CN104957981A - Explosion-proof glass body machining method - Google Patents
Explosion-proof glass body machining method Download PDFInfo
- Publication number
- CN104957981A CN104957981A CN201510422914.1A CN201510422914A CN104957981A CN 104957981 A CN104957981 A CN 104957981A CN 201510422914 A CN201510422914 A CN 201510422914A CN 104957981 A CN104957981 A CN 104957981A
- Authority
- CN
- China
- Prior art keywords
- glass body
- cup
- diaphragm
- explosion
- protection film
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention provides an explosion-proof glass body machining method. The explosion-proof glass body machining method is characterized by comprising the following steps that an explosion-proof glass body adopts the blowing technology, the outside of the explosion-proof glass body is sleeved with a protection film, the protection film is attached to the outer wall of the glass body to the greatest extent, and the outside of the glass body is totally wrapped with the protection film; the glass body and the protection film are heated together, and the protection film contracts to be attached to the outer wall of the glass body; the well heated protection film glass body is placed on a table-board and rotated, the portions, located on the upper stepped surface and the lower stepped surface, of the glass body are cut off by a knife; patterns and water gauge scales can be printed onto the protection film; the outside of the stepped surface of the glass body is sleeved with a bottom cover from top to bottom, the protection film is closed up to serve as a shield, and therefore the closed-up portion of the protection film is prevented from being torn off. By means of the explosion-proof glass body machining method, the explosion-proof glass body has the advantages that the structure is simple and reasonable, the machining and manufacturing procedures are less, the assembly is convenient and fast, the production efficiency is high, the explosion-proof effect is good, the service life is prolonged, safety and reliability are achieved, and appearance is beautiful and elegant.
Description
Technical field
The present invention relates to a kind of processing method of implosion guard cup cup.
Background technology
Electric kettle is one of conventional small household appliances, for heating water, can be used as again the container of water simultaneously, having feature easy to use.Prior art majority adopt glass bodice with play glue between heat-generating disc and be connected and seal, or, silica gel connects sealing, as: China Patent No. ZL200720171554.3 invention have employed following technical scheme: a kind of electric kettle, the kettle body comprising top and the equal opening in bottom and the electrical heating being connected to the heat-generating disc in kettle body under shed, the electric connector that can rotate arbitrarily and kettle are connected base, described kettle body is connected on heat-generating disc by fire-resistant nontoxic viscose glue, and described heat-generating disc is provided with temperature sensing and control and regulation device and level detecting device.Because glass bodice outside does not arrange Anticollision Measures, when non-normal use, glass bodice easily clashes into explosion and hurts sb.'s feelings, and there is security hidden trouble.Therefore, be necessary to be further improved.
Summary of the invention
Object of the present invention aims to provide a kind of processing method that is simple and reasonable, easy to assembly, both artistic and practical, a kind of implosion guard cup cup safely and reliably, to overcome weak point of the prior art.It is characterized in that by the processing method of a kind of implosion guard cup cup of this design, comprise the steps:
1) glass cup adopts technological process for blowing, and diaphragm is inserted in glass cup outside, and diaphragm is tried one's best cup outer wall, by outside for glass main body body all parcels;
2) heated together with diaphragm by glass cup, diaphragm shrinks fits with glass cup outer wall;
3) the diaphragm glass cup heated is placed on table top, the diaphragm on the upper and lower step surface of glass cup is cut down by its rotation cutter;
4) can printed patterns and water gauge scale on diaphragm;
5) bottom is placed on the outside of glass cup step surface from top to bottom, diaphragm is closed up as blocking, prevent diaphragm from closing up and be torn.
The processing method of implosion guard cup cup is used to use a kind of implosion guard cup cup through the present invention; cup is arranged main body body, upper shed, under shed, diaphragm; it is characterized in that described glass cup opening part is provided with step; step is connected with the outer smooth of main body body; the bending part of step and main body body and the outer setting diaphragm of main body body; diaphragm exceeds glass cup outer wall, and diaphragm is by glass cup outer wall and Outer shrink part or pouring mouth part clamping position.
Diaphragm on described cup and main body body outer wall shrink compact siro spinning technology of fitting to be fixed, and diaphragm is retracted to cup opening part step folding crook, becomes arc transition bending laminating to connect to in-flanges; Described diaphragm extends to step drop face and stops, and diaphragm end and cup opening part are kept at a distance and stopped, close up.
Diaphragm outer wall height on described cup and the drop of cup outer wall at least 0.01 millimeter, or the thickness of diaphragm at least 0.01 millimeter, diaphragm heat shrinkable is to cup opening part step folding crook, and diaphragm inwall and cup outer wall fit tightly.
The described diaphragm outer wall be heated along main body body moves and tightens up, and is consistent with the external body of main body body, diaphragm closing in position is less than the outer wall dimension of main body body, the working strength of described diaphragm laminating position reinforced glass cup main body body, silica gel sealing ring is installed, not easily cracking is extruded during heat-generating disc, or, glass main body external impact point of experiencing inwardly is shunk in diaphragm protection inwardly can not shrink cushioning effect of having split, or, diaphragm protection is inwardly shunk the experience sidepiece of external impact point of glass main body and externally can not be protruded and tear cup by pressurized, protection main body body surrounding uniform stressed, play cushioning effect, or, diaphragm inwardly shrink cover glass cup main body experience external impact time, power is let out at other positions of impact uniform conductive main body body, glass main body body externally can not protrude explosion by pressurized.
The upper shed of described glass cup, under shed arrange aduncate stage portion and connection and are arranged on round as a ball closing in limit below stage portion, and round as a ball closing in limit can not scratch the finger of silica gel sealing ring or direct labor.
Described glass cup under shed arranges silica gel sealing ring, heat-generating disc; round as a ball for glass cup bottom closing in limit is connected sealing with heat-generating disc parcel by silica gel sealing ring; or; silica gel sealing ring is arranged on round as a ball closing in limit, glass cup bottom and is connected crush seal with between heat-generating disc; described glass cup under shed outer setting bottom or base ring, the closing in position of diaphragm is blocked or is clamped between glass cup outer wall by the upper end of bottom or base ring or inside upper part wall.
The upper shed of described glass cup arranges aduncate stage portion, and diaphragm extends on the sidewall of aduncate stage portion, and the closing in position of diaphragm is blocked or is clamped between glass cup outer wall by stage portion outer setting contractibility or pouring mouth part; Round as a ball closing in limit arranges pouring mouth or round as a ball closing in limit and to be tightly connected pouring mouth part.
The upper shed of described glass cup arranges round as a ball closing in limit, and the top on round as a ball closing in limit arranges upper cover and covers with it.
Described diaphragm is shrink film, and shrink film is plastic material, and shrink film at least can heatproof 60 degree; Described shrink film is that annular is arranged on the outer wall of glass cup; Described shrink film is transparent or opaque setting.
The present invention has simple and reasonable, and processing and fabricating operation is few, fast easy to assembly, and production efficiency is high, and explosion-proof effect is good, and service life extends, safety and sanitation, the feature of appearance looks elegant gracefulness.
Accompanying drawing explanation
Fig. 1 is the structure sectional view of an embodiment implosion guard cup cup;
Fig. 2 is A place structure for amplifying schematic diagram in Fig. 1;
Fig. 3 is the structure sectional view of the second embodiment implosion guard cup cup;
Fig. 4 is the structure sectional view of the 3rd embodiment implosion guard cup cup;
Fig. 5 is the three-dimensional exploded view of implosion guard cup cup of the present invention;
Fig. 6 is the structure sectional view of implosion guard cup cup and sealing ring and heat-generating disc in embodiment;
Fig. 7 is the structure sectional view that in embodiment, implosion guard cup cup and contractibility or pouring mouth part assemble;
Fig. 8 is the structure sectional view that in another embodiment, implosion guard cup cup and contractibility or pouring mouth part and silica gel ring assemble.
Detailed description of the invention
Below in conjunction with drawings and Examples, the invention will be further described.
Embodiment
See Fig. 1-Fig. 8; a kind of implosion guard cup cup 11; comprise cup upper shed 4, under shed 5, diaphragm 1.9, contractibility or pouring mouth part 3.3, main body body 1.6, be arranged on heat-generating disc 3, sealing ring 2 and base 6 bottom glass cup 11; cup upper shed 4, under shed 5 place arrange round as a ball closing in limit 1.3; heat-generating disc 3 is provided with annular seal ring 2 with under shed 5 junction of glass cup 11, and sealing ring 2 adopts high temperature resistant, aging-resistant elastic silica gel to make.Inside implosion guard cup cup 1 upper shed 4, under shed 5, place is provided with step 1.2; step 1.2 is connected with the outer smooth of main body body 1.6; step 1.2 and the bending part 2.0 of main body body 1.6 and the outer setting diaphragm 1.9 of main body body 1.6; diaphragm 1.9 exceeds glass cup 1 outer wall, and diaphragm 1.9 is by glass cup 1 outer wall and Outer shrink part or pouring mouth part 3.3 clamping position.Outer shrink part or pouring mouth part 3.3 arrange cup upper shed 4, under shed 5 step folding crook 2.0, diaphragm 1.9 on cup shrinks with main body body 1.6 outer wall compact siro spinning technology of fitting to be fixed, diaphragm 1.9 is retracted to cup opening part step folding crook 2.0, becomes arc transition bending laminating to connect to in-flanges; Diaphragm 1.9 extends to step drop face and stops, and diaphragm 1.9 end and cup opening part are kept at a distance and stopped, close up.Diaphragm 1.9 outer wall height on cup and the drop of cup outer wall at least 0.01 millimeter; or; the thickness of diaphragm 1.9 at least 0.01 millimeter, diaphragm 1.9 heat shrinkable is to cup opening part step folding crook 2.0, and diaphragm 1.9 inwall and cup outer wall fit tightly.
Described diaphragm 1.9 outer wall be heated along main body body 1.6 moves and tightens up, and is consistent with the outside of main body body 1.6, diaphragm 1.9 position of closing up is less than the outer wall dimension of main body body 1.6, diaphragm 1.9 is fitted the working strength of position reinforced glass cup main body body 1.6, silica gel sealing ring is installed, not easily cracking is extruded during heat-generating disc, or, diaphragm 1.9 protects inwardly contraction glass main body body 1.6 inwardly can not shrink cushioning effect of having split by external impact point, or, diaphragm 1.9 is protected and is inwardly shunk glass main body body 1.6 and externally can not protrude and tear cup by pressurized by the sidepiece of external impact point, protection main body body 1.6 surrounding uniform stressed, play cushioning effect, or, when diaphragm 1.9 inwardly shrinks cover glass cup main body body 1.6 by external impact, power is let out at other positions of impact uniform conductive main body body 1.6, glass main body body 1.6 externally can not protrude explosion by pressurized.
Glass cup 1 under shed arranges silica gel sealing ring 2, heat-generating disc 3; round as a ball for glass cup 1 bottom closing in limit is wrapped up with heat-generating disc 3 and is connected sealing by silica gel sealing ring 2; or; silica gel sealing ring 2 is arranged on round as a ball closing in limit, glass cup 1 bottom and is connected crush seal with between heat-generating disc 3; described glass cup 1 under shed outer setting bottom or base ring 5.1, the closing in position of diaphragm 1.9 is blocked or is clamped between glass cup 1 outer wall by the upper end of bottom or base ring 5.1 or inside upper part wall.
The upper shed of described glass cup 1 arranges aduncate stage portion 1.2, diaphragm 1.9 extends on the sidewall of aduncate stage portion 1.2, and the closing in position of diaphragm 1.9 is blocked or is clamped between glass cup 1 outer wall by stage portion 1.2 outer setting contractibility or pouring mouth part; Round as a ball closing in limit arranges pouring mouth or round as a ball closing in limit and to be tightly connected pouring mouth part.
The bottom of glass cup 1 is provided with aduncate stage portion 1.1 and is connected the interior flanging 1.2 be arranged on below stage portion 1.1, the under shed 5 of interior flanging 1.2 arranges round as a ball closing in limit 1.3, smooth arc-shaped surface is arranged on round as a ball closing in limit 1.3, and it is downward that under shed 5 can be arranged to round as a ball closing in limit 1.3; Or under shed 5 can be arranged to round as a ball closing in limit 1.3 outward flanging 1.4; Or under shed 5 can be arranged to round as a ball closing in limit 1.3 to in-flanges 1.5, heat-generating disc 3 is assemblied in interior flanging 1.2, and base 5 and heat-generating disc 3 are mounted with also packing and are arranged on the outside of stage portion 1.1.Glass cup 1 is upper and lower opening setting, and wherein the under shed 5 of glass cup 1 is surrounded by the bottom of flanging in it 1.2, and interior flanging 1.2 is in inclination L shape structure; The round as a ball both sides, closing in limit 1.3 of interior flanging 1.2 and sealing ring 2 are fitted and are assembled, or the maximum outside diameter of the maximum outside diameter < heat-generating disc 3 of the internal diameter < sealing ring 2 of glass cup 1 under shed 5.Such design can utilize the principle of elastic-restoring force, and device can be made to combine more firm stable; Top outer and the inner side on the round as a ball closing in limit 1.3 of interior flanging 1.2 are fixed by sealing ring 2 packing; Or fixed by silica gel sealing heat-generating disc 5.2 packing; Or be sealedly connected and fixed by silica gel sealing heat-generating disc 5.2.Wherein the upper shed 4 of glass cup 1 is surrounded by round as a ball closing in limit 1.3, and the upper shed 4 on round as a ball closing in limit 1.3 can arrange pouring mouth 8 and maybe can arrange pouring mouth part, and pouring mouth 8 or pouring mouth part top arrange upper cover and covers.
Glass cup assembly method, comprises the following steps: 1) stretching sealing ring 2, and the heat-generating disc 3 upper and lower side being circular configuration is suppressed and put into sealing ring 2; 2) said modules bent gently, smooth suppressing to be placed in glass cup 1 in flanging 1.2 by round as a ball closing in limit 1.3; 3) at the bottom fit on temperature control connector 7 of heat-generating disc 3; 4) by corresponding to the bottom of base 6 or base ring 5.1 fit outside the stage portion 1.1 of glass cup 1, screw is adopted to be tightened up by base 6 by base 6, base 6 and heat-generating disc 3 are mounted with, or base 6 and silica gel sealing heat-generating disc 5.2 are mounted with, tightening up by screw, heat-generating disc 3 and sealing ring 2 pull downwards and are fastened with interior flanging 1.2 and round as a ball closing in limit 1.3, are close to outside bottom or base ring 5.1 and stage portion 1.1.
By assembling mode above, effectively improve the efficiency of assembling, saving installation time, decreasing assembly process, and prevent from preferably leaking.
Claims (1)
1. the processing method of an implosion guard cup cup is characterized in that, comprises the steps:
1) glass cup adopts technological process for blowing, and diaphragm is inserted in glass cup outside, and diaphragm is tried one's best cup outer wall, by outside for glass main body body all parcels;
2) heated together with diaphragm by glass cup, diaphragm shrinks fits with glass cup outer wall;
3) the diaphragm glass cup heated is placed on table top, the diaphragm on the upper and lower step surface of glass cup is cut down by its rotation cutter;
4) can printed patterns and water gauge scale on diaphragm;
5) bottom is placed on the outside of glass cup step surface from top to bottom, diaphragm is closed up as blocking, prevent diaphragm from closing up and be torn.