CN104772713B - New dry sanding paper - Google Patents
New dry sanding paper Download PDFInfo
- Publication number
- CN104772713B CN104772713B CN201510137834.1A CN201510137834A CN104772713B CN 104772713 B CN104772713 B CN 104772713B CN 201510137834 A CN201510137834 A CN 201510137834A CN 104772713 B CN104772713 B CN 104772713B
- Authority
- CN
- China
- Prior art keywords
- abrasive material
- material unit
- pad
- dry sanding
- gluing oxidant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
The present invention relates to dry sanding paper technical field, more particularly to new dry sanding paper.By paper substrate, gluing oxidant layer on paper substrate, is connected with, it is characterised in that be connected with abrasive material in the gluing oxidant layer;The abrasive material is made up of the first abrasive material unit that some groups are laterally distributed in gluing oxidant layer, and on the first abrasive material unit, the thickness of abrasive material is from left to right incrementally increased, and leaves space between per group of first abrasive material unit;The thickness for being equipped with abrasive material on the second abrasive material unit, and the second abrasive material unit between the first abrasive material unit in the gluing oxidant layer of gap from left to right progressively reduces;The paper substrate bottom surface is provided with the clamping device for being easy to clamp hand;New dry sanding paper is made to improve dry sanding paper service life.
Description
Technical field
The present invention relates to dry sanding paper technical field, more particularly to new dry sanding paper.
Background technology
It is a kind of to surfaces such as abrasive metal, timber that dry sanding paper is commonly called as rubber, so that its bright and clean smooth material;Frosted
Paper deadlocked various abrasive grits generally on body paper are formed;As dry sanding paper is in bruting process, in more violent friction
In, not only easily violent friction is produced on the surface of frosted grain in bruting process, and can also produce on dry sanding paper larger
Heat, accelerates the abrasion of mill sand grain surface under dual function of the heat with severe friction;To workpiece after frosted grain surface abrasion
The effect of polishing will be substantially reduced, and cause the life-span of dry sanding paper to substantially reduce.
The content of the invention
It is an object of the invention to provide a kind of new dry sanding paper for improving dry sanding paper service life.
Technical scheme is as follows,
New dry sanding paper, including paper substrate, are connected with gluing oxidant layer on paper substrate, it is characterised in that connect in the gluing oxidant layer
It is connected to abrasive material;The abrasive material is made up of the first abrasive material unit that some groups are laterally distributed in gluing oxidant layer, first mill
On material unit, the thickness of abrasive material is from left to right incrementally increased, and leaves space between per group of first abrasive material unit;Described first
Be equipped with the gluing oxidant layer of gap between abrasive material unit the thickness of abrasive material on the second abrasive material unit, and the second abrasive material unit from
It is left-to-right progressively to reduce;The paper substrate bottom surface is provided with the clamping device for being easy to clamp hand.
The gluing oxidant layer includes the primer layer for being coated in paper substrate surface, and the complex layer coated on primer layer.Pass through
Primer layer and complex layer are set, the abrasive material on first, second abrasive material is bonded in gluing oxidant layer.
The clamping device includes two first that are oppositely arranged on paper substrate both sides and installs pad, elastic webbing;The elastic webbing
Both sides are equipped with the second installation pad, and the second installation pad of the elastic webbing both sides is installed pad with first by attachment means and is connected.
Using cooperatively for pad is installed by first, second, in order to elastic webbing is removably attachable in base paper, realizes repeating profit
With;Due to adopting elastic webbing, different size of handss are adapted to.
The attachment means include the box being arranged on the first installation pad, and are arranged on the second installation pad and box
The ZIKOU for using cooperatively.By using cooperatively for box and ZIKOU, in order to elastic webbing is removably attachable in base paper.
The attachment means include the first Magnet being arranged on the first installation pad, and be arranged on the second installation pad with
The second Magnet that first Magnet is used cooperatively;First Magnet is contrary with the second Magnet magnetic.By first, second Magnet
Use cooperatively, to realize being detachably connected for elastic webbing.
The invention has the beneficial effects as follows:When using dry sanding paper, due to abrasive material on the first abrasive material unit thickness from a left side to
The right side incrementally increases, and defines a difference in height, therefore in polishing, grind the chip that comes will some directly from thicker
Abrasive material is made a clean sweep of, without making chip all get lodged in the gap between abrasive material;Further due to abrasive material on the first abrasive material unit
Thickness from left to right incrementally increase, when on the first abrasive material unit thicker one end abrasive material heavy wear so that thickness reduce
When, the abrasive material of the relatively low one end of thickness is still quite sharp, need to only change a direction and be continuing with, considerably increase new frosted
The service life of paper;As between the first abrasive material unit, gap is provided with abrasive material on the second abrasive material unit, and the second abrasive material unit
Thickness from left to right progressively reduce, be conducive to remaining to produce preferably polishing in the thickness lower of the first abrasive material unit abrasive material
Ability;Due to clamping device being arranged in the bottom surface of base paper, handss are fixed on dry sanding paper, are more convenient for using dry sanding paper.
Description of the drawings
By detailed description below in conjunction with the accompanying drawings, the aforesaid and other objects, features and advantages of the present invention will become
Obviously.
Wherein:Fig. 1 is schematic structural view of the invention;
Fig. 2 is surface texture schematic diagram of the present invention;
Fig. 3 is first, second magnet arrangement schematic diagram of the invention;
In accompanying drawing, 1 is paper substrate, and 2 is gluing oxidant layer, and 3 is abrasive material, and 4 is the first abrasive material unit, and 5 is the second abrasive material unit,
6 is primer layer, and 7 is complex layer, and 8 is the first installation pad, and 9 is elastic webbing, and 10 is the second installation pad, and 11 is the first Magnet, and 12 are
Second Magnet, 13 is the cavity with opening.
Specific embodiment
Embodiment 1
Referring to shown in Fig. 1-Fig. 3, new dry sanding paper, including paper substrate 1, gluing oxidant layer 2, the adhesive are connected with paper substrate
Abrasive material 3 is connected with layer;The gluing oxidant layer includes the primer layer for being coated in paper substrate surface, and answering of coating on primer layer
Glue-line;The abrasive material is made up of the first abrasive material unit 4 that some groups are laterally distributed in gluing oxidant layer, the first abrasive material unit
The thickness of upper abrasive material is from left to right incrementally increased, and leaves space between per group of first abrasive material unit;The first abrasive material list
Be equipped with the gluing oxidant layer of gap between unit the thickness of abrasive material on the second abrasive material unit 5, and the second abrasive material unit from a left side to
The right side progressively reduces;The paper substrate bottom surface is provided with the clamping device for being easy to clamp hand;The clamping device includes being oppositely arranged on
Two first of paper substrate both sides install pad 8, elastic webbing 9;The elastic webbing both sides are equipped with the second installation pad 10, the elastic webbing two
Second installation pad of side is installed pad with first by attachment means and is connected;The attachment means include being arranged on the first installation pad
On box, and be arranged on the ZIKOU use cooperatively with box on the second installation pad.When using dry sanding paper, due to the first mill
On material unit, the thickness of abrasive material is from left to right incrementally increased, and is defined a difference in height, therefore in polishing, is ground the chip for coming
Will some directly make a clean sweep of from thicker abrasive material, without making chip all get lodged in the gap between abrasive material;Further
, as the thickness of abrasive material on the first abrasive material unit is from left to right incrementally increased, when the mill of thicker one end on the first abrasive material unit
Material heavy wear need to only be changed a direction and continue to make so that when thickness is reduced, the abrasive material of the relatively low one end of thickness is still quite sharp
With;As between the first abrasive material unit, gap is provided with the thickness of abrasive material on the second abrasive material unit, and the second abrasive material unit
From left to right progressively reduce, be conducive to preferable polishing ability being produced in the thickness lower of the first abrasive material unit abrasive material;Enter one
Step, due to be the second abrasive material unit abrasive thickness between the higher one end of two adjacent the first abrasive material unit abrasive thickness compared with
Low one end, is not main polishing part, there is difference in height, leaves space in height, therefore leaves most sky
Between, the heat in order to generation of polishing is discharged;Due to arranging clamping device in the bottom surface of base paper, handss are fixed on dry sanding paper,
It is more convenient for using dry sanding paper, further says, by using cooperatively for box and ZIKOU, in order to elastic webbing is removably connected
It is connected in base paper, realizes recycling;Due to adopting elastic webbing, different size of handss are adapted to.
Embodiment 2
On the basis of embodiment 1, the attachment means include the first Magnet 11 being arranged on the first installation pad, and
It is arranged on the second Magnet 12 use cooperatively with the first Magnet on the second installation pad;First Magnet and the second Magnet magnetic phase
Instead.By using cooperatively for first, second Magnet, to realize being detachably connected for elastic webbing.
Embodiment 3
On the basis of embodiment 2, first Magnet can be filled in cavity 13 of the first installation pad side with opening.
As the first Magnet is detachably connected on the first installation pad, to avoid waste of resource, the first Magnet is made to realize recycling.
Embodiment 4
On the basis of embodiment 1, the gluing oxidant layer includes the primer layer 6 for being coated in paper substrate surface, and primer layer
The complex layer 7 of upper coating.By arranging primer layer and complex layer, the abrasive material on first, second abrasive material is bonded in gluing
In oxidant layer.
Preferably, the abrasive material on the first, second abrasive material unit adopts carborundum.Due to carborundum hardness and wear-resisting
Property is relatively good, to improve the service life of first, second abrasive material unit.
Preferably, the first, second abrasive material cell surface is coated heat molten type coating.Using heat molten type coating surface
Structure is finer and close, and the blockage resisting, anti-burning effect during use is more preferable;And it is completely solvent-free, nontoxic;Further, by
It is short in heat molten type coating production line, it is not necessary to oven drying, energy-saving, reduces cost.
The above, is only presently preferred embodiments of the present invention, not does any pro forma restriction to the present invention, it is every according to
According to any simple modification, equivalent variations made to above example in technical spirit of the invention, the guarantor of the present invention is each fallen within
Within the scope of shield.
Claims (5)
1. new dry sanding paper, including paper substrate, is connected with gluing oxidant layer on paper substrate, it is characterised in that connect in the gluing oxidant layer
There is abrasive material;The abrasive material is made up of the first abrasive material unit that some groups are laterally distributed in gluing oxidant layer, first abrasive material
On unit, the thickness of abrasive material is from left to right incrementally increased, and leaves space between per group of first abrasive material unit;First mill
The thickness of abrasive material on the second abrasive material unit, and the second abrasive material unit is equipped between material unit in the gluing oxidant layer of gap from a left side
Progressively reduce to the right side;The paper substrate bottom surface is provided with the clamping device for being easy to clamp hand.
2. new dry sanding paper according to claim 1, it is characterised in that the gluing oxidant layer includes being coated in paper substrate surface
Primer layer, and the complex layer coated on primer layer.
3. new dry sanding paper according to claim 1, it is characterised in that the clamping device includes being oppositely arranged on paper substrate
Two first of both sides install pad, elastic webbing;The elastic webbing both sides are equipped with the second installation pad, and the second of the elastic webbing both sides
Pad is installed and installs to pad with first by attachment means and be connected.
4. new dry sanding paper according to claim 3, it is characterised in that the attachment means include being arranged on the first installation
Box on pad, and it is arranged on the ZIKOU use cooperatively with box on the second installation pad.
5. new dry sanding paper according to claim 3, it is characterised in that the attachment means include being arranged on the first installation
The first Magnet on pad, and it is arranged on the second Magnet use cooperatively with the first Magnet on the second installation pad;First magnetic
Ferrum is contrary with the second Magnet magnetic.