CN104476083A - Constraint fixture for radiator core welding - Google Patents

Constraint fixture for radiator core welding Download PDF

Info

Publication number
CN104476083A
CN104476083A CN201410762426.0A CN201410762426A CN104476083A CN 104476083 A CN104476083 A CN 104476083A CN 201410762426 A CN201410762426 A CN 201410762426A CN 104476083 A CN104476083 A CN 104476083A
Authority
CN
China
Prior art keywords
cross bar
left end
slide block
weldering
radiator
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410762426.0A
Other languages
Chinese (zh)
Other versions
CN104476083B (en
Inventor
黄建川
余献彬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Chongqing Tokyo Radiator Co Ltd
Original Assignee
Chongqing Tokyo Radiator Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Chongqing Tokyo Radiator Co Ltd filed Critical Chongqing Tokyo Radiator Co Ltd
Priority to CN201410762426.0A priority Critical patent/CN104476083B/en
Publication of CN104476083A publication Critical patent/CN104476083A/en
Application granted granted Critical
Publication of CN104476083B publication Critical patent/CN104476083B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention provides a constraint fixture for radiator core welding. The constraint fixture comprises a body, a left clamping part and a right clamping part, wherein the left clamping part is arranged at the left end of the body; the right clamping part is arranged at the right end of the body; the body comprises a first transverse rod and a second transverse rod; the length of the first transverse rod is equal to that of the second transverse rod; the left clamping part connects the left end of the first transverse rod with the left end of the second transverse rod; the right clamping part connects the right end of the first transverse rod with the right end of the second transverse rod; a trapezoidal groove is formed in each of two ends of the first transverse rod and each of two ends of the second transverse rod; the distance between each trapezoidal groove and the corresponding end is 17.3mm, and the width of each trapezoidal groove is 5.2mm; sixty-six circular-arc-shaped grooves are uniformly formed in the middle parts of the first transverse rod and the second transverse rod and are formed between the trapezoidal grooves in the two ends; the spacing between every two adjacent circular-arc-shaped grooves is 8.2mm, and the diameter of each circular-arc-shaped groove is 3.5mm. The constraint fixture has the beneficial effects that a radiator core can be clamped by using the constraint fixture, and certain distance between the constraint fixture and a radiating pipe can be kept after the clamping by the constraint fixture.

Description

A kind of contained tool drying weldering for radiator centre
Technical field
The present invention relates to a kind of radiator centre and dry complementary equipment required when welding, particularly relate to the one adopted when a kind of 16 width radiator centres dry weldering and restrain tool.
Background technology
The contained tool drying weldering for radiator centre assembles and be used in baking weldering process clamping radiator centre, make it to be ensured by tool relative to the positional precision of fuse kludge, thus ensure that the radiator centre drying postwelding is not by the impact of workman's technical merit, makes the machining accuracy of product reach unanimity.This contained tool being used for radiator centre is mainly used in assembling in radiator centre manufacture process, dries welder's sequence.For the design of the contained tool of radiator centre for the purpose of ensureing that involved procedure requires, ensure emphatically assembling product size and dry weldering quality; Package size mainly refers to the spacing dimension of radiator centre two backplate, and all the other such as main leaf spacing dimensions are then ensured by kludge; Dry weldering quality and mainly refer to that, except baking soldering equipment relative parameters setting, restrain tool dries weldering quality impact on product, it mainly ensures with product quality and appearance and size.
In prior art, although the requirement on machining accuracy of product can be ensured at the assembling procedure of product, but in follow-up baking welder sequence, because contained tool is not usually adjusted to the right place (keeping certain spacing with radiating tube) by workman, under high temperature, (625 DEG C) dry weldering and cause contained tool to contact with radiating tube to cause the perforation of radiating tube or heat-radiation belt corrode to produce bad scrapping.
Summary of the invention
The shortcoming of prior art in view of the above, the object of the present invention is to provide a kind of contained tool drying weldering for radiator, prevent and produce the bad phenomenon such as adhesion ablation, perforation because of contained tool and radiating tube spacing deficiency in baking weldering process, improve and dry weldering quality.
For achieving the above object and other relevant objects, the invention provides a kind of contained tool drying weldering for radiator centre, comprise body, be arranged at the left clamping section of body left end and be arranged at the right clamping section of body right-hand member, described body comprises the first cross bar and second cross bar isometric with the first cross bar, the left end of the left end of the first cross bar and the second cross bar is flushed connection by left clamping section, the right-hand member of the right-hand member of the first cross bar and the second cross bar is flushed connection by right clamping section, first cross bar and the second cross bar are rectangular structure, the two ends of the first cross bar and the second cross bar two ends are provided with trapezoidal groove and each trapezoidal groove is 17.3mm to the distance of each end, the width of trapezoidal groove is 5.2mm, 66 circular grooves are evenly provided with and circular groove is arranged at the centre of the trapezoidal groove at two ends at the middle part of the first cross bar and the second cross bar, spacing between two adjacent circular grooves is 8.2mm, the diameter of circular groove is 3.5mm.Because radiator centre is when keeping flat, the surface of radiating tube usually outstanding radiator centre, therefore when with restraining the tool clamping radiator core period of the day from 11 p.m. to 1 a.m, the first cross bar and the second cross bar can with radiating tube adhesion, thus radiating tube burnt, bore a hole; When in order to do not allow the first cross bar and the second cross bar and the adhesion of radiating tube portion time, contained tool can be made again inadequate to the clamping force of radiator centre, the relative position of radiating tube and heat-radiation belt is offset in baking weldering process.Each trapezoidal groove is 17.3mm to the distance of each end, and this distance matches with the distance of the radiating tube at the edge of 16 width radiator centres to the edge of backplate; The width of trapezoidal groove is 5.2mm, the width of the radiating tube at the edge of this width and 16 width radiator centres matches, after contained tool so just can be made to clamp radiator centre, just the radiating tube at the edge of 16 width radiator centres can be contained in trapezoidal groove.The number of circular groove is 66, and the number of the radiating tube of the centre of this number and 16 width radiator centres matches; Spacing between two adjacent circular grooves is 8.2mm, this spacing be and 16 width radiator centres centre radiating tube between distance match; The width of circular groove is 3.5mm, the width of the radiating tube of the centre of this width and 16 width radiator centres matches, after contained tool so just can be made to clamp radiator centre, just the radiating tube of the centre of 16 width radiator centres can be contained in circular groove.Prevent and produce the bad phenomenon such as adhesion ablation, perforation because of contained tool and radiating tube spacing deficiency in baking weldering process, improve and dry weldering quality.
Further, described body comprises the first cross bar, second cross bar, first nut and the first screw rod, first cross bar left end and the second cross bar left end are provided with hollow structure, the inner side of the first cross bar left end and the inner side of the second cross bar left end is corresponding with hollow structure is provided with chute, the first slide block is provided with in the hollow structure of the first cross bar, the second slide block is provided with in the hollow structure of the second cross bar, second slide block is circular ring structure and the second slide block is provided with internal thread, left clamping section, the side of the first location division of left end and the second location division of left end is fixedly connected with the first slide block, left clamping section, the opposite side of the first location division of left end and the second location division of left end is fixedly connected with the second slide block, be threaded with the second slide block in the hollow structure that first screw rod is arranged on the second cross bar, first nut is arranged on outside the left end of the second cross bar, one end of first screw rod is connected with nut, the other end and second cross bar of the first screw rod are rotationally connected.Rotate the first nut, make the first bolt rotary, first screw rod makes the second slide block move, first location division of left clamping section, left end and the second location division of left end are moved along with the movement of the second slide block, this clamped width size of drying the contained tool of weldering for radiator centre can be made to regulate as required, thus be applicable to the size of multiple radiator centre.
Further, described body also comprises the second nut and the second screw rod, the arranged outside of the first cross bar left end has chute, and one end of the second screw rod is connected with the second nut outside the first cross bar, and the other end of the second cross bar is threaded with the first slide block by the chute outside the first cross bar.Due to after clamping part, only have left clamping section, the first location division of left end and the second location division of left end and the second slide block junction stressed, first slide block is free end, and the junction of the first location division of left clamping section, left end and the second location division of left end and the second slide block easily occurs stressed excessive and rupture.By arranging the second nut and the second screw rod, first slide block can be released when mobile, first slide position also can be fixed by the second nut and the second screw rod after determining, make junction stressed retarded of clamping part rear left clamping section, the first location division of left end and the second location division of left end and the second slide block, increase the service life.
Further, described contained tool 0Cr18Ni9 material making of drying weldering for radiator centre.Select this material to make, make the contained tool drying weldering for radiator centre have good corrosion resistance, heat resistance, low temperature intensity and mechanical performance, the hot-workabilities such as bending ram are good, without heat treatment hardening phenomenon, nonmagnetic.
Further, the described superficial layer of contained tool drying weldering for radiator centre is sprayed molybdenum layer, and hardness can reach 850-1050HV0.1, and coefficient of friction is low, and tensile property is good, anti-molten, wear resistance is good.
As mentioned above, a kind of contained tool drying weldering for radiator centre of the present invention, there is following beneficial effect: by the setting of trapezoidal groove and circular groove, both achieved and with contained tool, radiator centre had been clamped, achieve again contained tool clamping after and radiating tube maintain a certain distance, prevent the problems such as radiating tube generation in baking weldering process is burnt, perforation, improve and dry weldering quality.
Accompanying drawing explanation
Fig. 1 is shown as the front view drying the contained tool of weldering for radiator centre of the embodiment of the present invention.
Fig. 2 is shown as the top view drying the contained tool of weldering for radiator centre of the embodiment of the present invention.
Fig. 3 is shown as the left view drying the contained tool of weldering for radiator centre of the embodiment of the present invention.
Fig. 4 is shown as the rearview drying the contained tool of weldering for radiator centre of the embodiment of the present invention.
Fig. 5 is shown as the enlarged drawing at A place in Fig. 1.
Fig. 6 is shown as the enlarged drawing at B place in Fig. 1.
Reference numeral is expressed as follows:
1 body,
2 left clamping sections,
3 right clamping sections,
10 trapezoidal grooves,
11 circular grooves,
12 first cross bars,
13 second cross bars,
14 first nuts,
16 second nuts.
Detailed description of the invention
Below by way of specific instantiation, embodiments of the present invention are described, those skilled in the art the content disclosed by this description can understand other advantages of the present invention and effect easily.The present invention can also be implemented or be applied by detailed description of the invention different in addition, and the every details in this description also can based on different viewpoints and application, carries out various modification or change not deviating under spirit of the present invention.
Shown in Figure 1, the invention provides a kind of contained tool drying weldering for radiator centre, comprise body 1, be arranged at the left clamping section 2 of body 1 left end and be arranged at the right clamping section 3 of body 1 right-hand member.
In the present embodiment, please continue see shown in Fig. 1 to Fig. 6, described body 1 comprises the first cross bar 12, second cross bar 13, first nut 14 and the first screw rod.The left end of the left end of the first cross bar 12 and the second cross bar 13 is flushed connection by left clamping section 2, the right-hand member of the right-hand member of the first cross bar 12 and the second cross bar 13 is flushed connection by right clamping section 3, first cross bar 12 and the second cross bar 13 are rectangular structure, the two ends of the first cross bar 12 and the second cross bar 13 two ends are provided with trapezoidal groove 10 and each trapezoidal groove 10 is 17.3mm to the distance of each end, the width of trapezoidal groove 10 is 5.2mm, 66 circular grooves 11 are evenly provided with and circular groove 11 is arranged at the centre of the trapezoidal groove 10 at two ends at the middle part of the first cross bar 12 and the second cross bar 13, spacing between two adjacent circular grooves 11 is 8.2mm, the diameter of circular groove 11 is 3.5mm.
First cross bar 12 left end and the second cross bar 13 left end are provided with hollow structure, the inner side of the first cross bar 12 left end and the inner side of the second cross bar 13 left end is corresponding with hollow structure is provided with chute, the first slide block is provided with in the hollow structure of the first cross bar 12, the second slide block is provided with in the hollow structure of the second cross bar 13, second slide block is circular ring structure and the second slide block is provided with internal thread, the side of left clamping section 2 is fixedly connected with the first slide block, the opposite side of left clamping section 2 is fixedly connected with the second slide block, be threaded with the second slide block in the hollow structure that first screw rod is arranged on the second cross bar 13, first nut 14 is arranged on outside the left end of the second cross bar 13, one end of first screw rod is connected with nut, the other end and second cross bar 13 of the first screw rod are rotationally connected.Rotate the first nut, make the first bolt rotary, first screw rod makes the second slide block move, first location division 4 of left clamping section 2, left end and the second location division 5 of left end are moved along with the movement of the second slide block, this clamped width size of drying the contained tool of weldering for radiator centre can be made to regulate as required, thus be applicable to the size of multiple radiator centre.
Shown in Fig. 4, described body 1 also comprises the second nut 16 and the second screw rod, the arranged outside of the first cross bar 12 left end has chute, one end of second screw rod is connected with the second nut 16 outside the first cross bar 12, and the other end of the second cross bar 13 is threaded with the first slide block by the chute outside the first cross bar 12.Due to after clamping part, only have left clamping section 2, the first location division 4 of left end and the second location division 5 of left end and the second slide block junction stressed, first slide block is free end, and the junction of the first location division 4 of left clamping section 2, left end and the second location division 5 of left end and the second slide block easily occurs stressed excessive and rupture.By arranging the second nut 16 and the second screw rod, first slide block can be released when mobile, first slide position also can be fixed by the second nut 16 and the second screw rod after determining, make junction stressed retarded of clamping part rear left clamping section 2, the first location division 4 of left end and the second location division 5 of left end and the second slide block, increase the service life.
This is used for the contained tool 0Cr18Ni9 material making that radiator centre dries weldering.Select this material to make, make the contained tool drying weldering for radiator centre have good corrosion resistance, heat resistance, low temperature intensity and mechanical performance, the hot-workabilities such as bending ram are good, without heat treatment hardening phenomenon, nonmagnetic.
This superficial layer being used for the contained tool of radiator centre baking weldering is sprayed molybdenum layer.Superficial layer is sprayed molybdenum layer, and hardness can reach 850-1050HV0.1, and coefficient of friction is low, and tensile property is good, and anti-scuff wear ability is good.
Operation principle of the present invention: because radiator centre is when keeping flat, the surface of radiator centre usually given prominence to by radiating tube, therefore when with restraining the tool clamping radiator core period of the day from 11 p.m. to 1 a.m, the first cross bar 12 and the second cross bar 13 can and radiating tube adhesion, thus radiating tube burnt, bore a hole; When in order to not allow the first cross bar 12 and the second cross bar 13 with the adhesion of radiating tube portion, contained tool can be made again inadequate to the clamping force of radiator centre, the relative position of radiating tube and heat-radiation belt is offset in baking weldering process.Each trapezoidal groove 10 is 17.3mm to the distance of each end, and this distance matches with the distance of the radiating tube at the edge of 16 width radiator centres to the edge of backplate; The width of trapezoidal groove 10 is 5.2mm, the width of the radiating tube at the edge of this width and 16 width radiator centres matches, after contained tool so just can be made to clamp radiator centre, just the radiating tube at the edge of 16 width radiator centres can be contained in trapezoidal groove 10.The number of circular groove 11 is 66, and the number of the radiating tube of the centre of this number and 16 width radiator centres matches; Spacing between two adjacent circular grooves 11 is 8.2mm, this spacing be and 16 width radiator centres centre radiating tube between distance match; The width of circular groove 11 is 3.5mm, the width of the radiating tube of the centre of this width and 16 width radiator centres matches, after contained tool so just can be made to clamp radiator centre, just the radiating tube of the centre of 16 width radiator centres can be contained in circular groove 11.Prevent and produce the bad phenomenon such as adhesion ablation, perforation because of contained tool and radiating tube spacing deficiency in baking weldering process, improve and dry weldering quality.
Above-described embodiment is illustrative principle of the present invention and effect thereof only, but not for limiting the present invention.Any person skilled in the art scholar all without prejudice under spirit of the present invention and category, can modify above-described embodiment or changes.Therefore, such as have in art usually know the knowledgeable do not depart from complete under disclosed spirit and technological thought all equivalence modify or change, must be contained by claim of the present invention.

Claims (5)

1. one kind is dried the contained tool of weldering for radiator centre, comprise body (1), be arranged at the left clamping section (2) of body (1) left end and be arranged at the right clamping section (3) of body (1) right-hand member, it is characterized in that, described body (1) comprises the first cross bar (12) and second cross bar (13) isometric with the first cross bar (12), the left end of the left end of the first cross bar (12) and the second cross bar (13) is flushed connection by left clamping section (2), the right-hand member of the right-hand member of the first cross bar (12) and the second cross bar (13) is flushed connection by right clamping section (3), first cross bar (12) and the second cross bar (13) are rectangular structure, the two ends of the first cross bar (12) and the second cross bar (13) two ends are provided with trapezoidal groove (10) and each trapezoidal groove (10) is 17.3mm to the distance of each end, the width of trapezoidal groove (10) is 5.2mm, 66 circular grooves (11) are evenly provided with and circular groove (11) is arranged at the centre of the trapezoidal groove (10) at two ends at the middle part of the first cross bar (12) and the second cross bar (13), spacing between two adjacent circular grooves (11) is 8.2mm, the diameter of circular groove (11) is 3.5mm.
2. the contained tool drying weldering for radiator centre according to claim 1, it is characterized in that, described body (1) comprises the first nut (14) and the first screw rod, first cross bar (12) left end and the second cross bar (13) left end are provided with hollow structure, the inner side of the first cross bar (12) left end and the inner side of the second cross bar (13) left end is corresponding with hollow structure is provided with chute, the first slide block is provided with in the hollow structure of the first cross bar (12), the second slide block is provided with in the hollow structure of the second cross bar (13), second slide block is circular ring structure and the second slide block is provided with internal thread, the side of left clamping section (2) is fixedly connected with the first slide block, the opposite side of left clamping section (2) is fixedly connected with the second slide block, be threaded with the second slide block in the hollow structure that first screw rod is arranged on the second cross bar (13), first nut (14) is arranged on outside the left end of the second cross bar (13), one end of first screw rod is connected with nut, the other end and second cross bar (13) of the first screw rod are rotationally connected.
3. the contained tool drying weldering for radiator centre according to claim 2, it is characterized in that, described body (1) also comprises the second nut (16) and the second screw rod, the arranged outside of the first cross bar (12) left end has chute, one end of second screw rod is connected with the first cross bar (12) the second nut (16) outward, and the other end of the second cross bar (13) is threaded with the first slide block by the chute in the first cross bar (12) outside.
4. the contained tool drying weldering for radiator centre according to claim 1, is characterized in that, described contained tool 0Cr18Ni9 material making of drying weldering for radiator centre.
5. the contained tool drying weldering for radiator centre according to claim 1, is characterized in that, the described superficial layer drying the contained tool of weldering for radiator centre is sprayed molybdenum layer.
CN201410762426.0A 2014-12-11 2014-12-11 A kind of contained tool that dries weldering for radiator centre Active CN104476083B (en)