CN104028444A - Diamond saw blade appearance beautification method - Google Patents
Diamond saw blade appearance beautification method Download PDFInfo
- Publication number
- CN104028444A CN104028444A CN201410295468.8A CN201410295468A CN104028444A CN 104028444 A CN104028444 A CN 104028444A CN 201410295468 A CN201410295468 A CN 201410295468A CN 104028444 A CN104028444 A CN 104028444A
- Authority
- CN
- China
- Prior art keywords
- matrix
- saw blade
- varnish
- outward appearance
- diamond saw
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a diamond saw blade appearance beautification method. The matrix appearance of a saw blade can be beautified by painting double-color paint with the procedure including the steps of subjecting the matrix surface of the saw blade to rough polishing and finish polishing; cleaning up a welding line and the matrix surface of a tool bit by means of grinding and piece brushing; spraying varnish and drying the front side of a matrix and the reverse side of the matrix after turning over; utilizing a central circular plate to cover areas sprayed with the varnish in the center of the front side of the matrix and utilizing an outer ring plate to cover the tool bit; spraying colored paint on areas exposing between the central circular plate and the outer ring plate to cover the sprayed varnish to be dried, and utilizing the same method to spray the colored paint on the reverse side of the matrix to be dried; packaging for storage. Conventional saw blade appearance is substituted, so that customers can further infer features of products from the appearance of the products, the appearance of the products can convey information, and a better sales purpose can be achieved.
Description
(1) technical field:
The present invention relates to diamond cut instrument, be specially a kind of diamond saw blade outward appearance beautification method.
(2) background technology:
Diamond saw blade is used in the cutting of bituminous concrete, refractory brick and glass etc. that pottery, stone material, civil construction project are used in a large number.
Conventional diamond saw blade outward appearance lacquer spraying technique flow process is: rough polishing, and------spray the first finish paint---is dried---spray the second finish paint---oven dry---packing warehouse-in to brushing piece.
Traditional handicraft causes existing diamond saw blade appearance design color single, and matrix is unanimously that all black, full crocus, full silvery white or all-metal are blue, and the color of diamond saw blade is single easily imitated, and diseases caused by external factors are also attractive in appearance not.
(3) summary of the invention:
For the deficiencies in the prior art, the present invention proposes a kind of diamond saw blade outward appearance beautification method, its objective is in order to allow client can see matrix surface presentation quality, also beautified saw blade outward appearance simultaneously, to client, leave deep effect, improve product competitiveness in the market.
Can realize the diamond saw blade outward appearance beautification method of above-mentioned purpose, the matrix outward appearance of beautifying saw blade by spraying double-colored paint, its process is as follows:
1, the matrix surface of rough polishing and finishing polish saw blade.
2, by polishing and brushing piece mode, the weld seam of cutter head and matrix surface are cleaned out.
3,, in front side of matrix spray varnish oven dry, turn over one side at matrix back spraying varnish and dry.
4, with middle part plectane, cover front side of matrix center and sprayed varnish region, with peripheral ring flat-plate, cover cutter head, the region color spray paint spilling between middle part plectane and peripheral ring flat-plate is covered and sprayed varnish and dried, with same procedure spray matrix back side colored paint, also dry.
5, packing warehouse-in.
Best aesthetic is that the ratio that described varnish region accounts for matrix is chosen between 40%~60%.
The rough polishing of matrix is carried out in conventional 80 order abrasive bands, with 120 order abrasive bands, carries out the finishing polish of matrix.
Conventionally, described bake out temperature is chosen as 60 °~70 °, and drying time is chosen as 4min~8min.
Further requirement, described in spray paint and want evenly, can not have obvious part thick or local thin.
Beneficial effect of the present invention:
The present invention and common product appearance production cost are more or less the same, and use different pattern, color to decorate the appearance of product, can allow client see matrix surface, allow product have more the market competitiveness.
(4) accompanying drawing explanation:
Fig. 1 is the structural representation with the diamond saw blade of the inventive method production.
Fig. 2 (a) is for carrying out the enforcement schematic diagram of color spray lacquerer order to diamond saw blade in the inventive method.
Fig. 2 (b) is the top view of Fig. 2 (a).
Figure number sign: 1, saw blade; 2, middle part plectane; 3, peripheral ring flat-plate; 4, cutter head; 5, varnish region; 6, colored paint region.
(5) specific embodiment:
Below in conjunction with accompanying drawing illustrated embodiment, technical scheme of the present invention is described further.
The technological process of diamond saw blade outward appearance beautification method of the present invention is: rough polishing, and------brushing piece------dry and---spray second varnish and---dry---spray first surface colored paint---oven dry---spray the second complexion paint---oven dry---packing warehouse-in by spray first surface varnish in finishing polish.
As shown in Figure 1, the matrix external diameter of saw blade 1 of take is ¢ 336mm, diameter of bore ¢ 25.4mm, on matrix external diameter, weld cutter head 4, centered by centre bore, spray varnish in internal diameter ¢ 168 scopes, within the scope of all the other matrixes, crimson colored paint is example, and the concrete process of the inventive method technological process is:
1, the matrix surface of rough polishing and finishing polish saw blade 1.
1., the matrix of described saw blade 1 is contained in the axle of polishing machine workbench and locates, workbench inside is provided with electromagnet matrix is sucked.
2., open worktable rotary button and abrasive band rotary knob, worktable rotary; By polishing machine handle, abrasive band is moved down, encounter matrix surface, make that oil stain, rust staining and other impurity of matrix surface is polished to be fallen, make matrix surface look light and temporarily white.
Rough polishing adopts 80 order abrasive bands, finish polishing 120 order abrasive bands.
2, saw blade 1 is put on workbench, at sander, loads onto wire brush, the weld seam of cutter head 4 is beaten and cleaned down; Use again hairbrush that the dust brush of matrix surface is clean.
3, saw blade 1 is put on workbench, front side of matrix (simultaneously) has all been sprayed to varnish, the saw blade 1 that has sprayed varnish is kept flat and on small handcart, advances oven for drying; After oven dry, the spray matrix back side (another side) varnish uses the same method.
Described spray varnish wants evenly, can not have obvious part thick or local thin.
The bake out temperature of described baking oven is 60 °~70 °, and preferably 65 °, drying time is 4min~8min, preferably 5min.
4, the crimson colored paint of mode as shown in Fig. 2 (a), Fig. 2 (b).
1., make ¢ 168 middle part plectanes 2 and peripheral ring flat-plate 3 each, the dimension of inner and outer diameters of described peripheral ring flat-plate 3 is less than and is greater than the dimension of inner and outer diameters of cutter head 4, the effect of peripheral ring flat-plate 3 is to cover cutter head 4.
2., saw blade 1 is put on Paint spraying platform, with middle part plectane 2, having sprayed varnish region 5 within the scope of front side of matrix (simultaneously) central diameter ¢ 168mm, cover, with peripheral ring flat-plate 3, the position of cutter head 4 is covered, the varnish of the spray region spilling between middle part plectane 2 and peripheral ring flat-plate 3 is sprayed red paint and is become colored paint region 6, sprayed paint and rear middle part plectane 2 and peripheral ring flat-plate 3 have been taken down, saw blade 1 keeps flat and on small handcart, advances oven for drying; After oven dry, the spray matrix back side (another side) red paint uses the same method.
Described color spray paint wants evenly, can not have obvious part thick or local thin.
The bake out temperature of described baking oven is 60 °~70 °, and preferably 65 °, drying time is 4min~8min, preferably 5min.
5, packing warehouse-in.
In process of the present invention, the shared matrix ratio in described spray varnish region is 40%~60%, can determine to spray paint size or colored paint color according to saw blade 1 size and the design of spray varnish scope.
Adopt the inventive method that saw blade 1 outward appearance spray varnish is combined with colored paint, can increase saw blade 1 cosmetic look, can express the quality information of product, product is not easy imitated, client partly can be observed the quality of saw blade 1 matrix by varnish, thereby can further infer the characteristic of product, with this, improve the approval of client to product quality.
Although increased the link of spraying paint in the inventive method more, can make overall appearance effect improve 50%, comprehensive benefit is obvious.
Claims (5)
1. diamond saw blade outward appearance beautification method, is characterized in that: by spraying double-colored paint, beautify the matrix outward appearance of saw blade (1), its process is as follows:
1., the matrix surface of rough polishing and finishing polish saw blade (1);
2., by polishing and brushing piece mode, weld seam and the matrix surface of cutter head (4) are cleaned out;
3., at front side of matrix spray varnish and dry, turn over one side at matrix back spraying varnish and dry;
4., with middle part plectane (2), cover front side of matrix center and sprayed varnish region, with peripheral ring flat-plate (3), cover cutter head (4), the region color spray paint spilling between middle part plectane (2) and peripheral ring flat-plate (3) is covered and sprayed varnish and dried, with same procedure spray matrix back side colored paint, also dry;
5., packing warehouse-in.
2. diamond saw blade outward appearance beautification method according to claim 1, is characterized in that: it is 40%~60% that described varnish region accounts for matrix ratio.
3. diamond saw blade outward appearance beautification method according to claim 1 and 2, is characterized in that: with 80 order abrasive bands, carry out the rough polishing of matrix, with 120 order abrasive bands, carry out the finishing polish of matrix.
4. diamond saw blade outward appearance beautification method according to claim 1 and 2, is characterized in that: described bake out temperature is 60 °~70 °, and drying time is 4min~8min.
5. diamond saw blade outward appearance beautification method according to claim 1 and 2, is characterized in that: described in spray paint and want evenly, can not have obvious part thick or local thin.