CN104974830A - Preparation method for concentrated type anti-rust oil - Google Patents

Preparation method for concentrated type anti-rust oil Download PDF

Info

Publication number
CN104974830A
CN104974830A CN201510352116.6A CN201510352116A CN104974830A CN 104974830 A CN104974830 A CN 104974830A CN 201510352116 A CN201510352116 A CN 201510352116A CN 104974830 A CN104974830 A CN 104974830A
Authority
CN
China
Prior art keywords
parts
concentrated type
blending process
type anti
rust oil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510352116.6A
Other languages
Chinese (zh)
Inventor
李云军
陈蓉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201510352116.6A priority Critical patent/CN104974830A/en
Publication of CN104974830A publication Critical patent/CN104974830A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method for concentrated type anti-rust oil. The concentrated type anti-rust oil comprises the following components in parts by weight: 20 parts of barium petroleum sulfonate, 15 parts of zinc naphthenate, 35 parts of lamp kerosene, 30 parts of industrial vaseline, 0.3 part of wool fat and 0.1 part of benzotriazole, wherein the lamp kerosene is filtered by a 10-micron filter bag. The components are blended by full-automatic pulses, a temperature in a blending process is detected by a temperature sensor used in the blending process, and pulse frequency in the blending process is detected by a pulse frequency detecting circuit. The problem that a metal apparatus gets rusty in a storage and processing process is solved.

Description

Concentrated type slushing oil making method
Technical field
The present invention relates to chemistry, field of metallurgy, particularly, relate to a kind of concentrated type slushing oil making method.
Background technology
At present, machinery has become to be produced and requisite part in life, but the important materials of manufacturing machine is metal, but metal rusting problem affects the work-ing life of machinery always, especially in the preservation and manufacturing procedure of metal device.
Summary of the invention
The object of the invention is to, for the problems referred to above, propose a kind of concentrated type slushing oil making method, to realize the problem that solution metal device gets rusty in stock and the course of processing.
For achieving the above object, the technical solution used in the present invention is:
A kind of concentrated type slushing oil making method, each component, according to weight ratio, comprises, barium mahogany sulfonate 20 parts, zinc naphthenate 15 parts, illuminating kerosene 35 parts, industrial vaseline 30 parts, 0.3 part, lanolin, benzotriazole 0.1 part;
Illuminating kerosene is through the sock filtration of 10 μm;
Adopt full-automatic pulse to concoct above-mentioned each component, and use temperature sensor detects the temperature in blending process in harmonic process, use pulse-repetition testing circuit to detect the pulse-repetition in blending process.
Technical scheme of the present invention has following beneficial effect:
Technical scheme of the present invention, by blending slushing oil, adopts the method for physics, generates protective membrane in metallic surface, with the contact of isolated metallic surface and corrosives.Thus solve the problem that metal device gets rusty in stock and the course of processing.
Embodiment
A kind of concentrated type slushing oil making method, each component, according to weight ratio, comprises, barium mahogany sulfonate 20 parts, zinc naphthenate 15 parts, illuminating kerosene 35 parts, industrial vaseline 30 parts, 0.3 part, lanolin, benzotriazole 0.1 part;
Illuminating kerosene is through the sock filtration of 10 μm;
Adopt full-automatic pulse to concoct above-mentioned each component, and use temperature sensor detects the temperature in blending process in harmonic process, use pulse-repetition testing circuit to detect the pulse-repetition in blending process.
Sulfonated castor oil 2 parts can also be added in addition.
Last it is noted that the foregoing is only the preferred embodiments of the present invention, be not limited to the present invention, although with reference to previous embodiment to invention has been detailed description, for a person skilled in the art, it still can be modified to the technical scheme described in foregoing embodiments, or carries out equivalent replacement to wherein portion of techniques feature.Within the spirit and principles in the present invention all, any amendment done, equivalent replacement, improvement etc., all should be included within protection scope of the present invention.

Claims (1)

1. a concentrated type slushing oil making method, is characterized in that, each component, according to weight ratio, comprises, barium mahogany sulfonate 20 parts, zinc naphthenate 15 parts, illuminating kerosene 35 parts, industrial vaseline 30 parts, 0.3 part, lanolin, benzotriazole 0.1 part;
Illuminating kerosene is through the sock filtration of 10 μm;
Adopt full-automatic pulse to concoct above-mentioned each component, and use temperature sensor detects the temperature in blending process in harmonic process, use pulse-repetition testing circuit to detect the pulse-repetition in blending process.
CN201510352116.6A 2015-06-24 2015-06-24 Preparation method for concentrated type anti-rust oil Pending CN104974830A (en)