CN104045883A - Elastic rubber composition - Google Patents
Elastic rubber composition Download PDFInfo
- Publication number
- CN104045883A CN104045883A CN201410285455.2A CN201410285455A CN104045883A CN 104045883 A CN104045883 A CN 104045883A CN 201410285455 A CN201410285455 A CN 201410285455A CN 104045883 A CN104045883 A CN 104045883A
- Authority
- CN
- China
- Prior art keywords
- parts
- rubber
- rubber composition
- elastic rubber
- stearic acid
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to an elastic rubber composition. The elastic rubber composition comprises the following raw materials in parts by weight: 20-40 parts of chloroprene rubber, 10-18 parts of isoprene rubber, 5-14 parts of reinforcing agent, 5-11 parts of stearic acid, 6-10 parts of vulcanizing agent, 5-8 parts of vulcanization accelerator, 7-9 parts of naphthenic oil, 11-15 parts of butadiene rubber and 6-12 parts of high-abrasion-resistant carbon black. The elastic rubber composition disclosed by the invention has the beneficial effects that the rubber material has the advantages of good elasticity as well as good cold resistance and abrasion resistance.
Description
Technical field
The present invention relates to a kind of elastic caoutchouc composition, belong to rubber technology field.
Background technology
In general, rubber composition for footwear must be able to be made wearer's body weight, the load that bears motion generation and impact intensity of force, improves comfort level, security and the anti-skid of shoes.Fire-fighting footwear are to provide firefighter and wear in the severe environment such as fiery residence, the special type protection footwear that protection both feet and shank escape injury.What fire fighter was engaged in is the work that has certain risk, and the protection footwear of its dress need to possess waterproof simultaneously, heat insulation, anti-skidding, anti-ly pierce through, resistance toly pound, side and bear building-up close the performances such as firm, wear-resisting and resistance to complications.
Summary of the invention
For the deficiencies in the prior art, the problem to be solved in the present invention is, a kind of rubber is provided, and has good elasticity, also has winter hardiness and wear resistance.
For solving prior art problem, technical scheme provided by the invention is, a kind of elastic caoutchouc composition, and its raw material by following parts by weight is made:
Chloroprene rubber 20-40 part, synthetic polyisoprene 10-18 part, strengthening agent 5-14 part, stearic acid 5-11 part, vulcanizing agent 6-10 part, vulcanization accelerator 5-8 part, naphthenic oil 7-9 part, cis-1,4-polybutadiene rubber 11-15 part, high wear-resistant carbon black 6-12 part.
Optimisation technique scheme of the present invention is, a kind of elastic caoutchouc composition, and its raw material by following parts by weight is made:
30 parts of chloroprene rubbers, 14 parts of synthetic polyisoprenes, 9 parts of strengthening agents, 8 parts of stearic acid, 8 parts of vulcanizing agents, 6.5 parts of vulcanization accelerators, 8 parts of naphthenic oils, 13 parts of cis-1,4-polybutadiene rubbers, 9 parts of high wear-resistant carbon blacks.
The invention has the beneficial effects as follows: elastomeric material of the present invention has good elasticity, also there is winter hardiness and wear resistance.
Embodiment
embodiment 1
An elastic caoutchouc composition, its raw material by following parts by weight is made:
20 parts of chloroprene rubbers, 10 parts of synthetic polyisoprenes, 5 parts of strengthening agents, 5 parts of stearic acid, 6 parts of vulcanizing agents, 5 parts of vulcanization accelerators, 7 parts of naphthenic oils, 11 parts of cis-1,4-polybutadiene rubbers, 6 parts of high wear-resistant carbon blacks.
embodiment 2
An elastic caoutchouc composition, its raw material by following parts by weight is made:
40 parts of chloroprene rubbers, 18 parts of synthetic polyisoprenes, 14 parts of strengthening agents, 11 parts of stearic acid, 10 parts of vulcanizing agents, 8 parts of vulcanization accelerators, 9 parts of naphthenic oils, 15 parts of cis-1,4-polybutadiene rubbers, 12 parts of high wear-resistant carbon blacks.
embodiment 3
An elastic caoutchouc composition, its raw material by following parts by weight is made:
30 parts of chloroprene rubbers, 14 parts of synthetic polyisoprenes, 9 parts of strengthening agents, 8 parts of stearic acid, 8 parts of vulcanizing agents, 6.5 parts of vulcanization accelerators, 8 parts of naphthenic oils, 13 parts of cis-1,4-polybutadiene rubbers, 9 parts of high wear-resistant carbon blacks.
Claims (2)
1. an elastic caoutchouc composition, is characterized in that: its raw material by following parts by weight is made:
Chloroprene rubber 20-40 part, synthetic polyisoprene 10-18 part, strengthening agent 5-14 part, stearic acid 5-11 part, vulcanizing agent 6-10 part, vulcanization accelerator 5-8 part, naphthenic oil 7-9 part, cis-1,4-polybutadiene rubber 11-15 part, high wear-resistant carbon black 6-12 part.
2. rubber according to claim 1, is characterized in that: its raw material by following parts by weight is made:
30 parts of chloroprene rubbers, 14 parts of synthetic polyisoprenes, 9 parts of strengthening agents, 8 parts of stearic acid, 8 parts of vulcanizing agents, 6.5 parts of vulcanization accelerators, 8 parts of naphthenic oils, 13 parts of cis-1,4-polybutadiene rubbers, 9 parts of high wear-resistant carbon blacks.