CN103933715A - Manufacturing technique of grafting type shuttlecock - Google Patents

Manufacturing technique of grafting type shuttlecock Download PDF

Info

Publication number
CN103933715A
CN103933715A CN201410147661.7A CN201410147661A CN103933715A CN 103933715 A CN103933715 A CN 103933715A CN 201410147661 A CN201410147661 A CN 201410147661A CN 103933715 A CN103933715 A CN 103933715A
Authority
CN
China
Prior art keywords
feather
shuttlecock
grafting
fixed bar
accessory pinna
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410147661.7A
Other languages
Chinese (zh)
Inventor
李韵星
夏业斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI HUA LING FEATHER PRODUCTS Co Ltd
Original Assignee
ANHUI HUA LING FEATHER PRODUCTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI HUA LING FEATHER PRODUCTS Co Ltd filed Critical ANHUI HUA LING FEATHER PRODUCTS Co Ltd
Priority to CN201410147661.7A priority Critical patent/CN103933715A/en
Publication of CN103933715A publication Critical patent/CN103933715A/en
Pending legal-status Critical Current

Abstract

The invention relates to a manufacturing technique of a grafting type shuttlecock. The manufacturing technique of the grafting type shuttlecock comprises the following steps of (1) feather piece manufacturing, (2) feather piece selection, (3) shuttlecock head manufacturing, (4) feather fixing rod manufacturing, (5) grafting, (6) primary gluing, (7) string threading, (8) secondary gluing, (9) testing, and (10) packaging. The manufacturing technique of the grafting type shuttlecock has the advantages that the schematic design is reasonable, manufacturing is convenient, the machining quality of the grafting type shuttlecock can be guaranteed, the size of the formed shuttlecock can be reduced, the weight of the shuttlecock is reduced, and the flying performance of the shuttlecock is improved to a certain degree.

Description

A kind of manufacturing process of grafting formula shuttlecock
Technical field
The present invention relates to shuttlecock processing technique field, specifically a kind of manufacturing process of grafting formula shuttlecock.
Background technology
Along with the raising of people's living standard, people more and more pay attention to motion and combine with work, and shuttlecock is widely loved by the people as a kind of motion of fashion.The technology of shuttlecock is also constantly being improved and is upgrading, more and more money shuttlecocks start to come into people's sight line, as the shuttlecock of all-plastic shuttlecock, imitative feather etc., and the shuttlecock of grafting formula is as a kind of new style, and the technique of its manufacture becomes again the focus that people pay close attention to.
Summary of the invention
Technical problem to be solved by this invention is to provide a kind of conceptual design reasonably, conveniently to manufacture, and can guarantee the technique of grafting formula shuttlecock crudy, i.e. a kind of manufacturing process of grafting formula shuttlecock.
Technical problem to be solved by this invention realizes by the following technical solutions:
A manufacturing process for grafting formula shuttlecock, this technique comprises following processing step:
1) accessory pinna manufacture:
A) ted: natural feather is dried under burning sun, utilize ultraviolet sterilization;
B) select: select the feather of suitable length, and marshalling, put into holding box;
C) stamping-out: stamping-out feather length is 39.5mm, the overall length of hair bar is 48.5mm, adopts this length can greatly reduce the volume after shuttlecock moulding, has reduced the heavy burden of shuttlecock, has improved to a certain extent the flying quality of shuttlecock;
2) accessory pinna is selected: select the accessory pinna that bow comparatively approaches and put together;
3) make bulb: utilize mould one-shot forming processing bulb, and on bulb jack;
4) make feather fixed bar: utilize the Integratively formed feather fixed bar of making of mould;
5) grafting: by step 2) in accessory pinna inserting step 4) in feather fixed bar in, adopt the mode of grafting can improve the resistance to degree of beating of shuttlecock, extend the service life of shuttlecock;
6) gluing: smear thermoplastic mould glue at the interface of accessory pinna and feather fixed bar, normal temperature is cooling, adopts thermoplastic mould glue to solve the not resistance to defect of beating that traditional glue exists, and has strengthened the bonding strength of accessory pinna and feather fixed bar;
7) reach the standard grade: reaching the standard grade in the middle part of the plumage bar to feather on the machine of reaching the standard grade and the middle part of feather fixed bar, reaches the standard grade and can improve the bonding strength of shuttlecock;
8) second glue spreading: thermoplastic mould glue is smeared to by the place of reaching the standard grade in step 7, and normal temperature is cooling;
9) test: the shuttlecock after grafting is carried out to stability test and service test;
10) encapsulation.
The invention has the beneficial effects as follows: it is rational, convenient manufacture that the present invention has conceptual design, can guarantee grafting formula shuttlecock crudy, the moulding volume that has dwindled shuttlecock, has reduced the heavy burden of shuttlecock, has improved to a certain extent the flying quality of shuttlecock.
Detailed description of the invention
For technological means, creation characteristic that the present invention is realized, reach object and effect is easy to understand, below the present invention is further set forth.
A manufacturing process for grafting formula shuttlecock, this technique comprises following processing step:
1) accessory pinna manufacture:
A) ted: natural feather is dried under burning sun, utilize ultraviolet sterilization;
B) select: select the feather of suitable length, and marshalling, put into holding box;
C) stamping-out: stamping-out feather length is 39.5mm, the overall length of hair bar is 48.5mm, adopts this length can greatly reduce the volume after shuttlecock moulding, has reduced the heavy burden of shuttlecock, has improved to a certain extent the flying quality of shuttlecock;
2) accessory pinna is selected: select the accessory pinna that bow comparatively approaches and put together;
3) make bulb: utilize mould one-shot forming processing bulb, and on bulb jack;
4) make feather fixed bar: utilize the Integratively formed feather fixed bar of making of mould;
5) grafting: by step 2) in accessory pinna inserting step 4) in feather fixed bar in, adopt the mode of grafting can improve the resistance to degree of beating of shuttlecock, extend the service life of shuttlecock;
6) gluing: smear thermoplastic mould glue at the interface of accessory pinna and feather fixed bar, normal temperature is cooling, adopts thermoplastic mould glue to solve the not resistance to defect of beating that traditional glue exists, and has strengthened the bonding strength of accessory pinna and feather fixed bar;
7) reach the standard grade: reaching the standard grade in the middle part of the plumage bar to feather on the machine of reaching the standard grade and the middle part of feather fixed bar, reaches the standard grade and can improve the bonding strength of shuttlecock;
8) second glue spreading: thermoplastic mould glue is smeared to by the place of reaching the standard grade in step 7, and normal temperature is cooling;
9) test: the shuttlecock after grafting is carried out to stability test and service test;
10) encapsulation.
Implement according to above-mentioned processing step, can complete the manufacturing to grafting formula shuttlecock.
More than show and described general principle of the present invention, principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what in above-described embodiment and description, describe is principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.The claimed scope of the present invention is defined by appending claims and equivalent thereof.

Claims (1)

1. a manufacturing process for grafting formula shuttlecock, is characterized in that: this technique comprises following processing step:
1) accessory pinna manufacture:
A) ted: natural feather is dried under burning sun, utilize ultraviolet sterilization;
B) select: select the feather of suitable length, and marshalling, put into holding box;
C) stamping-out: stamping-out feather length is 39.5mm, the overall length of hair bar is 48.5mm;
2) accessory pinna is selected: select the accessory pinna that bow comparatively approaches and put together;
3) make bulb: utilize mould one-shot forming processing bulb, and on bulb jack;
4) make feather fixed bar: utilize the Integratively formed feather fixed bar of making of mould;
5) grafting: by step 2) in accessory pinna inserting step 4) in feather fixed bar in;
6) gluing: smear thermoplastic mould glue at the interface of accessory pinna and feather fixed bar, normal temperature is cooling;
7) reach the standard grade: reach the standard grade in the middle part of the plumage bar to feather on the machine of reaching the standard grade and the middle part of feather fixed bar;
8) second glue spreading: thermoplastic mould glue is smeared to by the place of reaching the standard grade in step 7, and normal temperature is cooling;
9) test: the shuttlecock after grafting is carried out to stability test and service test;
10) encapsulation.
CN201410147661.7A 2014-04-04 2014-04-04 Manufacturing technique of grafting type shuttlecock Pending CN103933715A (en)