CN104498120A - Smoke-abatement sulfur-fixation environment-friendly coal and preparation method thereof - Google Patents

Smoke-abatement sulfur-fixation environment-friendly coal and preparation method thereof Download PDF

Info

Publication number
CN104498120A
CN104498120A CN201410609460.4A CN201410609460A CN104498120A CN 104498120 A CN104498120 A CN 104498120A CN 201410609460 A CN201410609460 A CN 201410609460A CN 104498120 A CN104498120 A CN 104498120A
Authority
CN
China
Prior art keywords
smoke
coal
sulfur
parts
ferrocene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410609460.4A
Other languages
Chinese (zh)
Inventor
汪承武
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410609460.4A priority Critical patent/CN104498120A/en
Publication of CN104498120A publication Critical patent/CN104498120A/en
Pending legal-status Critical Current

Abstract

The invention discloses smoke-abatement sulfur-fixation environment-friendly coal and a preparation method thereof. The smoke-abatement sulfur-fixation environment-friendly coal comprises the following compositions in parts by weight: 60-80 parts of raw coal, 10-30 parts of ore asphalt, 4-15 parts of quicklime, 0.2-0.7 parts of ferrocene, and 0.3-0.8 parts of an industrial salt. The above smoke-abatement sulfur-fixation environment-friendly coal employs a high-molecular organic compound-ore asphalt as a basic raw material, and employs ferrocene, the industrial salt and ore aslphat for giving play to effect of fixing sulfur in the reaction, so that sulfur dioxide in the fire coal is reacted and generates magnesium sulfide and calcium sulfide which are kept in ash residue, and the discharge capacity of sulfur dioxide when raw coal is combusted is reduced. Ferrocene, quicklime and ore asphalt give play to the smoke abatement effect. The added industrial salt enables the smoke-abatement sulfur-fixation environment-friendly coal to have relatively fast combustion speed and full combustion during combustion, enables black smoke generated in the raw coal combustion process to become green smoke or white smoke, reduces the smoke release time to be less than 2 min, and relatively accords with environment protection idea.

Description

Smoke-eliminating sulfur-fixing environment protection coal and preparation method thereof
Technical field
The present invention relates to energy field, particularly relate to smoke-eliminating sulfur-fixing environment protection coal and preparation method thereof.
Background technology
At present, coal, as a kind of fuel, obtains applying very widely in many fields of society.The use of coal has penetrated into all respects of people's life.
Usually, the state difference that coal exists by it mainly can be divided into four kinds, i.e. raw coal, lump coal, coal dust and moulded coal.Wherein, raw coal refers to and directly obtains in progress of coal mining, primarily of the Mixture Density Networks of lump coal and coal dust composition; Lump coal refers to not containing coal dust, and coal cinder size is all greater than the coal of 6mm; Coal dust refers to that the coal particle size contained all is less than the coal of 3mm; Moulded coal refers to and directly to be added water by coal dust and even or add water after coal dust is mixed appropriate lime or clay evenly, then is pressed into the coal with certain specified shape with model.
But all there is the problem that quantity discharged is large and flue dust is larger of sulfurous gas in above-mentioned coal, environmental pollution is serious when burning.
Summary of the invention
Based on this, be necessary smoke-eliminating sulfur-fixing environment protection coal providing a kind of smoke-eliminating sulfur-fixing effective and preparation method thereof.
A kind of smoke-eliminating sulfur-fixing environment protection coal, by weight, comprises following component:
Raw coal 60-80 part, ore deposit pitch 10-30 part, unslaked lime 4-15 part, ferrocene 0.2-0.7 part, Industrial Salt 0.3-0.8 part.
Adopt ferrocene, unslaked lime and ore deposit pitch, good smoke effect can be played.The weight part controlling ferrocene is 2-3 part, both can realize good smoke effect, and can reduce production cost again.
Wherein in an embodiment, by weight, raw coal 68-72 part, ore deposit pitch 16-26 part, unslaked lime 4-10 part, ferrocene 0.4-0.6 part, Industrial Salt 0.4-0.6 part.
Wherein in an embodiment,
By weight, following component is comprised:
70 parts, raw coal, ore deposit pitch 25 parts, unslaked lime 4 parts, ferrocene 0.5 part, Industrial Salt 0.5 part.
The preparation method of above-mentioned smoke-eliminating sulfur-fixing environment protection coal, comprises the following steps:
Get the raw coal of 60-80 weight part, the mineral bitumen of 10-30 weight part, the unslaked lime of 4-15 weight part, stir, add the ferrocene of 0.2-0.7 weight part and the Industrial Salt of 0.3-0.8 weight part, again stir, obtain smoke-eliminating sulfur-fixing environment protection coal.
Wherein in an embodiment, by weight, raw coal 68-72 part, ore deposit pitch 16-26 part, unslaked lime 4-10 part, ferrocene 0.4-0.6 part, Industrial Salt 0.4-0.6 part.。
Wherein in an embodiment, 70 parts, raw coal, ore deposit pitch 25 parts, unslaked lime 4 parts, ferrocene 0.5 part, Industrial Salt 0.5 part.Above-mentioned smoke-eliminating sulfur-fixing environment protection coal have employed macromolecular organic compound-ore deposit pitch as basic raw material, adopt ferrocene, Industrial Salt and ore deposit pitch can play the effect of solid sulphur in the reaction, make the reaction of the sulfurous gas in fire coal generation magnesium sulfate and calcium sulfate remain in lime-ash, reduce the quantity discharged of sulfurous gas during raw coal combustion.Ferrocene, unslaked lime and ore deposit pitch can play the effect of smoke elimination.Add Industrial Salt, can make smoke-eliminating sulfur-fixing environment protection coal in combustion combustionvelocity accelerate, sufficient combustion, makes the black smoke in raw coal combustion become blue or green cigarette or white cigarette, is shortened to the time of releasing of flue gas and be less than 2 minutes, more meet the theory of environmental protection.
Embodiment
For enabling above-mentioned purpose of the present invention, feature and advantage become apparent more, are described in detail below to the specific embodiment of the present invention.Set forth a lot of detail in the following description so that fully understand the present invention.But the present invention can be much different from alternate manner described here to implement, those skilled in the art can when without prejudice to doing similar improvement when intension of the present invention, therefore the present invention is by the restriction of following public concrete enforcement.
The smoke-eliminating sulfur-fixing environment protection coal of one embodiment, by weight, comprises following component:
Raw coal 60-80 part, ore deposit pitch 10-30 part, unslaked lime 4-15 part, ferrocene 0.2-0.7 part, Industrial Salt 0.3-0.8 part.Wherein, raw coal refers to that the run-of-mine coal (ROM coal) excavated from ground or underground mining removes the coal after spoil, pyrite through screening processing.Ore deposit pitch, also known as rock asphalt, oil is subject to earth's crust extruding and contacts to gradually change with air, water being formed at nature for a long time.Be the natural rock of calcium carbonate by main component, burn at moderate temperatures, after getting rid of the carbonic acid gas decomposited, gained be that main component is unslaked lime with calcium oxide.Industrial Salt refers to crude salt.
The preparation method of above-mentioned smoke-eliminating sulfur-fixing environment protection coal, comprises the following steps:
Get the raw coal of 60-80 weight part, the mineral bitumen of 10-30 weight part, the unslaked lime of 4-15 weight part, stir, add the ferrocene of 0.2-0.7 weight part and the Industrial Salt of 0.3-0.8 weight part, again stir, obtain smoke-eliminating sulfur-fixing environment protection coal.
With specific embodiment, elaboration detailed is further done to smoke-eliminating sulfur-fixing environment protection coal below.
Embodiment 1
A kind of smoke-eliminating sulfur-fixing environment protection coal, comprises following component:
70 kilograms, raw coal, ore deposit pitch 25 kilograms, unslaked lime 4 kilograms, ferrocene 0.5 kilogram, Industrial Salt 0.5 kilogram.
The preparation method of above-mentioned smoke of gunpowder solid sulfur coal is:
Get 70 kilograms, raw coal, mineral bitumen 25 kilograms, unslaked lime 4 kilograms, stirs, and adds ferrocene 0.5 kilogram, and Industrial Salt 0.5 kilogram, stirs again, obtains smoke-eliminating sulfur-fixing environment protection coal.
Embodiment 2
A kind of smoke-eliminating sulfur-fixing environment protection coal, comprises following component:
60 kilograms, raw coal, ore deposit pitch 10 kilograms, unslaked lime 4 kilograms, ferrocene 0.2 kilogram, Industrial Salt 0.3 kilogram.
The preparation method of above-mentioned smoke of gunpowder solid sulfur coal is:
Get 60 kilograms, raw coal, mineral bitumen 10 kilograms, unslaked lime 4 kilograms, stirs, and adds ferrocene 0.2 kilogram, and Industrial Salt 0.3 kilogram, stirs again, obtains smoke-eliminating sulfur-fixing environment protection coal.
Embodiment 3
A kind of smoke-eliminating sulfur-fixing environment protection coal, comprises following component:
80 kilograms, raw coal, ore deposit pitch 30 kilograms, unslaked lime 15 kilograms, ferrocene 0.7 kilogram, Industrial Salt 0.8 kilogram.
The preparation method of above-mentioned smoke of gunpowder solid sulfur coal is:
Get 80 kilograms, raw coal, mineral bitumen 30 kilograms, unslaked lime 10 kilograms, stirs, and adds ferrocene 0.7 kilogram, and Industrial Salt 0.8 kilogram, stirs again, obtains smoke-eliminating sulfur-fixing environment protection coal.
The smoke-eliminating sulfur-fixing environment protection coal of Example 1 1500 grams, carries out fugitive constituent, ash, fixed carbon, combustion card and sulfur to it and measures, and meanwhile, adopt 1500 grams of raw coal as a control group, the data obtained are as shown in table 1:
The smoke-eliminating sulfur-fixing environment protection coal of table 1 embodiment 1 and raw coal measurement result table
Fugitive constituent Ash content Fixed carbon Combustion card Sulfur Sulphur content (mg/m in flue gas 3 The time of releasing of flue gas
Raw coal 26.32 17.89 54.65 6435 6.83 3200 >=10-14 minute
The smoke-eliminating sulfur-fixing environment protection coal of embodiment 1 24.30 21.2 53.5 6310 3.81 1500 ≤ 2 minutes
Can be learnt by table 1, the smoke-eliminating sulfur-fixing environment protection coal of the embodiment 1 of equal in quality is compared with raw coal, and the sulfureous in flue gas content quantity discharged of the smoke-eliminating sulfur-fixing environment protection coal of embodiment 1 reduces 50% than raw coal, time of releasing of flue gas fewer than raw coal 70%.Namely the quantity discharged of sulfurous gas when the smoke of gunpowder solid sulfur coal of embodiment 1 can reduce raw coal combustion, shortens the time of releasing of flue gas, more meets the theory of environmental protection.
Embodiment 2
A kind of smoke of gunpowder solid sulfur coal, comprises following component:
60 kilograms, raw coal, ore deposit pitch 10 kilograms, unslaked lime 5 kilograms, hexamethylenetetramine 1 kilogram, SODIUMNITRATE 1 kilogram, 1 kilogram, Potcrate, ferrocene 2 kilograms, borax 1 kilogram.
Preparation method is with embodiment 1.
Embodiment 3
A kind of smoke-eliminating sulfur-fixing environment protection coal, comprises following component:
80 kilograms, raw coal, ore deposit pitch 30 kilograms, unslaked lime 15 kilograms, hexamethylenetetramine 2 kilograms, SODIUMNITRATE 1 kilogram, 1 kilogram, Potcrate, ferrocene 2 kilograms, borax 1 kilogram.
Preparation method is with embodiment 1.
The above embodiment only have expressed several embodiment of the present invention, and it describes comparatively concrete and detailed, but therefore can not be interpreted as the restriction to the scope of the claims of the present invention.It should be pointed out that for the person of ordinary skill of the art, without departing from the inventive concept of the premise, can also make some distortion and improvement, these all belong to protection scope of the present invention.Therefore, the protection domain of patent of the present invention should be as the criterion with claims.

Claims (6)

1. a smoke-eliminating sulfur-fixing environment protection coal, is characterized in that, by weight, comprises following component:
Raw coal 60-80 part, ore deposit pitch 10-30 part, unslaked lime 4-15 part, ferrocene 0.2-0.7 part, Industrial Salt 0.3-0.8 part.
2. smoke-eliminating sulfur-fixing environment protection coal according to claim 1, is characterized in that, by weight, and raw coal 68-72 part, ore deposit pitch 16-26 part, unslaked lime 4-10 part, ferrocene 0.4-0.6 part, Industrial Salt 0.4-0.6 part.
3. smoke-eliminating sulfur-fixing environment protection coal according to claim 1, is characterized in that, by weight, comprises following component:
70 parts, raw coal, ore deposit pitch 25 parts, unslaked lime 4 parts, ferrocene 0.5 part, Industrial Salt 0.5 part.
4. a preparation method for smoke-eliminating sulfur-fixing environment protection coal, is characterized in that, comprises the following steps:
Get the raw coal of 60-80 weight part, the mineral bitumen of 10-30 weight part, the unslaked lime of 4-15 weight part, stir, add the ferrocene of 0.2-0.7 weight part and the Industrial Salt of 0.3-0.8 weight part, again stir, obtain smoke-eliminating sulfur-fixing environment protection coal.
5. the preparation method of smoke-eliminating sulfur-fixing environment protection coal according to claim 4, is characterized in that, by weight, and raw coal 68-72 part, ore deposit pitch 16-26 part, unslaked lime 4-10 part, ferrocene 0.4-0.6 part, Industrial Salt 0.4-0.6 part.
6. the preparation method of smoke-eliminating sulfur-fixing environment protection coal according to claim 4, is characterized in that, 70 parts, raw coal, ore deposit pitch 25 parts, unslaked lime 4 parts, ferrocene 0.5 part, Industrial Salt 0.5 part.
CN201410609460.4A 2014-11-04 2014-11-04 Smoke-abatement sulfur-fixation environment-friendly coal and preparation method thereof Pending CN104498120A (en)