CN104556733A - Manufacturing method for printing ink on glass screen - Google Patents

Manufacturing method for printing ink on glass screen Download PDF

Info

Publication number
CN104556733A
CN104556733A CN201510048387.2A CN201510048387A CN104556733A CN 104556733 A CN104556733 A CN 104556733A CN 201510048387 A CN201510048387 A CN 201510048387A CN 104556733 A CN104556733 A CN 104556733A
Authority
CN
China
Prior art keywords
glass
printing
screen
ink
glass screen
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510048387.2A
Other languages
Chinese (zh)
Inventor
徐春雪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHANGJIAGANG DELITE NEW MATERIAL Co Ltd
Original Assignee
ZHANGJIAGANG DELITE NEW MATERIAL Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHANGJIAGANG DELITE NEW MATERIAL Co Ltd filed Critical ZHANGJIAGANG DELITE NEW MATERIAL Co Ltd
Priority to CN201510048387.2A priority Critical patent/CN104556733A/en
Publication of CN104556733A publication Critical patent/CN104556733A/en
Pending legal-status Critical Current

Abstract

The invention discloses a manufacturing method for printing ink on a glass screen. The method comprises the following steps: cleaning the surface of glass by using water, and drying to obtain the glass with a clean surface; arranging a silk screen around the glass, and performing silk screen printing on the frame of the glass by adopting leadless ink at 160-200 DEG C for 20-40 minutes; and performing cooling forming on the glass after printing for use. Therefore, according to the manufacturing method for printing the ink on the glass screen, disclosed by the invention, the glass screen obtained by virtue of the method can make up defects of the existing glass screen in use, the whole glass screen looks beautiful and decent, and people are not visually affected during watching; and an operation method is simple, the temperature required by the method is not high, the heating time is short, and the adopted raw materials are environment-friendly and cheap.

Description

The manufacture method of printing-ink on a kind of glass screen
Technical field
The present invention relates to glass manufacturing area, particularly relate to the manufacture method of printing-ink on a kind of glass screen.
Background technology
Glass screen, has another name called transparent screen.As its name suggests, transparency, Penetration ration are exactly its maximum feature.Can be applied to the display screen that indoor have good light transmission, its brightness can accomplish that meeting viewing on daytime uses, and can customize by the demand pel spacing of client.Glass screen has frivolous, that module is thoroughly high feature, also will meet attractive in appearance simultaneously.But existing glass screen use in surrounding tackiness agent stick on electronic component, tackiness agent or glue can visually see, and affect attractive in appearance.
Summary of the invention
The technical problem that the present invention mainly solves is to provide the manufacture method of printing-ink on a kind of glass screen, and the glass screen obtained is elegant in appearance, and result of use is good.
For solving the problems of the technologies described above, the technical scheme that the present invention adopts is: the manufacture method providing printing-ink on a kind of glass screen, and comprising step is:
(1) with water, glass surface is cleaned, dry the glass obtaining surface clean;
(2) carry out silk screen arrangement to the surrounding of described glass, and adopt unleaded ink to carry out silk screen printing to the frame of described glass, temperature is 160-200 DEG C, and the time is 20-40 minute;
(3) use the glass cools be completed for printing is shaping.
In a preferred embodiment of the present invention, described in step (1), drying time is 1-2 hour.
In a preferred embodiment of the present invention, described in step (2), the temperature of silk screen printing is 180 DEG C.
In a preferred embodiment of the present invention, the time of silk screen printing described in step (2) is 30 minutes.
The invention has the beneficial effects as follows: the manufacture method of printing-ink on glass screen of the present invention, the glass screen obtained by the method can make up the deficiency that existing glass screen exists on using, entirety is made to seem elegant in appearance, people are visually unaffected when watching, working method is simple, the temperature needed is not high, and the time of heating is short, and the raw material environmental protection of employing is inexpensive.
Embodiment
Be clearly and completely described to the technical scheme in the embodiment of the present invention below, obviously, described embodiment is only a part of embodiment of the present invention, instead of whole embodiments.Based on the embodiment in the present invention, those of ordinary skill in the art, not making other embodiments all obtained under creative work prerequisite, belong to the scope of protection of the invention.
Embodiment one:
There is provided the manufacture method of printing-ink on a kind of glass screen, comprising step is:
(1) with water, glass surface is cleaned, dry 2 hours, obtain the glass of surface clean;
(2) carry out silk screen arrangement to the surrounding of described glass, and adopt unleaded ink to carry out silk screen printing to the frame of described glass, temperature is 200 DEG C, and the time is 20 minutes;
(3) use the glass cools be completed for printing is shaping.
Embodiment two:
There is provided the manufacture method of printing-ink on a kind of glass screen, comprising step is:
(1) with water, glass surface is cleaned, dry 1 hour, obtain the glass of surface clean;
(2) carry out silk screen arrangement to the surrounding of described glass, and adopt unleaded ink to carry out silk screen printing to the frame of described glass, temperature is 160 DEG C, and the time is 40 minutes;
(3) use the glass cools be completed for printing is shaping.
Embodiment three:
There is provided the manufacture method of printing-ink on a kind of glass screen, comprising step is:
(1) with water, glass surface is cleaned, dry 1.5 hours, obtain the glass of surface clean;
(2) carry out silk screen arrangement to the surrounding of described glass, and adopt unleaded ink to carry out silk screen printing to the frame of described glass, temperature is 180 DEG C, and the time is 30 minutes;
(3) use the glass cools be completed for printing is shaping.
The invention has the beneficial effects as follows:
One, the glass screen obtained by the method can make up the deficiency that existing glass screen exists on using, and make entirety seem elegant in appearance, people are visually unaffected when watching;
Two, the operation of this manufacture method is upper simple, and the temperature of needs is not high, and the time of heating is short, and the raw material environmental protection of employing is inexpensive.
The foregoing is only embodiments of the invention; not thereby the scope of the claims of the present invention is limited; every utilize description of the present invention to do equivalent structure or equivalent flow process conversion; or be directly or indirectly used in other relevant technical field, be all in like manner included in scope of patent protection of the present invention.

Claims (4)

1. the manufacture method of printing-ink on glass screen, it is characterized in that, comprising step is:
(1) with water, glass surface is cleaned, dry the glass obtaining surface clean;
(2) carry out silk screen arrangement to the surrounding of described glass, and adopt unleaded ink to carry out silk screen printing to the frame of described glass, temperature is 160-200 DEG C, and the time is 20-40 minute;
(3) use the glass cools be completed for printing is shaping.
2. the manufacture method of printing-ink on glass screen according to claim 1, it is characterized in that, described in step (1), drying time is 1-2 hour.
3. the manufacture method of printing-ink on glass screen according to claim 1, it is characterized in that, described in step (2), the temperature of silk screen printing is 180 DEG C.
4. the manufacture method of printing-ink on glass screen according to claim 1, it is characterized in that, the time of silk screen printing described in step (2) is 30 minutes.
CN201510048387.2A 2015-01-30 2015-01-30 Manufacturing method for printing ink on glass screen Pending CN104556733A (en)