CN104895199A - Construction method for guaranteeing thickness quality of coating waterproof layer - Google Patents

Construction method for guaranteeing thickness quality of coating waterproof layer Download PDF

Info

Publication number
CN104895199A
CN104895199A CN201510365224.7A CN201510365224A CN104895199A CN 104895199 A CN104895199 A CN 104895199A CN 201510365224 A CN201510365224 A CN 201510365224A CN 104895199 A CN104895199 A CN 104895199A
Authority
CN
China
Prior art keywords
construction
coating
waterproof layer
primary coat
waterproofing course
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510365224.7A
Other languages
Chinese (zh)
Inventor
王吉福
程文涛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANDONG HUIYUAN BUILDING MATERIALS (GROUP) Co Ltd
Original Assignee
SHANDONG HUIYUAN BUILDING MATERIALS (GROUP) Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANDONG HUIYUAN BUILDING MATERIALS (GROUP) Co Ltd filed Critical SHANDONG HUIYUAN BUILDING MATERIALS (GROUP) Co Ltd
Priority to CN201510365224.7A priority Critical patent/CN104895199A/en
Publication of CN104895199A publication Critical patent/CN104895199A/en
Pending legal-status Critical Current

Abstract

The invention discloses a construction method for guaranteeing thickness quality of a coating waterproof layer. The construction method comprises the following steps: 1) cleaning a base layer: treatment of fine part node; 2) constructing a first waterproof layer by a special coating of primer; 3) constructing a second waterproof layer and constructing by using the special coating of which color is different from the primer of the first waterproof layer; 4) constructing the third waterproof layer by using the special coating of which color is different from the primer of the first waterproof layer and the second waterproof layer; 5) water accumulation test->galling protection layer.

Description

A kind of construction method that can ensure coating waterproof layer thickness qualities
Technical field
The present invention relates to waterproof construction and water-repellent paint applied technical field, construction when particularly controlling and ensure that water-repellent paint does waterproofing course meets technological requirement, reaches thickness qualities requirement.
Background technology
Coating water-proof can form integral seamless confining bed due to it, can trapping water proof completely, can completely cut off extraneous rainwater, moisture, all pernicious gases completely to the infringement of waterproof matrix; Coating water-proof construction technology easily supports and holds, and construction equipment is simple, all can not make waterproofing course overall continuously by placing restrictions on of any complicated shape of basic unit; But water-repellent paint reaches above-mentioned effect, be must by the thickness of the quality of material and waterproofing course as ensureing; Coating waterproof layer in some sense its product is only coating, only after brushing is in basic unit, by generating waterproofing course after the physical and chemical reaction consolidation of coating itself; The completion of water-repellent paint waterproofing course needs multipass brushing, therefore use inferior materials and turn out substandard goods, manufacture in a rough and slipshod way and will to have an opportunity to take advantage of when negligent supervision, the thickness of coating waterproof layer is the key of waterproof effect and durable years, but coating water-proof layer thickness does not resemble directly perceived, all even controllability coiled material, its thickness determines according to coating pass during construction.Reach design thickness and often need multipass brushing.
At present, what generally use in industry is all same color coating, and directly can not supervise, check whether and carried out multipass brushing as requested, therefore, this has also become a difficult problem for coating water-proof layer thickness and quality management &control.
Summary of the invention
Object of the present invention is for providing a kind of construction method that can ensure coating waterproof layer thickness qualities, this intuitively see often all over coating the even situation of brushing and directly can be checked through whether be multipass brushing and which time what can directly recognize brushing is, can make that water-repellent paint thickness is effectively controlled, water-repellent paint construction quality is guaranteed, effect is directly perceived, visible.
For solving the problems of the technologies described above, technical scheme of the present invention is:
A construction method for coating waterproof layer thickness qualities can be ensured, it is characterized in that: comprise the following steps:
1), basic unit is cleared up: detail treatment process;
2), first construction of waterproof layer, use the construction of primary coat special coating;
3), second construction of waterproof layer, use color differ from first waterproofing course primary coat special coating construction;
4), the 3rd road construction of waterproof layer, use color differ from first construction of waterproof layer, second construction of waterproof layer primary coat special coating construction;
5), water-storing test → plucking topping.
It is below the further improvement to technique scheme
In step 1, waterproof matrix requires firm, dry, smooth, no-sundries; Uneven place and crack must be floating by cement mortar.
In step 2, use deployed primary coat special coating, the primary coat special coating that scumbling one deck 0.2 ~ 0.3 ㎜ is thick carries out pretreatment to basic unit.
In step 3, brush second waterproofing course again after slubbing primary coat film is done solid work, the middle painting special coating of the construction usage white of second waterproofing course; By vertical direction coating between every layer.
In step 4, treat that second waterproofing course film is done solid work, brush the 3rd road waterproofing course again after 24 hours, the primary coat special coating of the construction usage grey of the 3rd road waterproofing course.
By coating craft or electric stirring 3-5 minute during construction, be evenly brushed in basic unit with plastics or rubber flap.
The feature that patent water-repellent paint construction shunting multipass brushing of the present invention requires, utilizes the construction method of shunting color separation to realize waterproof construction visualized, effective guarantee coating thickness quality.
Below in conjunction with embodiment and detailed description of the invention, technique scheme is made further improvements.
Detailed description of the invention
Embodiment, a kind of construction method that can ensure coating waterproof layer thickness qualities, comprises the following steps:
1), basic unit is cleared up: detail treatment process;
2), first construction of waterproof layer, use the construction of primary coat special coating;
3), second construction of waterproof layer, use color differ from first waterproofing course primary coat special coating construction;
4), the 3rd road construction of waterproof layer, use color differ from first construction of waterproof layer, second construction of waterproof layer primary coat special coating construction;
5), water-storing test → plucking topping.
In step 1, waterproof matrix requires firm, dry, smooth, no-sundries.Uneven place and crack must be floating by cement mortar;
In step 2, use deployed primary coat special coating (rust), (the primary coat special coating that 0.2 ~ 0.3 ㎜ is thick carries out pretreatment to basic unit to scumbling one deck;
In step 3, brush second waterproofing course again after slubbing primary coat film is done solid work, the middle painting special coating of the construction usage white of second waterproofing course; By vertical direction coating between every layer;
In step 4, treat that second waterproofing course film is done solid work, brush the 3rd road waterproofing course again after general 24 hours, the primary coat special coating of the construction usage grey of the 3rd road waterproofing course.
By coating craft or electric stirring 3-5 minute during construction, be evenly brushed in basic unit with plastics or rubber flap.
First waterproofing course, second waterproofing course and the 3rd road waterproofing course, by vertical direction coating between every layer.
Following content is should be noted that during construction:
1, the coating opening packaging should be finished at 30 minutes, forbade to contact with water before curing of coating;
2, construction temperature higher than 5 DEG C, can should be constructed within basic unit's moisture percentage 5%;
3, waterproofing course is forbidden before not solidifying completely to trample on or operation;
4, No Open Flames in job site.
It is visualized that this patent can realize waterproof construction, effective guarantee coating thickness quality; The completion of existing water-repellent paint waterproofing course needs multipass brushing equally, owing to being all homochromy coating, therefore use inferior materials and turn out substandard goods, manufacture in a rough and slipshod way and will to have an opportunity to take advantage of when negligent supervision, the thickness of coating waterproof layer is the key of waterproof effect and durable years, but owing to being all homochromy coating, coating water-proof layer thickness does not resemble directly perceived, all even controllability coiled material, and its thickness determines according to coating pass during construction.Reach design thickness and often need multipass brushing.
At present, what generally use in industry is all same color coating, and directly can not supervise, check whether and carried out multipass brushing as requested, therefore, this has also become a difficult problem for coating water-proof layer thickness and quality management &control; This patent makes omnidistance directly perceived, the visual effective guarantee coating thickness quality of coating water-proof construction.

Claims (6)

1. can ensure a construction method for coating waterproof layer thickness qualities, it is characterized in that: comprise the following steps:
1), basic unit is cleared up: detail treatment process;
2), first construction of waterproof layer, use the construction of primary coat special coating;
3), second construction of waterproof layer, use color differ from first waterproofing course primary coat special coating construction;
4), the 3rd road construction of waterproof layer, use color differ from first construction of waterproof layer, second construction of waterproof layer primary coat special coating construction;
5), water-storing test → plucking topping.
2. a kind of construction method that can ensure coating waterproof layer thickness qualities as claimed in claim 1, is characterized in that: in step 1, and waterproof matrix requires firm, dry, smooth, no-sundries; Uneven place and crack must be floating by cement mortar.
3. a kind of construction method that can ensure coating waterproof layer thickness qualities as claimed in claim 1, is characterized in that:
In step 2, use deployed primary coat special coating, (the primary coat special coating that 0.2 ~ 0.3 ㎜ is thick carries out pretreatment to basic unit to scumbling one deck.
4. a kind of construction method that can ensure coating waterproof layer thickness qualities as claimed in claim 1, is characterized in that:
In step 3, brush second waterproofing course again after slubbing primary coat film is done solid work, the middle painting special coating of the construction usage white of second waterproofing course; By vertical direction coating between every layer.
5. a kind of construction method that can ensure coating waterproof layer thickness qualities as claimed in claim 1, is characterized in that:
In step 4, treat that second waterproofing course film is done solid work, brush the 3rd road waterproofing course again after 24 hours, the primary coat special coating of the construction usage grey of the 3rd road waterproofing course.
6. a kind of construction method that can ensure coating waterproof layer thickness qualities as claimed in claim 1, is characterized in that:
By coating craft or electric stirring 3-5 minute during construction, be evenly brushed in basic unit with plastics or rubber flap.
CN201510365224.7A 2015-06-29 2015-06-29 Construction method for guaranteeing thickness quality of coating waterproof layer Pending CN104895199A (en)