CN104290482A - Quick lustering process - Google Patents

Quick lustering process Download PDF

Info

Publication number
CN104290482A
CN104290482A CN201410495752.XA CN201410495752A CN104290482A CN 104290482 A CN104290482 A CN 104290482A CN 201410495752 A CN201410495752 A CN 201410495752A CN 104290482 A CN104290482 A CN 104290482A
Authority
CN
China
Prior art keywords
carrier
polishing technique
quick
quick polishing
technique according
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410495752.XA
Other languages
Chinese (zh)
Inventor
付云
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI ZHONGCAI PRINTING Co Ltd
Original Assignee
ANHUI ZHONGCAI PRINTING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI ZHONGCAI PRINTING Co Ltd filed Critical ANHUI ZHONGCAI PRINTING Co Ltd
Priority to CN201410495752.XA priority Critical patent/CN104290482A/en
Publication of CN104290482A publication Critical patent/CN104290482A/en
Pending legal-status Critical Current

Abstract

The invention discloses a quick lustering process and relates to the field of printing. The quick lustering process is characterized by comprising the first step of removing impurities of carriers, the second step of coating the carriers obtained in the first step with oil polish, the third step of drying the carriers obtained in the second step, the fourth step of cooling the carriers obtained in the third step, and the fifth step of collecting and packing the carriers obtained in the fourth step. The quick lustering process has the advantages that the impurities on the surfaces of the carriers are cleaned up, it is clear that the impurities on the surfaces of the carriers can not produce scratches, the probability that the backs of the carriers are sticky is low, the glossiness is good, and the abrasion resistance is high.

Description

A kind of quick polishing technique
Technical field
The present invention relates to print field, be specifically related to a kind of quick polishing technique.
Background technology
On be only coated with last layer water white coating at printed matter surface, form a kind of thin and even transparent optical bright layers at printed matter surface after solidification, play the technique of finish machining functions strengthening carrier surface smoothness, protection printing figure message, be called as glazing process.On only in order to beautify printed matter, protection printed matter, strengthen printed matter the effect of publicity and improve the practical value of printed matter.Printed matter surface after glazing seems more smooth, and make incident light produce non-uniform reflection, ink layer is brighter.On only adopt oil polish to carry out surperficial coating waste water to printed matter.Before finally processing printed document after printing, the surface of adequate measures to paper or cardboard printed document is taked to carry out protectiveness process.Printed matter after glazing at the bright film of face cap last layer.
Glazing not only can strengthen surface-brightening, protection printing figure message, and does not affect the recycling of paper.Therefore, the Surface Machining of the printings such as packing carton, books, picture album, pictorial poster is widely used in.But glazing process easily goes wrong in batch production process at present, as: carrier surface has the impurity do not removed, and carrier surface cleaning produces scratch, produces sticky back of the body phenomenon, the problems such as glossiness is high not in carrier the other side process.Market needs a kind ofly utilize batch production and effectively can improve the glazing process of carrier polishing effect.
Summary of the invention
The object of the invention is the defect for above-mentioned prior art, provide a kind of quick polishing technique, there is upper ray velocity fast, effective advantage.
Object of the present invention can be achieved through the following technical solutions:
A kind of quick polishing technique, comprises the following steps:
1) impurity of carrier is removed;
2) to step 1) carrier coating oil polish;
3) to step 2) carrier dry;
4) to step 3) carrier cool;
5) by step 4) carrier carry out receipts dress.
Preferably, step 1) described removing carrier surface impurity for point absorbing a carrier surface impurity by taking out, scratch can not be caused to carrier surface while absorbing carrier surface impurity, guarantee carrier polishing effect.
Preferably, described oil polish is water lustering oil, and described water lustering oil comprises barras, animi resin and alkali soluble resin, and the formula rate of three kinds of resins is 1:1:1, and cost is low, nonpoisonous and tasteless, glossiness is high and wearability is strong.
Preferably, described coating process is roller coat, contributes to oil polish and is uniformly coated on carrier, and easily realizes producing in enormous quantities.
Preferably, step 3) described oven dry is by infrared baking, effectively accelerate the drying being coated with oil polish carrier, bake out temperature is 80 ~ 100 DEG C.
Preferably, step 4) described in be cooled to and dispelled the heat by electric fan, not only can effectively realize accelerating dry after the cooling of carrier, can also step 3 be realized) to fail dry carrier dry further.
Beneficial effect of the present invention: the present invention has carrier surface impurity and cleans out, knows that carrier surface impurity can not produce scratch, sticky back of the body phenomenon occurs that possibility is low, glossiness good, wearability is strong, easily realizes the advantages such as production in enormous quantities.
Detailed description of the invention
Embodiment 1
A kind of quick polishing technique, comprises the following steps:
1) by taking out point impurity absorbing carrier surface impurity carrier;
2) to step 1) carrier roller coat water lustering oil;
3) to step 2) carrier carry out infrared baking;
4) to step 3) carrier carry out electric fan heat radiation;
5) by step 4) carrier carry out receipts dress.
By taking out a point absorption carrier surface impurity, scratch can not be caused to carrier surface while absorbing carrier surface impurity, ensureing carrier polishing effect.
Water lustering oil comprises: barras, animi resin and alkali soluble resin, and the formula rate of three kinds of resins is 1:1:1.
Roller coat contributes to oil polish and is uniformly coated on carrier, and easily realizes producing in enormous quantities.
Infrared baking effectively accelerates the drying being coated with oil polish carrier, and bake out temperature is 95 DEG C.
Electric fan heat radiation not only can effectively realize accelerating dry after the cooling of carrier, can also step 3 be realized) to fail dry carrier dry further.
Embodiment 2
A kind of quick polishing technique, comprises the following steps:
1) by taking out point impurity absorbing carrier surface impurity carrier;
2) to step 1) carrier roller coat water lustering oil;
3) to step 2) carrier carry out infrared baking;
4) to step 3) carrier carry out electric fan heat radiation;
5) by step 4) carrier carry out receipts dress.
By taking out a point absorption carrier surface impurity, scratch can not be caused to carrier surface while absorbing carrier surface impurity, ensureing carrier polishing effect.
Water lustering oil comprises: barras, animi resin and alkali soluble resin, and the formula rate of three kinds of resins is 1:1:1.
Roller coat contributes to oil polish and is uniformly coated on carrier, and easily realizes producing in enormous quantities.
Infrared baking effectively accelerates the drying being coated with oil polish carrier, and bake out temperature is 90 DEG C, and drying tunnel length is 2 meters.
Electric fan heat radiation not only can effectively realize accelerating dry after the cooling of carrier, can also step 3 be realized) to fail dry carrier dry further.
More than show and describe general principle of the present invention and principal character and advantage of the present invention.The technology people of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and description just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (6)

1. a quick polishing technique, is characterized in that comprising the following steps:
1) impurity of carrier is removed;
2) to step 1) carrier coating oil polish;
3) to step 2) carrier dry;
4) to step 3) carrier cool;
5) by step 4) carrier carry out receipts dress.
2. quick polishing technique according to claim 1, is characterized in that: step 1) described removing carrier surface impurity is for by taking out point an absorption carrier surface impurity.
3. quick polishing technique according to claim 1, is characterized in that: step 2) described oil polish is water lustering oil, described water lustering oil comprises barras, animi resin and alkali soluble resin, and the formula rate of three kinds of resins is 1:1:1.
4. quick polishing technique according to claim 1, is characterized in that: step 2) described coating process is roller coat.
5. quick polishing technique according to claim 1, is characterized in that: step 3) described oven dry is for by infrared baking, and bake out temperature is 80 ~ 100 DEG C.
6. quick polishing technique according to claim 1, is characterized in that: step 4) described in be cooled to and dispelled the heat by electric fan.
CN201410495752.XA 2014-09-24 2014-09-24 Quick lustering process Pending CN104290482A (en)