CN103660001A - Method for producing wooden barrel - Google Patents

Method for producing wooden barrel Download PDF

Info

Publication number
CN103660001A
CN103660001A CN201310727748.7A CN201310727748A CN103660001A CN 103660001 A CN103660001 A CN 103660001A CN 201310727748 A CN201310727748 A CN 201310727748A CN 103660001 A CN103660001 A CN 103660001A
Authority
CN
China
Prior art keywords
wooden barrel
production method
blank
wooden
adhesive
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310727748.7A
Other languages
Chinese (zh)
Inventor
贺彬
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUHU KANGER WOOD PRODUCTS Co Ltd
Original Assignee
WUHU KANGER WOOD PRODUCTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUHU KANGER WOOD PRODUCTS Co Ltd filed Critical WUHU KANGER WOOD PRODUCTS Co Ltd
Priority to CN201310727748.7A priority Critical patent/CN103660001A/en
Publication of CN103660001A publication Critical patent/CN103660001A/en
Pending legal-status Critical Current

Abstract

The invention discloses a method for producing a wooden barrel. The method comprises the following steps that one side of each wall plate of the wooden barrel and one side of a bottom plate of the wooden barrel are slotted, and the other side of each wall plate of the wooden barrel and the other side of the bottom plate of the wooden barrel are provided with protrusions matched with slots; the slot and the protrusion, which correspond to each other, of each wall plate are coated with adhesive and clamped, and a plurality of side wall plates are arranged in sequence to form a wooden barrel blank; the wooden barrel blank is tightened and fixed through at least one first ribbon; the bottom of the inner side face of the wooden barrel blank is provided with a bottom annular groove in a chisel mode; the slot and the protrusion, which correspond to each other, of the bottom plate are coated with adhesive and clamped, and the wall plates are arranged in sequence to form a barrel bottom; at least one first ribbon and part of side wall plates of the wooden barrel blank are dismounted, then the barrel bottom is installed in the annular groove and fixed through the adhesive, and the dismounted wall plates are arranged in the wooden barrel blank again; the wooden barrel blank is tightened and fixed again through at least one second ribbon, and grinding and the waterproof processing are carried out on the wooden barrel. The provided wooden barrel can still contain water and cannot leak water even when being placed in the dried environment for a long time.

Description

The production method of wooden barrel
Technical field
The present invention relates to the production field of wooden barrel, particularly, relate to a kind of production method of wooden barrel.
Background technology
In prior art, in the production method of wooden barrel, first use the bonding bucket of the adhesive end, then with adhesive by the wallboard of bucket be arranged in order be bonded in barrel at the bottom of on form bucket, then in the outside of bucket, pricks hoop processing, with this, guarantee to combine closely between the plank of wooden barrel.If but wooden barrel in dry environment after long-time placement, again discharging water to use tends to leak, this is the technical problem that the industry is needed solution badly.
Summary of the invention
Object of the present invention to discharge water once again and uses the defect of leaking in order to overcome after wooden barrel is placed in dry environment, provides a kind of assurance wooden barrel in various environment, to use all watertight production methods.
To achieve these goals, the invention provides a kind of production method of wooden barrel, wherein, the method comprises the steps: that opposite side is made the projection coordinating with described fluting by the both sides of the wallboard of wooden barrel and base plate one side fluting; By the corresponding fluting of wallboard and protruding coated with adhesive and engage, be arranged in order a plurality of sidewall panelings to surround wooden barrel blank; With at least one the first band, tighten fixing described wooden barrel blank; In the bottom of described wooden barrel blank medial surface, cutter is established bottom annular recess; By the corresponding fluting of base plate and protruding coated with adhesive and engage, be arranged in order a plurality of wallboards and form a bucket end; Dismantle the partial sidewall plate of described at least one the first band and described wooden barrel blank, so that the described bucket end is arranged in described cannelure and with adhesive and is fixed, then the wallboard of dismounting is reinstalled to described wooden barrel blank; With at least one the second band, again tighten fixing described wooden barrel blank again; And wooden barrel is polished and water-proofing treatment.
Preferably, described adhesive is white glue with vinyl.
Preferably, described the first band and/or described the second band are stainless stirrup.
Preferably, described method also comprises, is polished in the bottom of wooden barrel blank.
Preferably, described method also comprises the pretreatment to described sidewall paneling and described base plate, and concrete steps are as follows: described plank is carried out to superheated steam processing; And at 75-100 ℃ of dry 3-4h.
Preferably, the condition that described superheated steam is processed is: 130-160 ℃, relative humidity are that 50-80% and processing time are 30-60min.
Preferably, the condition that described superheated steam is processed is: 140-150 ℃, relative humidity are that 60-70% and processing time are 35-45min.
Preferably, described water-proofing treatment is for spraying paint or directly brushing tung oil.
The process of spraying paint preferably, is sprayed finish paint one time after spraying twice priming paint again.
Preferably, after spraying paint, at room temperature dry in the shade, and then the processing of spraying paint together under carrying out.
Compared with the production method of doing again barrel wall at the bottom of first doing in prior art barrel, it is fastening that wallboard in the bucket wall of this method uses band to carry out, also can there is crack because of the internal stress at the bottom of bucket and between wallboard, the production method of wooden barrel provided by the invention is first done barrel wall and is arranged on barrel wall at the bottom of by bucket, between the wallboard of bucket like this, bonding can be good at avoided the internal stress between plate and plate, thereby makes wooden barrel can reach the effect of anti-division, preventing water leakage completely.
Other features and advantages of the present invention partly in detail are described the specific embodiment subsequently.
Accompanying drawing explanation
Accompanying drawing is to be used to provide a further understanding of the present invention, and forms a part for description, is used from explanation the present invention, but is not construed as limiting the invention with the specific embodiment one below.In the accompanying drawings:
Fig. 1 be wooden barrel provided by the invention a kind of embodiment of production method flow chart; And
Fig. 2 be the another kind of embodiment of the production method of wooden barrel provided by the invention flow chart.
The specific embodiment
Below in conjunction with accompanying drawing, the specific embodiment of the present invention is elaborated.Should be understood that, the specific embodiment described herein only, for description and interpretation the present invention, is not limited to the present invention.
Fig. 1 be wooden barrel provided by the invention a kind of embodiment of production method flow chart, as seen from the figure, the method comprises the steps: S02, by the both sides of the wallboard of wooden barrel and base plate one side fluting, opposite side is made the projection coordinating with described fluting; S03, by the corresponding fluting of wallboard and protruding coated with adhesive and engage, is arranged in order a plurality of sidewall panelings to surround wooden barrel blank; S04, tightens fixing described wooden barrel blank with at least one the first band; S06, in the bottom of described wooden barrel blank medial surface, cutter is established bottom annular recess; S07, by the corresponding fluting of base plate and protruding coated with adhesive and engage, is arranged in order a plurality of wallboards and forms a bucket end; S08, dismantles the partial sidewall plate of described at least one the first band and described wooden barrel blank, so that the described bucket end is arranged in described cannelure and with adhesive and is fixed, then the wallboard of dismounting is reinstalled to described wooden barrel blank; S09, more again tighten fixing described wooden barrel blank with at least one the second band; And S11, wooden barrel is polished and water-proofing treatment.
Compared with the production method of doing again barrel wall at the bottom of first doing in prior art barrel, it is fastening that wallboard in the bucket wall of this method uses band to carry out, also can there is crack because of the internal stress at the bottom of bucket and between wallboard, the production method of wooden barrel provided by the invention is first done barrel wall and is arranged on barrel wall at the bottom of by bucket, adjacent wallboard of while, between adjacent wallboard and wallboard and base plate, be all adopt groove and projection to cooperatively interact and groove and projection between have the mode of adhesive to combine, bondingly between the wallboard of bucket like this can be good at avoiding the internal stress between plate and plate, thereby make wooden barrel can reach anti-division completely, the effect of preventing water leakage.
Preferably, described adhesive is white glue with vinyl, this is because white glue with vinyl be take water and obtained as decentralized medium carries out emulsion polymerisation as adhesive to adopt white glue with vinyl, a kind of aqueous, environmental protective glue, there is good film-forming property simultaneously, adhesion strength is high, curing rate is fast, the diluted alkaline of resistance to diluted acid is good, easy to use, low price and containing the series of advantages such as organic solvent.
Preferably, described the first band and/or described the second band can be stainless stirrup, and stainless stirrup is toughness easy fracture very much not only, wooden barrel is often in the larger environment of humidity simultaneously, and band easily gets rusty, therefore adopt stainless stirrup, can not make because of getting rusty band corrosion, cause economic loss.
Preferably, described method also can comprise, S05, polish in bottom to wooden barrel blank, polishing is being driven cannelure later like this, height at the bottom of the distance bucket of cannelure will be in full accord like this, can difficulty be installed because of cause cannelure not make at grade barrel because wooden barrel blank bottom level is inconsistent at the bottom of.
In one embodiment, described method also can comprise the pretreatment to described sidewall paneling and described base plate, and concrete steps are as follows:
(1) described plank is carried out to superheated steam processing; And
(2) at 75-100 ℃ of dry 3-4h.
After adopting first superheated steam like this, dry processing can reduce timber implosion, and the timber top layer extension residual deformation of generation implosion can be carried out hot and humid processing to timber and be eliminated before dry run finishes.In processing procedure, timber top layer produces compressed residual distortion because adding hygral expansion, offsets with original extension residual deformation, after processing, unnecessary moisture is evaporated, with internal layer timber, shrink, thereby can not produce residual deformation in timber, therefore timber implosion is also eliminated.Preferably, the condition that described superheated steam is processed is: 130-160 ℃, relative humidity are that 50-80% and processing time are 30-60min.Further preferably, the condition that described superheated steam is processed is: 140-150 ℃, relative humidity are that 60-70% and processing time are 35-45min.
Water-proofing treatment in method described above can be sprays paint or directly brushes tung oil.The process of spraying paint preferably, is sprayed finish paint one time after spraying twice priming paint again.Further preferably, after spraying paint, at room temperature dry in the shade, and then the processing of spraying paint together under carrying out.Such water-proofing treatment not only can prevent stave humidity compared with overall situation in and rot, simultaneously lacquer painting can cover plate and plate gap, further prevents that seeping water from appearring in wooden barrel, and mopping can also bring effect attractive in appearance.
By the following examples content of the present invention is further elaborated:
Embodiment 1
As described in Figure 2, S01, is first to process 40min 55% time by the wallboard of wooden barrel and base plate at 130 ℃, relative humidity to the concrete steps of this embodiment, the dry 3h at 80 ℃ by wallboard and base plate; S02, then, by the both sides of the wallboard of wooden barrel and base plate one side fluting, opposite side is made the projection coordinating with described fluting; S03, coats the corresponding fluting of wallboard and projection white glue with vinyl and engages, and is arranged in order a plurality of sidewall panelings to surround wooden barrel blank; S04, tightens fixing described wooden barrel blank with at least one the first stainless stirrup; S05, polishes to the bottom of wooden barrel blank; S06, in the bottom of described wooden barrel blank medial surface, cutter is established bottom annular recess; S07, coats the corresponding fluting of base plate and projection white glue with vinyl and engages, and is arranged in order a plurality of base plates and forms the bucket end; S08, dismantles the partial sidewall plate of described at least one the first stainless stirrup and described wooden barrel blank, so that the described bucket end is arranged in described cannelure and with white glue with vinyl and is fixed, then the wallboard of dismounting is reinstalled to described wooden barrel blank; S09, more again tighten fixing described wooden barrel blank with at least one the second stainless stirrup; And S10, to wooden barrel spray spray again a finish paint after twice priming paint and spray paint after at room temperature dry in the shade, and then the processing of spraying paint together under carrying out, so just obtains wooden barrel A1.
Then A1 is placed at 100 ℃ and is dried 5 hours, then wooden barrel is filled to water, show that wooden barrel is water-tight.
Embodiment 2
Embodiment 2 is that superheated steam is processed and the dry condition of processing is with embodiment 1 difference: 145 ℃, relative humidity be 60% and the processing time be 50min, dry 4h at 90 ℃ then, the wooden barrel that the present embodiment obtains is A2.Then A2 is placed at 110 ℃ and is dried 5 hours, then wooden barrel is filled to water, show that wooden barrel is water-tight.
Embodiment 3
Embodiment 3 is that superheated steam is processed and the dry condition of processing is with embodiment 1 difference: 160 ℃, relative humidity be 80% and the processing time be 60min, dry 4h at 100 ℃ then, the wooden barrel that the present embodiment obtains is A3.Then A3 is placed at 120 ℃ and is dried 5 hours, then wooden barrel is filled to water, show that wooden barrel is water-tight.
Below describe by reference to the accompanying drawings the preferred embodiment of the present invention in detail; but; the present invention is not limited to the detail in above-mentioned embodiment; within the scope of technical conceive of the present invention; can carry out multiple simple variant to technical scheme of the present invention, these simple variant all belong to protection scope of the present invention.
It should be noted that in addition, each concrete technical characterictic described in the above-mentioned specific embodiment, in reconcilable situation, can combine by any suitable mode, for fear of unnecessary repetition, the present invention is to the explanation no longer separately of various possible combinations.
In addition, between various embodiment of the present invention, also can be combined, as long as it is without prejudice to thought of the present invention, it should be considered as content disclosed in this invention equally.

Claims (10)

1. a production method for wooden barrel, is characterized in that, the method comprises the steps:
By the both sides of the wallboard of wooden barrel and base plate one side fluting, opposite side is made the projection coordinating with described fluting;
By the corresponding fluting of wallboard and protruding coated with adhesive and engage, be arranged in order a plurality of sidewall panelings to surround wooden barrel blank;
With at least one the first band, tighten fixing described wooden barrel blank;
In the bottom of described wooden barrel blank medial surface, cutter is established bottom annular recess;
By the corresponding fluting of base plate and protruding coated with adhesive and engage, be arranged in order a plurality of wallboards and form a bucket end;
Dismantle the partial sidewall plate of described at least one the first band and described wooden barrel blank, so that the described bucket end is arranged in described cannelure and with adhesive and is fixed, then the wallboard of dismounting is reinstalled to described wooden barrel blank;
With at least one the second band, again tighten fixing described wooden barrel blank again; And
Wooden barrel is polished and water-proofing treatment.
2. the production method of wooden barrel according to claim 1, wherein, described adhesive is white glue with vinyl.
3. the production method of wooden barrel according to claim 1, wherein, described the first band and/or described the second band are stainless stirrup.
4. the production method of wooden barrel according to claim 1, wherein, described method also comprises, is polished in the bottom of described wooden barrel blank.
5. the production method of wooden barrel according to claim 1, wherein, described method also comprises the pretreatment to described sidewall paneling and described base plate, concrete steps are as follows:
Described plank is carried out to superheated steam processing; And
At 75-100 ℃ of dry 3-4h.
6. the production method of wooden barrel according to claim 5, wherein, the condition that described superheated steam is processed is: 130-160 ℃, relative humidity are that 50-80% and processing time are 30-60min.
7. the production method of wooden barrel according to claim 6, wherein, the condition that described superheated steam is processed is: 140-150 ℃, relative humidity are that 60-70% and processing time are 35-45min.
8. the production method of wooden barrel according to claim 1, wherein, described water-proofing treatment is for spraying paint or directly brushing tung oil.
9. the production method of wooden barrel according to claim 8, wherein, described in the process of spraying paint spray again finish paint one time after for twice priming paint of spray.
10. the production method of wooden barrel according to claim 8, wherein, at room temperature dries in the shade after spraying paint, and then the processing of spraying paint together under carrying out.
CN201310727748.7A 2013-12-24 2013-12-24 Method for producing wooden barrel Pending CN103660001A (en)