CN103707465A - Plastic injection mould for mobile phone shell - Google Patents
Plastic injection mould for mobile phone shell Download PDFInfo
- Publication number
- CN103707465A CN103707465A CN201410004871.0A CN201410004871A CN103707465A CN 103707465 A CN103707465 A CN 103707465A CN 201410004871 A CN201410004871 A CN 201410004871A CN 103707465 A CN103707465 A CN 103707465A
- Authority
- CN
- China
- Prior art keywords
- plate
- mobile phone
- phone shell
- fixed head
- slide block
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a plastic injection mould for a mobile phone shell. The plastic injection mould comprises a movable mould side machine fixing plate, a fixed mould side machine fixing plate, a male mould plate and a female mould plate, wherein the male mould plate and the female mould plate are encircled to form a cavity; the male mould plate is fixedly provided with a first inverted hook matched with an inverted buckle at one end of the mobile phone shell, the lower end of the first inverted hook is connected with an ejector rod, a fixed plate is fixedly provided with a second inverted hook matched with another inverted buckle at the other end of the mobile phone shell; the fixed plate is fixedly provided with a first inclined stretching tip and a second inclined stretching tip; the female mould plate is provided with a first sliding block and a second sliding block; and a first avoidance hole matched with the first inclined stretching tip is formed in the first sliding block, and a second avoidance hole matched with the second inclined stretching tip is formed in the second sliding block. According to the plastic injection mould for the mobile phone shell disclosed by the invention, mutually matched avoidance mechanisms are arranged on the male mould plate and the female mould plate, so that the plastic injection processing of the inverted buckle parts of the mobile phone shell becomes feasible and simple; and moreover, the plastic injection mould is simple in mould opening working procedure and high in processing efficiency.
Description
Technical field
The present invention relates to a kind of injection mold, particularly relate to a kind of mobile phone shell injection mold.
Background technology
The height of Tool and Die Technology level is the important symbol of weighing manufacturing industry level height.In Japan, mould is called as " motive power that enters affluent society "; In Germany, mould is called as " emperor in metal-processing industry ".At Chinese mould, be called as " mothers of all trades " always.The output value of the formed final goods of mould is the hundreds of times of mould self output value.With mould, producing high accuracy, high complexity, high uniformity, high production rate and the low consumption that product shows, is that other machining manufactures can not be compared.Thereby, mould be otherwise known as " benefit amplifier ".Someone also likens mould to " money press ".
Yet existing mobile phone shell injection mold only can the simple product of processing structure.For some baroque products, especially there is the mobile phone shell of back-off, use traditional injection mold can not complete its processing.This just need to use special injection mould processing, and special injection mold often has the shortcoming that die sinking operation is loaded down with trivial details, and working (machining) efficiency is poor.
Summary of the invention
The object of the invention is for above-mentioned the deficiencies in the prior art, a kind of mobile phone shell injection mold that can process having the mobile phone shell of back-off is provided.
For achieving the above object, the technical solution used in the present invention is as follows.
A kind of mobile phone shell injection mold, comprise dynamic model side board fixed head, cover half side board fixed head, described dynamic model side board fixed head is aligned in sequence with bottom plate, lower liftout plate, upper ejector plate, mould pin, fixed head, male model plate from top to bottom, described cover half side board fixed head is aligned in sequence with bakelite plate, upper mounted plate, heat flux plates, scraping wings, caster from top to bottom, and described caster and described male model plate surround die cavity; The middle part of dynamic model side board fixed head and bottom plate is provided with top roller, on bottom plate, male model plate and upper mounted plate, is provided with thimble, is provided with guide pillar on fixed head, and described guide pillar is through male model plate; On described caster, be provided with the guide pin bushing matching with described guide pillar, on described caster, be also provided with the geat being connected with die cavity and water cover; On described male model plate, be installed with the first barb matching with the back-off of mobile phone shell one end, the lower end of described the first barb is connected with push rod, on described fixed head, be installed with the second barb matching with the back-off of the mobile phone shell other end, described the second barb is through male model plate; On described fixed head, be installed with first and tiltedly stretch the tip and second and tiltedly stretch the tip, first tiltedly stretches the tip and second tiltedly stretches the tip all through male model plate; On described caster, be provided with the first slide block and the second slide block, on described the first slide block, be provided with first projection of stretching to die cavity, on described the second slide block, be provided with second projection of stretching to die cavity; On described the first slide block, be provided with tiltedly stretch with first that the tip matches first dodge hole, on described the second slide block, be provided with tiltedly stretch with second that the tip matches second dodge hole.
Further, be also installed with the voussoir near described the second barb on described fixed head, described voussoir is through the through die cavity of male model plate.
Further, described the first slide block and the second slide block are arranged on described caster by the first spring and the second spring respectively.
Further, the profile of the free end of described the first projection and mobile phone shell one end matches, and the profile of the free end of described the second projection and the mobile phone shell other end matches.
The invention has the beneficial effects as follows: mobile phone shell injection mold of the present invention, by the avoiding mechanism cooperatively interacting is set on male model plate and caster, make the injection molding at mobile phone shell back-off position become feasible simple, and die sinking operation of the present invention is simple, working (machining) efficiency is high.
Accompanying drawing explanation
Fig. 1 is the overall structure schematic diagram of mobile phone shell injection mold of the present invention in die opening state.
Fig. 2 is that mobile phone shell injection mold of the present invention closes the partial structurtes schematic diagram of the state of closing in male and female template.
Fig. 3 is that mobile phone shell injection mold of the present invention closes the partial structurtes schematic diagram of the state of closing in male model plate and fixed head.
Fig. 4 is the partial structurtes schematic diagram of mobile phone shell injection mold of the present invention in male model plate and fixed head released state.
Fig. 5 is the partial structurtes schematic diagram of mobile phone shell injection mold of the present invention in male model plate and caster released state.
In figure, 10-male model plate, 14-guide pillar, 15-thimble, 20-caster, 24-guide pin bushing, 25-geat waters cover, 31-dynamic model side board fixed head, 32-bottom plate, liftout plate under 33-, 34-upper ejector plate, 35-mould pin, 36-fixed head, 41-cover half side board fixed head, 42-bakelite plate, 43-upper mounted plate, 44-hot-fluid version, 45-scraping wings, 50-top roller, 60-mobile phone shell, 111-first tiltedly stretches the tip, 112-voussoir, 113-the first barb, 114-the second barb, 115-second tiltedly stretches the tip, 211-the first slide block, 212-first dodges hole, 213-the first spring, 214-the first projection, 215-the second slide block, 216-second dodges hole, 217-the second spring, 218-the second projection.
The specific embodiment
In order to make object of the present invention, technical scheme and advantage clearer, below in conjunction with drawings and Examples, the present invention is described in further detail.Should be appreciated that specific embodiment described herein, only in order to explain the present invention, is not intended to limit the present invention.
Mobile phone shell injection mold of the present invention as Figure 1-Figure 5, comprise and draw together dynamic model side board fixed head 31, cover half side board fixed head 41, dynamic model side board fixed head 31 is aligned in sequence with bottom plate 32, lower liftout plate 33, upper ejector plate 34, mould pin 35, fixed head 36, male model plate 10 from top to bottom, cover half side board fixed head 41 is aligned in sequence with bakelite plate 42, upper mounted plate 43, heat flux plates 44, scraping wings 45, caster 20 from top to bottom, and caster 20 surrounds die cavity with male model plate 10; The middle part of dynamic model side board fixed head 31 and bottom plate 32 is provided with top roller 50, top roller 50 is for ejecting lower liftout plate 33, on bottom plate 32, male model plate 10 and upper mounted plate 34, be provided with thimble 15, be provided with guide pillar 14 on fixed head 36, guide pillar 14 is through male model plate 10; On caster 20, be provided with the guide pin bushing 24 matching with guide pillar 14, on caster 20, be also provided with the geat being connected with die cavity and water cover 25; On male model plate 10, be installed with the first barb 113 matching with the back-off of mobile phone shell 60 one end, the lower end of the first barb 113 is connected with push rod, on fixed head 36, be installed with the second barb 114, the second barbs 114 of matching with the back-off of mobile phone shell 60 other ends through male model plate 10; On fixed head 36, be also installed with the voussoir 112 near the second barb 114, voussoir 112 is through the through die cavity of male model plate 10; On fixed head 36, being installed with first tiltedly stretches the tip 111 and second and tiltedly stretches the tip 112, the first and tiltedly stretch the tip 111 and second and tiltedly stretch the tip 112 all through male model plate 10; On caster 20, be provided with the first slide block 211 and the second slide block 215, the first slide block 211 and the second slide block 215 are arranged on caster 20 by the first spring 213 and the second spring 217 respectively, on the first slide block 211, be provided with on the first projection 214, the second slide blocks 215 that stretch to die cavity and be provided with second projection 218 of stretching to die cavity; The profile of the free end of the first projection 214 and mobile phone shell 60 one end matches, and the profile of the free end of the second projection 218 and mobile phone shell 60 other ends matches.On the first slide block 211, be provided with tiltedly stretch with first that the tip 111 matches first dodge on 212, the second slide blocks of hole 215 be provided with tiltedly stretch with second that the tip 115 matches second dodge hole 216.
Details are as follows for the course of work of mobile phone shell injection mold of the present invention.
Fig. 1 is the state after mobile phone shell injection mold of the present invention die sinking, and now, mobile phone shell is ejected, and male model plate 10 is away from caster 20, and male model plate 10 and fixed head 36, scraping wings 45 and heat flux plates 44, caster 20 and scraping wings 45 are in separated position.Correspondingly, first tiltedly stretches the tip 111 and second and tiltedly stretches the tip 115 and all from first, dodge hole 212 and second respectively and dodge hole 216 and depart from.
Put into after hot pressing product, through scraping wings and heat flux plates, close close, caster and scraping wings close and close after operation, under the acting in conjunction of thimble and top roller, male model plate and caster start to close and close, the state after male model plate and caster close and close as shown in Figure 2.Referring to Fig. 2, first tiltedly stretches the tip 111 and second tiltedly stretches the tip 115 and is inserted into respectively first and dodges hole 212 and second and dodge in hole 216.Owing to dodging hole, be oblique, drive thus the first slide block 211 and the second slide block 215 to slide to die cavity direction.Meanwhile, the first spring 213 and the second spring 217 are in compressive state.The first barb 113 stretches into die cavity and inserts the back-off of mobile phone shell one end, and the second barb 114 stretches into die cavity, and the inwall of mobile phone shell is arrived in its upper end.
After male model plate and caster close and close, under the effect of top roller, fixed head moves upward and closes and close with male model plate.Fig. 3 is that mobile phone shell injection mold of the present invention closes the partial structurtes schematic diagram of the state of closing in male model plate and fixed head, as shown in Figure 3, now, first tiltedly stretches the tip 111 and second tiltedly stretches the tip 115 and continues respectively to dodge hole 212 and second to first and dodge hole 216 and stretch into, stretching in process continues to drive the first slide block 211 and the second slide block 215 to slide to die cavity, until first projection the 214 and second projection 218 respectively with the end fit of mobile phone shell, and the first spring 213 and the second spring 217 are also further compressed.Under top roller effect, voussoir 112 moves upward and arrives at the inwall of mobile phone shell and the second barb 114 is outwards pushed with the back-off of the mobile phone shell other end and coincide.
Male model plate and fixed head close and close rear beginning injection moulding, pressurize and refrigerating work procedure, injection moulding, pressurize and cooling after, scraping wings successively separates with heat flux plates and caster, under the effect of thimble, male model plate separates with fixed head subsequently.Fig. 4 is the partial structurtes schematic diagram of mobile phone shell injection mold of the present invention in male model plate and fixed head released state, as shown in Figure 4, first tiltedly stretches the tip 111 and second tiltedly stretches the tip 115 and from first, dodges hole 212 and second respectively and dodge hole 216 and exit, the first spring 213 and the second spring 217 are because the pressure being subject to reduces and partial reset, thereby drive the first slide block 211 and the second slide block 215 away from die cavity, the first projection 214 is separated with mobile phone shell two ends with the second projection 218.Voussoir 112 moves downward, the extruding of the second barb 114 eliminated, and separated due to the second projection 218 and mobile phone shell end simultaneously, the second barb 114 is removed and the coincideing of mobile phone shell back-off.
Fig. 5 is the partial structurtes schematic diagram of mobile phone shell injection mold of the present invention in male model plate and caster released state, under the effect of thimble, first tiltedly stretches the tip 111 and second tiltedly stretches the tip 115 and from first, dodges hole 212 and second completely respectively and dodge hole 216 and exit, the pressure that the first spring 213 and the second spring 217 are subject to disappears and resets completely, thereby drives the first slide block 211 and the second slide block 215 to reset.
After male model plate is separated with caster, the top roller jack-up that makes progress, thus push rod ejects the first barb finished product is ejected, and after finished product ejects, takes away.
Mobile phone shell injection mold of the present invention, by the avoiding mechanism cooperatively interacting is set on male model plate and caster, make the injection molding at mobile phone shell back-off position become feasible simple, and die sinking operation of the present invention is simple, directly, by the just energy die sinking that ejects of thimble, working (machining) efficiency is high.
The foregoing is only preferred embodiment of the present invention, be not used for limiting practical range of the present invention; If do not depart from the spirit and scope of the present invention, the present invention is modified or is equal to replacement, all should be encompassed in the middle of the protection domain of the claims in the present invention.
Claims (4)
1. a mobile phone shell injection mold, comprise dynamic model side board fixed head, cover half side board fixed head, described dynamic model side board fixed head is aligned in sequence with bottom plate, lower liftout plate, upper ejector plate, mould pin, fixed head, male model plate from top to bottom, described cover half side board fixed head is aligned in sequence with bakelite plate, upper mounted plate, heat flux plates, scraping wings, caster from top to bottom, and described caster and described male model plate surround die cavity; Wherein,
The middle part of dynamic model side board fixed head and bottom plate is provided with top roller, on bottom plate, male model plate and upper mounted plate, is provided with thimble, is provided with guide pillar on fixed head, and described guide pillar is through male model plate;
On described caster, be provided with the guide pin bushing matching with described guide pillar, on described caster, be also provided with the geat being connected with die cavity and water cover;
It is characterized in that,
On described male model plate, be installed with the first barb matching with the back-off of mobile phone shell one end, the lower end of described the first barb is connected with push rod, on described fixed head, be installed with the second barb matching with the back-off of the mobile phone shell other end, described the second barb is through male model plate;
On described fixed head, be installed with first and tiltedly stretch the tip and second and tiltedly stretch the tip, first tiltedly stretches the tip and second tiltedly stretches the tip all through male model plate;
On described caster, be provided with the first slide block and the second slide block, on described the first slide block, be provided with first projection of stretching to die cavity, on described the second slide block, be provided with second projection of stretching to die cavity;
On described the first slide block, be provided with tiltedly stretch with first that the tip matches first dodge hole, on described the second slide block, be provided with tiltedly stretch with second that the tip matches second dodge hole.
2. mobile phone shell injection mold according to claim 1, is characterized in that, is also installed with the voussoir near described the second barb on described fixed head, and described voussoir is through the through die cavity of male model plate.
3. mobile phone shell injection mold according to claim 1 and 2, is characterized in that, described the first slide block and the second slide block are arranged on described caster by the first spring and the second spring respectively.
4. mobile phone shell injection mold according to claim 3, is characterized in that, the profile of the free end of described the first projection and mobile phone shell one end matches, and the profile of the free end of described the second projection and the mobile phone shell other end matches.