CN103737949A - Coating process method applied to plastic film double-drawing machine - Google Patents

Coating process method applied to plastic film double-drawing machine Download PDF

Info

Publication number
CN103737949A
CN103737949A CN201310747660.1A CN201310747660A CN103737949A CN 103737949 A CN103737949 A CN 103737949A CN 201310747660 A CN201310747660 A CN 201310747660A CN 103737949 A CN103737949 A CN 103737949A
Authority
CN
China
Prior art keywords
coating
film
process method
coating process
plastic
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310747660.1A
Other languages
Chinese (zh)
Inventor
林史衡
王立华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
GUANGDONG SHUYE ENVIRONMENTAL PROTECTION TECHNOLOGY CO LTD
Original Assignee
GUANGDONG SHUYE ENVIRONMENTAL PROTECTION TECHNOLOGY CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by GUANGDONG SHUYE ENVIRONMENTAL PROTECTION TECHNOLOGY CO LTD filed Critical GUANGDONG SHUYE ENVIRONMENTAL PROTECTION TECHNOLOGY CO LTD
Priority to CN201310747660.1A priority Critical patent/CN103737949A/en
Publication of CN103737949A publication Critical patent/CN103737949A/en
Pending legal-status Critical Current

Abstract

The invention relates to a coating process method applied to plastic production equipment and discloses an environment-friendly and energy-saving coating process method. The coating process method comprises the following steps: (1) starting to draw a plastic film through a plastic double-drawing machine; (2) horizontally drawing the plastic film through the plastic double-drawing machine; (3) during horizontal drawing, coating the horizontally-drawn plastic film with an aqueous solvent; and (4) stabilizing the tension of the coated film after drawing, namely performing sizing operation, and drying a coating. According to the coating process method, the film is coated with the aqueous solvent before being horizontally drawn and sized, so that gas harmful to a human body and the environment cannot be emitted; meanwhile, the coating is dried at high temperature of 200-250 DEG C reached during sizing operation. Through an experiment, the drying effect is quite good, the coating drying and the sizing operation are almost performed simultaneously, so that a great amount of electric energy is saved, and the beneficial effects of environmental protection and energy conservation can be achieved.

Description

A kind of technological process for coating that is applied to the two machine drawings of plastic sheeting
Technical field
The present invention relates to a kind of technological process for coating, specifically, is a kind of technological process for coating that is applied to plastics-production equipment.
Background technology
Industrial manufacture composite film material or extrusion coating paper material, can adopt technological process for coating to be realized, traditional coating process is in operation process, must use the raw material of organic solvents such as containing acetone, chloroform, and to utilize the equipment such as bellows to dry it after coating, will give off harmful gas so in this course, this class gas equally also can contaminated air and welding.This is the technological deficiency that existing coating process exists.
Summary of the invention
The present invention discloses a kind of environmental protection and energy-conservation technological process for coating.
The present invention is achieved in that a kind of technological process for coating that is applied to the two machine drawings of plastics, comprises the steps.
Step 1: the two machine drawings of plastics start drawing plastic film.
Step 2: the two machine drawings of plastics are carried out horizontal drawing to film.
Step 3: when carrying out horizontal drawing, use aqueous solvent to be coated with operation to the film after horizontal drawing.
Step 4: the film after coating is carried out to the stable of drawing-off back pull, and the operation of shaping, also dries Coating simultaneously.
Described aqueous solvent is methyl alcohol and/or ethanol.
Temperature during described sizing operation is 200-250 degrees Celsius.
Temperature during described sizing operation is 230 degrees Celsius.
Use process of the present invention, due to film is horizontal draw after and before shaping film, use aqueous solvent to be coated with operation to film, can not discharge human body and the harmful gas of environment, high temperature while simultaneously utilizing sizing operation reaches the temperature of 200-250 degrees Celsius dries coating, through experiment, its drying effect is very good, dries coating and almost carries out with sizing operation simultaneously, simultaneously also save a large amount of electric energy, can reach environmental protection and energy-conservation beneficial effect.
The specific embodiment
The present invention is a kind of technological process for coating, is to be applied to a kind of technological process for coating on the two this membrane production equipments of machine drawing of plastic sheeting.Mainly on the activity bases of the two machine drawings of traditional plastic sheeting, added coating process, plastic sheeting is horizontal draw operation after, use aqueous solvent to be coated with operation to the horizontal operation film afterwards that draws, then carry out the stable of film drawing-off post-tensioning, carry out the sizing operation of film, operating temperature now reaches 200-250 degrees Celsius, in shaping film, the coating after coating is dried, its drying effect is good, coated and dried and shaping film are carried out simultaneously, both at operation process, can not discharge human body and the harmful gas of environment, also saved a large amount of electric energy, can reach environmental protection and energy-conservation technique effect.
The specific embodiment
Embodiment 1: a kind of technological process for coating that is applied to the two machine drawings of plastics, comprises the steps.
Step 1: the two machine drawings of plastics start drawing plastic film.
Step 2: the two machine drawings of plastics are carried out horizontal drawing to film.
Step 3: when carrying out horizontal drawing, use aqueous solvent to be coated with operation to the film after horizontal drawing.
Step 4: the film after coating is carried out to the stable of drawing-off back pull, and the operation of shaping, also dries Coating simultaneously.
In procedure, having adopted aqueous solvent is methyl alcohol.And the temperature when sizing operation is 200 degrees Celsius.
Embodiment 2: a kind of technological process for coating that is applied to the two machine drawings of plastics, comprises the steps.
Step 1: the two machine drawings of plastics start drawing plastic film.
Step 2: the two machine drawings of plastics are carried out horizontal drawing to film.
Step 3: when carrying out horizontal drawing, use aqueous solvent to be coated with operation to the film after horizontal drawing.
Step 4: the film after coating is carried out to the stable of drawing-off back pull, and the operation of shaping, also dries Coating simultaneously.
In procedure, having adopted aqueous solvent is ethanol.And the temperature when sizing operation is 250 degrees Celsius.
Embodiment 3: a kind of technological process for coating that is applied to the two machine drawings of plastics, comprises the steps.
Step 1: the two machine drawings of plastics start drawing plastic film.
Step 2: the two machine drawings of plastics are carried out horizontal drawing to film.
Step 3: when carrying out horizontal drawing, use aqueous solvent to be coated with operation to the film after horizontal drawing.
Step 4: the film after coating is carried out to the stable of drawing-off back pull, and the operation of shaping, also dries Coating simultaneously.
In procedure, having adopted aqueous solvent is methyl alcohol and ethanol, and both quality proportionings are 2:1.And the temperature when sizing operation is 230 degrees Celsius.
Embodiment 4: a kind of technological process for coating that is applied to the two machine drawings of plastics, comprises the steps.
Step 1: the two machine drawings of plastics start drawing plastic film.
Step 2: the two machine drawings of plastics are carried out horizontal drawing to film.
Step 3: when carrying out horizontal drawing, use aqueous solvent to be coated with operation to the film after horizontal drawing.
Step 4: the film after coating is carried out to the stable of drawing-off back pull, and the operation of shaping, also dries Coating simultaneously.
In procedure, having adopted aqueous solvent is ethanol, and both quality proportionings are 2:1.And the temperature when sizing operation is 210 degrees Celsius.

Claims (4)

1. a technological process for coating that is applied to the two machine drawings of plastic sheeting, comprises the steps:
Step 1: the two machine drawings of plastics start drawing plastic film;
Step 2: the two machine drawings of plastics are carried out horizontal drawing to film;
Step 3: when carrying out horizontal drawing, use aqueous solvent to be coated with operation to the film after horizontal drawing;
Step 4: the film after coating is carried out to the stable of drawing-off back pull, and the operation of shaping, also dries Coating simultaneously.
2. the technological process for coating that is applied to the two machine drawings of plastic sheeting as claimed in claim 1, is characterized in that: described aqueous solvent is methyl alcohol and/or ethanol.
3. the technological process for coating that is applied to the two machine drawings of plastic sheeting as claimed in claim 1, temperature during described sizing operation is 200-250 degrees Celsius.
4. the technological process for coating that is applied to the two machine drawings of plastic sheeting as claimed in claim 3, temperature during described sizing operation is 230 degrees Celsius.
CN201310747660.1A 2013-12-31 2013-12-31 Coating process method applied to plastic film double-drawing machine Pending CN103737949A (en)