CN103737916A - Bonding process for blade pocket holes of shutter - Google Patents

Bonding process for blade pocket holes of shutter Download PDF

Info

Publication number
CN103737916A
CN103737916A CN201310694538.2A CN201310694538A CN103737916A CN 103737916 A CN103737916 A CN 103737916A CN 201310694538 A CN201310694538 A CN 201310694538A CN 103737916 A CN103737916 A CN 103737916A
Authority
CN
China
Prior art keywords
sack
blade
sticking
point
technique
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310694538.2A
Other languages
Chinese (zh)
Inventor
余建鸣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Lander Industrial Zhejiang Co Ltd
Original Assignee
Lander Industrial Zhejiang Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lander Industrial Zhejiang Co Ltd filed Critical Lander Industrial Zhejiang Co Ltd
Priority to CN201310694538.2A priority Critical patent/CN103737916A/en
Publication of CN103737916A publication Critical patent/CN103737916A/en
Pending legal-status Critical Current

Abstract

The invention relates to the field of technical processes of curtains and specifically relates to a bonding process for blade pocket holes of a shutter. The bonding process comprises the steps of hot melting treatment, dispensing of the pocket holes, pressing of blades, cooling and curing, and is specifically as follows: firstly directly loading an RT-4892 type glue stick into a dispensing machine, heating for melting to obtain a hot-melt adhesive, then fast dropping 3-5 drops of the RT-4892 type hot-melt adhesive into the blade pocket holes, mutually pressing the upper and the lower surfaces of the blade pocket holes through a pressing mechanism of the dispensing machine, and fast cooling the blade pocket holes after pressing within 0.5 second to solidify the hot-melt adhesive. The method provided by the invention has the advantages of convenience in use and simplicity in operation, the blade pocket holes can be firmly sealed, the quality of the blades can not be damaged, the aesthetic appearance of the blades can be ensured, and the suction of dust can be simultaneously blocked.

Description

A kind of blade of louver window sack technique for sticking
Technical field
The present invention relates to curtain technical matters field, be specifically related to a kind of blade of louver window sack technique for sticking.
Background technology
Shutter is the soft dress ornament of a kind of family new house, and effectively injecting of shielding of ultraviolet, protects furniture be not subject to ultraviolet impact and fade.And the blade of shutter is the pith of adjusting louver window, in order to strengthen, support and regulating action, conventionally can in terylene Weave type blade, penetrate two glass rods, yet for sack two ends place's not sealing-in always of inserting glass rod, when for a long time after indoor suspension, easily suck dust, cause cleaning difficulty; Moreover cross special process and process due to vanes, make face coat there is antiultraviolet, fire-retardant, refuse the functions such as water, cause the bonding sealing of sack very difficult, and easily produce chemical reaction while directly adopting heat treatment sealing, damaged blade quality, affects outward appearance.
Summary of the invention
In order to overcome the deficiencies in the prior art, the object of the present invention is to provide a kind of blade of louver window sack technique for sticking, described technique for sticking can be divided into following steps:
A, hot melt are processed: solid gum is directly packed in point gum machine, and heat fused, obtains PUR;
B, sack point glue: at blade, enter sack place dropping point melten gel fast;
C, blade pressing: upper and lower two faces of blade sack are laminated by point gum machine laminating mechanism;
D, cooling curing: the blade sack after the bonding pressing fast cooling PUR that makes solidifies.
As preferably, described solid gum is selected from RT-4892 type solid gum.
As preferably, the heating-up temperature scope of described solid gum is room temperature to 150 ℃, forms the PUR of transparent and homogeneous under high temperature after heat fusing.
As preferably, described point gum machine can be selected from full-automatic glue-dropping machine, hot melt adhesive injecting machine, Opel point gum machine, automatic ration point gum machine, and described point gum machine is provided with the two point needle head that can insert sack.
As preferably, the PUR amount that in described step B, each dispensing needle head is clicked and entered rapidly each sack is controlled at 3-5 and drips, and some glue speed was controlled in 0.2 second, and glue is complete exits rapidly for point.
As preferably, in described step C, laminating mechanism pressing sack while hot, lives sack sealing-in rapidly the PUR that splashes into sack.
As preferably, in described step D, laminating mechanism makes blade quenching but, guarantees PUR condensation cure in 0.5 second.
Beneficial effect:
Method provided by the invention is easy to use, simple to operate, and both firmly blade sack was lived in sealing-in, can damaged blade quality, can guarantee blade aesthetic appearance again, and effectively blocked dust suction simultaneously.
The specific embodiment
Embodiment 1
Adopt Opel point gum machine, first RT-4892 type solid gum is directly packed in point gum machine, be heated to 150 ℃ solid gum is melted completely, obtain PUR; Blade is placed on Opel point gum machine workbench, and two point needle head enters 3 of sack place dropping point melten gels at blade simultaneously, and it is 0.1 second that the some glue time is controlled, and exits fast syringe needle; By point gum machine laminating mechanism, upper and lower two faces of blade sack are laminated again; Blade sack after bonding pressing is cooling fast, makes PUR cooled and solidified in 0.5 second.
Embodiment 2
Adopt automatic ration glue machine, first each dropping quantity and rate of addition are set, then RT-4892 type solid gum is packed in point gum machine, while being heated to 150 ℃, solid gum melts completely, obtains PUR; Blade is placed on automatic dispensing machine workbench, and two point needle head enters sack place dropping point melten gel at blade automatically, dropwises the rear syringe needle that automatically exits fast, and point gum machine laminating mechanism makes upper and lower two faces of blade sack be laminated automatically simultaneously; Blade sack after pressing is automatically cooling in 0.5 second, and PUR solidifies.
Specific embodiment described herein is only to the explanation for example of the present invention's spirit.Those skilled in the art can make various modifications or supplement or adopt similar mode to substitute described specific embodiment, but can't depart from spirit of the present invention or surmount the defined scope of appended claims.
Although more used the terms such as heat treatment, pressing, cooling curing herein, do not got rid of the possibility of using other term.Use these terms to be only used to describe more easily and explain essence of the present invention; They are construed to any additional restriction is all contrary with spirit of the present invention.

Claims (7)

1. a blade of louver window sack technique for sticking, is characterized in that: described technique for sticking can be divided into following steps:
A, hot melt are processed: solid gum is directly packed in point gum machine, and heat fused, obtains PUR;
B, sack point glue: at blade, enter sack place dropping point melten gel fast;
C, blade pressing: upper and lower two faces of blade sack are laminated by point gum machine laminating mechanism;
D, cooling curing: the blade sack after the bonding pressing fast cooling PUR that makes solidifies.
2. a kind of blade of louver window sack technique for sticking as claimed in claim 1, is characterized in that: described solid gum is selected from RT-4892 type solid gum.
3. a kind of blade of louver window sack technique for sticking as claimed in claim 1, is characterized in that: the heating-up temperature scope of described solid gum is room temperature to 150 ℃, forms the PUR of transparent and homogeneous under high temperature after heat fusing.
4. profit requires a kind of blade of louver window sack technique for sticking described in 1, it is characterized in that: described point gum machine can be selected from full-automatic glue-dropping machine, hot melt adhesive injecting machine, Opel point gum machine, automatic ration point gum machine, described point gum machine is provided with the two point needle head that can insert sack.
5. profit requires a kind of blade of louver window sack technique for sticking described in 1, it is characterized in that: the PUR amount that in described step B, each dispensing needle head is clicked and entered rapidly each sack is controlled at 3-5 and drips, and some glue speed was controlled in 0.2 second, and glue is complete exits rapidly for point.
6. profit requires a kind of blade of louver window sack technique for sticking described in 1, it is characterized in that: laminating mechanism pressing sack while hot in described step C, lives sack sealing-in rapidly the PUR that splashes into sack.
7. a kind of blade of louver window sack technique for sticking as claimed in claim 1, is characterized in that: in described step D, laminating mechanism makes blade quenching but, guarantees PUR condensation cure in 0.5 second.
CN201310694538.2A 2013-12-17 2013-12-17 Bonding process for blade pocket holes of shutter Pending CN103737916A (en)