CN104861896A - 一种环保性木材胶黏剂及其制备方法 - Google Patents

一种环保性木材胶黏剂及其制备方法 Download PDF

Info

Publication number
CN104861896A
CN104861896A CN201410797213.1A CN201410797213A CN104861896A CN 104861896 A CN104861896 A CN 104861896A CN 201410797213 A CN201410797213 A CN 201410797213A CN 104861896 A CN104861896 A CN 104861896A
Authority
CN
China
Prior art keywords
feature
environmental protection
wood adhesives
montmorillonite
protection based
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410797213.1A
Other languages
English (en)
Inventor
不公告发明人
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410797213.1A priority Critical patent/CN104861896A/zh
Publication of CN104861896A publication Critical patent/CN104861896A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种环保性木材胶黏剂及其制备方法。本发明的一种环保性木材胶黏剂,其组分按质量百分数配比为:聚乙烯醇15%~20%、聚乙烯吡咯烷酮5%~8%、丙苯乳液15%~25%、纳米二氧化硅溶胶20%~40%、有机蒙脱土8%~15%、封闭型水性异氰酸酯交联剂2%~10%、烷基酚聚氧乙烯醚1%~3%,所述纳米二氧化硅溶胶中的固体含量占25wt%~30wt%,所述有机蒙脱土为表面经过十八烷基二羟乙基甲基氯化铵活化处理、且粒径在25nm~75nm的钠基蒙脱土。本发明的有益效果是,与现有技术相比,本发明具有粘接力强、耐水性能好、无毒环保等优点,易于推广应用。

Description

一种环保性木材胶黏剂及其制备方法
技术领域
本发明涉及木材加工技术领域,具体地说是一种环保性木材胶黏剂及其制备方法。
背景技术
我国是世界人造板生产第一大国,相应地每年将消耗大量的木材胶黏剂用于木材加工。当前我国木材胶黏剂仍主要是以传统酚醛、脲醛、三聚氰胺甲醛树脂为主,对石化原料依赖程度高,产品价格波动大的问题依然突出。脲醛树脂胶黏剂价格便宜,但游离甲醛等有毒残余量高,不耐水,产品档次较低;酚醛树脂胶黏剂具有有毒残余低、胶合强度高,耐水等优点,产品档次较高,但原料苯酚价格较高,故难于在我国大规模应用。三聚氰胺甲醛树脂胶黏剂也同样存在残余甲醛等物质对环境和人体有害,从而限制了其应用。
发明内容
本发明的目的在于提供一种高效、环保和粘接力强的一种环保性木材胶黏剂及其制备方法。
本发明解决其技术问题所采用的技术方案是:一种环保性木材胶黏剂,其组分按质量百分数配比为:聚乙烯醇15%~20%、聚乙烯吡咯烷酮5%~8%、丙苯乳液15%~25%、纳米二氧化硅溶胶20%~40%、有机蒙脱土8%~15%、封闭型水性异氰酸酯交联剂2%~10%、烷基酚聚氧乙烯醚1%~3%。
所述聚乙烯醇的聚合度为1700~2000、醇解度在88%~98%范围。
所述聚乙烯吡咯烷酮的平均分子量K值为30。
所述丙苯乳液的固体含量占40wt%~50wt%,pH为8~9。
所述纳米二氧化硅溶胶中的固体含量占25wt%~30wt%。
所述有机蒙脱土为表面经过十八烷基二羟乙基甲基氯化铵活化处理、且粒径在25nm~75nm的钠基蒙脱土。
上述的一种环保性木材胶黏剂的制备方法为:按重量配比称取各组分,然后加入搅拌器中,混合20~50min,制成均匀、稳定的混合液,即得本发明的一种环保性木材胶黏剂。
本发明的有益效果是,与现有技术相比,本发明具有粘接力强、耐水性能好、无毒环保等优点,易于推广应用。
具体实施方式
下面结合具体的优选实施例来进一步说明本发明的技术方案。
实施例1:
一种环保性木材胶黏剂,其组分按质量百分数配比为:聚乙烯醇20%、聚乙烯吡咯烷酮8%、丙苯乳液25%、纳米二氧化硅溶胶20%、有机蒙脱土15%、封闭型水性异氰酸酯交联剂10%、烷基酚聚氧乙烯醚2%,所述聚乙烯醇的聚合度为1700~2000、醇解度在88%~98%范围,所述聚乙烯吡咯烷酮的平均分子量K值为30,所述丙苯乳液的固体含量占40wt%~50wt%,pH为8~9,所述纳米二氧化硅溶胶中的固体含量占25wt%~30wt%,所述有机蒙脱土为表面经过十八烷基二羟乙基甲基氯化铵活化处理、且粒径在25nm~75nm的钠基蒙脱土。
制备方法:按重量配比称取各组分,然后加入搅拌器中,混合20~50min,制成均匀、稳定的混合液,即得本发明的一种环保性木材胶黏剂。
实施例2:
一种环保性木材胶黏剂,其组分按质量百分数配比为:聚乙烯醇15%、聚乙烯吡咯烷酮5%、丙苯乳液25%、纳米二氧化硅溶胶40%、有机蒙脱土8%、封闭型水性异氰酸酯交联剂6%、烷基酚聚氧乙烯醚1%,所述聚乙烯醇的聚合度为1700~2000、醇解度在88%~98%范围,所述聚乙烯吡咯烷酮的平均分子量K值为30,所述丙苯乳液的固体含量占40wt%~50wt%,pH为8~9,所述纳米二氧化硅溶胶中的固体含量占25wt%~30wt%,所述有机蒙脱土为表面经过十八烷基二羟乙基甲基氯化铵活化处理、且粒径在25nm~75nm的钠基蒙脱土。
制备方法同实施例1。

Claims (4)

1.一种环保性木材胶黏剂,其特征在于,其组分按质量百分数配比为:聚乙烯醇15%~20%、聚乙烯吡咯烷酮5%~8%、丙苯乳液15%~25%、纳米二氧化硅溶胶20%~40%、有机蒙脱土8%~15%、封闭型水性异氰酸酯交联剂2%~10%、烷基酚聚氧乙烯醚1%~3%。
2.根据权利要求1所述的一种环保性木材胶黏剂,其特征在于,所述纳米二氧化硅溶胶中的固体含量占25wt%~30wt%。
3.根据权利要求1所述的一种环保性木材胶黏剂,其特征在于,所述有机蒙脱土为表面经过十八烷基二羟乙基甲基氯化铵活化处理、且粒径在25nm~75nm的钠基蒙脱土。
4.根据权利要求1所述的一种环保性木材胶黏剂的制备方法,其特征在于,包括以下步骤:按重量配比称取各组分,然后加入搅拌器中,混合20~50min,制成均匀、稳定的混合液,即得本发明的一种环保性木材胶黏剂。
CN201410797213.1A 2014-12-22 2014-12-22 一种环保性木材胶黏剂及其制备方法 Pending CN104861896A (zh)