CN104514180A - Production method of wallpaper backside waterproof coating liquid - Google Patents

Production method of wallpaper backside waterproof coating liquid Download PDF

Info

Publication number
CN104514180A
CN104514180A CN201310446651.9A CN201310446651A CN104514180A CN 104514180 A CN104514180 A CN 104514180A CN 201310446651 A CN201310446651 A CN 201310446651A CN 104514180 A CN104514180 A CN 104514180A
Authority
CN
China
Prior art keywords
wallpaper
parts
production method
coating liquid
water resistant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310446651.9A
Other languages
Chinese (zh)
Inventor
李继升
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Qingdao Shousheng Industrial Co Ltd
Original Assignee
Qingdao Shousheng Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qingdao Shousheng Industrial Co Ltd filed Critical Qingdao Shousheng Industrial Co Ltd
Priority to CN201310446651.9A priority Critical patent/CN104514180A/en
Publication of CN104514180A publication Critical patent/CN104514180A/en
Pending legal-status Critical Current

Abstract

The invention discloses a production method of a wallpaper backside waterproof coating liquid. The coating liquid is composed of the following components in parts by weight: 50 to 60 parts of acrylic acid latex, 30 to 40 parts of grinded calcium carbonate, 1.2 to 1.5 parts of polyacrylic acid viscosity adjusting agent, and 1 to 2 parts of waterproof sizing agent; and is prepared by evenly mixing all the components together. The production method is simple, the formula is reasonable, and the production cost is low, so the production method is suitable for industrial production. The wallpaper coated by the coating liquid has a very good waterproof performance and strength; so that the backside that is adhered on the wall of the wallpaper will not be damaged by mildew due to stuffiness and dampness; moreover, the strength of the wallpaper is high, thus the wallpaper will not be torn and broken when the wallpaper is adhered to the wall by an adhesive, and the service life of wallpaper is guaranteed.

Description

The production method of wallpaper back side water resistant coating fluid
 
Technical field
The invention belongs to wallpaper coating fluid technical field, be specifically related to the production method of a kind of wallpaper back side water resistant coating fluid.
 
Background technology
Now conventional internal wall finishing material, except wallpaper, also has coating, sheet material etc., but by contrast, the advantage that wallpaper has other ornament materials not have: artistry, convenience, easily maintain, functional and economy etc.Wallpaper is as the ornament materials that can beautify the environment, all applicable in a lot of place, such as: domestic paper, commercial space, administrative space, gaming space etc.But wallpaper in use, needs to press close to body of wall, the WATER RESISTANCE of the wallpaper that prior art is produced is more weak, and during stickup, intensity is lower, and the service life of wallpaper is shorter.
 
Summary of the invention
In order to overcome the above-mentioned technical problem that prior art field exists, the object of the invention is to, provide the production method of a kind of wallpaper back side water resistant coating fluid, method is simple, and the page after this coating solution has good gas permeability and anti-scrubbing character.
The production method of the wallpaper back side provided by the invention water resistant coating fluid, comprises the following steps: (1) prepares raw material: the weight portion of raw-material component and each component is: acrylic latex 50-60 parts, grinding calcium carbonate 30-40 parts, polyacrylic acid viscosity modifier 1.2-1.5 parts, water resistant sizing agent 1-2 parts; (2), after being mixed by the whole components described in step (1), water resistant coating fluid is made.
The production method of the wallpaper back side provided by the invention water resistant coating fluid, its beneficial effect is, production method is simple, batching rationally, production cost also lower, be beneficial to industrial production; Page after this coating solution has good WATER RESISTANCE and intensity, thus vexed the wetting of back side generation avoiding metope is gone mouldy, and has stronger intensity, thus when making the wallpaper back side adopt adhesive to paste, can not tear, broken, ensure that the service life of wallpaper.
 
Detailed description of the invention
Below in conjunction with an embodiment, the production method of the wallpaper back side provided by the invention water resistant coating fluid is described in detail.
 
Embodiment
The production method of the wallpaper back side water resistant coating fluid of the present embodiment, comprises the following steps: (1) prepares raw material: the weight portion of raw-material component and each component is: acrylic latex 50 parts, grinding calcium carbonate 35 parts, polyacrylic acid viscosity modifier 1.2 parts, water resistant sizing agent 1.5 parts; (2), after being mixed by the whole components described in step (1), water resistant coating fluid is made.

Claims (1)

1. a production method for wallpaper back side water resistant coating fluid, is characterized in that: comprise the following steps: (1) prepares raw material: the weight portion of raw-material component and each component is: acrylic latex 50-60 parts, grinding calcium carbonate 30-40 parts, polyacrylic acid viscosity modifier 1.2-1.5 parts, water resistant sizing agent 1-2 parts; (2), after being mixed by the whole components described in step (1), water resistant coating fluid is made.
CN201310446651.9A 2013-09-27 2013-09-27 Production method of wallpaper backside waterproof coating liquid Pending CN104514180A (en)