CN104672761A - Method for prolonging storage time and service life of petroleum resin product - Google Patents

Method for prolonging storage time and service life of petroleum resin product Download PDF

Info

Publication number
CN104672761A
CN104672761A CN201510057462.1A CN201510057462A CN104672761A CN 104672761 A CN104672761 A CN 104672761A CN 201510057462 A CN201510057462 A CN 201510057462A CN 104672761 A CN104672761 A CN 104672761A
Authority
CN
China
Prior art keywords
petroleum resin
storage time
service life
resin product
storage
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510057462.1A
Other languages
Chinese (zh)
Inventor
程鹏飞
赵洪福
姜远静
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
XINJIANG DUSHANZI TIANLI INDUSTRIAL Co Ltd
Original Assignee
XINJIANG DUSHANZI TIANLI INDUSTRIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by XINJIANG DUSHANZI TIANLI INDUSTRIAL Co Ltd filed Critical XINJIANG DUSHANZI TIANLI INDUSTRIAL Co Ltd
Priority to CN201510057462.1A priority Critical patent/CN104672761A/en
Publication of CN104672761A publication Critical patent/CN104672761A/en
Pending legal-status Critical Current

Abstract

The invention discloses a method for prolonging the storage time and service life of a petroleum resin product. The method comprises the following steps: performing cationic polymerization to obtain polymer liquid by taking pentane as a solvent, aluminum trichloride as a catalyst and monoolefine and 1,3-pentadiene as raw materials; performing alkaline washing and water scrubbing so as to deactivate the catalyst and remove the catalyst and other impurities; performing normal-pressure and reduced-pressure stripping to remove the pentane solvent and oligomer; and adding a liquid antioxidant before granulating and packaging. According to the method for prolonging the storage time and service life of the petroleum resin product disclosed by the invention, the resin product added with the antioxidant is better than the resin products without the antioxidant in terms of storage time and service life.

Description

A kind ofly improve the storage of petroleum resin products and the method in work-ing life
Technical field
The present invention relates to and a kind ofly improve the storage of petroleum resin products and the method in work-ing life.
Background technology
At present, there is the existence of the problems such as storage time short, use procedure oxidation is serious in petroleum resin great majority market produced.
Summary of the invention
The technical problem to be solved in the present invention overcomes existing defect, provides a kind of storage of raising petroleum resin products and the method in work-ing life that effectively can strengthen storage time and work-ing life.
Object of the present invention carrys out specific implementation by the following technical programs:
Improve the storage of petroleum resin products and the method in work-ing life,
1) take pentane as solvent, aluminum chloride is catalyzer, with monoolefine, m-pentadiene for raw material, carries out cationoid polymerisation, obtain polymer fluid;
2) wash through subtracting and wash, make catalyst deactivation, removing catalyzer and other impurity;
3) then pentane solvent and oligopolymer is removed through normal, steam stripping at reduced pressure;
4) liquid antioxidant is added before entering granulation packaging again.
Preferably, in described step 4), the add-on of oxidation inhibitor is the 0.064wt% of raw material total feed.
Preferably, the polyreaction of described step 1), carries out in carbon five tripping device.
Beneficial effect of the present invention:
The storage of raising petroleum resin products provided by the invention and the method in work-ing life, add the rosin products that the rosin products after oxidation inhibitor did not add oxidation inhibitor before the life-span of storage time and use procedure is all better than.
Accompanying drawing explanation
Accompanying drawing is used to provide a further understanding of the present invention, and forms a part for specification sheets, together with embodiments of the present invention for explaining the present invention, is not construed as limiting the invention.In the accompanying drawings:
Fig. 1 is the inventive method schema.
Embodiment
Below in conjunction with accompanying drawing, the preferred embodiments of the present invention are described, should be appreciated that preferred embodiment described herein is only for instruction and explanation of the present invention, is not intended to limit the present invention.
Improve the storage of petroleum resin products and the method in work-ing life, see Fig. 1,
1) take pentane as solvent, aluminum chloride is catalyzer, with monoolefine, m-pentadiene for raw material, carries out cationoid polymerisation, obtain polymer fluid in carbon five tripping device;
2) wash through subtracting and wash, make catalyst deactivation, removing catalyzer and other impurity;
3) then pentane solvent and oligopolymer is removed through normal, steam stripping at reduced pressure;
4) add liquid antioxidant before entering granulation packaging again, the add-on of oxidation inhibitor is the 0.064wt% of raw material total feed.
The foregoing is only the preferred embodiments of the present invention, be not limited to the present invention, although with reference to previous embodiment to invention has been detailed description, for a person skilled in the art, it still can be modified to the technical scheme described in foregoing embodiments, or carries out equivalent replacement to wherein portion of techniques feature.Within the spirit and principles in the present invention all, any amendment done, equivalent replacement, improvement etc., all should be included within protection scope of the present invention.

Claims (3)

1. improve the storage of petroleum resin products and the method in work-ing life, it is characterized in that:
1) take pentane as solvent, aluminum chloride is catalyzer, with monoolefine, m-pentadiene for raw material, carries out cationoid polymerisation, obtain polymer fluid;
2) wash through subtracting and wash, make catalyst deactivation, removing catalyzer and other impurity;
3) then pentane solvent and oligopolymer is removed through normal, steam stripping at reduced pressure;
4) liquid antioxidant is added before entering granulation packaging again.
2. the storage of raising petroleum resin products according to claim 1 and the method in work-ing life, is characterized in that: in described step 4), the add-on of oxidation inhibitor is the 0.064wt% of raw material total feed.
3. the storage of raising petroleum resin products according to claim 1 and 2 and the method in work-ing life, is characterized in that: the polyreaction of described step 1), carries out in carbon five tripping device.
CN201510057462.1A 2015-02-04 2015-02-04 Method for prolonging storage time and service life of petroleum resin product Pending CN104672761A (en)