- CN104927128A CN104927128A CN201510301994.5A CN201510301994A CN104927128A CN 104927128 A CN104927128 A CN 104927128A CN 201510301994 A CN201510301994 A CN 201510301994A CN 104927128 A CN104927128 A CN 104927128A
- Authority
- CN
- China
- Prior art keywords
- parts
- rubber
- gasoline
- blending method
- proportioning
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C08—ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
- C08L—COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
- C08L9/00—Compositions of homopolymers or copolymers of conjugated diene hydrocarbons
- C08L9/06—Copolymers with styrene
-
- C—CHEMISTRY; METALLURGY
- C08—ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
- C08L—COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
- C08L2205/00—Polymer mixtures characterised by other features
- C08L2205/03—Polymer mixtures characterised by other features containing three or more polymers in a blend
- C08L2205/035—Polymer mixtures characterised by other features containing three or more polymers in a blend containing four or more polymers in a blend
Landscapes
- Chemical & Material Sciences (AREA)
- Health & Medical Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Medicinal Chemistry (AREA)
- Polymers & Plastics (AREA)
- Organic Chemistry (AREA)
- Compositions Of Macromolecular Compounds (AREA)
Abstract
The invention discloses a blending method of retreading rubber. The blending method comprises the following steps: uniformly mixing all raw materials except gasoline according to a proportion to obtain a mixture; putting the mixture into an internal mixer to obtain a rubber compound; uniformly mixing the rubber compound with gasoline according to another proportion to obtain the retreading rubber. Through the adoption of the retreading rubber prepared according to the blending method, the defects such as high abrasion possibility, short service life and poor environmental friendliness of the prior art are overcome, so that the advantages of low abrasion possibility, long service life and high environmental friendliness are realized.
Description
Technical field
The present invention relates to automobile technical field, particularly, relate to a kind of concocting method of tyre rebuilding glue.
Background technology
Tire is one of vitals of automobile, and it directly contacts with road surface, and impact suffered when automotive suspension relaxes running car jointly, ensures that automobile has good driving comfort and ride performance; Ensure that there is good tack on wheel and road surface, improve the traction property of automobile, braking and the property passed through; Subject the weight of automobile, tire on automobile the vital role that rises more and more be subject to people's attention.
At present, market get on the car tire be easy to wearing and tearing, the tire after wearing and tearing can only scrap process, and this not only wastes social resources, also pollutes ecotope.
Realizing in process of the present invention, contriver finds at least to exist in prior art easy to wear, the defect such as work-ing life is short and the feature of environmental protection is poor.
Summary of the invention
The object of the invention is to, for the problems referred to above, propose a kind of concocting method of tyre rebuilding glue, to realize not easy to wear, long service life and the good advantage of the feature of environmental protection.
For achieving the above object, the technical solution used in the present invention is: a kind of concocting method of tyre rebuilding glue, comprising:
(1) by each component of following parts by weight proportioning:
Natural standard rubber: 15 parts;
Petroleum resin: 16 parts;
Smoke sheet rubber: 19 parts;
Styrene-butadiene rubber(SBR): 26 parts;
Adhesionpromoter: 4 parts;
Tackiness agent: 4 parts;
High wear-resistant carbon black: 3.8 parts;
High-dispersity white carbon black: 2.6 parts;
Protective agent: 5.5 parts;
Sulphur: 3.2 parts;
Vulcanizing agent: 2.8 parts;
Ultraaccelerator: 1.2 parts;
Sulfenamide type accelerators: 0.9 part;
Thiazole accelerator: 0.4 part;
Zinc oxide: 1.04 parts;
Stearic acid: 0.85 part;
Gasoline: 42 parts;
(2) each raw material except gasoline is thick by proportioning mixing, put into Banbury mixer and make rubber unvulcanizate, then this rubber unvulcanizate and gasoline are mixed the concocting method making tyre rebuilding glue by proportioning.
The concocting method of the tyre rebuilding glue of various embodiments of the present invention, owing to comprising: each raw material except gasoline is thick by proportioning mixing, puts into Banbury mixer and makes rubber unvulcanizate, then this rubber unvulcanizate and gasoline are mixed the concocting method making tyre rebuilding glue by proportioning; Thus defect easy to wear in prior art, work-ing life is short and the feature of environmental protection is poor can be overcome, to realize not easy to wear, long service life and the good advantage of the feature of environmental protection.
Other features and advantages of the present invention will be set forth in the following description, and, partly become apparent from specification sheets, or understand by implementing the present invention.
Below by embodiment, technical scheme of the present invention is described in further detail.
Embodiment
Below the preferred embodiments of the present invention are described, should be appreciated that preferred embodiment described herein is only for instruction and explanation of the present invention, is not intended to limit the present invention.
According to the embodiment of the present invention, provide a kind of concocting method of tyre rebuilding glue, comprising:
(1) by each component of following parts by weight proportioning:
Natural standard rubber: 15 parts;
Petroleum resin: 16 parts;
Smoke sheet rubber: 19 parts;
Styrene-butadiene rubber(SBR): 26 parts;
Adhesionpromoter: 4 parts;
Tackiness agent: 4 parts;
High wear-resistant carbon black: 3.8 parts;
High-dispersity white carbon black: 2.6 parts;
Protective agent: 5.5 parts;
Sulphur: 3.2 parts;
Vulcanizing agent: 2.8 parts;
Ultraaccelerator: 1.2 parts;
Sulfenamide type accelerators: 0.9 part;
Thiazole accelerator: 0.4 part;
Zinc oxide: 1.04 parts;
Stearic acid: 0.85 part;
Gasoline: 42 parts;
(2) each raw material except gasoline is thick by proportioning mixing, put into Banbury mixer and make rubber unvulcanizate, then this rubber unvulcanizate and gasoline are mixed the concocting method making tyre rebuilding glue by proportioning.
Technical scheme of the present invention, empirical tests, can not destroy the balance of tire, improves Using Life of Tyre; On the other hand, also take full advantage of junked tire, saved social resources, protected ecotope; Further, the tire of renovation in use there will not be old carcass and newly turns over delamination between parts sizing material, bulge and other quality problems, and safety in utilization is better.
Last it is noted that the foregoing is only the preferred embodiments of the present invention, be not limited to the present invention, although with reference to previous embodiment to invention has been detailed description, for a person skilled in the art, it still can be modified to the technical scheme described in foregoing embodiments, or carries out equivalent replacement to wherein portion of techniques feature.Within the spirit and principles in the present invention all, any amendment done, equivalent replacement, improvement etc., all should be included within protection scope of the present invention.
Claims (1)
1. a concocting method for tyre rebuilding glue, is characterized in that, comprising:
(1) by each component of following parts by weight proportioning:
Natural standard rubber: 15 parts;
Petroleum resin: 16 parts;
Smoke sheet rubber: 19 parts;
Styrene-butadiene rubber(SBR): 26 parts;
Adhesionpromoter: 4 parts;
Tackiness agent: 4 parts;
High wear-resistant carbon black: 3.8 parts;
High-dispersity white carbon black: 2.6 parts;
Protective agent: 5.5 parts;
Sulphur: 3.2 parts;
Vulcanizing agent: 2.8 parts;
Ultraaccelerator: 1.2 parts;
Sulfenamide type accelerators: 0.9 part;
Thiazole accelerator: 0.4 part;
Zinc oxide: 1.04 parts;
Stearic acid: 0.85 part;
Gasoline: 42 parts;
(2) each raw material except gasoline is thick by proportioning mixing, put into Banbury mixer and make rubber unvulcanizate, then this rubber unvulcanizate and gasoline are mixed the concocting method making tyre rebuilding glue by proportioning.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201510301994.5A CN104927128A (en) | 2015-06-05 | 2015-06-05 | Blending method of retreading rubber |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201510301994.5A CN104927128A (en) | 2015-06-05 | 2015-06-05 | Blending method of retreading rubber |
Publications (1)
Publication Number | Publication Date |
---|---|
CN104927128A true CN104927128A (en) | 2015-09-23 |
Family
ID=54114567
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201510301994.5A Pending CN104927128A (en) | 2015-06-05 | 2015-06-05 | Blending method of retreading rubber |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN104927128A (en) |
Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US20070112120A1 (en) * | 2000-07-31 | 2007-05-17 | Didier Vasseur | Tread for a tire |
CN101200625A (en) * | 2007-11-01 | 2008-06-18 | 中橡集团曙光橡胶工业研究设计院 | Formula of adhesive agent for aircraft tire renewing |
CN102086353A (en) * | 2009-12-07 | 2011-06-08 | 四川轮胎橡胶(集团)股份有限公司 | Intermediate adhesive material for retreaded tires |
CN103013382A (en) * | 2012-12-24 | 2013-04-03 | 桂林电子科技大学 | Adhesive used for tire retreading via pre-cured treading method |
CN103183846A (en) * | 2013-02-06 | 2013-07-03 | 招远市鹏泰轮胎翻新有限公司 | Slick tire retread rubber for special mine underground carry-scraper |
-
2015
- 2015-06-05 CN CN201510301994.5A patent/CN104927128A/en active Pending
Patent Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US20070112120A1 (en) * | 2000-07-31 | 2007-05-17 | Didier Vasseur | Tread for a tire |
CN101200625A (en) * | 2007-11-01 | 2008-06-18 | 中橡集团曙光橡胶工业研究设计院 | Formula of adhesive agent for aircraft tire renewing |
CN102086353A (en) * | 2009-12-07 | 2011-06-08 | 四川轮胎橡胶(集团)股份有限公司 | Intermediate adhesive material for retreaded tires |
CN103013382A (en) * | 2012-12-24 | 2013-04-03 | 桂林电子科技大学 | Adhesive used for tire retreading via pre-cured treading method |
CN103183846A (en) * | 2013-02-06 | 2013-07-03 | 招远市鹏泰轮胎翻新有限公司 | Slick tire retread rubber for special mine underground carry-scraper |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN102086353B (en) | Intermediate adhesive material for retreaded tires | |
KR101442216B1 (en) | Rubber composition for tire tread and tire manufactured by using the same | |
EP2752447B1 (en) | Pneumatic tire | |
JP2007145898A (en) | Rubber composition for coating carcass cord and tire having carcass using the same | |
CN104262699A (en) | Steel wire protective layer repair adhesive for retreading radial aircraft tire and application of steel wire protective layer repair adhesive | |
CN103131059A (en) | Rubber material and method for manufacturing automobile control arm lining with rubber material | |
CN103980556B (en) | A kind of high abrasion, high strength heavy load automobile tire tyre retreading prevulcanized tire tread rubber | |
JPWO2017061442A1 (en) | Rubber composition and tire | |
JPWO2017061441A1 (en) | Rubber composition for tire tread and tire | |
CN103642083A (en) | Sidewall rubber of environment-friendly and cut-resistance off-the-road tire | |
CN105801942A (en) | Formula of tread rubber of low-rolling-resistance semi-steel radial tire | |
CN104356454A (en) | Tread rubber composition containing 1,2-syndiotatic polybutadiene and preparation method of tread rubber composition | |
CN104927109A (en) | Blending technology of retreading rubber | |
CN104927128A (en) | Blending method of retreading rubber | |
CN106279806A (en) | A kind of rubber composition in endurance all-steel load-bearing radial tire face | |
CN104927108A (en) | Blending technology of retreading rubber | |
CN104927105A (en) | Retreading rubber | |
CN104927130A (en) | Preparation method of retreading rubber | |
CN104927129A (en) | Preparation technology of retreading rubber | |
CN104927104A (en) | Blending method of retreading rubber | |
CN104927131A (en) | Blending method of retreading rubber | |
CN104927103A (en) | Dedicated retreading rubber | |
CN104927102A (en) | Producing method of retreading rubber | |
CN104341640A (en) | Shock absorbing rubber | |
CN104927107A (en) | Formula of retreading rubber |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
RJ01 | Rejection of invention patent application after publication | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20150923 |