CN104826782A - Oil paint processing method for redwood furniture - Google Patents
Oil paint processing method for redwood furniture Download PDFInfo
- Publication number
- CN104826782A CN104826782A CN201510191157.1A CN201510191157A CN104826782A CN 104826782 A CN104826782 A CN 104826782A CN 201510191157 A CN201510191157 A CN 201510191157A CN 104826782 A CN104826782 A CN 104826782A
- Authority
- CN
- China
- Prior art keywords
- mahogany furniture
- processing method
- polishing
- husky
- furniture
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to an oil paint processing method for redwood furniture. The oil paint processing method comprises following steps: S1, adopting NO.180 nubuck for carrying out green-pressing operation to the redwood furniture; S2, adopting NO.240 nubuck for troweling oil putty; S3, adopting NO.240 nubuck for firstly polishing the redwood furniture; S4, adopting NO.320 nubuck for secondarily troweling oil putty; S5, selecting one kind of nubuck for secondarily polishing the redwood furniture; S6, plastering the redwood furniture with raw lacquer; S7, waxing the redwood furniture; and S8 performing polishing treatment to the redwood furniture. The oil paint processing method for the redwood furniture has following beneficial effects: with uniformly processed oil paint, fine polishing process, a smooth surface and the gentle color, quality of the overall furniture is enhanced; and the method can save much more oil paint with high efficiency.
Description
Technical field
The present invention relates to field of furniture, be specifically related to a kind of paint processing method of mahogany furniture.
Background technology
At present, mahogany furniture is as a kind of top-grade furniture, and people are also more and more harsher to its quality requirements.Especially, for the paint treatment process in mahogany furniture manufacturing process, whether its outward appearance directly having influence on furniture meets the requirement of people to quality.In prior art, the problem that the process of paint processing method ubiquity paint is even not, technique for grinding is meticulous not of mahogany furniture, Given this, the paint process quality of existing mahogany furniture needs to be further improved.
Summary of the invention
The object of this invention is to provide a kind of paint processing method of mahogany furniture, to solve the problem of prior art.
The present invention solves the technical scheme that above technical problem adopts: a kind of paint processing method of mahogany furniture, is characterized in that, described method comprises the steps:
S1, adopts No. 180 husky skins to carry out breaking green compact to described mahogany furniture;
S2, adopts No. 240 husky skins to criticize putty;
S3, adopts No. 240 husky skins to carry out first time polishing to mahogany furniture;
S4, adopts No. 320 husky skins to carry out second time batch putty;
S5, chooses a kind of to the polishing of mahogany furniture work second time from multiple husky skin;
S6, for raw lacquer broken by described mahogany furniture;
S7, for described mahogany furniture is waxed;
S8, carries out polishing to mahogany furniture.
Preferably, step S5 specifically comprises: according to the glossiness requirement of mahogany furniture, and corresponding one of choosing from No. 320 husky skins, No. 400 husky skins, No. 600 husky skins, No. 800 husky skins, No. 1000 husky skins, No. 1500 husky skins, No. 2000 husky skins carries out second time polishing.
Preferably, at least carry out in step S6 breaking raw lacquer three times, need once to polish after having broken raw lacquer at every turn.
Preferably, the time of described first time polishing is between 10-15 minute.
Preferably, the time of described second time polishing is between 5-10 minute.
Preferably, wool is adopted to carry out polishing in the method.
Compared to prior art, the paint processing method paint process of mahogany furniture of the present invention is even, technique for grinding is meticulous, smooth surface, and color and luster is gentle, many to the quality bonus point of whole furniture, and the method saves paint more, and efficiency is high.
Accompanying drawing explanation
In order to be illustrated more clearly in the embodiment of the present application or technical scheme of the prior art, be briefly described to the accompanying drawing used required in embodiment or description of the prior art below, apparently, the accompanying drawing that the following describes is only some embodiments recorded in the application, for those of ordinary skill in the art, under the prerequisite not paying creative work, other accompanying drawing can also be obtained according to these accompanying drawings.
Fig. 1 is the schematic flow sheet of the paint processing method of mahogany furniture in the embodiment of the present invention.
Detailed description of the invention
For making the object, technical solutions and advantages of the present invention clearly understand, below in conjunction with detailed description of the invention also with reference to accompanying drawing, the present invention is described in more detail.Should be appreciated that, these describe just exemplary, and do not really want to limit the scope of the invention.In addition, in the following description, the description to known features and technology is eliminated, to avoid unnecessarily obscuring concept of the present invention.
With reference to shown in Fig. 1, in the specific embodiment of the invention, a kind of paint processing method of mahogany furniture, is characterized in that, described method comprises the steps:
S1, adopts No. 180 husky skins to carry out breaking green compact to described mahogany furniture;
S2, adopts No. 240 husky skins to criticize putty;
S3, adopts No. 240 husky skins to carry out first time polishing to mahogany furniture;
S4, adopts No. 320 husky skins to carry out second time batch putty;
S5, chooses a kind of to the polishing of mahogany furniture work second time from multiple husky skin;
S6, for raw lacquer broken by described mahogany furniture;
S7, for described mahogany furniture is waxed;
S8, carries out polishing to mahogany furniture.
In order to realize the present invention better, preferably, step S5 specifically comprises: according to the glossiness requirement of mahogany furniture, and corresponding one of choosing from No. 320 husky skins, No. 400 husky skins, No. 600 husky skins, No. 800 husky skins, No. 1000 husky skins, No. 1500 husky skins, No. 2000 husky skins carries out second time polishing.According to the requirement of material, the larger polishing of the model effect out of husky skin is thinner, and for No. 2000 husky skins, the effect out of polishing is smooth and bright like a mirror, has Yu Ze to feel.Preferably, at least carry out in step S6 breaking raw lacquer three times, need once to polish after having broken raw lacquer at every turn.Preferably, the time of described first time polishing is between 10-15 minute.Preferably, the time of described second time polishing is between 5-10 minute.Preferably, adopt wool to carry out polishing in the method, be certainly not limited to wool.
Compared to prior art, the paint processing method paint process of mahogany furniture of the present invention is even, technique for grinding is meticulous, smooth surface, and color and luster is gentle, many to the quality bonus point of whole furniture, and the method saves paint more, and efficiency is high.
It should be noted that, in this article, the such as relational terms of first and second grades and so on is only used for an entity or operation to separate with another entity or operating space, and not necessarily requires or imply the relation that there is any this reality between these entities or operation or sequentially.And, term " comprises ", " comprising " or its any other variant are intended to contain comprising of nonexcludability, thus make to comprise the process of a series of key element, method, article or equipment and not only comprise those key elements, but also comprise other key elements clearly do not listed, or also comprise by the intrinsic key element of this process, method, article or equipment.When not more restrictions, the key element limited by statement " comprising ... ", and be not precluded within process, method, article or the equipment comprising described key element and also there is other identical element.
With above-mentioned according to desirable embodiment of the present invention for enlightenment, by above-mentioned description, relevant staff in the scope not departing from this invention technological thought, can carry out various change and amendment completely.The technical scope of this invention is not limited to the content on description, must determine its technical scope according to right.
Claims (6)
1. a paint processing method for mahogany furniture, is characterized in that, described method comprises the steps:
S1, adopts No. 180 husky skins to carry out breaking green compact to described mahogany furniture;
S2, adopts No. 240 husky skins to criticize putty;
S3, adopts No. 240 husky skins to carry out first time polishing to mahogany furniture;
S4, adopts No. 320 husky skins to carry out second time batch putty;
S5, chooses a kind of to the polishing of mahogany furniture work second time from multiple husky skin;
S6, for raw lacquer broken by described mahogany furniture;
S7, for described mahogany furniture is waxed;
S8, carries out polishing to mahogany furniture.
2. the paint processing method of mahogany furniture according to claim 1, it is characterized in that, step S5 specifically comprises: according to the glossiness requirement of mahogany furniture, and corresponding one of choosing from No. 320 husky skins, No. 400 husky skins, No. 600 husky skins, No. 800 husky skins, No. 1000 husky skins, No. 1500 husky skins, No. 2000 husky skins carries out second time polishing.
3. the paint processing method of mahogany furniture according to claim 2, is characterized in that, at least carries out breaking raw lacquer three times in step S6, needs once to polish after having broken raw lacquer at every turn.
4. the paint processing method of mahogany furniture according to claim 3, is characterized in that, the time of described first time polishing is between 10-15 minute.
5. the paint processing method of mahogany furniture according to claim 4, is characterized in that, the time of described second time polishing is between 5-10 minute.
6. the paint processing method of mahogany furniture according to claim 5, is characterized in that, adopts wool to carry out polishing in the method.