,仿佛在水中游动的鱼定格在那一刻,看起来更加立体。但是现在的树脂画都是人手工绘制,对人的绘画技能要求高,要求绘画人经过长期的学习才能绘出具有艺术感的树脂画。因此,需要一种可以工业生产、不受绘画人的艺术造诣影响的3D打印的树脂画。
发明内容
本发明的目的是提供一种3D打印的树脂画、制备其的设备和方法,通过使用透明材料制成基体,作为背景,使用画体作为主要表现点,以实现树脂画的工业化生产,免除对人的艺术水平的限制,提高生产效率,降低作品的成本,以克服现有技术存在的上述不足。
本发明的目的是通过以下技术方案来实现的:
3D打印的树脂画,其包括透明材料经3D打印制成的基体、嵌设在基体内的颜料经3D打印制成的画体。
进一步的,所述基体由树脂制成。
制备树脂画的设备,其包括模具和3D打印机,所述3D打印机上安装有基体墨盒和颜料墨盒,所述基体墨盒内盛装有透明材质的基体墨,所述颜料墨盒内盛装有颜料制成的颜料墨;所述模具具有一开口向上的容纳腔室,所述3D打印机的打印区域设有固定所述模具的底部的夹具;所述3D打印机包括模型存储单元,所述模型存储单元内存储有3D模型的数据。
进一步的,该设备还包括固化装置,所述固化装置包括热风机、热风输送管道和热风喷嘴,所述热风输送管道的一端与所述热风机的出风口连通,所述热风输送管道的另一端与所述热风喷嘴连通,所述热风喷嘴的出风口的位置和出风角度均可调节地设置。
制备树脂画的方法,依次包括如下步骤:
S1、将模具开口向上地放置在3D打印机的打印区域;
S2、在模具中依次打印出第一层、...和第N层,打印每一层时,位于该层下面的一层已固化;
S3、待第N层打印完毕并且固化后脱模。
进一步的,在步骤S2和步骤S3中向每一层吹热风。
本发明的有益效果为:
通过使用透明材料制成基体,作为背景,使用画体作为主要表现点,以实现树脂画的工业化生产,免除对人的艺术水平的限制,提高生产效率,降低作品的成本;逐层打印,提高了树脂画的表现力;使用固化装置加速每层树脂打印好后的固化,缩短固化时间,提高了作业效率,降低了对仓储空间的占用,同时缩减了制备成本。
附图说明
图1是本发明的结构示意图。
图中:1、基体;2、画体。
具体实施方式
优选实施方式
如图1所示,3D打印的树脂画,其包括透明材料经3D打印制成的基体1、嵌设在基体1内的颜料经3D打印制成的画体2。基体1由树脂、透明塑料等透明材制成。
制备树脂画的设备,其包括模具和3D打印机,3D打印机上安装有基体墨盒和颜料墨盒,基体墨盒内盛装有透明材质的基体墨,颜料墨盒内盛装有颜料制成的颜料墨;模具具有一开口向上的容纳腔室,3D打印机的打印区域设有固定模具的底部的夹具;3D打印机包括模型存储单元,模型存储单元内存储有3D模型的数据。
该设备还包括固化装置,固化装置包括热风机、热风输送管道和热风喷嘴,热风输送管道的一端与热风机的出风口连通,热风输送管道的另一端与热风喷嘴连通,热风喷嘴的出风口的位置和出风角度均可调节地设置。
制备树脂画的方法,依次包括如下步骤:
S1、将模具开口向上地放置在3D打印机的打印区域;
S2、在模具中依次打印出第一层、...和第N层,打印每一层时,位于该层下面的一层已固化;
S3、待第N层打印完毕并且固化后脱模。
在步骤S2和步骤S3中向每一层吹热风。
采用上述的设备和方法制备树脂画时,3D打印机工作,调取预先存储在模型存储单元内的3D模型数据,并分层打印出各层,并且打印过程中利用固化装置向每一层吹热风,使得树脂的固化加速,直到最上面一层打印完毕并固化后,从模具中取出本发明所述的3D打印树脂画即可,通过使用透明材料制成基体1,作为背景,使用画体2作为主要表现点,以实现树脂画的工业化生产,免除对人的艺术水平的限制,提高生产效率,降低作品的成本;逐层打印,提高了树脂画的表现力;使用固化装置加速每层树脂打印好后的固化,缩短固化时间,提高了作业效率,降低了对仓储空间的占用,同时缩减了制备成本。

Claims (1)

1.一种3D打印制备树脂画的方法,其特征在于,树脂画包括透明材料经3D打印制成的基体、嵌设在基体内的颜料经3D打印制成的画体;所述基体由树脂制成;
制备树脂画的设备,包括模具和3D打印机,所述3D打印机上安装有基体墨盒和颜料墨盒,所述基体墨盒内盛装有透明材质的基体墨,所述颜料墨盒内盛装有颜料制成的颜料墨;所述模具具有一开口向上的容纳腔室,所述3D打印机的打印区域设有固定所述模具的底部的夹具;所述3D打印机包括模型存储单元,所述模型存储单元内存储有3D模型的数据;
所述设备还包括固化装置,所述固化装置包括热风机、热风输送管道和热风喷嘴,所述热风输送管道的一端与所述热风机的出风口连通,所述热风输送管道的另一端与所述热风喷嘴连通,所述热风喷嘴的出风口的位置和出风角度均可调节地设置;
制备树脂画的方法,依次包括如下步骤:
S1、将模具开口向上地放置在3D打印机的打印区域;
S2、在模具中依次打印出第一层、...和第N层,打印每一层时,位于该层下面的一层已固化;
S3、待第N层打印完毕并且固化后脱模;
其中,在步骤S2和步骤S3中向每一层吹热风。
CN201510448510.XA 2015-07-28 2015-07-28 3d打印的树脂画、制备其的设备和方法 Expired - Fee Related CN104999849B (zh)