CN104250933A - Preparation method for aromatic polyester fiber - Google Patents

Preparation method for aromatic polyester fiber Download PDF

Info

Publication number
CN104250933A
CN104250933A CN201410455855.3A CN201410455855A CN104250933A CN 104250933 A CN104250933 A CN 104250933A CN 201410455855 A CN201410455855 A CN 201410455855A CN 104250933 A CN104250933 A CN 104250933A
Authority
CN
China
Prior art keywords
aromatic
preparation
fiber
staple fiber
polyester staple
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410455855.3A
Other languages
Chinese (zh)
Inventor
陆新生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU BLUE FIBRE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd
Original Assignee
JIANGSU BLUE FIBRE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU BLUE FIBRE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd filed Critical JIANGSU BLUE FIBRE SCIENCE AND TECHNOLOGY DEVELOPMENT Co Ltd
Priority to CN201410455855.3A priority Critical patent/CN104250933A/en
Publication of CN104250933A publication Critical patent/CN104250933A/en
Pending legal-status Critical Current

Abstract

The invention discloses a preparation method for aromatic polyester fiber. The preparation method comprises preparation of polyester short fiber and adsorption of polyester short fiber to an aromatic. Conventional polyester fiber is functionalized, and the prepared aromatic polyester fiber has long-acting aromatic smell. Fragrance adding processing can be again performed according to an aromatic smell favored by a user self, so that the aromatic smell of the aromatic fiber can be selected again.

Description

A kind of preparation method of aromatic polyester fiber
Technical field
The present invention relates to functional polyester fibre technology field, that be specifically related to is a kind of preparation method of aromatic polyester fiber.
Background technology
In the last few years, global environment problem was on the rise, and energy crisis is increasingly sharpened, and extreme weather conditions are frequently existing.Therefore, the industries such as new material, new forms of energy, bioengineering, information technology more and more receive the concern of people, and in daily life, people are for the health environment-friendly of daily necessities, and the attention rate of sleeping effect is more and more higher.Under this new background, the demand with health environment-friendly material is also more and more urgent.And the main body of functional fiber is terylene, and terylene belongs to polyester fiber, this fiber can 100% recycle, to environment close friend very.
Fragrance has the special function of optimizing the environment and optimizing personal image, more and more close with the relation of people's daily life.The mood that it can affect people even produces the impact of physiology aspect on people.Live and work under the environment of fragrance, can dispelling fatigue, pleasant mental and body, increase work efficiency.Such as: the fragrance of rose can be cleared away melancholy or dejected, makes to be in a cheerful frame of mind; Jasmin is elegant pleasant, has the effect of pacifying nerve, warm mood, raising adaptability to changes; The fragrance energy refreshment eyesight improving of lavender, alleviate anxiety, improve depressive state; The fragrance of violet can stimulate olfactory nerves easily, is directly delivered to brain, thus the psychological condition of mediator, dispelling fatigue, releases the pressure, and is that mood is safe and joyful; The fragrance of cloves can be releived the unhappy or uncomfortable in chest sense produced because of mood pent-up; The fragrance of gardenia has stronger anti-flue dust and the ability of anti-harmful gas, can cover niff, improve domestic environment; Apple fragrance can obviously eliminate psychological sense of depression, improves insomnia; Lemonene can fresh air, environmental protect, fatigue of releiving; Pineapple perfume (or spice) can fresh air; Orange perfume (or spice) can be eliminated feeling jittery, have the effect of anger processed, makes that people reduces anxiety, positive, mood is tranquiler.In addition, some fragrance can also stimulate generation quiet type brain wave or stimulable type brain wave.
Summary of the invention
The object of the invention is to the above problem overcoming prior art existence, a kind of preparation method of aromatic polyester fiber is provided, by traditional polyester fiber functionalization, the obtained aromatic polyester fiber with long-acting aromatic odor.
For realizing above-mentioned technical purpose, reach above-mentioned technique effect, the present invention is achieved through the following technical solutions:
A preparation method for aromatic polyester fiber, comprises the preparation of polyester staple fiber and polyester staple fiber to the absorption of aromatic;
The preparation of described polyester staple fiber comprises:
Step 1, chip drying;
Melt spinning is carried out in step 2, dried PET section, and melt arrives Xu Leng heat preservation zone after spinnerets ejection, forms melt stream, by cooling quench curing molding, then arrive feeding means, make as-spun fibre boundling, last winding shaping by oil supply feedwater;
Step 3, the silk of winding carried out boundling process, oil bath drawing-off, curling, drying and shaping and oven dry;
The absorption of described polyester staple fiber to aromatic comprises:
Step 1, complete coated environmental protection essence capsule is dissolved in ethanolic solution is diluted to aromatic;
Step 2, polyester staple fiber is immersed in aromatic, keep a period of time at ambient pressure, take out oven dry after fully sucking and obtain fragrant fiber; Or after adopting spray process to process polyester fiber, cure obtained.
Further, the step 1 of the preparation of described polyester staple fiber adopts vacuum drum drying box, vacuum 0.8Mpa, and drying time is 20-22 hour, and baking temperature is 60-90 DEG C.
In the step 2 of the preparation of described polyester staple fiber, spinning temperature is 250-290 DEG C, Xu Leng temperature is 150-180 DEG C, and lateral blowing wind speed is 0.35m/s, and wind-warm syndrome is 19-20 DEG C, and winding speed is 1300m/min.
Further, in the step 3 of the preparation of described polyester staple fiber, oil bath drawing-off groove temperature is 60-75 DEG C, and oven temperature is 110-120 DEG C, heat setting temperature 125-150 DEG C, and heat-setting time is 15-30min.
Further, the mass ratio of described polyester staple fiber to coated environmental protection essence capsule complete in the step 1 of the absorption of aromatic and ethanolic solution is (0.1-0.25): 1.
Further, described polyester staple fiber is 1:10 to polyester staple fiber described in the step 2 of the absorption of aromatic and aromatic mass ratio.
The invention has the beneficial effects as follows:
1, the fragrant fiber that dipping blending method and spray process are made belongs to physical modification, not only do not change the macromolecular chain structure of high polymer, remain the intrinsic advantage of original fiber, with the addition of again new material simultaneously, give fiber some new performance by changing aggregated structure, wearability is also had greatly improved;
2, flood method that is blended and spray process simple, the fibrous material that combination property is good can be obtained, there is larger theory and practical value.Adopt this suction to compose fragrant method, fragrant fiber without any restriction, easily forms specific fragrance effect to the boiling point of aromatic substance;
3, after aromatic odor disperses, the aromatic odor also can liked according to oneself re-starts perfuming process, and the aromatic odor of fragrant fiber can be reselected.
The fragrant fiber that the present invention produces has multiple odor type, can bring health environmental protection, the anxiety that contributes to releiving, alleviates anxiety, relieving mental strain and helping sleep, and to human temperature and non-stimulated, most people are ready to accept.
Accompanying drawing explanation
Fig. 1 is fabrication processing of the present invention.
Detailed description of the invention
Below with reference to the accompanying drawings and in conjunction with the embodiments, describe the present invention in detail.
Embodiment
With reference to shown in Fig. 1, a kind of preparation method of aromatic polyester fiber, comprises the preparation of polyester staple fiber and polyester staple fiber to the absorption of aromatic;
The preparation of described polyester staple fiber comprises:
Step 1) drying of cutting into slices, adopt vacuum drum drying box to carry out drying to section, vacuum 0.8Mpa, drying time is 20-22 hour, and baking temperature is 60-90 DEG C.Baking temperature is higher, and better, but the viscosity that too high baking temperature can make PET cut into slices reduces degree increase to dry effect, even makes section its colour changed into yellow, affects spinning quality.Along with the continuity of drying time, moisture is constantly vaporized, the Mass lost of wet stock, and the free water content of material levels off to zero;
Step 2) dried PET section carries out melt spinning on LHFJ03 spinning machine, melt arrives Xu Leng heat preservation zone after spinnerets ejection, forms melt stream, by cooling quench curing molding, then feeding means is arrived, make as-spun fibre boundling, last winding shaping by oil supply feedwater, spinning temperature is 250-290 DEG C, Xu Leng temperature is 150-180 DEG C, lateral blowing wind speed is 0.35m/s, and wind-warm syndrome is 19-20 DEG C, and winding speed is 1300m/min;
Step 3) silk of winding is carried out boundling process, through oil bath drawing-off, add polyester staple fiber finish, its weight is the 2%-3% of raw material gross weight simultaneously, after oil bath, carry out stretch processing, send into again after stretching crimping machine curling, then carry out drying and shaping to baking oven, deliver to cutting machine again from dryer silk out to cut off, oil bath drawing-off groove temperature is 60-75 DEG C, and oven temperature is 110-120 DEG C, heat setting temperature 125-150 DEG C, the time is 15-30min;
The absorption of described polyester staple fiber to aromatic comprises:
Step 1) by complete coated environmental protection essence capsule with mass ratio (0.1-0.25): 1 is dissolved in ethanolic solution and is diluted to aromatic;
Step 2) polyester staple fiber is immersed in aromatic, keep a period of time at ambient pressure, take out oven dry after fully sucking and obtain fragrant fiber, described polyester staple fiber and aromatic mass ratio are 1:10; Or after adopting spray process to process polyester fiber, cure obtained.
Polyester staple fiber to the absorption principle of spices is: the process of polyester fiber absorption perfume molecules is by spices affinity in fiber, i.e. the difference in chemical potential of spices in solution and fiber, to be adsorbed spices by fiber micropore and spread.
Further, the spices selected by the present invention has following requirement: as far as possible from the extract of plant, requires, except the sense of smell with pleasant aroma, also will have certain physical therapy function simultaneously.Such as wormwood fragrance can have certain syngignoscism and natural anthelminthic effect.Therefore the aromatic that the present invention adopts roughly has following features: the plant perfume adopted, has pleasing scent, health environment-friendly, the anxiety that contributes to releiving, alleviates anxiety, relieving mental strain and helping sleep, and to human temperature and non-stimulated, most people are ready to accept.Such as Jasmine, rose, lavender, cloves, violet, wormwood, gardenia, apple, lemon, pineapple, orange etc.
Table 1 is for carrying out performance test table after fiber test manufacture
As shown in Table 1, carry out performance test after fiber test manufacture, aromatic remains (28 days): 93%, implements long lasting quality test grading: 4 grades (the highest 5 grades) according to Nippon Standard JISL0217.
The foregoing is only the preferred embodiments of the present invention, be not limited to the present invention, for a person skilled in the art, the present invention can have various modifications and variations.Within the spirit and principles in the present invention all, any amendment done, equivalent replacement, improvement etc., all should be included within protection scope of the present invention.

Claims (6)

1. a preparation method for aromatic polyester fiber, is characterized in that: comprise the preparation of polyester staple fiber and polyester staple fiber to the absorption of aromatic;
The preparation of described polyester staple fiber comprises:
Step 1, chip drying;
Melt spinning is carried out in step 2, dried PET section, and melt arrives Xu Leng heat preservation zone after spinnerets ejection, forms melt stream, by cooling quench curing molding, then arrive feeding means, make as-spun fibre boundling, last winding shaping by oil supply feedwater;
Step 3, the silk of winding carried out boundling process, oil bath drawing-off, curling, drying and shaping and oven dry;
The absorption of described polyester staple fiber to aromatic comprises:
Step 1, complete coated environmental protection essence capsule is dissolved in ethanolic solution is diluted to aromatic;
Step 2, polyester staple fiber is immersed in aromatic, keep a period of time at ambient pressure, take out oven dry after fully sucking and obtain fragrant fiber; Or after adopting spray process to process polyester fiber, cure obtained fragrant fiber.
2. the preparation method of a kind of aromatic polyester fiber according to claim 1, it is characterized in that: the step 1 of the preparation of described polyester staple fiber adopts vacuum drum drying box, vacuum 0.8Mpa, drying time is 20-22 hour, and baking temperature is 60-90 DEG C.
3. the preparation method of a kind of aromatic polyester fiber according to claim 1, it is characterized in that: in the step 2 of the preparation of described polyester staple fiber, spinning temperature is 250-290 DEG C, Xu Leng temperature is 150-180 DEG C, lateral blowing wind speed is 0.35m/s, wind-warm syndrome is 19-20 DEG C, and winding speed is 1300m/min.
4. the preparation method of a kind of aromatic polyester fiber according to claim 1, it is characterized in that: in the step 3 of the preparation of described polyester staple fiber, oil bath drawing-off groove temperature is 60-75 DEG C, oven temperature is 110-120 DEG C, heat setting temperature 125-150 DEG C, and heat-setting time is 15-30min.
5. the preparation method of a kind of aromatic polyester fiber according to claim 1, is characterized in that: the mass ratio of described polyester staple fiber to coated environmental protection essence capsule complete in the step 1 of the absorption of aromatic and ethanolic solution is (0.1-0.25): 1.
6. the preparation method of a kind of aromatic polyester fiber according to claim 1, is characterized in that: described polyester staple fiber is 1:10 to polyester staple fiber described in the step 2 of the absorption of aromatic and aromatic mass ratio.
CN201410455855.3A 2014-09-09 2014-09-09 Preparation method for aromatic polyester fiber Pending CN104250933A (en)